EN 10028-5 Carbon Steel Plates
SHH STEEL offers EN 10028-5-compliant P355M/P460M thermomechanical fine grain steel plates. EN 10028-5 specifies flat products for welding in pressure equipment with high yield strength. Efficient, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
EN 10028-5 P460ML2 Steel Plate | P460ML2 TMCP -50°C Vessel Plate
EN 10028-5 P460ML2 is European TMCP fine-grain low-temperature vessel plate, steel number 1.8838. Yield is 460 MPa at ≤16 mm. Impact is −50 °C. SHH STEEL supplies P460ML2 worldwide as a global steel mill sourcing partner.View More -
EN 10028-5 P460ML1 Steel Plate | P460ML1 TMCP -40°C Vessel Plate
EN 10028-5 P460ML1 is European TMCP fine-grain low-temperature vessel plate, steel number 1.8837. Yield is 460 MPa at ≤16 mm. Impact is −40 °C. SHH STEEL supplies P460ML1 worldwide as a global steel mill sourcing partner.View More -
EN 10028-5 P460M Steel Plate | P460M TMCP Vessel Plate supplier
EN 10028-5 P460M is European TMCP fine-grain vessel plate, steel number 1.8826. Yield is 460 MPa at ≤16 mm. Tensile is 570–720 MPa. SHH STEEL supplies P460M worldwide as a global steel mill sourcing partner.View More -
EN 10028-5 P420ML2 Steel Plate | P420ML2 TMCP -50°C Vessel Plate
EN 10028-5 P420ML2 is European TMCP fine-grain low-temperature vessel plate, steel number 1.8836. Yield is 420 MPa at ≤16 mm. Impact is −50 °C. SHH STEEL supplies P420ML2 worldwide as a global steel mill sourcing partner.View More -
EN 10028-5 P420ML1 Steel Plate | P420ML1 TMCP -40°C Vessel Plate
EN 10028-5 P420ML1 is European TMCP fine-grain low-temperature vessel plate, steel number 1.8835. Yield is 420 MPa at ≤16 mm. Impact is −40 °C. SHH STEEL supplies P420ML1 worldwide as a global steel mill sourcing partner.View More -
EN 10028-5 P420M Steel Plate | P420M TMCP Vessel Plate supplier
EN 10028-5 P420M is European TMCP fine-grain vessel plate, steel number 1.8827. Yield is 420 MPa at ≤16 mm. Tensile is 520–680 MPa. SHH STEEL supplies P420M worldwide as a global steel mill sourcing partner.View More -
EN 10028-5 P355ML2 Steel Plate | P355ML2 TMCP -50°C Vessel Plate
EN 10028-5 P355ML2 is European TMCP fine-grain low-temperature vessel plate, steel number 1.8833. Yield is 355 MPa at ≤16 mm. Impact is −50 °C. SHH STEEL supplies P355ML2 worldwide as a global steel mill sourcing partner.View More -
EN 10028-5 P355ML1 Steel Plate | P355ML1 TMCP -40°C Vessel Plate
EN 10028-5 P355ML1 is European TMCP fine-grain low-temperature vessel plate, steel number 1.8832. Yield is 355 MPa at ≤16 mm. Impact is −40 °C. SHH STEEL supplies P355ML1 worldwide as a global steel mill sourcing partner.View More -
EN 10028-5 P355M Steel Plate | P355M TMCP Vessel Plate supplier
EN 10028-5 P355M is European TMCP fine-grain vessel plate, steel number 1.8821. Yield is 355 MPa at ≤16 mm. Tensile is 450–610 MPa. SHH STEEL supplies P355M worldwide as a global steel mill sourcing partner.View More
EN 10028-5 Carbon Steel Plates
Boiler & Pressure Vessel Steel Plates
SHH STEEL, a trusted Pressure Vessel Steel Plates exporter, produces and exports pressure vessel steel plates for boilers, tanks, and petrochemical applications. Our plates, like ASTM A516 Grade 70, offer high tensile strength and toughness, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for boiler steel plates and custom high-pressure solutions.
Boiler & Pressure Vessel Steel Plates
ASME SA-36/SA-36M
JIS G4109
JIS G3119
JIS G3120
ASME SA302
JIS G3126
ASTM A302
JIS G3127
ASME SA225
BS 1501
ASTM A225
DIN 17155
ASME SA455
EN 10120
ASME SA562
GB 6654
ASTM A455
GB/T 6653
ASTM A562
JIS G 3116
ASME SA841
ASME SA553
GB/T 713.3-2023
ASTM A553
GB/T 713.4-2023
GB/T 713.5-2023
ASME SA516
GOST 5520
ASTM A516/516M
GB/T 3077
GB/T 3274
DIN 17102
GB/T 24511
GB/T 24512
GB/T 3077
ASTM A285
ASME SA285
ASTM A515
ASME SA515
ASTM A299
ASTM A517/A517M
ASME SA299
ASTM A204
ASME SA517/SA517M
ASME SA204
ASTM A203
ASME SA203
ASTM A353
ASME SA353
ASTM A387
ASME SA387
ASTM A537
ASME SA537
JIS G3115
GB/T 713.2-2023
GB/T 19189
GB/T 3531
EN 10028-2
EN 10028-3
EN 10028-4
EN 10028-5
EN 10028-6
JIS G3103
ISO 9328-2
X