Product Showcase
ASME SA299 Carbon Steel Plates
SHH STEEL offers ASME SA299-compliant Grade A/B carbon-manganese-silicon steel plates. ASME SA299 specifies plates for moderate-temperature pressure vessels with improved toughness. Weldable, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASME SA299 Grade B Steel Plate | SA299 Gr.B Mn-Si Vessel Plate
ASME SA299 Grade B is the higher-strength manganese-silicon carbon vessel plate under ASME SA-299/SA-299M. Tensile 550–690 MPa, yield 325 MPa to 25 mm. Direct Mill Supply by SHH STEEL for SA299 Gr.B / A299 Gr.B with 3.1 or 3.2 certificates.View More -
ASME SA299 Grade A Steel Plate | SA299 Gr.A Mn-Si Vessel Plate
ASME SA299 Grade A is a manganese-silicon carbon vessel plate under ASME SA-299/SA-299M. Tensile 515–655 MPa, yield 290 MPa to 25 mm. SHH STEEL supplies SA299 Gr.A / A299 Gr.A mill-direct with 3.1 or 3.2 certificates.View More
ASME SA299 Carbon Steel Plates
Boiler & Pressure Vessel Steel Plates
SHH STEEL, a trusted Pressure Vessel Steel Plates exporter, produces and exports pressure vessel steel plates for boilers, tanks, and petrochemical applications. Our plates, like ASTM A516 Grade 70, offer high tensile strength and toughness, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for boiler steel plates and custom high-pressure solutions.
Boiler & Pressure Vessel Steel Plates
ASME SA-36/SA-36M
JIS G4109
JIS G3119
JIS G3120
ASME SA302
JIS G3126
ASTM A302
JIS G3127
ASME SA225
BS 1501
ASTM A225
DIN 17155
ASME SA455
EN 10120
ASME SA562
GB 6654
ASTM A455
GB/T 6653
ASTM A562
JIS G 3116
ASME SA841
ASME SA553
GB/T 713.3-2023
ASTM A553
GB/T 713.4-2023
GB/T 713.5-2023
ASME SA516
GOST 5520
ASTM A516/516M
GB/T 3077
GB/T 3274
DIN 17102
GB/T 24511
GB/T 24512
GB/T 3077
ASTM A285
ASME SA285
ASTM A515
ASME SA515
ASTM A299
ASTM A517/A517M
ASME SA299
ASTM A204
ASME SA517/SA517M
ASME SA204
ASTM A203
ASME SA203
ASTM A353
ASME SA353
ASTM A387
ASME SA387
ASTM A537
ASME SA537
JIS G3115
GB/T 713.2-2023
GB/T 19189
GB/T 3531
EN 10028-2
EN 10028-3
EN 10028-4
EN 10028-5
EN 10028-6
JIS G3103
ISO 9328-2
X