GB/T 713.2-2023

Product Showcase

GB/T 713.2-2023 Carbon Steel Plates

SHH STEEL supplies GB/T 713.2-2023 steel plates and strips for pressure equipment as China steel mill-Direct Supply. This part covers non-alloy and alloy steels with specified temperature properties for boilers, pressure vessels and related equipment at service temperatures not lower than -20 °C. Typical grades include Q245R, Q345R, Q370R, Q420R, Q460R, 15CrMoR, 14Cr1MoR, 12Cr2Mo1R, 12Cr1MoVR, 18MnMoNbR and 13MnNiMoR. It replaces GB/T 713-2014 and GB/T 35012-2018. Strip and coil-cut plate up to 25.4 mm; single-rolled plate 3–250 mm. Competitive mill price, cut-to-size service, fast delivery and full MTCs.

GB/T 713 07Cr2AlMoR Cr-Al-Mo pressure vessel steel plate, sulfur-corrosion resistant, normalized and tempered, SHH STEEL

GB/T 713 07Cr2AlMoR Steel Plate | 07Cr2AlMoR Vessel Plate

GB/T 713 07Cr2AlMoR is Chinese Cr-Al-Mo boiler and pressure-vessel plate. Yield is 260 MPa at 6–36 mm. Tensile is 420–580 MPa. SHH STEEL supplies 07Cr2AlMoR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 12Cr1MoVR 1Cr-0.3Mo-V pressure vessel steel plate, normalized and tempered, SHH STEEL

GB/T 713 12Cr2Mo1VR Steel Plate | 12Cr2Mo1VR Cr-Mo-V Vessel Plate

GB/T 713 12Cr2Mo1VR is Chinese 2.25Cr-1Mo-V boiler and pressure-vessel plate. Yield is 310 MPa in the usual band. Tensile is 520–680 MPa. SHH STEEL supplies 12Cr2Mo1VR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 12Cr1MoVR 1Cr-0.3Mo-V pressure vessel steel plate, normalized and tempered, SHH STEEL

GB/T 713 12Cr1MoVR Steel Plate | 12Cr1MoVR Cr-Mo-V Vessel Plate

GB/T 713 12Cr1MoVR is Chinese 1Cr-0.3Mo-V boiler and pressure-vessel plate. Yield is 245 MPa at 6–60 mm. Tensile is 440–590 MPa. SHH STEEL supplies 12Cr1MoVR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 12Cr2Mo1R 2.25Cr-1Mo pressure vessel steel plate, normalized and tempered, SHH STEEL

GB/T 713 12Cr2Mo1R Steel Plate | 12Cr2Mo1R Cr-Mo Vessel Plate

GB/T 713 12Cr2Mo1R is Chinese 2.25Cr-1Mo boiler and pressure-vessel plate. Yield is 310 MPa in the usual band. Tensile is 520–680 MPa. SHH STEEL supplies 12Cr2Mo1R worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 14Cr1MoR 1.25Cr-0.5Mo pressure vessel steel plate, normalized and tempered, SHH STEEL

GB/T 713 14Cr1MoR Steel Plate | 14Cr1MoR Cr-Mo Vessel Plate

GB/T 713 14Cr1MoR is Chinese 1.25Cr-0.5Mo boiler and pressure-vessel plate. Yield is 310 MPa at 6–100 mm. Tensile is 520–680 MPa. SHH STEEL supplies 14Cr1MoR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 15CrMoR 1Cr-0.5Mo pressure vessel steel plate, normalized and tempered, SHH STEEL

GB/T 713 15CrMoR Steel Plate | 15CrMoR Cr-Mo Vessel Plate

GB/T 713 15CrMoR is Chinese 1.25Cr-0.5Mo boiler and pressure-vessel plate. Yield is 295 MPa at 6–60 mm. Tensile is 450–590 MPa. SHH STEEL supplies 15CrMoR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.SEO Title
View More
GB/T 713 13MnNiMoR Mn-Ni-Mo pressure vessel steel plate, normalized and tempered, ReL 390 MPa, SHH STEEL

GB/T 713 13MnNiMoR Steel Plate | 13MnNiMoR Vessel Plate

GB/T 713 13MnNiMoR is Chinese Mn-Ni-Mo boiler and pressure-vessel plate. Yield is 390 MPa at 30–100 mm. Tensile is 570–720 MPa. SHH STEEL supplies 13MnNiMoR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 18MnMoNbR Mn-Mo-Nb pressure vessel steel plate, normalized and tempered, ReL 400 MPa, SHH STEEL

GB/T 713 18MnMoNbR Steel Plate | 18MnMoNbR Vessel Plate

GB/T 713 18MnMoNbR is Chinese Mn-Mo-Nb boiler and pressure-vessel plate. Yield is 400 MPa at 30–60 mm. Tensile is 570–720 MPa. SHH STEEL supplies 18MnMoNbR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 Q460R high-strength pressure vessel steel plate, ReL 460 MPa class, normalized, SHH STEEL

GB/T 713 Q460R Steel Plate | Q460R Pressure Vessel Plate

GB/T 713 Q460R / Q460 R is Chinese high-strength boiler and pressure-vessel plate. Yield is 460 MPa in the thin band. Tensile is 630–750 MPa. SHH STEEL supplies Q460R worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 Q420R high-strength pressure vessel steel plate, ReL 420 MPa, normalized, Charpy −20 °C, SHH STEEL

GB/T 713 Q420R Steel Plate | Q420R Pressure Vessel Plate

GB/T 713 Q420R / Q420 R is Chinese high-strength boiler and pressure-vessel plate. Yield is 420 MPa at 10–20 mm. Tensile is 590–720 MPa. SHH STEEL supplies Q420R worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 Q370R pressure vessel steel plate, ReL 370 MPa, normalized, Charpy −20 °C, SHH STEEL

GB/T 713 Q370R Steel Plate | Q370R Pressure Vessel Plate

GB/T 713 Q370R / Q370 R is Chinese fine-grain boiler and pressure-vessel plate. Yield is 370 MPa at 6–16 mm. Tensile is 530–630 MPa. SHH STEEL supplies Q370R worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
GB/T 713 Q245R pressure vessel steel plate, ReL 245 MPa, hot rolled or normalized C-Mn plate, SHH STEEL

GB/T 713 Q245R Steel Plate | Q245R Pressure Vessel Plate

GB/T 713 Q245R / Q245 R is Chinese carbon boiler and pressure-vessel plate. Yield is 245 MPa at 3–16 mm. Tensile is 400–520 MPa. SHH STEEL supplies Q245R worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
View More
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X