DIN 17102 StE500 high-strength fine-grain steel plate, 500 MPa yield class, SHH STEEL

DIN 17102 StE500 Steel Plate | StE500 Fine Grain Steel

DIN 17102 StE500 / StE 500 is weldable normalized fine-grain steel plate. Yield is 500 MPa at ≤16 mm. Tensile is typically 610–770 MPa at ≤70 mm. SHH STEEL supplies StE500 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
Keywords
DIN 17102 StE500, StE500, StE 500, STE500, DIN17102 StE500, P500N, S500N, fine grain structural steel, StE500 supplier
Equivalent Grades
DIN 17102 StE500 (1.8907) / EN 10025-3 S500N (near) / EN 10028-3 P500N (near) / ASTM A514 (QT, not equal) / JIS G3106 SM570 (lower) / GB/T 1591 Q500C (structural near) — Material Specification: DIN 17102 (withdrawn) — Delivery: Normalized (N) or Normalized-rolled; TMCP/QT by agreement
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
How StE / WStE / TStE / EStE Differ at 500
Material Comparison
Fine-Grain Structural Service at 500 MPa
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is DIN 17102 StE500 Steel ?

DIN 17102 StE500, also written StE 500, STE500, DIN17102 StE500 and StE500 steel plate, is a weldable normalized fine-grain structural steel under DIN 17102. StE means the basic / room-temperature quality. Yield in the thin band is 500 MPa. Tensile at ≤70 mm is typically 610–770 MPa. This is the highest common strength step in DIN 17102. Conversion tables usually put it next to P500N / S500N when those names exist on the project file. It is not StE460. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade. Plate is produced to DIN 17102 and shipped to buyers in the USA, Europe, Middle East and Southeast Asia.

A purchase order that only says “500 fine grain” is incomplete. Write DIN 17102 StE500. Do not ship StE460 against a StE500 drawing and call 40 MPa extra yield a free upgrade.

DIN 17102 is a legacy specification. New European work often stops at S460N / P460N under EN 10025-3 or moves to TMCP / QT books. Replacement projects still name StE500 when an old German calculation or mill qualification stays on DIN.

This page is not DIN 17100 St52-3. DIN 17100 is ordinary structural steel. DIN 17102 is fine-grain, killed, normally normalized. This page is not SA516 Gr.70. Grade 70 is ASME carbon vessel plate at 260 MPa yield. StE500 is 500 MPa yield fine-grain plate. It is not ASTM A36 steel plate. It is not QT alloy under ASME SA387 or ASME SA543.

Company scope: global steel mill sourcing partner – SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade DIN 17102 StE500 / StE 500 Confirmed
Product Specification DIN 17102 Applied
Quality letter StE = basic / room temperature Confirmed
Steel type Killed, weldable, fine grain Confirmed
Usual delivery Normalized Confirmed
Yield idea 500 MPa at ≤16 mm Confirmed
Related modern names P500N / S500N when used Confirm on order
Supply role Global steel mill sourcing partner SHH STEEL
Markets USA, Europe, Middle East, Southeast Asia FOB / CIF as ordered
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in structural steel plates and high strength low alloy plates. Vessel comparisons belong next to pressure vessel steel plates and ASME SA516, not as automatic substitutes.

Chemical Composition

DIN 17102 StE500 / StE 500 uses a manganese and microalloy band that supports the 500 MPa yield step. Product analysis is slightly wider than heat analysis.

Heat Analysis and Product Analysis — DIN 17102 StE500 (typical limits)

Element Heat Analysis (%) Product Analysis (%)
Carbon (C), max 0.20 0.22
Silicon (Si) 0.10 – 0.60 0.10 – 0.65
Manganese (Mn) 1.00 – 1.70 0.95 – 1.75
Phosphorus (P), max 0.035 0.040
Sulfur (S), max 0.030 0.035
Nitrogen (N), max 0.020 0.022
Aluminium (Al), min (total, when used for grain) 0.020 0.018
Chromium (Cr), max 0.30 0.35
Copper (Cu), max 0.20 0.25
Molybdenum (Mo), max 0.10 0.12
Nickel (Ni), max 0.80 0.85
Niobium (Nb), max 0.05 0.06
Vanadium (V), max 0.22 0.24
Nb + Ti + V, max 0.24 0.26

StE460 uses a similar residual idea at a lower yield step. TStE500 and EStE500 tighten P and S. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.

Mechanical Properties

Yield starts at 500 MPa at ≤16 mm and falls as thickness rises.

Tensile and Yield — DIN 17102 StE500 (typical published bands)

Thickness (mm) Yield ReH min (MPa) Tensile Rm (MPa)
≤16 500 610 – 770 (≤70 mm band)
16 – 35 490 610 – 770
35 – 50 480 610 – 770
50 – 70 470 610 – 770
70 – 100 460 600 – 760
100 – 150 450 590 – 750
Density 7.85 g/cm³ 7.85 g/cm³

Do not quote 500 MPa yield on an 80 mm plate. Do not treat 610–770 MPa tensile as permission to stamp SA516 Gr.70, SA737 Gr.C or SA738 Gr.B.

Impact is the reason buyers pick DIN 17102 instead of DIN 17100. StE500 is the basic quality. If the drawing names −20 °C or −50 °C, the order may actually need TStE500 or EStE500. Write the test temperature on the purchase order.

How StE / WStE / TStE / EStE Differ at 500

Grade Quality idea Notes
StE500 Basic / room-temperature fine grain This page
WStE500 Elevated temperature (Warm) Same yield idea, warm service
TStE500 Low temperature (Tief) Same yield idea, colder impact
EStE500 Special low temperature Tightest C / P / S in the 500 family

Same 500 MPa yield idea. Different impact and, on T/E, tighter residuals. SHH STEEL will not ship StE500 against a TStE500 impact temperature without a written change.

Material Comparison

Grade Route Strength idea Swap?
DIN 17102 StE460 Normalized fine grain 460 / ~570–720 No
DIN 17102 StE500 Normalized fine grain 500 / ~610–770 This page
P460N / S460N EN 10028-3 / EN 10025-3 Maps to StE460 No
SA516 Gr.70 Carbon vessel 260 / 485–620 No
SA737 Gr.C HSLA vessel 415 / 550–690 No
EN 10025-6 S500Q QT structural Different route No

SA203 Gr.A, SA285 Gr.C and SA299 Gr.A are vessel plates. None of them is StE500.

Fine-Grain Structural Service at 500 MPa

DIN 17102 StE500 / StE 500 is selected when the drawing wants fine-grain, weldable, normalized plate at the 500 MPa step: frames, tanks, machinery and other work still calculated to the old German book. It is not QT S500Q. It is not automatically a Section VIII plate. If the vessel is ASME, the drawing should name an ASME or ASTM grade such as SA516 Gr.70, SA537 Cl.1 or SA738 Gr.A.

SHH STEEL supplies this plate to fabricators in the United States, Europe, the Middle East and Southeast Asia. It is not nickel low-temp plate like SA203 Gr.D or SA203 Gr.E. It is not QT Ni-Cr-Mo like SA543 Type B Cl.1. It is not Cr-Mo like SA387 Gr.22 Cl.2. Stainless inquiries belong on ASME SA240 or ASTM A240.

Weldability

StE500 is killed fine-grain C-Mn-microalloy steel at the highest common DIN 17102 strength step. Welding is production welding, and Code welding when the equipment is a vessel.

Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the 610–770 MPa tensile band, not a SA387 Gr.12 Cl.2 Cr-Mo procedure and not a QT procedure from SA517 Gr.F. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is normalized DIN 17102 StE500 / StE 500 plate. Fine-grain practice and normalize are the product idea. As-rolled shipment is a special agreement.

If the vessel or structure will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the QT route used on SA738 Gr.B or SA737 Gr.C. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.

The certificate lists DIN 17102 StE500 (and StE 500 if requested); heat number; heat analysis; product analysis when ordered; tensile results to the correct thickness column; normalize statement; impact when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to an EN 500 name is available only when chemistry, tensile and impact all fit that EN edition.

Dimensions

Usual supply range from SHH STEEL for StE500 fine grain steel:

  • Thickness: commonly 6 mm – 150 mm. Confirm any request above 150 mm against mill capability
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm
  • Cut-to-length plates and nest sizes inside those limits

Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.

Tolerances

Dimensional limits follow the mill rolling standard named on the order, commonly EN 10029 for plate when the buyer is in Europe. Do not apply ASTM A36/A36M structural tolerances to a DIN fine-grain plate without writing them. UT to EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.

Supplementary Requirements

Most export DIN 17102 StE500 / StE 500 orders add extras. SHH STEEL does not assume them.

Charpy details. Temperature, energy, location and orientation. If the temperature is −40 °C or −50 °C, confirm whether the grade should be TStE500 or EStE500.

Product analysis. Add this when the destination file wants finished-plate chemistry, not only ladle chemistry.

Simulated PWHT. When the equipment will be stress-relieved.

NDE. UT per the named method.

Z-direction / through-thickness testing. When the drawing names Z15 / Z25 / Z35.

Third-party. EN 10204 3.2, with inspectors arranged for US, European or Middle East documentation packages.

Equivalent Material Grades

These names are project-comparison grades. They are not automatic substitutes.

Designation Standard / region Notes
DIN 17102 StE500 / StE 500 DIN 17102 Name on this page
StE460 DIN 17102 Lower step ≈ P460N / S460N
WStE500 DIN 17102 Elevated-temperature sister
TStE500 DIN 17102 Low-temperature sister
EStE500 DIN 17102 Special low-temperature sister
P500N / S500N EN when used Confirm edition
SA516 Gr.70 SA-516 Vessel carbon, different book
ASTM A516 A516 family Related vessel family
EN 10025-6 S500Q QT structural Different route

ASME SA515 and ASME SA662 are not StE500.

Applications

Industry Typical components
Highest-strength DIN 17102 fine-grain structures DIN 17102 StE500 frames and StE 500 plates
Tanks and process steelwork STE500 courses
Dual-certified export StE500 plate from SHH STEEL when the drawing keeps the DIN name
Fabrication StE500 cut to nest sizes

Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.B, A516 Grade 70, SA533 Type C Cl.2, SA517 Gr.P, SA738 Gr.C.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN and JIS steel to the USA, Europe, Middle East and Southeast Asia. Origin is mill-direct, China origin. We do not treat DIN 17102 StE500 as an Asia-only stock item. Inquiry packages are written for fabricators and EPC buyers in Houston, Rotterdam, Antwerp, Jebel Ali, Dammam, Singapore and surrounding ports.

Typical trade terms:

  • FOB Shanghai
  • CIF Houston
  • CIF Rotterdam
  • CIF Jebel Ali
  • Other CIF / CFR ports on request (Los Angeles, New York, Hamburg, Genoa, Jeddah, Mundra, Ho Chi Minh)

Typical lead time for DIN 17102 StE500 / StE 500:

  • Ex-stock / ready plate: about 5–7 days after order confirmation, subject to actual warehouse size and cutting
  • Mill rolling, standard normalize: about 45 days
  • Special heat treatment, simulated PWHT, 3.2 hold or extra NDE: about 2 months

Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading for US, European or Middle East projects. Packing is seaworthy, with edge protection and marking in English as specified on the order.

If the buyer actually needs QT S500Q, say so on the inquiry. Do not assume a domestic Chinese certificate format will pass at destination.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS steel to the USA, Europe, the Middle East and Southeast Asia. On DIN 17102 StE500 / StE 500 that means mill pricing, StE500 chemistry reported as heat analysis and as product analysis when ordered, recorded normalize, tensile results to the correct thickness column, 500 MPa yield in the thin band, 3.1 as standard and 3.2 when specified. Trade terms include FOB Shanghai and CIF Houston / Rotterdam / Jebel Ali.

We keep the grade on the order. StE500 is not StE460. StE500 is not TStE500. StE500 is not S500Q. DIN 17102 is not DIN 17100. StE500 is not SA516 Gr.70. StE500 is not SA387 Gr.22 Cl.2. If the drawing names QT 500 MPa, we will not ship normalized StE500 and call the routes the same.

Company scope: global steel mill sourcing partner – SHH STEEL.

FAQ

What is StE500 steel plate?
StE500 is a DIN 17102 weldable normalized fine-grain steel with the basic quality letter. Yield is 500 MPa at ≤16 mm and tensile is typically 610–770 MPa at ≤70 mm. Buyers also write StE 500, STE500 and DIN17102 StE500. SHH STEEL supplies this plate as a global steel mill sourcing partner.
What is the equivalent of StE500?
Some files compare it with P500N / S500N. Confirm the named EN edition. It is not S500Q QT plate.
How is StE500 different from StE460?
StE460 yield is 460 MPa in the thin band and tensile is typically 570–720 MPa. StE500 yield is 500 MPa and tensile is typically 610–770 MPa.
Is StE500 the same as S500Q?
No. S500Q is quenched and tempered under EN 10025-6. StE500 is normalized under DIN 17102.
Can SHH STEEL ship DIN 17102 StE500 outside Asia?
Yes. SHH STEEL is a global steel mill sourcing partner. We supply this plate to the USA, Europe, the Middle East and Southeast Asia on FOB Shanghai or CIF Houston / Rotterdam / Jebel Ali.
What is the delivery time for StE500?
Ex-stock about 5–7 days. Standard mill normalize about 45 days. Special heat treatment, simulated PWHT or 3.2 inspection about 2 months.
Can SHH STEEL issue EN 10204 3.2 for StE500?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged when written on the order.
What is the density of StE 500?
7.85 g/cm³.

Conclusion

DIN 17102 StE500 Steel Plate, also searched as StE 500, STE500 and DIN17102 StE500, is weldable normalized fine-grain steel under DIN 17102 at the 500 MPa yield step, typically 610–770 MPa tensile at ≤70 mm, the highest common strength step in this book. Whether the inquiry says DIN 17102 StE500, StE 500 or StE500 steel plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with StE500 chemistry, recorded normalize, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies DIN 17102 StE500 / StE500 Fine Grain Steel to the USA, Europe, the Middle East and Southeast Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.

Contact SHH STEEL for mill rolling, stock inquiry, impact testing, 3.2 inspection or a quotation.

DIN 17102 StE500 Steel Plate, StE 500, STE500, DIN17102 StE500, P500N, S500N, fine grain structural steel, StE500 supplier, global steel mill sourcing partner SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X