DIN 17102 EStE500 Steel Plate | EStE500 Fine Grain Steel
What is DIN 17102 EStE500 Steel?
DIN 17102 EStE500, also written EStE 500, ESTE500, DIN17102 EStE500 and EStE500 steel plate, is a weldable normalized fine-grain structural steel under DIN 17102. The E prefix is the special low-temperature quality — colder and cleaner than TStE500. Yield in the thin band is still 500 MPa. Tensile at ≤70 mm is still typically 610–770 MPa. This is the highest common special-low-temp step in DIN 17102. Conversion tables usually put it next to P500NL2 when that name exists on the project file. It is not EStE460. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade. Plate is produced to DIN 17102 and shipped to buyers in the USA, Europe, Middle East and Southeast Asia.
A purchase order that only says “500 NL2 fine grain” is incomplete if the drawing still names DIN. Write DIN 17102 EStE500 and the impact temperature. Do not ship StE500, WStE500 or TStE500 against an EStE500 drawing. Do not ship EStE460 because the yield step is wrong.
DIN 17102 is a legacy specification. New European pressure work often stops at P460NL2 or moves to other books. Replacement projects still name EStE500 when an old German calculation or mill qualification stays on DIN.
This page is not DIN 17100 St52-3. It is not SA516 Gr.70. It is not nickel plate like SA203 Gr.A or SA203 Gr.D. It is not ASTM A36 steel plate. It is not QT alloy under ASME SA387 or ASME SA543.
Company scope: global steel mill sourcing partner – SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | DIN 17102 EStE500 / EStE 500 | Confirmed |
| Product Specification | DIN 17102 | Applied |
| Quality letter | E = special low temperature | Confirmed |
| Steel type | Killed, weldable, fine grain | Confirmed |
| Usual delivery | Normalized | Confirmed |
| Yield idea | 500 MPa at ≤16 mm | Confirmed |
| Related modern name | P500NL2 when used | Confirm on order |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | USA, Europe, Middle East, Southeast Asia | FOB / CIF as ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in structural steel plates, high strength low alloy plates and next to pressure vessel steel plates. ASME carbon comparisons belong on ASME SA516 and ASME SA662, not as automatic substitutes.
Chemical Composition
DIN 17102 EStE500 / EStE 500 is the cleanest 500 column in this book. Product analysis is slightly wider than heat analysis.
Heat Analysis and Product Analysis — DIN 17102 EStE500 (typical limits)
| Element | Heat Analysis (%) | Product Analysis (%) |
|---|---|---|
| Carbon (C), max | 0.16 | 0.18 |
| Silicon (Si) | 0.10 – 0.60 | 0.10 – 0.65 |
| Manganese (Mn) | 1.00 – 1.70 | 0.95 – 1.75 |
| Phosphorus (P), max | 0.025 | 0.030 |
| Sulfur (S), max | 0.015 | 0.020 |
| Nitrogen (N), max | 0.020 | 0.022 |
| Aluminium (Al), min (total, when used for grain) | 0.020 | 0.018 |
| Chromium (Cr), max | 0.30 | 0.35 |
| Copper (Cu), max | 0.20 | 0.25 |
| Molybdenum (Mo), max | 0.10 | 0.12 |
| Nickel (Ni), max | 0.80 | 0.85 |
| Niobium (Nb), max | 0.05 | 0.06 |
| Vanadium (V), max | 0.22 | 0.24 |
| Nb + Ti + V, max | 0.24 | 0.26 |
Compare the 500 family:
| Grade | C max (heat) | P max (heat) | S max (heat) |
|---|---|---|---|
| StE500 / WStE500 | 0.20 | 0.035 | 0.030 |
| TStE500 | 0.18 | 0.030 | 0.025 |
| EStE500 | 0.16 | 0.025 | 0.015 |
Do not ship a TStE500 heat as EStE500. If the order dual-names P500NL2, residuals must also fit that EN edition. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.
Mechanical Properties
Room-temperature yield and tensile follow the 500 family. Special low-temperature impact is why the E letter exists.
Room-temperature properties — DIN 17102 EStE500 (typical published bands)
| Thickness (mm) | Yield ReH min (MPa) | Tensile Rm (MPa) |
|---|---|---|
| ≤16 | 500 | 610 – 770 (≤70 mm band) |
| 16 – 35 | 490 | 610 – 770 |
| 35 – 50 | 480 | 610 – 770 |
| 50 – 70 | 470 | 610 – 770 |
| 70 – 100 | 460 | 600 – 760 |
| 100 – 150 | 450 | 590 – 750 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Do not quote 500 MPa yield on an 80 mm plate. Do not treat 610–770 MPa tensile as permission to stamp SA516 Gr.70, SA662 Gr.A or SA285 Gr.A.
Impact for EStE500 is the special low-temperature package. Write the test temperature, orientation and energy on the order. Do not assume a TStE500 coupon covers EStE500.
How StE / WStE / TStE / EStE Differ at 500
| Grade | Quality idea | Notes |
|---|---|---|
| StE500 | Basic / room-temperature fine grain | Same yield idea |
| WStE500 | Elevated temperature (Warm) | Warm service |
| TStE500 | Low temperature (Tief) | Low-temp quality |
| EStE500 | Special low temperature | This page |
Same 500 MPa yield idea. E is not a marketing letter on TStE500. E has lower carbon, lower P and S, and a colder quality idea. SHH STEEL will not ship TStE500 against an EStE500 purchase order without a written change.
Material Comparison
| Grade | Route | Strength / service idea | Swap? |
|---|---|---|---|
| DIN 17102 EStE460 | Normalized fine grain | 460 / ~570–720, special low-temp | No |
| DIN 17102 StE500 | Normalized fine grain | 500 / ~610–770, basic quality | No |
| DIN 17102 TStE500 | Normalized fine grain | 500 / ~610–770, low-temp quality | No |
| DIN 17102 EStE500 | Normalized fine grain | 500 / ~610–770, special low-temp | This page |
| P460NL2 | EN 10028-3 | Maps to EStE460 | No |
| SA516 Gr.70 | Carbon vessel | 260 / 485–620 | No |
| SA662 Gr.B | C-Mn-Si low-temp vessel | Different book | No |
| SA203 Gr.E | 3.5Ni vessel | Nickel toughness, not EStE | No |
SA285 Gr.C, SA299 Gr.B and SA737 Gr.C are also vessel or HSLA plates. None of them is EStE500.
Special Low-Temperature Fine-Grain Service at 500 MPa
DIN 17102 EStE500 / EStE 500 is selected for welded structures and pressure equipment that need the coldest fine-grain package at the 500 MPa yield step: low-temperature tanks, cold-climate steelwork and other work still calculated to the old German book. It is not QT S500QL1. It is not automatically an ASME Section VIII plate. If the vessel is ASME, the drawing should name an ASME or ASTM grade such as SA516 Gr.70, SA662 Gr.C or SA537 Cl.1.
SHH STEEL supplies this plate to fabricators in the United States, Europe, the Middle East and Southeast Asia. It is not nickel low-temp plate like SA203 Gr.B or SA203 Gr.F. Those grades use nickel. EStE500 uses fine grain, low residuals and normalize. It is not QT Ni-Cr-Mo like SA543 Type B Cl.3. It is not Cr-Mo like SA387 Gr.22 Cl.2 or SA387 Gr.11 Cl.2. Stainless inquiries belong on ASME SA240 or ASTM A240.
Weldability
EStE500 is killed fine-grain C-Mn-microalloy steel with the lowest C / P / S in the 500 family. Welding is production welding, and Code welding when the equipment is a vessel.
Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the 610–770 MPa tensile band, not a SA387 Gr.12 Cl.2 Cr-Mo procedure and not a QT procedure from SA517 Gr.Q. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized DIN 17102 EStE500 / EStE 500 plate. Fine-grain practice and normalize are the product idea. As-rolled shipment is a special agreement and is a poor fit for a special low-temperature quality.
If the vessel or structure will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the QT route used on SA738 Gr.B or SA737 Gr.B. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.
The certificate lists DIN 17102 EStE500 (and EStE 500 if requested); heat number; heat analysis including the tighter C / P / S; product analysis when ordered; tensile results to the correct thickness column; normalize statement; impact at the named temperature. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to P500NL2 is available only when chemistry, tensile and impact all fit that EN edition.
Dimensions
Usual supply range from SHH STEEL for EStE500 fine grain steel:
- Thickness: commonly 6 mm – 150 mm. Confirm any request above 150 mm against mill capability
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
- Cut-to-length plates and nest sizes inside those limits
Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.
Tolerances
Dimensional limits follow the mill rolling standard named on the order, commonly EN 10029 for plate when the buyer is in Europe. Do not apply ASTM A36/A36M structural tolerances to a DIN fine-grain plate without writing them. UT to EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.
Supplementary Requirements
Most export DIN 17102 EStE500 / EStE 500 orders add extras. SHH STEEL does not assume them.
Charpy details. Temperature, energy, location and orientation. This is the reason EStE500 exists. Write the temperature explicitly.
Product analysis. Add this when the destination file wants finished-plate chemistry, not only ladle chemistry.
Simulated PWHT. When the equipment will be stress-relieved.
NDE. UT per the named method.
Z-direction / through-thickness testing. When the drawing names Z15 / Z25 / Z35.
Restricted residuals. Some European files copy EN NL2 options onto EStE500. Write those options on the order.
Third-party. EN 10204 3.2, with inspectors arranged for US, European or Middle East documentation packages.
Equivalent Material Grades
These names are project-comparison grades. They are not automatic substitutes.
| Designation | Standard / region | Notes |
|---|---|---|
| DIN 17102 EStE500 / EStE 500 | DIN 17102 | Name on this page |
| P500NL2 | EN when used | Confirm edition |
| TStE500 | DIN 17102 | Low-temperature sister |
| EStE460 | DIN 17102 | Lower E step ≈ P460NL2 |
| StE500 | DIN 17102 | Basic quality |
| SA516 Gr.70 | SA-516 | Vessel carbon, different book |
| SA662 Gr.A | SA-662 | Related low-temp carbon vessel |
| ASTM A516 | A516 family | Related vessel family |
| EN 10025-6 S500QL1 | QT structural | Different route |
ASME SA515 is not EStE500.
Applications
| Industry | Typical components |
|---|---|
| Special low-temperature fine-grain equipment | DIN 17102 EStE500 shells and EStE 500 plates |
| Cold-service tanks and process steelwork | ESTE500 courses |
| Dual-certified export | EStE500 plate from SHH STEEL when the drawing keeps the DIN name |
| Fabrication | EStE500 cut to nest sizes |
Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA302 Gr.A, SA204 Gr.B, A516 Grade 70, SA533 Type C Cl.1, SA517 Gr.P, SA738 Gr.C.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN and JIS steel to the USA, Europe, Middle East and Southeast Asia. Origin is mill-direct, China origin. We do not treat DIN 17102 EStE500 as an Asia-only stock item. Inquiry packages are written for fabricators and EPC buyers in Houston, Rotterdam, Antwerp, Jebel Ali, Dammam, Singapore and surrounding ports.
Typical trade terms:
- FOB Shanghai
- CIF Houston
- CIF Rotterdam
- CIF Jebel Ali
- Other CIF / CFR ports on request (Los Angeles, New York, Hamburg, Genoa, Jeddah, Mundra, Ho Chi Minh)
Typical lead time for DIN 17102 EStE500 / EStE 500:
- Ex-stock / ready plate: about 5–7 days after order confirmation, subject to actual warehouse size and cutting
- Mill rolling, standard normalize: about 45 days
- Special heat treatment, simulated PWHT, 3.2 hold or extra NDE: about 2 months
Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading for US, European or Middle East projects. Packing is seaworthy, with edge protection and marking in English as specified on the order.
If the buyer actually needs QT S500QL1, say so on the inquiry. If the buyer needs a PED / 3.2 file, say so on the inquiry. Do not assume a domestic Chinese certificate format will pass at destination.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS steel to the USA, Europe, the Middle East and Southeast Asia. On DIN 17102 EStE500 / EStE 500 that means mill pricing, EStE500 chemistry with tight C / P / S reported as heat analysis and as product analysis when ordered, recorded normalize, tensile results to the correct thickness column, impact at the named special low temperature, 3.1 as standard and 3.2 when specified. Trade terms include FOB Shanghai and CIF Houston / Rotterdam / Jebel Ali.
We keep the prefix and the number on the order. EStE500 is not TStE500. EStE500 is not StE500. EStE500 is not WStE500. EStE500 is not EStE460. EStE500 is not S500QL1. DIN 17102 is not DIN 17100. EStE500 is not SA516 Gr.70. EStE500 is not SA387 Gr.22 Cl.2. If the drawing names TStE500, we will not ship EStE500 and call the grades the same just because yield is 500 MPa.
Company scope: global steel mill sourcing partner – SHH STEEL.
FAQ
-
What is EStE500 steel plate?
- EStE500 is a DIN 17102 weldable normalized fine-grain steel with the special low-temperature quality letter. Yield is 500 MPa at ≤16 mm and tensile is typically 610–770 MPa at ≤70 mm. Buyers also write EStE 500, ESTE500 and DIN17102 EStE500. SHH STEEL supplies this plate as a global steel mill sourcing partner.
-
What is the equivalent of EStE500?
- Some files compare it with P500NL2. Confirm the named EN edition. It is not S500QL1 QT plate.
-
What is the difference between EStE500 and TStE500?
- Yield and tensile look the same. EStE500 has lower carbon, lower phosphorus and lower sulfur, and a colder quality idea. Do not ship TStE500 against an EStE500 drawing.
-
EStE500 vs SA203 Grade D — which one for low temperature?
- Different books. SA203 Grade D is 3.5Ni pressure-vessel plate. EStE500 is fine-grain C-Mn-microalloy steel with a special low-temperature letter. Use the grade named on the drawing.
-
What is the chemical composition of EStE500?
- Typical heat limits are C 0.16 max, Si 0.10–0.60, Mn 1.00–1.70, P 0.025 max, S 0.015 max. Product analysis is slightly wider. SHH STEEL reports heat analysis on every certificate and product analysis when ordered.
-
What Charpy temperature should I specify for EStE500?
- Write the temperature, energy, location and orientation. Special low-temperature comparison is commonly −50 °C. Do not write only “impact tested” and do not assume a TStE500 coupon covers EStE500.
-
Can EStE500 be used for pressure vessels?
- Yes, when the project still names DIN 17102 or accepts a named EN dual mark. It is not an automatic ASME Section VIII grade.
-
How do you weld EStE500?
- Treat it as killed fine-grain C-Mn-microalloy steel with low residuals. Match consumables to the 610–770 MPa tensile band, control hydrogen, and qualify the WPS to the applicable code.
-
What thickness of EStE500 plate can SHH STEEL supply?
- Common supply is 6–150 mm thick, 1500–4000 mm wide and 3000–12000 mm long.
-
Where can I buy EStE500 steel plate?
- SHH STEEL supplies DIN 17102 EStE500 to the USA, Europe, the Middle East and Southeast Asia on FOB Shanghai or CIF Houston / Rotterdam / Jebel Ali.
-
Do I need EN 10204 3.1 or 3.2 for EStE500?
- EN 10204 3.1 is standard. EN 10204 3.2 is arranged when written on the order.
-
What is the delivery time for EStE500?
- Ex-stock about 5–7 days. Standard mill normalize about 45 days. Special heat treatment, simulated PWHT or 3.2 inspection about 2 months.
Conclusion
DIN 17102 EStE500 Steel Plate, also searched as EStE 500, ESTE500 and DIN17102 EStE500, is weldable normalized fine-grain steel under DIN 17102 for special low-temperature service at the 500 MPa yield step, typically 610–770 MPa tensile at ≤70 mm, with the tightest C / P / S in the 500 family. Whether the inquiry says DIN 17102 EStE500, EStE 500 or EStE500 steel plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with EStE500 chemistry, recorded normalize, named impact temperature, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies DIN 17102 EStE500 / EStE500 Fine Grain Steel to the USA, Europe, the Middle East and Southeast Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.
Contact SHH STEEL for mill rolling, stock inquiry, dual P500NL2 marking when eligible, impact testing, 3.2 inspection or a quotation.
DIN 17102 EStE500 Steel Plate, EStE 500, ESTE500, DIN17102 EStE500, P500NL2, special low temperature fine grain steel, EStE500 supplier, global steel mill sourcing partner SHH STEEL