EN 10028-3

Product Showcase

EN 10028-3 Carbon Steel Plates

SHH STEEL offers EN 10028-3-compliant P275NH/P355NH weldable fine grain steel plates. EN 10028-3 specifies normalized or normalized rolled steels for pressure vessels with improved toughness. Structural, certified quality, competitive prices, customizable. Trust SHH STEEL!

EN 10028-3 P275N Steel Plate | P275N Fine Grain Vessel Plate - SHH STEEL

EN 10028-3 P275N Steel Plate | P275N Fine Grain Vessel Plate supplier

EN 10028-3 P275N / 1.0486 is normalized fine-grain vessel plate. Yield is 275 MPa to 16 mm and tensile is 390–510 MPa. SHH STEEL supplies P275N worldwide as a global steel mill sourcing partner.
View More
EN 10028-3 P460NH normalized elevated-temperature fine-grain pressure vessel steel plate, 1.8935, SHH STEEL

EN 10028-3 P460NH Steel Plate | P460NH Fine Grain Vessel Plate supplier

EN 10028-3 P460NH is European normalized fine-grain vessel plate with elevated-temperature properties, steel number 1.8935. Yield is 460 MPa at ≤16 mm. Tensile is 570–720 MPa. SHH STEEL supplies P460NH worldwide as a global steel mill sourcing partner.SEO Title
View More
EN 10028-3 P460NL2 normalized special low-temperature pressure vessel steel plate, −50 °C, 1.8918, SHH STEEL

EN 10028-3 P460NL2 Steel Plate | P460NL2 -50°C Vessel Plate supplier

EN 10028-3 P460NL2 is European normalized fine-grain low-temperature vessel plate, steel number 1.8918. Yield is 460 MPa at ≤16 mm. Impact is −50 °C. SHH STEEL supplies P460NL2 worldwide as a global steel mill sourcing partner.
View More
EN 10028-3 P460NL1 normalized low-temperature pressure vessel steel plate, −40 °C, 1.8915, SHH STEEL

EN 10028-3 P460NL1 Steel Plate | P460NL1 -40°C Vessel Plate supplier

EN 10028-3 P460NL1 is European normalized fine-grain low-temperature vessel plate, steel number 1.8915. Yield is 460 MPa at ≤16 mm. Impact is −40 °C. SHH STEEL supplies P460NL1 worldwide as a global steel mill sourcing partner.
View More
EN 10028-3 P355NL2 normalized special low-temperature pressure vessel steel plate, −50 °C, 1.1106, SHH STEEL

EN 10028-3 P355NL2 Steel Plate | P355NL2 -50°C Vessel Plate supplier

EN 10028-3 P355NL2 is European normalized fine-grain low-temperature vessel plate, steel number 1.1106. Yield is 355 MPa at ≤16 mm. Impact is −50 °C. SHH STEEL supplies P355NL2 worldwide as a global steel mill sourcing partner.
View More
EN 10028-3 P355NL1 normalized low-temperature pressure vessel steel plate, −40 °C, 1.0566, SHH STEEL

EN 10028-3 P355NL1 Steel Plate | P355NL1 -40°C Vessel Plate supplier

EN 10028-3 P355NL1 is European normalized fine-grain low-temperature vessel plate, steel number 1.0566. Yield is 355 MPa at ≤16 mm. Impact is −40 °C. SHH STEEL supplies P355NL1 worldwide as a global steel mill sourcing partner.
View More
EN 10028-3 P355NH normalized elevated-temperature fine-grain pressure vessel steel plate, 1.0565, SHH STEEL

EN 10028-3 P355NH Steel Plate | P355NH Fine Grain Vessel Plate supplier

EN 10028-3 P355NH is European normalized fine-grain vessel plate with elevated-temperature properties, steel number 1.0565. Yield is 355 MPa at ≤16 mm. Tensile is 490–630 MPa. SHH STEEL supplies P355NH worldwide as a global steel mill sourcing partner.
View More
EN 10028-3 P355N normalized fine-grain pressure vessel steel plate, 1.0562, SHH STEEL

EN 10028-3 P355N Steel Plate | P355N Fine Grain Vessel Plate supplier

EN 10028-3 P355N is European normalized fine-grain vessel plate, steel number 1.0562. Yield is 355 MPa at ≤16 mm. Tensile is 490–630 MPa. SHH STEEL supplies P355N worldwide as a global steel mill sourcing partner.
View More
EN 10028-3 P275NL2 normalized special low-temperature pressure vessel steel plate, −50 °C, 1.1104, SHH STEEL

EN 10028-3 P275NL2 Steel Plate | P275NL2 -50°C Vessel Plate supplier

EN 10028-3 P275NL2 is European normalized fine-grain low-temperature vessel plate, steel number 1.1104. Yield is 275 MPa at ≤16 mm. Impact is −50 °C. SHH STEEL supplies P275NL2 worldwide as a global steel mill sourcing partner.
View More
EN 10028-3 P275NL1 normalized low-temperature pressure vessel steel plate, −40 °C, 1.0488, SHH STEEL

EN 10028-3 P275NL1 Steel Plate | P275NL1 -40°C Vessel Plate supplier

EN 10028-3 P275NL1 is European normalized fine-grain low-temperature vessel plate, steel number 1.0488. Yield is 275 MPa at ≤16 mm. Impact is −40 °C. SHH STEEL supplies P275NL1 worldwide as a global steel mill sourcing partner.
View More
EN 10028-3 P275NH normalized fine-grain pressure vessel steel plate, 1.0487, SHH STEEL

EN 10028-3 P275NH Steel Plate | P275NH Fine Grain Vessel Plate supplier

EN 10028-3 P275NH is European normalized fine-grain vessel plate, steel number 1.0486. Yield is 275 MPa at ≤16 mm. Tensile is 390–510 MPa. SHH STEEL supplies P275NH worldwide as a global steel mill sourcing partner. SEO Title
View More
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X