GB/T 713.4-2023 Carbon Steel Plates

SHH STEEL supplies GB/T 713.4-2023 nickel-alloy steel plates with specified low-temperature properties as Factory-Direct Supply and export. This part replaces GB/T 24510-2017 and also covers 08Ni3DR and 06Ni9DR previously listed in GB/T 3531-2014. Typical grades are 08Ni3DR, 07Ni5DR, 06Ni7DR and 06Ni9DR for pressure equipment down to -196 °C, including LNG and cryogenic vessels. Competitive mill price, cut-to-size service, fast delivery and full MTCs.

GB/T 713.4-2023 06Ni7DR 7% nickel cryogenic pressure vessel steel plate, Charpy −196 °C, SHH STEEL

GB/T 713.4 06Ni7DR Steel Plate | 06Ni7DR 7Ni Low Temp Vessel Plate

GB/T 713.4 06Ni7DR is Chinese 7% nickel low-temperature vessel plate added in 2023. Yield is 550 MPa in the mid-thickness band. Tensile is 680–820 MPa. Delivery is QT. SHH STEEL supplies 06Ni7DR worldwide. FOB Shanghai / CIF Singapore / Hamburg / Callao.
View More
GB/T 713.4-2023 07Ni5DR 5% nickel low-temperature pressure vessel steel plate, quenched and tempered, SHH STEEL

GB/T 713.4 07Ni5DR Steel Plate | 07Ni5DR 5Ni Low Temp Vessel Plate

GB/T 713.4 07Ni5DR is Chinese 5% nickel low-temperature vessel plate. Yield is 370 MPa at 5–30 mm. Tensile is 530–700 MPa. Delivery is QT. SHH STEEL supplies 07Ni5DR worldwide as a global steel mill sourcing partner. FOB Shanghai / CIF Busan / Rotterdam / Manzanillo.
View More
GB/T 713.4-2023 08Ni3DR 3.5% nickel low-temperature pressure vessel steel plate, Charpy −100 °C, SHH STEEL

GB/T 713.4 08Ni3DR Steel Plate | 08Ni3DR 3.5Ni -100°C Vessel Plate

GB/T 713.4 08Ni3DR is Chinese 3.5% nickel low-temperature vessel plate for service down to -100 °C. Yield is 320 MPa at 6–60 mm. Tensile is 490–620 MPa. SHH STEEL supplies 08Ni3DR worldwide as a global steel mill sourcing partner. FOB Shanghai / CIF Houston / Antwerp / Ulsan.
View More
GB/T 713.4-2023 06Ni9DR 9% nickel cryogenic pressure vessel steel plate, Charpy −196 °C, SHH STEEL

GB/T 713.4 06Ni9DR Steel Plate | 06Ni9DR 9Ni -196°C Vessel Plate

GB/T 713.4 06Ni9DR is Chinese 9% nickel cryogenic vessel plate for service down to -196 °C. Yield is 560 MPa at 5–30 mm. Tensile is 680–820 MPa. SHH STEEL supplies 06Ni9DR worldwide as a global steel mill sourcing partner. FOB Shanghai / CIF Dahej / Zeebrugge / Mizushima.
View More
Boiler & Pressure Vessel Steel Plates Supplier | SHH STEEL – A516, A537, A285, P355GH

Boiler & Pressure Vessel Steel Plates

SHH STEEL, a trusted Pressure Vessel Steel Plates exporter, produces and exports pressure vessel steel plates for boilers, tanks, and petrochemical applications. Our plates, like ASTM A516 Grade 70, offer high tensile strength and toughness, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for boiler steel plates and custom high-pressure solutions.

Boiler & Pressure Vessel Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X