Product Showcase
GB/T 713.3-2023 Carbon Steel Plates
SHH STEEL supplies GB/T 713.3-2023 low-alloy steel plates with specified low-temperature properties as Factory-Direct Supply and export. This part replaces GB/T 3531-2014 and covers plates for pressure equipment with a minimum service temperature of -70 °C, thickness 5–120 mm. Typical grades include 16MnDR, 15MnNiNbDR, Q420DR, Q460DR, 13MnNiDR and 11MnNiMoDR. Competitive mill price, cut-to-size service, fast delivery and full MTCs.
-

GB/T 713.3 Q460DR Steel Plate | Q460DR Low Temp Vessel Plate
GB/T 713.3 Q460DR is Chinese high-strength low-temperature vessel plate added in 2023. Yield is 460 MPa at 6–20 mm. Tensile is 630–730 MPa. Impact is −40 °C. SHH STEEL supplies Q460DR worldwide. FOB Shanghai / CIF Colombo / Alexandria / Valparaiso.View More -

GB/T 713.3 Q420DR Steel Plate | Q420DR Low Temp Vessel Plate
GB/T 713.3 Q420DR is Chinese high-strength low-temperature vessel plate added in 2023. Yield is 420 MPa at 6–20 mm. Tensile is 590–720 MPa. Impact is −40 °C. SHH STEEL supplies Q420DR worldwide. FOB Shanghai / CIF Port Klang / Santos / Gioia Tauro.View More -

GB/T 713.3 11MnNiMoDR Steel Plate | 11MnNiMoDR Low Temp Vessel Plate
GB/T 713.3 11MnNiMoDR is Chinese QT Mn-Ni-Mo low-temperature vessel plate added in 2023. Yield is 420 MPa at 5–60 mm. Tensile is 560–670 MPa. Impact is −70 °C. SHH STEEL supplies 11MnNiMoDR worldwide. FOB Shanghai / CIF Ho Chi Minh / Barcelona / Yokohama.View More -

GB/T 713.3 13MnNiDR Steel Plate | 13MnNiDR Low Temp Vessel Plate
GB/T 713.3 13MnNiDR is Chinese Mn-Ni low-temperature vessel plate added in the 2023 book. Yield is 345 MPa at 5–36 mm. Tensile is 490–610 MPa. Impact is −60 °C. SHH STEEL supplies 13MnNiDR worldwide. FOB Shanghai / CIF Laem Chabang / Mumbai / Callao.View More -

GB/T 713.3 15MnNiNbDR Steel Plate | 15MnNiNbDR -50°C Vessel Plate
GB/T 713.3 15MnNiNbDR is Chinese Ni-Nb low-temperature vessel plate for service down to -50 °C. Yield is 370 MPa at 6–16 mm. Tensile is 530–630 MPa. SHH STEEL supplies 15MnNiNbDR worldwide as a global steel mill sourcing partner. FOB Shanghai / CIF Busan / Hamburg / Durban.View More -

GB/T 713.3 09MnNiDR Steel Plate | 09MnNiDR -70°C Vessel Plate
GB/T 713.3 09MnNiDR is Chinese nickel low-temperature vessel plate for service down to -70 °C. Yield is 300 MPa at 6–16 mm. Tensile is 440–570 MPa. SHH STEEL supplies 09MnNiDR worldwide as a global steel mill sourcing partner. FOB Shanghai / CIF Singapore / Antwerp / Manzanillo.View More -

GB/T 713.3 16MnDR Steel Plate | 16MnDR -40°C Vessel Plate
GB/T 713.3 16MnDR is Chinese low-temperature pressure-vessel plate for service down to -40 °C. Yield is 315 MPa at 5–16 mm. Tensile is 490–620 MPa. SHH STEEL supplies 16MnDR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More
GB/T 713.3-2023 Carbon Steel Plates

Boiler & Pressure Vessel Steel Plates
SHH STEEL, a trusted Pressure Vessel Steel Plates exporter, produces and exports pressure vessel steel plates for boilers, tanks, and petrochemical applications. Our plates, like ASTM A516 Grade 70, offer high tensile strength and toughness, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for boiler steel plates and custom high-pressure solutions.
Boiler & Pressure Vessel Steel Plates
ASME SA-36/SA-36M
ASME SA302
ASTM A302
ASME SA225
ASTM A225
ASME SA455
ASME SA562
ASTM A455
ASTM A562
ASME SA841
GB/T 713.3-2023
GB/T 713.4-2023
GB/T 713.5-2023
ASME SA516
GOST 5520
ASTM A516/516M
GB/T 3077
GB/T 3274
DIN 17102
GB/T 24511
GB/T 24512
GB/T 3077
ASTM A285
ASME SA285
ASTM A515
ASME SA515
ASTM A299
ASTM A517/A517M
ASME SA299
ASTM A204
ASME SA517/SA517M
ASME SA204
ASTM A203
ASME SA203
ASTM A353
ASME SA353
ASTM A387
ASME SA387
ASTM A537
ASME SA537
JIS G3115
GB/T 713.2-2023
GB/T 19189
GB/T 3531
EN 10028-2
EN 10028-3
EN 10028-4
EN 10028-5
EN 10028-6
JIS G3103
ISO 9328-2
X