ISO 9328-2

Product Showcase

ISO 9328-2 Carbon Steel Plates

SHH STEEL offers ISO 9328-2-compliant P265GH/P355GH and 16Mo3/13CrMo4-5 steel plates. ISO 9328-2 specifies technical delivery conditions for plates and strip for pressure equipment made of non-alloy and alloy steels with specified elevated-temperature properties. Standard-compliant, certified quality, competitive prices, customizable. Trust SHH STEEL!

ISO 9328-2 PT480GH Steel Plate | PT480GH Elevated-Temp Pressure Plate | ISO 9328-2 elevated-temperature pressure vessel plate - SHH STEEL

ISO 9328-2 PT480GH Steel Plate | PT480GH Elevated-Temp Pressure Plate

ISO 9328-2 PT480GH steel plate is a non-alloy elevated-temperature pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Non-alloy-quality steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 PT450GH Steel Plate | PT450GH Elevated-Temp Pressure Plate | ISO 9328-2 elevated-temperature pressure vessel plate - SHH STEEL

ISO 9328-2 PT450GH Steel Plate | PT450GH Elevated-Temp Pressure Plate

ISO 9328-2 PT450GH steel plate is a non-alloy elevated-temperature pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Non-alloy-quality steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 PT410GH Steel Plate | PT410GH Elevated-Temp Pressure Plate | ISO 9328-2 elevated-temperature pressure vessel plate - SHH STEEL

ISO 9328-2 PT410GH Steel Plate | PT410GH Elevated-Temp Pressure Plate

ISO 9328-2 PT410GH steel plate is a non-alloy elevated-temperature pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Non-alloy-quality steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 19MnMoNi6-5 Steel Plate | 19MnMoNi6-5 Mn-Mo-Ni Pressure Vessel Plate | ISO 9328-2 Mn-Mo-Ni pressure vessel plate - SHH STEEL

ISO 9328-2 19MnMoNi6-5 Steel Plate | 19MnMoNi6-5 Mn-Mo-Ni Pressure Vessel Plate

ISO 9328-2 19MnMoNi6-5 steel plate is a manganese-molybdenum-nickel pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 19MnMoNi5-5 Steel Plate | 19MnMoNi5-5 Mn-Mo-Ni Pressure Vessel Plate | ISO 9328-2 Mn-Mo-Ni pressure vessel plate - SHH STEEL

ISO 9328-2 19MnMoNi5-5 Steel Plate | 19MnMoNi5-5 Mn-Mo-Ni Pressure Vessel Plate

ISO 9328-2 19MnMoNi5-5 steel plate is a manganese-molybdenum-nickel pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 19MnMo6-5 Steel Plate | 19MnMo6-5 Mn-Mo Pressure Vessel Plate | ISO 9328-2 Mn-Mo pressure vessel plate - SHH STEEL

ISO 9328-2 19MnMo6-5 Steel Plate | 19MnMo6-5 Mn-Mo Pressure Vessel Plate

ISO 9328-2 19MnMo6-5 steel plate is a manganese-molybdenum pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 19MnMo5-5 Steel Plate | 19MnMo5-5 Mn-Mo Pressure Vessel Plate | ISO 9328-2 Mn-Mo pressure vessel plate - SHH STEEL

ISO 9328-2 19MnMo5-5 Steel Plate | 19MnMo5-5 Mn-Mo Pressure Vessel Plate

ISO 9328-2 19MnMo5-5 steel plate is a manganese-molybdenum pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 19MnMo4-5 Steel Plate | 19MnMo4-5 Mn-Mo Pressure Vessel Plate | ISO 9328-2 Mn-Mo pressure vessel plate - SHH STEEL

ISO 9328-2 19MnMo4-5 Steel Plate | 19MnMo4-5 Mn-Mo Pressure Vessel Plate

ISO 9328-2 19MnMo4-5 steel plate is a manganese-molybdenum pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 14CrMoV9-10 Steel Plate | 14CrMoV9-10 Cr-Mo-V Pressure Vessel Plate | ISO 9328-2 Cr-Mo-V pressure vessel plate - SHH STEEL

ISO 9328-2 14CrMoV9-10 Steel Plate | 14CrMoV9-10 Cr-Mo-V Pressure Vessel Plate

ISO 9328-2 14CrMoV9-10 steel plate is a chromium-molybdenum-vanadium pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 14CrMo9-10 Steel Plate | 14CrMo9-10 Cr-Mo Pressure Vessel Plate | ISO 9328-2 Cr-Mo pressure vessel plate - SHH STEEL

ISO 9328-2 14CrMo9-10 Steel Plate | 14CrMo9-10 Cr-Mo Pressure Vessel Plate

ISO 9328-2 14CrMo9-10 steel plate is a chromium-molybdenum pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 13CrMoV12-10 Steel Plate | 13CrMoV12-10 Cr-Mo-V Pressure Vessel Plate | ISO 9328-2 Cr-Mo-V pressure vessel plate - SHH STEEL

ISO 9328-2 13CrMoV12-10 Steel Plate | 13CrMoV12-10 Cr-Mo-V Pressure Vessel Plate

ISO 9328-2 13CrMoV12-10 steel plate is a chromium-molybdenum-vanadium pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
View More
ISO 9328-2 13CrMo4-5 Steel Plate | 13CrMo4-5 Cr-Mo Pressure Vessel Plate | ISO 9328-2 Steel - SHH STEEL

ISO 9328-2 13CrMo4-5 Steel Plate | 13CrMo4-5 Cr-Mo Pressure Vessel Plate

ISO 9328-2 13CrMo4-5 steel plate is specified for pressure-equipment flat products under ISO 9328-2:2018, Edition 4. Alloy special steel classification and the applicable Annex A route must be retained on the material order. SHH STEEL reviews plate dimensions, delivery condition, testing and inspection-document requirements before confirming supply; grade names alone do not establish service suitability.