DIN 17102 WStE460 elevated-temperature fine-grain steel plate, P460NH, SHH STEEL

DIN 17102 WStE460 Steel Plate | WStE460 Fine Grain Steel

DIN 17102 WStE460 / WStE 460 is weldable normalized fine-grain steel for elevated-temperature service. Yield is 460 MPa at ≤16 mm. Tensile is typically 570–720 MPa at ≤70 mm. SHH STEEL supplies WStE460 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
Keywords
DIN 17102 WStE460, WStE460, WStE 460, WSTE460, DIN17102 WStE460, P460NH, WStE460 equivalent, elevated temperature fine grain steel, WStE460 supplier
Equivalent Grades:
DIN 17102 WStE460 / EN 10028-3 P460NH / ASTM A572 Gr 65 (no high-temp proof stress) / GB Q460R (near) — Material Specification: DIN 17102 (withdrawn) — Delivery: Normalized (N)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
How StE / WStE / TStE / EStE Differ at 460
Material Comparison
Elevated-Temperature Fine-Grain Service at 460 MPa
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is DIN 17102 WStE460 Steel?

DIN 17102 WStE460, also written WStE 460, WSTE460, DIN17102 WStE460 and WStE460 steel plate, is a weldable normalized fine-grain structural steel under DIN 17102. The W prefix means Warm — elevated-temperature quality. Yield in the thin band is still 460 MPa. Tensile at ≤70 mm is still typically 570–720 MPa. This is the DIN 17102 warm line that conversion tables map to P460NH. It is not WStE420 and not WStE500. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade. Plate is produced to DIN 17102 and shipped to buyers in the USA, Europe, Middle East and Southeast Asia.

A purchase order that only says “460 NH fine grain” is incomplete if the drawing still names DIN. Write DIN 17102 WStE460. Do not ship StE460 against a WStE460 drawing because StE is basic quality. Do not ship TStE460 against a WStE460 drawing because T is low-temperature quality. Do not ship WStE420 or WStE500 because the yield step is wrong.

DIN 17102 is a legacy specification. New European pressure work usually names P460NH. Replacement projects still name WStE460 when an old German calculation or mill qualification stays on DIN.

This page is not DIN 17100 St52-3. It is not SA516 Gr.70. It is not SA515 Gr.70. It is not ASTM A36 steel plate. It is not QT alloy under ASME SA387 or ASME SA543.

Company scope: global steel mill sourcing partner – SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade DIN 17102 WStE460 / WStE 460 Confirmed
Product Specification DIN 17102 Applied
Quality letter W = elevated temperature Confirmed
Steel type Killed, weldable, fine grain Confirmed
Usual delivery Normalized Confirmed
Yield idea 460 MPa at ≤16 mm Confirmed
Related modern name P460NH Confirm on order
Supply role Global steel mill sourcing partner SHH STEEL
Markets USA, Europe, Middle East, Southeast Asia FOB / CIF as ordered
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in structural steel plates, high strength low alloy plates and next to pressure vessel steel plates. ASME carbon comparisons belong on ASME SA516 and ASME SA515, not as automatic substitutes.

Chemical Composition

DIN 17102 WStE460 / WStE 460 uses the same 460 chemistry family as StE460. TStE460 and EStE460 tighten P and S. Product analysis is slightly wider than heat analysis.

Heat Analysis and Product Analysis — DIN 17102 WStE460 (typical limits)

Element Heat Analysis (%) Product Analysis (%)
Carbon (C), max 0.20 0.22
Silicon (Si) 0.10 – 0.60 0.10 – 0.65
Manganese (Mn) 1.00 – 1.70 0.95 – 1.75
Phosphorus (P), max 0.035 0.040
Sulfur (S), max 0.030 0.035
Nitrogen (N), max 0.020 0.022
Aluminium (Al), min (total, when used for grain) 0.020 0.018
Chromium (Cr), max 0.30 0.35
Copper (Cu), max 0.20 0.25
Molybdenum (Mo), max 0.10 0.12
Nickel (Ni), max 0.80 0.85
Niobium (Nb), max 0.05 0.06
Vanadium (V), max 0.20 0.22
Nb + Ti + V, max 0.22 0.24

If the order dual-names P460NH, residuals and P/S must also fit EN 10028-3 of the named edition. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.

Mechanical Properties

Room-temperature yield and tensile follow the 460 family. Elevated-temperature proof stress is why the W letter exists.

Room-temperature properties — DIN 17102 WStE460 (typical published bands)

Thickness (mm) Yield ReH min (MPa) Tensile Rm (MPa)
≤16 460 570 – 720 (≤70 mm band)
16 – 35 450 570 – 720
35 – 50 440 570 – 720
50 – 70 430 570 – 720
70 – 100 420 560 – 710
100 – 150 410 550 – 700
Density 7.85 g/cm³ 7.85 g/cm³

Do not quote 460 MPa yield on an 80 mm plate. When the order dual-names P460NH, elevated-temperature values come from EN 10028-3, not from a copied StE460 room-temperature coupon. Do not treat 570–720 MPa tensile as permission to stamp SA516 Gr.70, SA515 Gr.65 or SA204 Gr.B.

Impact for WStE460 is not the TStE / EStE low-temperature package. Write the test temperature on the order. If the drawing names −50 °C, the grade is probably TStE460 or EStE460, not WStE460.

How StE / WStE / TStE / EStE Differ at 460

Grade Quality idea Typical modern comparison
StE460 Basic / room-temperature fine grain P460N / S460N
WStE460 Elevated temperature (Warm) P460NH
TStE460 Low temperature (Tief) P460NL1 / S460NL
EStE460 Special low temperature P460NL2

Same 460 MPa yield idea. Different impact package and different design temperature. SHH STEEL will not ship WStE460 against a TStE460 impact temperature without a written change.

Material Comparison

Grade Route Strength / service idea Swap?
DIN 17102 WStE420 Normalized fine grain 420 / ~530–680, warm quality No
DIN 17102 StE460 Normalized fine grain 460 / ~570–720, basic quality No
DIN 17102 WStE460 Normalized fine grain 460 / ~570–720, warm quality This page
DIN 17102 WStE500 Normalized fine grain 500 yield, warm quality No
P460NH EN 10028-3 Closest vessel replacement Comparison only
SA516 Gr.70 Carbon vessel 260 / 485–620 No
SA515 Gr.70 Intermediate/high-temp carbon Different book No
SA204 Gr.A Mo vessel Different book No

SA203 Gr.A, SA299 Gr.B and SA737 Gr.B are vessel or HSLA plates. None of them is WStE460.

Elevated-Temperature Fine-Grain Service at 460 MPa

DIN 17102 WStE460 / WStE 460 is selected for welded structures and pressure equipment that need fine-grain toughness plus a warm-service designation at the 460 MPa yield step: process vessels, boilers, heat exchangers and steelwork still calculated to the old German book. It is the practical DIN counterpart to P460NH. It is not automatically an ASME Section VIII plate. If the vessel is ASME, the drawing should name an ASME or ASTM grade such as SA516 Gr.70, SA515 Gr.60 or SA204 Gr.C.

SHH STEEL supplies this plate to fabricators in the United States, Europe, the Middle East and Southeast Asia. It is not nickel low-temp plate like SA203 Gr.D or SA203 Gr.E. It is not QT Ni-Cr-Mo like SA543 Type B Cl.2. It is not Cr-Mo like SA387 Gr.22 Cl.2 or SA387 Gr.11 Cl.2. Stainless inquiries belong on ASME SA240 or ASTM A240.

Weldability

WStE460 is killed fine-grain C-Mn-microalloy steel at a higher strength step than WStE420. Welding is production welding, and Code welding when the equipment is a vessel.

Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the 570–720 MPa tensile band, not a SA387 Gr.12 Cl.2 Cr-Mo procedure and not a QT procedure from SA517 Gr.Q. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is normalized DIN 17102 WStE460 / WStE 460 plate. Fine-grain practice and normalize are the product idea. As-rolled shipment is a special agreement.

If the vessel will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the QT route used on SA738 Gr.A or SA737 Gr.C. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.

The certificate lists DIN 17102 WStE460 (and WStE 460 if requested); heat number; heat analysis; product analysis when ordered; tensile results to the correct thickness column; normalize statement; impact and elevated-temperature proof stress when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to P460NH is available only when chemistry, tensile, impact and elevated-temperature values all fit the named EN edition.

Dimensions

Usual supply range from SHH STEEL for WStE460 fine grain steel:

  • Thickness: commonly 6 mm – 150 mm. Confirm any request above 150 mm against mill capability
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm
  • Cut-to-length plates and nest sizes inside those limits

Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.

Tolerances

Dimensional limits follow the mill rolling standard named on the order, commonly EN 10029 for plate when the buyer is in Europe. Do not apply ASTM A36/A36M structural tolerances to a DIN fine-grain plate without writing them. UT to EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.

Supplementary Requirements

Most export DIN 17102 WStE460 / WStE 460 orders add extras. SHH STEEL does not assume them.

Charpy details. Temperature, energy, location and orientation. Warm quality is not a −50 °C grade.

Elevated-temperature proof stress. Required when dual-naming P460NH or when the calculation uses warm allowable stress. Name the test temperature.

Product analysis. Add this when the destination file wants finished-plate chemistry, not only ladle chemistry.

Simulated PWHT. When the equipment will be stress-relieved.

NDE. UT per the named method.

Z-direction / through-thickness testing. When the drawing names Z15 / Z25 / Z35.

Third-party. EN 10204 3.2, with inspectors arranged for US, European or Middle East documentation packages.

Equivalent Material Grades

These names are project-comparison grades. They are not automatic substitutes.

Designation Standard / region Notes
DIN 17102 WStE460 / WStE 460 DIN 17102 Name on this page
P460NH EN 10028-3 Closest modern vessel comparison
StE460 DIN 17102 Basic quality ≈ P460N / S460N
WStE420 DIN 17102 Lower warm step ≈ P420NH
WStE500 DIN 17102 Higher warm step
TStE460 DIN 17102 Low-temperature sister ≈ P460NL1 / S460NL
SA516 Gr.60 SA-516 Vessel carbon, different book
SA515 Gr.60 SA-515 Intermediate/higher temperature carbon
ASTM A516 A516 family Related vessel family
ASME SA515 SA-515 family Related high-temp carbon family

ASME SA662 is not WStE460.

Applications

Industry Typical components
Elevated-temperature fine-grain equipment DIN 17102 WStE460 shells and WStE 460 plates
Process vessels and hot service steelwork WSTE460 courses
Dual-certified export WStE460 / P460NH plate from SHH STEEL when chemistry fits
Fabrication WStE460 cut to nest sizes

Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.C, A516 Grade 70, SA533 Type C Cl.1, SA517 Gr.P, SA738 Gr.C.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN and JIS steel to the USA, Europe, Middle East and Southeast Asia. Origin is mill-direct, China origin. We do not treat DIN 17102 WStE460 as an Asia-only stock item. Inquiry packages are written for fabricators and EPC buyers in Houston, Rotterdam, Antwerp, Jebel Ali, Dammam, Singapore and surrounding ports.

Typical trade terms:

  • FOB Shanghai
  • CIF Houston
  • CIF Rotterdam
  • CIF Jebel Ali
  • Other CIF / CFR ports on request (Los Angeles, New York, Hamburg, Genoa, Jeddah, Mundra, Ho Chi Minh)

Typical lead time for DIN 17102 WStE460 / WStE 460:

  • Ex-stock / ready plate: about 5–7 days after order confirmation, subject to actual warehouse size and cutting
  • Mill rolling, standard normalize: about 45 days
  • Special heat treatment, simulated PWHT, 3.2 hold or extra NDE: about 2 months

Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading for US, European or Middle East projects. Packing is seaworthy, with edge protection and marking in English as specified on the order.

If the buyer needs dual P460NH marking for a European file, say so on the inquiry. If the buyer needs a PED / 3.2 file, say so on the inquiry. Do not assume a domestic Chinese certificate format will pass at destination.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS steel to the USA, Europe, the Middle East and Southeast Asia. On DIN 17102 WStE460 / WStE 460 that means mill pricing, WStE460 chemistry reported as heat analysis and as product analysis when ordered, recorded normalize, tensile results to the correct thickness column, 460 MPa yield in the thin band, 3.1 as standard and 3.2 when specified. Trade terms include FOB Shanghai and CIF Houston / Rotterdam / Jebel Ali.

We keep the prefix and the number on the order. WStE460 is not StE460. WStE460 is not TStE460. WStE460 is not WStE420. WStE460 is not WStE500. DIN 17102 is not DIN 17100. WStE460 is not SA516 Gr.70. WStE460 is not SA387 Gr.22 Cl.2. If the drawing names −50 °C impact, we will not ship WStE460 and call it TStE460.

Company scope: global steel mill sourcing partner – SHH STEEL.

FAQ

What is WStE460 steel plate?
WStE460 is a DIN 17102 weldable normalized fine-grain steel with the Warm quality letter. Yield is 460 MPa at ≤16 mm and tensile is typically 570–720 MPa at ≤70 mm. Buyers also write WStE 460, WSTE460 and DIN17102 WStE460. SHH STEEL supplies this plate as a global steel mill sourcing partner.
What is the equivalent of WStE460?
The usual modern comparison is P460NH. StE460 is the basic-quality sister. TStE460 is the low-temperature sister. Dual marking is possible only when chemistry, tensile, impact and elevated-temperature proof stress all fit the named EN edition.
What is the difference between WStE460 and StE460?
Yield and tensile look the same. StE460 is basic quality and maps to P460N / S460N. WStE460 is elevated-temperature quality and maps to P460NH. The W letter means elevated-temperature proof stress belongs on the order.
Can WStE460 be used for pressure vessels?
Yes, when the project still names DIN 17102 or accepts P460NH dual marking. It is not an automatic ASME Section VIII grade.
What temperature can WStE460 be used at?
Warm quality means elevated-temperature service, not cryogenic service. Write the design temperature and the proof-stress test temperature on the order. If you need −40 °C or −50 °C Charpy, you probably need TStE460 or EStE460.
What is the chemical composition of WStE460?
Typical heat limits are C 0.20 max, Si 0.10–0.60, Mn 1.00–1.70, P 0.035 max, S 0.030 max, with Nb and V for grain refinement. Product analysis is slightly wider. SHH STEEL reports heat analysis on every certificate and product analysis when ordered.
How do you weld WStE460?
Treat it as killed fine-grain C-Mn-microalloy steel. Match consumables to the 570–720 MPa tensile band, control hydrogen, and qualify the WPS to the applicable code.
What thickness of WStE460 plate can SHH STEEL supply?
Common supply is 6–150 mm thick, 1500–4000 mm wide and 3000–12000 mm long.
Where can I buy WStE460 steel plate?
SHH STEEL supplies DIN 17102 WStE460 to the USA, Europe, the Middle East and Southeast Asia on FOB Shanghai or CIF Houston / Rotterdam / Jebel Ali.
Do I need EN 10204 3.1 or 3.2 for WStE460?
EN 10204 3.1 is standard. EN 10204 3.2 is arranged when written on the order.
What is the density of WStE 460?
7.85 g/cm³.

Conclusion

DIN 17102 WStE460 Steel Plate, also searched as WStE 460, WSTE460 and DIN17102 WStE460, is weldable normalized fine-grain steel under DIN 17102 for elevated-temperature service at the 460 MPa yield step, typically 570–720 MPa tensile at ≤70 mm, and the usual DIN counterpart to P460NH. Whether the inquiry says DIN 17102 WStE460, WStE 460 or WStE460 steel plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with WStE460 chemistry, recorded normalize, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies DIN 17102 WStE460 / WStE460 Fine Grain Steel to the USA, Europe, the Middle East and Southeast Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.

Contact SHH STEEL for mill rolling, stock inquiry, dual P460NH marking when eligible, impact testing, elevated-temperature proof stress, 3.2 inspection or a quotation.

DIN 17102 WStE460 Steel Plate, WStE 460, WSTE460, DIN17102 WStE460, P460NH, elevated temperature fine grain steel, WStE460 supplier, global steel mill sourcing partner SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X