GOST 5520

Product Showcase

GOST 5520 Carbon Steel Plates

SHH STEEL offers GOST 5520-compliant 16K/20K carbon steel plates. GOST 5520 specifies boiler and vessel steels for welded construction at moderate pressures. Robust, certified quality, competitive prices, customizable. Trust SHH STEEL!

GOST 5520 12Kh1MF Steel Plate | 12Kh1MF Cr-Mo-V Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 12Kh1MF Steel Plate | 12Kh1MF Cr-Mo-V Boiler & Pressure Vessel Plate

GOST 5520 12Kh1MF (12Х1МФ) steel plate is chromium-molybdenum-vanadium alloy boiler and vessel steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–50 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 12KhM Steel Plate | 12KhM Cr-Mo Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 12KhM Steel Plate | 12KhM Cr-Mo Boiler & Pressure Vessel Plate

GOST 5520 12KhM (12ХМ) steel plate is chromium-molybdenum alloy boiler and vessel steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–160 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 10Kh2M Steel Plate | 10Kh2M Cr-Mo Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 10Kh2M Steel Plate | 10Kh2M Cr-Mo Boiler & Pressure Vessel Plate

GOST 5520 10Kh2M (10Х2М) steel plate is chromium-molybdenum alloy boiler and vessel steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 8–50 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 10G2S1 Steel Plate | 10G2S1 Low-Alloy Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 10G2S1 Steel Plate | 10G2S1 Low-Alloy Boiler & Pressure Vessel Plate

GOST 5520 10G2S1 (10Г2С1) steel plate is low-carbon manganese-silicon alloy boiler and vessel steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–160 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 09G2S Steel Plate | 09G2S Low-Alloy Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 09G2S Steel Plate | 09G2S Low-Alloy Boiler & Pressure Vessel Plate

GOST 5520 09G2S (09Г2С) steel plate is low-carbon manganese-silicon alloy boiler and vessel steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–160 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 17G1S Steel Plate | 17G1S Mn-Si Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 17G1S Steel Plate | 17G1S Mn-Si Boiler & Pressure Vessel Plate

GOST 5520 17G1S (17Г1С) steel plate is manganese-silicon boiler and vessel steel, classified as non-alloy in the 2017 edition for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–50 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 17GS Steel Plate | 17GS Mn-Si Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 17GS Steel Plate | 17GS Mn-Si Boiler & Pressure Vessel Plate

GOST 5520 17GS (17ГС) steel plate is manganese-silicon boiler and vessel steel, classified as non-alloy in the 2017 edition for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–50 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 16GS Steel Plate | 16GS Mn-Si Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 16GS Steel Plate | 16GS Mn-Si Boiler & Pressure Vessel Plate

GOST 5520 16GS (16ГС) steel plate is manganese-silicon boiler and vessel steel, classified as non-alloy in the 2017 edition for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–160 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 22K Steel Plate | 22K Carbon Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 22K Steel Plate | 22K Carbon Boiler & Pressure Vessel Plate

GOST 5520 22K (22К) steel plate is non-alloy carbon boiler steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–120 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 20K Steel Plate | 20K Carbon Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 20K Steel Plate | 20K Carbon Boiler & Pressure Vessel Plate

GOST 5520 20K (20К) steel plate is non-alloy carbon boiler steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–60 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 18K Steel Plate | 18K Carbon Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 18K Steel Plate | 18K Carbon Boiler & Pressure Vessel Plate

GOST 5520 18K (18К) steel plate is non-alloy carbon boiler steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–60 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
GOST 5520 16K Steel Plate | 16K Carbon Boiler & Pressure Vessel Plate | GOST 5520 Steel - SHH STEEL

GOST 5520 16K Steel Plate | 16K Carbon Boiler & Pressure Vessel Plate

GOST 5520 16K (16К) steel plate is non-alloy carbon boiler steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–60 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
View More
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X