GB/T 13296

Product Showcase

GB/T 13296 Stainless Steel Products

SHH STEEL offers GB/T 13296-compliant 304/316 stainless steel tubes. GB/T 13296 specifies seamless stainless steel tubes for boilers and heat exchangers, ideal for high-temperature and high-pressure environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!

GB/T 13296 06Cr18Ni12Mo2Cu2 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr18Ni12Mo2Cu2 Seamless Stainless Steel Tube

GB/T 13296 06Cr18Ni12Mo2Cu2 seamless stainless steel tube (316Cu-class / UNS S31688, S31688), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 022Cr19Ni13Mo3 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 022Cr19Ni13Mo3 Seamless Stainless Steel Tube

GB/T 13296 022Cr19Ni13Mo3 seamless stainless steel tube (317L / UNS S31703, S31703), austenitic, Table 3 cast analysis, Rm min 480 MPa / Rp0.2 min 175 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 06Cr19Ni13Mo3 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr19Ni13Mo3 Seamless Stainless Steel Tube

GB/T 13296 06Cr19Ni13Mo3 seamless stainless steel tube (317 / UNS S31708, S31708), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More

GB/T 13296 022Cr17Ni12Mo2N Seamless Stainless Steel Tube

GB/T 13296 022Cr17Ni12Mo2N seamless stainless steel tube (316LN / UNS S31653, S31653), austenitic, Table 3 cast analysis, Rm min 550 MPa / Rp0.2 min 245 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 06Cr17Ni12Mo2N Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr17Ni12Mo2N Seamless Stainless Steel Tube

GB/T 13296 06Cr17Ni12Mo2N seamless stainless steel tube (316N / UNS S31658, S31658), austenitic, Table 3 cast analysis, Rm min 550 MPa / Rp0.2 min 275 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 06Cr17Ni12Mo2Ti Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr17Ni12Mo2Ti Seamless Stainless Steel Tube

GB/T 13296 06Cr17Ni12Mo2Ti seamless stainless steel tube (316Ti / UNS S31668, S31668), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 07Cr17Ni12Mo2 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 07Cr17Ni12Mo2 Seamless Stainless Steel Tube

GB/T 13296 07Cr17Ni12Mo2 seamless stainless steel tube (316H / UNS S31609, S31609), austenitic, Table 3 cast analysis, Rm min 480 MPa / Rp0.2 min 175 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 022Cr17Ni12Mo2 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 022Cr17Ni12Mo2 Seamless Stainless Steel Tube

GB/T 13296 022Cr17Ni12Mo2 seamless stainless steel tube (316L / UNS S31603, S31603), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 06Cr17Ni12Mo2 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr17Ni12Mo2 Seamless Stainless Steel Tube

GB/T 13296 06Cr17Ni12Mo2 seamless stainless steel tube (316 / UNS S31608, S31608), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 20Cr25Ni20 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 20Cr25Ni20 Seamless Stainless Steel Tube

GB/T 13296 20Cr25Ni20 seamless stainless steel tube (310 / UNS S31000, S31020), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 16Cr23Ni13 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 16Cr23Ni13 Seamless Stainless Steel Tube

GB/T 13296 16Cr23Ni13 seamless stainless steel tube (309 / UNS S30900, S30920), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More
GB/T 13296 06Cr25Ni20 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr25Ni20 Seamless Stainless Steel Tube

GB/T 13296 06Cr25Ni20 seamless stainless steel tube (310S / UNS S31008, S31008), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
View More

GB/T 13296 Stainless Steel Products

GB/T 13296 06Cr13 Seamless Stainless Steel Tube GB/T 13296 008Cr27Mo Seamless Stainless Steel Tube GB/T 13296 10Cr17 Seamless Stainless Steel Tube GB/T 13296 022Cr21Ni25Mo7N Seamless Stainless Steel Tube
GB/T 13296 015Cr21Ni26Mo5Cu2 Seamless Stainless Steel Tube GB/T 13296 015Cr20Ni18Mo6CuN Seamless Stainless Steel Tube GB/T 13296 07Cr18Ni11Nb Seamless Stainless Steel Tube GB/T 13296 06Cr18Ni11Nb Seamless Stainless Steel Tube
GB/T 13296 07Cr19Ni11Ti Seamless Stainless Steel Tube GB/T 13296 06Cr18Ni11Ti Seamless Stainless Steel Tube GB/T 13296 06Cr18Ni13Si4 Seamless Stainless Steel Tube GB/T 13296 022Cr18Ni14Mo2Cu2 Seamless Stainless Steel Tube
GB/T 13296 06Cr18Ni12Mo2Cu2 Seamless Stainless Steel Tube GB/T 13296 022Cr19Ni13Mo3 Seamless Stainless Steel Tube GB/T 13296 06Cr19Ni13Mo3 Seamless Stainless Steel Tube GB/T 13296 022Cr17Ni12Mo2N Seamless Stainless Steel Tube
GB/T 13296 06Cr17Ni12Mo2N Seamless Stainless Steel Tube GB/T 13296 06Cr17Ni12Mo2Ti Seamless Stainless Steel Tube GB/T 13296 07Cr17Ni12Mo2 Seamless Stainless Steel Tube GB/T 13296 022Cr17Ni12Mo2 Seamless Stainless Steel Tube
GB/T 13296 06Cr17Ni12Mo2 Seamless Stainless Steel Tube GB/T 13296 20Cr25Ni20 Seamless Stainless Steel Tube GB/T 13296 16Cr23Ni13 Seamless Stainless Steel Tube GB/T 13296 06Cr25Ni20 Seamless Stainless Steel Tube
GB/T 13296 06Cr23Ni13 Seamless Stainless Steel Tube GB/T 13296 022Cr19Ni10N Seamless Stainless Steel Tube GB/T 13296 06Cr19Ni10N Seamless Stainless Steel Tube GB/T 13296 07Cr19Ni10 Seamless Stainless Steel Tube
GB/T 13296 022Cr19Ni10 Seamless Stainless Steel Tube GB/T 13296 06Cr19Ni10 Seamless Stainless Steel Tube GB/T 13296 12Cr18Ni9 Seamless Stainless Steel Tube
Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X