GB/T 13296 06Cr17Ni12Mo2N Seamless Stainless Steel Tube
What is GB/T 13296 06Cr17Ni12Mo2N Seamless Stainless Steel Tube
Boiler and heat-exchanger packages written to Chinese product standards look to GB/T 13296-2023 rather than inventing a mill grade from AISI shorthand alone. 06Cr17Ni12Mo2N is the Table 3/4 Chinese grade name for this austenitic chemistry (S31658). Nitrogen separates this mark from ordinary 06Cr17Ni12Mo2 on the strength side.
Mill path for 06Cr17Ni12Mo2N: manufacture symbol W-C/W-H, Table 4 heat treatment, Table 3 cast chemistry, Table 4 tensile floors, hydrostatic or eddy-current E3H, ultrasonic U2. SHH STEEL can make and supply the grade to that stack. Typical use: higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr17Ni12Mo2N before production starts. Application context for 06Cr17Ni12Mo2N stays higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles.
Body text may mention 316N / UNS S31658 (unified S31658) for cross-reference, but the H1 and order line stay on 06Cr17Ni12Mo2N. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket.
Order the standard the drawing and regulatory file actually require. Inside this 13296 series, compare 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N, 06Cr19Ni13Mo3 before stretching surface finish or wall alone. Duty thread: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor.
Inside this GB/T 13296 series, compare GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 022Cr17Ni12Mo2N, GB/T 13296 06Cr19Ni10N, GB/T 13296 06Cr19Ni13Mo3. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP316.
When 06Cr17Ni12Mo2N pipe sits beside plate on the same BOM, the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 4237 06Cr17Ni12Mo2N. See also the GB/T 4237 hub for related plate designations. Confirm 06Cr17Ni12Mo2N OD × wall and plate thickness on separate drawings.
Chemical Composition of GB/T 13296 06Cr17Ni12Mo2N
Table 3 sets the melt limits for 06Cr17Ni12Mo2N. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Highlight band: C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 10.00–13.00, Cr 16.00–18.00, Mo 2.00–3.00. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 3. Alias note: 316N / UNS S31658.
The composition table below is the cast window SHH STEEL quotes against for 06Cr17Ni12Mo2N. Edition framing is GB/T 13296-2023. Use thread: higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr17Ni12Mo2N before the order is acknowledged. Size practice for 06Cr17Ni12Mo2N remains mid OD cold-finished stock for strength-driven walls.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo | N |
|---|---|---|---|---|---|---|---|---|---|
| 06Cr17Ni12Mo2N | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.015 | 10.00–13.00 | 16.00–18.00 | 2.00–3.00 | 0.10–0.16 |
UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 06Cr17Ni12Mo2N (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 316N / UNS S31658, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 06Cr17Ni12Mo2N against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 06Cr17Ni12Mo2N before the heat is booked.
Mechanical Properties of GB/T 13296 06Cr17Ni12Mo2N
Table 4 mechanical acceptance for 06Cr17Ni12Mo2N: Rm min 550 MPa, Rp0.2 min 275 MPa, elongation min 35%. Note: UNCERTAIN — provisional vs paid Table 3/4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Delivery framing: solution annealed. Sampling follows the batch rules for 06Cr17Ni12Mo2N.
Elevated-temperature Annex A Rp0.2 and Annex B 100000 h rupture tables name only selected H marks — check whether 06Cr17Ni12Mo2N appears before citing those numbers in a design note. Density 7.98 kg/dm³.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 06Cr17Ni12Mo2N | 550 | 275 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 06Cr17Ni12Mo2N. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1010–1150 °C, rapid cool. UNCERTAIN — provisional vs paid Table 3/4. Density 7.98 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 06Cr17Ni12Mo2N
For 06Cr17Ni12Mo2N, the mill path is pierce / extrude / draw — never ERW or automatic-arc under GB/T 13296. Delivery is heat-treated and pickled unless overall ground/bored or protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO. Seamless W-C and W-H routes are the only valid order paths for 06Cr17Ni12Mo2N under GB/T 13296.
After hot or cold working, 06Cr17Ni12Mo2N is heat-treated per Table 4 and finished to the ordered surface. Straightness limits differ for W-H (≤2.0 mm/m) and W-C (≤1.5 mm/m); full-length bow ≤0.15% of length. Pickling or bright-anneal decisions for 06Cr17Ni12Mo2N stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Application context for 06Cr17Ni12Mo2N stays higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles.
Straightness, end finish, and marking for 06Cr17Ni12Mo2N are checked before bundling so tubesheet fit-up crews receive usable lengths. Caution: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket. Hydrostatic pressure or eddy-current class for 06Cr17Ni12Mo2N is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Weld-shop note tied to 06Cr17Ni12Mo2N: 316L/N-aware fillers; avoid soft under-matched deposits.
Dimensions and Tolerances for GB/T 13296 06Cr17Ni12Mo2N
Minimum-wall ordering is common for HX duty on 06Cr17Ni12Mo2N: W-C min-wall tolerance is +20%S/0 for D≤38 mm and +22%S/0 above; W-H min-wall is +0.90/0 mm for S≤4.0 mm and +25%S/0 above. Confirm nominal-wall versus min-wall language on the PO. Tolerance basis for 06Cr17Ni12Mo2N follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside 06Cr17Ni12Mo2N: Mo plus N: PREN and strength move together versus plain 316-class.
Bevel geometry, land, and ID cleanliness notes for 06Cr17Ni12Mo2N belong on the acknowledgement when automatic welding to the tubesheet is planned. Apps: higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles. Fixed lengths and multiple cut lengths for 06Cr17Ni12Mo2N are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 06Cr17Ni12Mo2N: 316L/N-aware fillers; avoid soft under-matched deposits.
Equivalent Grades for GB/T 13296 06Cr17Ni12Mo2N
Buyers searching under 316N / UNS S31658 still need the GB/T 13296 06Cr17Ni12Mo2N row locked on the acknowledgement. Inside austenitic practice the mechanical table and inspection clauses of GB/T 13296 control acceptance, not a brochure equivalent. Duty context: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 06Cr17Ni12Mo2N | Governing tube grade for this page |
| Commercial / UNS (body only) | 316N / UNS S31658 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
When the service outgrows 06Cr17Ni12Mo2N, move to a sister rather than stretching the alias: GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 022Cr17Ni12Mo2N, GB/T 13296 06Cr19Ni10N, GB/T 13296 06Cr19Ni13Mo3. Apps context: higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles. Full list under GB/T 13296. Dual marking is a purchase-order option that still requires every limit that matters for 06Cr17Ni12Mo2N to be verified on the heat.
Heat Treatment and Delivery Condition for GB/T 13296 06Cr17Ni12Mo2N
Table 4 schedules 06Cr17Ni12Mo2N at 1010–1150 °C, rapid cool. Protective-atmosphere bright anneal may omit pickle when agreed. Grain-size extras: per family practice. Caution: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket. Recorded furnace charts for 06Cr17Ni12Mo2N should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 06Cr17Ni12Mo2N caution visible here: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket.
Recorded cool method for 06Cr17Ni12Mo2N matters as much as peak temperature — rapid cool versus air/slow cool is a family identity issue. Density 7.98 kg/dm³. Field heat treatment of 06Cr17Ni12Mo2N after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 06Cr17Ni12Mo2N: Mo plus N: PREN and strength move together versus plain 316-class.
Corrosion Resistance of GB/T 13296 06Cr17Ni12Mo2N
Select 06Cr17Ni12Mo2N when the process side matches this framing: Mo plus N: PREN and strength move together versus plain 316-class. Sister upgrades on the same hub include 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N, 06Cr19Ni13Mo3. Role: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. Coupon orientation, weld condition, and surface finish for 06Cr17Ni12Mo2N belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Weld-shop note tied to 06Cr17Ni12Mo2N: 316L/N-aware fillers; avoid soft under-matched deposits.
Oxidation-first marks and PREN-first marks in this series are not interchangeable — 06Cr17Ni12Mo2N sits on the Mo plus N: PREN and strength move together versus plain 316-class side of that split. Caution: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr17Ni12Mo2N rather than relying on wall thickness alone. Weld-shop note tied to 06Cr17Ni12Mo2N: 316L/N-aware fillers; avoid soft under-matched deposits.
Applications of GB/T 13296 06Cr17Ni12Mo2N Seamless Tube
Exchanger and boiler designers reach for 06Cr17Ni12Mo2N when: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. Common sketch: higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles. Caution on the datasheet: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket. Spool fabricators should copy 06Cr17Ni12Mo2N onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Application context for 06Cr17Ni12Mo2N stays higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles.
U-bend radius, heat treatment after bending, and tubesheet weld details for 06Cr17Ni12Mo2N belong in the fabrication specification, not only in the mill PO. Caution: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket. Commissioning teams benefit when the as-built dossier repeats 06Cr17Ni12Mo2N beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 06Cr17Ni12Mo2N remains mid OD cold-finished stock for strength-driven walls.
Weldability of GB/T 13296 06Cr17Ni12Mo2N
Shop guidance for 06Cr17Ni12Mo2N: 316L/N-aware fillers; avoid soft under-matched deposits. Autogenous orbital welds to tubesheets need clean ID and controlled heat input. Family: austenitic. Procedure qualification for 06Cr17Ni12Mo2N should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 06Cr17Ni12Mo2N caution visible here: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket.
Post-weld heat treatment of 06Cr17Ni12Mo2N is uncommon for austenitics but may be specified for stabilised marks or ferritic toughness — write it explicitly. Caution: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket. Consumable lot control and shielding-gas notes for 06Cr17Ni12Mo2N stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 06Cr17Ni12Mo2N caution visible here: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket.
Surface Finishes for GB/T 13296 06Cr17Ni12Mo2N
Surface condition for 06Cr17Ni12Mo2N is part of the tube identity under GB/T 13296. Order annealed/pickled as default HX or process supply, then add bright anneal or polish only with OD/ID scope named. Keep caution visible: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
SHH STEEL sequences pickle, optional passivation, and any agreed polish for 06Cr17Ni12Mo2N after the heat-treatment evidence is on the certificate. Free-iron control and packing discipline matter as much as Ra numbers for long tube life in the field. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (06Cr17Ni12Mo2N).
Inspection and Testing for GB/T 13296 06Cr17Ni12Mo2N
Batch rules for 06Cr17Ni12Mo2N: same grade, heat, size, and heat-treatment lot. Sampling counts follow OD/wall thresholds in the standard. Role: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. Sampling plans for 06Cr17Ni12Mo2N keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 06Cr17Ni12Mo2N: 316L/N-aware fillers; avoid soft under-matched deposits.
Witness points for 06Cr17Ni12Mo2N (hydro, UT, IGC) should be booked before the tubes leave the finishing bay. Duty: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. Non-conforming 06Cr17Ni12Mo2N lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Corrosion framing beside 06Cr17Ni12Mo2N: Mo plus N: PREN and strength move together versus plain 316-class.
Packaging and Shipping for GB/T 13296 06Cr17Ni12Mo2N
Export crates for 06Cr17Ni12Mo2N protect thin-wall HX stock against handling dents that would fail UT or tubesheet fit-up. Role: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. Bundle tickets for 06Cr17Ni12Mo2N repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 06Cr17Ni12Mo2N: 316L/N-aware fillers; avoid soft under-matched deposits.
Claims handling for 06Cr17Ni12Mo2N starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Duty: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. Desiccant and wrap choices for 06Cr17Ni12Mo2N follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 06Cr17Ni12Mo2N caution visible here: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket.
Loose tubes of 06Cr17Ni12Mo2N are avoided; strapped bundles keep heat lots together for MTC matching. Role: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. Claims handling for 06Cr17Ni12Mo2N starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 06Cr17Ni12Mo2N: 316L/N-aware fillers; avoid soft under-matched deposits.
Why Choose SHH STEEL
Why buyers stay with SHH STEEL for 06Cr17Ni12Mo2N: written acknowledgements that name W-C/W-H and Table 4 heat treatment before melt, plus MTCs that repeat the Chinese grade. Caution: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket. SHH STEEL can produce and supply 06Cr17Ni12Mo2N against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Size practice for 06Cr17Ni12Mo2N remains mid OD cold-finished stock for strength-driven walls.
Engineering support for 06Cr17Ni12Mo2N includes clarifying min-wall versus nominal-wall language and Annex A/B applicability before the heat is melted. Caution: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket. SHH STEEL can make 06Cr17Ni12Mo2N to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. This paragraph is locked to 06Cr17Ni12Mo2N duty: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor.
Supply Capability
Supply capability for 06Cr17Ni12Mo2N: W-C and W-H seamless routes, pickled or bright, plain or bevelled ends, random or fixed lengths. SHH STEEL can make the grade when melt and finishing slots align. Apps: higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr17Ni12Mo2N when the mill schedule allows. Corrosion framing beside 06Cr17Ni12Mo2N: Mo plus N: PREN and strength move together versus plain 316-class.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 06Cr17Ni12Mo2N (S31658) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes for 06Cr17Ni12Mo2N centre on cold-finished mid-OD HX tubes and selected hot-finished boiler walls; ask for the current matrix against your datasheet. Apps: higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr17Ni12Mo2N once design pressure and corrosion allowance are clear. Application context for 06Cr17Ni12Mo2N stays higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles.
Lead time for 06Cr17Ni12Mo2N tracks melt booking, finishing, and any third-party holds — send the full test matrix with the RFQ. Role: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. SHH STEEL can produce trial lengths of 06Cr17Ni12Mo2N for procedure qualification before bulk release when the project calendar needs it. Size practice for 06Cr17Ni12Mo2N remains mid OD cold-finished stock for strength-driven walls.
FAQ
-
What is GB/T 13296 06Cr17Ni12Mo2N seamless stainless steel tube used for?
- GB/T 13296 06Cr17Ni12Mo2N is seamless stainless tube for boilers and heat exchangers — higher-pressure chloride HX, compact condensers, and weight-sensitive Mo bundles. Role summary: nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. It is a Chinese product standard grade (S31658), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
-
Is GB/T 13296 06Cr17Ni12Mo2N seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr17Ni12Mo2N when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 06Cr17Ni12Mo2N?
- 06Cr17Ni12Mo2N is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr17Ni12Mo2N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr17Ni12Mo2N compare with sister grades 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N?
- 06Cr17Ni12Mo2N is filed as austenitic. Typical sisters on the same RFQ are 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N. Design caution: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr17Ni12Mo2N?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 316N / UNS S31658 the same as ordering 06Cr17Ni12Mo2N?
- No. 316N / UNS S31658 is a commercial / UNS cross-walk for body text (unified S31658). The purchase order should lock GB/T 13296 and 06Cr17Ni12Mo2N so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 06Cr17Ni12Mo2N?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr17Ni12Mo2N within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: mid OD cold-finished stock for strength-driven walls. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 06Cr17Ni12Mo2N be welded on site?
- Shop guidance: 316L/N-aware fillers; avoid soft under-matched deposits. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr17Ni12Mo2N?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN vs paid Table 3/4; N band must appear on the melt ticket Sister pointers: 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 06Cr17Ni12Mo2N with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr17Ni12Mo2N does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 06Cr17Ni12Mo2N?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr17Ni12Mo2N when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 06Cr17Ni12Mo2N is seamless stainless steel tube for boilers and heat exchangers — nitrogen-strengthened Mo austenitic tube when HX design needs both PREN and a higher proof floor. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.