GB/T 13296 06Cr18Ni11Nb Seamless Stainless Steel Tube
What is GB/T 13296 06Cr18Ni11Nb Seamless Stainless Steel Tube
GB/T 13296-2023 is the Chinese national standard for seamless stainless steel tubes for boilers and heat exchangers — replacing the 2013 edition. Grade 06Cr18Ni11Nb (unified number S34778) sits in the austenitic set. Niobium replaces titanium as the stabilising element on this mark.
SHH STEEL can produce and supply GB/T 13296 06Cr18Ni11Nb as seamless W-C or W-H tube across the enquiry OD×wall band, heat-treated per Table 4, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium.
Shop language may still say “347 tube,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 13296 and 06Cr18Ni11Nb so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
Scope discipline: 06Cr18Ni11Nb is seamless boiler/HX tube under GB/T 13296, not fluid-transport pipe under GB/T 14976 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include 07Cr18Ni11Nb, 06Cr18Ni11Ti, 06Cr19Ni10, 06Cr17Ni12Mo2Ti. Role reminder: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium.
Inside this GB/T 13296 series, compare GB/T 13296 07Cr18Ni11Nb, GB/T 13296 06Cr18Ni11Ti, GB/T 13296 06Cr19Ni10, GB/T 13296 06Cr17Ni12Mo2Ti. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP347.
Chemical Composition of GB/T 13296 06Cr18Ni11Nb
Cast analysis for GB/T 13296 06Cr18Ni11Nb follows Table 3. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 9.00–12.00, Cr 17.00–19.00, Nb 10C–1.10. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 347 / UNS S34778; unified number S34778. Corrosion thread: Nb stabilisation for HAZ integrity; chloride PREN still Mo-free.
Chemical limits for 06Cr18Ni11Nb under GB/T 13296-2023 appear in the table underneath. Source priority is the 2023 Table 3 extract (xtd). If your client specification cites a 2013 footnote, send it before the heat is melted. Duty thread: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr18Ni11Nb before the order is acknowledged. This paragraph is locked to 06Cr18Ni11Nb duty: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium.
| Grade | C | Si | Mn | P | S | Ni | Cr | Nb |
|---|---|---|---|---|---|---|---|---|
| 06Cr18Ni11Nb | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.015 | 9.00–12.00 | 17.00–19.00 | 10C–1.10 |
Mechanical Properties of GB/T 13296 06Cr18Ni11Nb
Ambient tensile floors for 06Cr18Ni11Nb come from GB/T 13296 Table 4: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: stabilisation after solution anneal by agreement. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
Hardness testing is by agreement for wall ≥1.7 mm; Table 5 bands differ for special marks such as 06Cr18Ni13Si4 and the high-Mo austenitics. Density reference for 06Cr18Ni11Nb is 8.03 kg/dm³. Hydrostatic proof uses P=2SR/D with R at 60% of Table 4 Rp0.2, capped at 20 MPa.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 06Cr18Ni11Nb | 520 | 205 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 06Cr18Ni11Nb. Heat treatment (Table 4): 980–1150 °C, rapid cool. stabilisation after solution anneal by agreement. Density 8.03 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 06Cr18Ni11Nb
SHH STEEL can produce 06Cr18Ni11Nb as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 4 heat treatment and pickle (or bright anneal) as ordered. Plain ends are default; bevels by agreement when the tubesheet weld prep needs it. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.
Steelmaking for 06Cr18Ni11Nb is electric-arc or converter with secondary refining, or electroslag remelting. Pickling follows heat treatment unless bright protective-atmosphere practice or overall machining allows omission. Size practice: W-C HX with optional stabilisation heat treatment. Pickling or bright-anneal decisions for 06Cr18Ni11Nb stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Application context for 06Cr18Ni11Nb stays refinery HX, chemical steam coils, and welded bundles preferring Nb over Ti.
Eddy-current testing to GB/T 7735 E3H may replace hydrostatic proof when agreed; ultrasonic testing to GB/T 5777 U2 remains a standard acceptance path for 06Cr18Ni11Nb. Role: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. Hydrostatic pressure or eddy-current class for 06Cr18Ni11Nb is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Keep the 06Cr18Ni11Nb caution visible here: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
Dimensions and Tolerances for GB/T 13296 06Cr18Ni11Nb
Dimensions and tolerances for 06Cr18Ni11Nb follow GB/T 13296 Table 1. Usual length is 2000–12000 mm. W-H OD tolerance is ±1.25%D for D≤140 mm and ±1%D above; W-C uses absolute OD bands from ±0.10 mm (D≤25) up through ±0.5%D for D>159 mm. Size hint: W-C HX with optional stabilisation heat treatment. Tolerance basis for 06Cr18Ni11Nb follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for 06Cr18Ni11Nb remains W-C HX with optional stabilisation heat treatment.
Out-of-roundness and wall unevenness for 06Cr18Ni11Nb shall not exceed 80% of the OD and wall tolerances respectively. Full-length camber ≤0.15% of tube length. Duty: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. Fixed lengths and multiple cut lengths for 06Cr18Ni11Nb are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 06Cr18Ni11Nb caution visible here: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
Equivalent Grades for GB/T 13296 06Cr18Ni11Nb
Lock 06Cr18Ni11Nb on the PO when the datasheet owner wants GB/T 13296 seamless stainless boiler / heat-exchanger tube. Commercial talk as 347 / UNS S34778 is fine in emails; mill paperwork must still show GB/T 13296 06Cr18Ni11Nb. Application framing: refinery HX, chemical steam coils, and welded bundles preferring Nb over Ti
– Caution locked in What-is / Corrosion / FAQ: Nb 10C–1.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 06Cr18Ni11Nb | Governing tube grade for this page |
| Commercial / UNS (body only) | 347 / UNS S34778 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | 347 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Order discipline for 06Cr18Ni11Nb still points at GB/T 13296, not the brochure alias. Neighbours GB/T 13296 07Cr18Ni11Nb, GB/T 13296 06Cr18Ni11Ti, GB/T 13296 06Cr19Ni10, GB/T 13296 06Cr17Ni12Mo2Ti each carry their own mechanical table. Category hub: GB/T 13296. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (06Cr18Ni11Nb).
For 06Cr18Ni11Nb, vertical navigation stays form-specific — tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is GB/T 4237 06Cr18Ni11Nb. Do not stretch a 06Cr18Ni11Nb pipe certificate onto plate.
Heat Treatment and Delivery Condition for GB/T 13296 06Cr18Ni11Nb
Heat treatment for 06Cr18Ni11Nb follows Table 4: 980–1150 °C, rapid cool. Delivery condition: solution annealed. SHH STEEL records furnace charts that support the temperature and cool method claimed on the certificate. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni11Nb unless the mark is on the exemption list.
Field heat treatment of 06Cr18Ni11Nb after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni11Nb unless the mark is on the exemption list. Field heat treatment of 06Cr18Ni11Nb after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for 06Cr18Ni11Nb stays refinery HX, chemical steam coils, and welded bundles preferring Nb over Ti.
Corrosion Resistance of GB/T 13296 06Cr18Ni11Nb
Corrosion behaviour of 06Cr18Ni11Nb in boiler/HX service: Nb stabilisation for HAZ integrity; chloride PREN still Mo-free. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni11Nb unless the mark is on the exemption list. Medium risk note: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
If operating chlorides, temperature, or under-deposit geometry change after award, reopen the alloy choice for 06Cr18Ni11Nb rather than relying on wall thickness alone. Apps: refinery HX, chemical steam coils, and welded bundles preferring Nb over Ti. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr18Ni11Nb rather than relying on wall thickness alone. Weld-shop note tied to 06Cr18Ni11Nb: 347/308L fillers; keep Nb strategy on repairs.
Applications of GB/T 13296 06Cr18Ni11Nb Seamless Tube
Typical applications for GB/T 13296 06Cr18Ni11Nb: refinery HX, chemical steam coils, and welded bundles preferring Nb over Ti. Duty summary: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. SHH STEEL can produce and supply the sizes and tests those packages need when the mill schedule allows. Spool fabricators should copy 06Cr18Ni11Nb onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 06Cr18Ni11Nb remains W-C HX with optional stabilisation heat treatment.
Spool and bundle fabricators should copy 06Cr18Ni11Nb onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Role: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. Commissioning teams benefit when the as-built dossier repeats 06Cr18Ni11Nb beside heat numbers, linking isometric revisions to the same mill certificates. Keep the 06Cr18Ni11Nb caution visible here: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
Weldability of GB/T 13296 06Cr18Ni11Nb
Weldability of 06Cr18Ni11Nb: 347/308L fillers; keep Nb strategy on repairs. Procedure qualification should use the same product form and wall class as production, including the seamless finish that will ship. Caution: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows. Procedure qualification for 06Cr18Ni11Nb should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 06Cr18Ni11Nb caution visible here: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
Shielding-gas and purge notes for 06Cr18Ni11Nb stay with the WPS package so site crews cannot improvise. Apps: refinery HX, chemical steam coils, and welded bundles preferring Nb over Ti. Consumable lot control and shielding-gas notes for 06Cr18Ni11Nb stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 06Cr18Ni11Nb caution visible here: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
Surface Finishes for GB/T 13296 06Cr18Ni11Nb
Iron-free handling after pickle matters for 06Cr18Ni11Nb — carbon-steel strapping stains show up later as rust blooms on finished tube. Standard route is solution annealed and pickled when HT is specified; polish scope must name the surface. Apps: refinery HX, chemical steam coils, and welded bundles preferring Nb over Ti
– Caution locked in What-is / Corrosion / FAQ: Nb 10C–1.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
OD stencil ink on 06Cr18Ni11Nb should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows. Close bundles only after free-iron and burn marks are cleared. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 06Cr18Ni11Nb.
Inspection and Testing for GB/T 13296 06Cr18Ni11Nb
Inspection for 06Cr18Ni11Nb includes melt analysis, tensile tests, hydrostatic or eddy-current E3H, ultrasonic U2, and size/straightness checks. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni11Nb unless the mark is on the exemption list. Flattening applies for wall ≤10 mm; flaring for D≤150 mm and wall ≤10 mm.
Non-conforming 06Cr18Ni11Nb lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Documents: GB/T 2102 / EN 10204 3.1 style as ordered. Non-conforming 06Cr18Ni11Nb lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Corrosion framing beside 06Cr18Ni11Nb: Nb stabilisation for HAZ integrity; chloride PREN still Mo-free.
Packaging and Shipping for GB/T 13296 06Cr18Ni11Nb
Packaging for 06Cr18Ni11Nb uses capped ends, wrapped bundles or wooden crates, and waterproof protection matched to the voyage. Bundle tickets repeat grade, heat, size, and quantity. Size hint: W-C HX with optional stabilisation heat treatment. Bundle tickets for 06Cr18Ni11Nb repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 06Cr18Ni11Nb caution visible here: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
Marking on 06Cr18Ni11Nb includes standard, grade, heat number, size, and manufacture symbol so site receiving can match crates to the packing list without opening every wrap. Desiccant and wrap choices for 06Cr18Ni11Nb follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 06Cr18Ni11Nb: 347/308L fillers; keep Nb strategy on repairs.
SHH STEEL can adjust crate schedules for 06Cr18Ni11Nb when staggered retubing deliveries are on the project calendar. Weld-shop note: 347/308L fillers; keep Nb strategy on repairs. Claims handling for 06Cr18Ni11Nb starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the 06Cr18Ni11Nb caution visible here: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows.
Why Choose SHH STEEL
SHH STEEL can produce and supply GB/T 13296 06Cr18Ni11Nb against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Duty: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. SHH STEEL can produce and supply 06Cr18Ni11Nb against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Corrosion framing beside 06Cr18Ni11Nb: Nb stabilisation for HAZ integrity; chloride PREN still Mo-free.
SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr18Ni11Nb when the mill schedule allows. Sisters on the same hub: 07Cr18Ni11Nb, 06Cr18Ni11Ti, 06Cr19Ni10, 06Cr17Ni12Mo2Ti. SHH STEEL can make 06Cr18Ni11Nb to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Weld-shop note tied to 06Cr18Ni11Nb: 347/308L fillers; keep Nb strategy on repairs.
Supply Capability
SHH STEEL can produce and supply GB/T 13296 06Cr18Ni11Nb seamless tube to the enquiry size list with Table 3 chemistry, Table 4 heat treatment and tensile floors, and the NDT/hydro stack the datasheet names. Role: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr18Ni11Nb when the mill schedule allows. Size practice for 06Cr18Ni11Nb remains W-C HX with optional stabilisation heat treatment.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 06Cr18Ni11Nb (S34778) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes: SHH STEEL can supply 06Cr18Ni11Nb in common HX OD×min-wall bands and boiler straight lengths; non-stock walls and U-bend radii are rolled to order. Confirm W-C versus W-H before booking. Duty: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr18Ni11Nb once design pressure and corrosion allowance are clear. Corrosion framing beside 06Cr18Ni11Nb: Nb stabilisation for HAZ integrity; chloride PREN still Mo-free.
SHH STEEL can produce trial bends and qualification lengths of 06Cr18Ni11Nb ahead of bulk release when the exchanger fabricator needs WPS coupons. Weld-shop: 347/308L fillers; keep Nb strategy on repairs. SHH STEEL can produce trial lengths of 06Cr18Ni11Nb for procedure qualification before bulk release when the project calendar needs it. Application context for 06Cr18Ni11Nb stays refinery HX, chemical steam coils, and welded bundles preferring Nb over Ti.
FAQ
-
What is GB/T 13296 06Cr18Ni11Nb seamless stainless steel tube used for?
- GB/T 13296 06Cr18Ni11Nb is seamless stainless tube for boilers and heat exchangers — refinery HX, chemical steam coils, and welded bundles preferring Nb over Ti. Role summary: Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. It is a Chinese product standard grade (S34778), not an automatic ASTM A213 certificate.
-
Is GB/T 13296 06Cr18Ni11Nb seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr18Ni11Nb when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 06Cr18Ni11Nb?
- 06Cr18Ni11Nb is delivered solution annealed under GB/T 13296. Table 4 reference: 980–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr18Ni11Nb so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr18Ni11Nb compare with sister grades 07Cr18Ni11Nb, 06Cr18Ni11Ti, 06Cr19Ni10?
- 06Cr18Ni11Nb is filed as austenitic. Typical sisters on the same RFQ are 07Cr18Ni11Nb, 06Cr18Ni11Ti, 06Cr19Ni10. Design caution: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr18Ni11Nb?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 347 / UNS S34778 the same as ordering 06Cr18Ni11Nb?
- No. 347 / UNS S34778 is a commercial / UNS cross-walk for body text (unified S34778). The purchase order should lock GB/T 13296 and 06Cr18Ni11Nb so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 06Cr18Ni11Nb?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr18Ni11Nb within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: W-C HX with optional stabilisation heat treatment. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 06Cr18Ni11Nb be welded on site?
- Shop guidance: 347/308L fillers; keep Nb strategy on repairs. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr18Ni11Nb?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Nb 10C–1.10 is identity; solution band 980–1150 °C differs from many 18-8 rows Sister pointers: 07Cr18Ni11Nb, 06Cr18Ni11Ti, 06Cr19Ni10. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 06Cr18Ni11Nb with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr18Ni11Nb does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 06Cr18Ni11Nb?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr18Ni11Nb when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 06Cr18Ni11Nb is seamless stainless steel tube for boilers and heat exchangers — Nb-stabilised 18-8 austenitic tube for weld-decay resistance with niobium rather than titanium. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 07Cr18Ni11Nb, 06Cr18Ni11Ti, 06Cr19Ni10. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.