What is GB/T 13296 06Cr19Ni10 Seamless Stainless Steel Tube
GB/T 13296-2023 is the Chinese national standard for seamless stainless steel tubes for boilers and heat exchangers — replacing the 2013 edition. Grade 06Cr19Ni10 (unified number S30408) sits in the austenitic set. It is the default Chinese 304-class mark under GB/T 13296, not an automatic ASTM A213 TP304 certificate.
SHH STEEL can produce and supply GB/T 13296 06Cr19Ni10 as seamless W-C or W-H tube across the enquiry OD×wall band, heat-treated per Table 4, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum.
Shop language may still say “304 tube,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 13296 and 06Cr19Ni10 so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: welded corrosive service near the 0.08% C ceiling prefers 022Cr19Ni10 or a stabilised sister rather than stretching wall alone.
Scope discipline: 06Cr19Ni10 is seamless boiler/HX tube under GB/T 13296, not fluid-transport pipe under GB/T 14976 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include 022Cr19Ni10, 07Cr19Ni10, 06Cr19Ni10N, 12Cr18Ni9. Role reminder: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum.
Inside this GB/T 13296 series, compare GB/T 13296 022Cr19Ni10, GB/T 13296 07Cr19Ni10, GB/T 13296 06Cr19Ni10N, GB/T 13296 12Cr18Ni9. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP304.
When 06Cr19Ni10 pipe sits beside plate on the same BOM, the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 3280 06Cr19Ni10. See also the GB/T 4237 hub for related plate designations. Keep 06Cr19Ni10 acceptance text on the governing pipe/tube standard.
Chemical Composition of GB/T 13296 06Cr19Ni10
Cast analysis for GB/T 13296 06Cr19Ni10 follows Table 3. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 8.00–11.00, Cr 18.00–20.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 304 / UNS S30408; unified number S30408. Corrosion thread: passive 18-8 film handles aqueous and mild chemical HX media; chloride pitting and under-deposit attack set the first upgrade trigger.
Chemical limits for 06Cr19Ni10 under GB/T 13296-2023 appear in the table underneath. Source priority is the 2023 Table 3 extract (xtd). If your client specification cites a 2013 footnote, send it before the heat is melted. Duty thread: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr19Ni10 before the order is acknowledged. Keep the 06Cr19Ni10 caution visible here: welded corrosive service near the 0.08% C ceiling prefers 022Cr19Ni10 or a stabilised sister rather than stretching wall alone.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 06Cr19Ni10 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.015 | 8.00–11.00 | 18.00–20.00 |
Mechanical Properties of GB/T 13296 06Cr19Ni10
Ambient tensile floors for 06Cr19Ni10 come from GB/T 13296 Table 4: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: welded corrosive service near the 0.08% C ceiling prefers 022Cr19Ni10 or a stabilised sister rather than stretching wall alone.
Hardness testing is by agreement for wall ≥1.7 mm; Table 5 bands differ for special marks such as 06Cr18Ni13Si4 and the high-Mo austenitics. Density reference for 06Cr19Ni10 is 7.93 kg/dm³. Hydrostatic proof uses P=2SR/D with R at 60% of Table 4 Rp0.2, capped at 20 MPa.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 06Cr19Ni10 | 520 | 205 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 06Cr19Ni10. Heat treatment (Table 4): 1010–1150 °C, rapid cool. Density 7.93 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 06Cr19Ni10
Seamless is not optional wording for 06Cr19Ni10: the standard limits manufacture to W-C or W-H seamless routes for boiler and heat-exchanger tube. Pick W-C when OD precision and U-bend finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 13296 line item. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.
Steelmaking for 06Cr19Ni10 is electric-arc or converter with secondary refining, or electroslag remelting. Pickling follows heat treatment unless bright protective-atmosphere practice or overall machining allows omission. Size practice: W-C mid-bore OD×min wall for straight lengths and U-bends; W-H when tonnage and thicker wall favour hot finish. Pickling or bright-anneal decisions for 06Cr19Ni10 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Size practice for 06Cr19Ni10 remains W-C mid-bore OD×min wall for straight lengths and U-bends; W-H when tonnage and thicker wall favour hot finish.
Eddy-current testing to GB/T 7735 E3H may replace hydrostatic proof when agreed; ultrasonic testing to GB/T 5777 U2 remains a standard acceptance path for 06Cr19Ni10. Role: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. Hydrostatic pressure or eddy-current class for 06Cr19Ni10 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Weld-shop note tied to 06Cr19Ni10: 308/308L fillers; purge and heat-input control matter when the tube stays in corrosive condensate.
Dimensions and Tolerances for GB/T 13296 06Cr19Ni10
Dimensions and tolerances for 06Cr19Ni10 follow GB/T 13296 Table 1. Usual length is 2000–12000 mm. W-H OD tolerance is ±1.25%D for D≤140 mm and ±1%D above; W-C uses absolute OD bands from ±0.10 mm (D≤25) up through ±0.5%D for D>159 mm. Size hint: W-C mid-bore OD×min wall for straight lengths and U-bends; W-H when tonnage and thicker wall favour hot finish.
Out-of-roundness and wall unevenness for 06Cr19Ni10 shall not exceed 80% of the OD and wall tolerances respectively. Full-length camber ≤0.15% of tube length. Duty: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. Fixed lengths and multiple cut lengths for 06Cr19Ni10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 06Cr19Ni10 duty: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum.
Equivalent Grades for GB/T 13296 06Cr19Ni10
Under GB/T 13296, 06Cr19Ni10 is the governing seamless stainless boiler / heat-exchanger tube designation on this page. Commercial shorthand such as 304 / UNS S30408 helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the GB/T 13296 06Cr19Ni10 line. ASTM A213 / A269 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 06Cr19Ni10 | Governing tube grade for this page |
| Commercial / UNS (body only) | 304 / UNS S30408 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | 304 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Read the notes column literally for 06Cr19Ni10: related chemistry is not automatic dual-cert. Cross-check GB/T 13296 022Cr19Ni10, GB/T 13296 07Cr19Ni10, GB/T 13296 06Cr19Ni10N, GB/T 13296 12Cr18Ni9 when Mo, stabilisation, or carbon ceilings change the selection. Hub: GB/T 13296. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (06Cr19Ni10).
Heat Treatment and Delivery Condition for GB/T 13296 06Cr19Ni10
Heat treatment for 06Cr19Ni10 follows Table 4: 1010–1150 °C, rapid cool. Delivery condition: solution annealed. SHH STEEL records furnace charts that support the temperature and cool method claimed on the certificate. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr19Ni10 unless the mark is on the exemption list.
Field heat treatment of 06Cr19Ni10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr19Ni10 unless the mark is on the exemption list. Field heat treatment of 06Cr19Ni10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 06Cr19Ni10 remains W-C mid-bore OD×min wall for straight lengths and U-bends; W-H when tonnage and thicker wall favour hot finish.
Corrosion Resistance of GB/T 13296 06Cr19Ni10
Corrosion behaviour of 06Cr19Ni10 in boiler/HX service: passive 18-8 film handles aqueous and mild chemical HX media; chloride pitting and under-deposit attack set the first upgrade trigger. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr19Ni10 unless the mark is on the exemption list. Medium risk note: welded corrosive service near the 0.08% C ceiling prefers 022Cr19Ni10 or a stabilised sister rather than stretching wall alone.
If operating chlorides, temperature, or under-deposit geometry change after award, reopen the alloy choice for 06Cr19Ni10 rather than relying on wall thickness alone. Apps: feedwater heaters, condenser tubes in mild water, steam coils, and plant HX bundles that still say “304 seamless”. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr19Ni10 rather than relying on wall thickness alone. Corrosion framing beside 06Cr19Ni10: passive 18-8 film handles aqueous and mild chemical HX media; chloride pitting and under-deposit attack set the first upgrade trigger.
Applications of GB/T 13296 06Cr19Ni10 Seamless Tube
Typical applications for GB/T 13296 06Cr19Ni10: feedwater heaters, condenser tubes in mild water, steam coils, and plant HX bundles that still say “304 seamless”. Duty summary: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. SHH STEEL can produce and supply the sizes and tests those packages need when the mill schedule allows.
Spool and bundle fabricators should copy 06Cr19Ni10 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Role: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. Commissioning teams benefit when the as-built dossier repeats 06Cr19Ni10 beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to 06Cr19Ni10 duty: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum.
Weldability of GB/T 13296 06Cr19Ni10
Weldability of 06Cr19Ni10: 308/308L fillers; purge and heat-input control matter when the tube stays in corrosive condensate. Procedure qualification should use the same product form and wall class as production, including the seamless finish that will ship. Caution: welded corrosive service near the 0.08% C ceiling prefers 022Cr19Ni10 or a stabilised sister rather than stretching wall alone.
Shielding-gas and purge notes for 06Cr19Ni10 stay with the WPS package so site crews cannot improvise. Apps: feedwater heaters, condenser tubes in mild water, steam coils, and plant HX bundles that still say “304 seamless”. Consumable lot control and shielding-gas notes for 06Cr19Ni10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 06Cr19Ni10 duty: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum.
Surface Finishes for GB/T 13296 06Cr19Ni10
Typical GB/T 13296 supply for 06Cr19Ni10 is a clean pickle after the required heat treatment, with bright anneal reserved for scale-free OD/ID appearance and ground/polished finishes reserved for written roughness targets. Free-iron control starts at the finishing bay, not at commissioning. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (06Cr19Ni10).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Reject grinding burns, embedded free iron, and unrepaired undercut on 06Cr19Ni10 before bundles close. Passivation analogues (A967-style) are optional extras — the governing step remains correct heat treatment under GB/T 13296 for this austenitic mark. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 06Cr19Ni10.
Inspection and Testing for GB/T 13296 06Cr19Ni10
Inspection for 06Cr19Ni10 includes melt analysis, tensile tests, hydrostatic or eddy-current E3H, ultrasonic U2, and size/straightness checks. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr19Ni10 unless the mark is on the exemption list. Flattening applies for wall ≤10 mm; flaring for D≤150 mm and wall ≤10 mm.
Non-conforming 06Cr19Ni10 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Documents: GB/T 2102 / EN 10204 3.1 style as ordered. Non-conforming 06Cr19Ni10 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. This paragraph is locked to 06Cr19Ni10 duty: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum.
Packaging and Shipping for GB/T 13296 06Cr19Ni10
Packaging for 06Cr19Ni10 uses capped ends, wrapped bundles or wooden crates, and waterproof protection matched to the voyage. Bundle tickets repeat grade, heat, size, and quantity. Size hint: W-C mid-bore OD×min wall for straight lengths and U-bends; W-H when tonnage and thicker wall favour hot finish. Bundle tickets for 06Cr19Ni10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 06Cr19Ni10: passive 18-8 film handles aqueous and mild chemical HX media; chloride pitting and under-deposit attack set the first upgrade trigger.
Marking on 06Cr19Ni10 includes standard, grade, heat number, size, and manufacture symbol so site receiving can match crates to the packing list without opening every wrap. Desiccant and wrap choices for 06Cr19Ni10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. This paragraph is locked to 06Cr19Ni10 duty: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum.
SHH STEEL can adjust crate schedules for 06Cr19Ni10 when staggered retubing deliveries are on the project calendar. Weld-shop note: 308/308L fillers; purge and heat-input control matter when the tube stays in corrosive condensate. Claims handling for 06Cr19Ni10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 06Cr19Ni10 stays feedwater heaters, condenser tubes in mild water, steam coils, and plant HX bundles that still say “304 seamless”.
Why Choose SHH STEEL
SHH STEEL can produce and supply GB/T 13296 06Cr19Ni10 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Duty: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. SHH STEEL can produce and supply 06Cr19Ni10 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Weld-shop note tied to 06Cr19Ni10: 308/308L fillers; purge and heat-input control matter when the tube stays in corrosive condensate.
SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr19Ni10 when the mill schedule allows. Sisters on the same hub: 022Cr19Ni10, 07Cr19Ni10, 06Cr19Ni10N, 12Cr18Ni9. SHH STEEL can make 06Cr19Ni10 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Corrosion framing beside 06Cr19Ni10: passive 18-8 film handles aqueous and mild chemical HX media; chloride pitting and under-deposit attack set the first upgrade trigger.
Supply Capability
SHH STEEL can produce and supply GB/T 13296 06Cr19Ni10 seamless tube to the enquiry size list with Table 3 chemistry, Table 4 heat treatment and tensile floors, and the NDT/hydro stack the datasheet names. Role: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr19Ni10 when the mill schedule allows. Keep the 06Cr19Ni10 caution visible here: welded corrosive service near the 0.08% C ceiling prefers 022Cr19Ni10 or a stabilised sister rather than stretching wall alone.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 06Cr19Ni10 (S30408) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes: SHH STEEL can supply 06Cr19Ni10 in common HX OD×min-wall bands and boiler straight lengths; non-stock walls and U-bend radii are rolled to order. Confirm W-C versus W-H before booking. Duty: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr19Ni10 once design pressure and corrosion allowance are clear. Size practice for 06Cr19Ni10 remains W-C mid-bore OD×min wall for straight lengths and U-bends; W-H when tonnage and thicker wall favour hot finish.
SHH STEEL can produce trial bends and qualification lengths of 06Cr19Ni10 ahead of bulk release when the exchanger fabricator needs WPS coupons. Weld-shop: 308/308L fillers; purge and heat-input control matter when the tube stays in corrosive condensate. SHH STEEL can produce trial lengths of 06Cr19Ni10 for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to 06Cr19Ni10: 308/308L fillers; purge and heat-input control matter when the tube stays in corrosive condensate.
FAQ
-
What is GB/T 13296 06Cr19Ni10 seamless stainless steel tube used for?
- GB/T 13296 06Cr19Ni10 is seamless stainless tube for boilers and heat exchangers — feedwater heaters, condenser tubes in mild water, steam coils, and plant HX bundles that still say “304 seamless”. Role summary: workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. It is a Chinese product standard grade (S30408), not an automatic ASTM A213 certificate.
-
Is GB/T 13296 06Cr19Ni10 seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr19Ni10 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 06Cr19Ni10?
- 06Cr19Ni10 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr19Ni10 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr19Ni10 compare with sister grades 022Cr19Ni10, 07Cr19Ni10, 06Cr19Ni10N?
- 06Cr19Ni10 is filed as austenitic. Typical sisters on the same RFQ are 022Cr19Ni10, 07Cr19Ni10, 06Cr19Ni10N. Design caution: welded corrosive service near the 0.08% C ceiling prefers 022Cr19Ni10 or a stabilised sister rather than stretching wall alone Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr19Ni10?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 304 / UNS S30408 the same as ordering 06Cr19Ni10?
- No. 304 / UNS S30408 is a commercial / UNS cross-walk for body text (unified S30408). The purchase order should lock GB/T 13296 and 06Cr19Ni10 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 06Cr19Ni10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr19Ni10 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: W-C mid-bore OD×min wall for straight lengths and U-bends; W-H when tonnage and thicker wall favour hot finish. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 06Cr19Ni10 be welded on site?
- Shop guidance: 308/308L fillers; purge and heat-input control matter when the tube stays in corrosive condensate. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: welded corrosive service near the 0.08% C ceiling prefers 022Cr19Ni10 or a stabilised sister rather than stretching wall alone
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr19Ni10?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: welded corrosive service near the 0.08% C ceiling prefers 022Cr19Ni10 or a stabilised sister rather than stretching wall alone Sister pointers: 022Cr19Ni10, 07Cr19Ni10, 06Cr19Ni10N. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 06Cr19Ni10 with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr19Ni10 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 06Cr19Ni10?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr19Ni10 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 06Cr19Ni10 is seamless stainless steel tube for boilers and heat exchangers — workhorse 18-8 austenitic seamless tube for Chinese boiler and heat-exchanger specs without molybdenum. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr19Ni10, 07Cr19Ni10, 06Cr19Ni10N. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.