GB/T 13296 06Cr13 Seamless Stainless Steel Tube
What is GB/T 13296 06Cr13 Seamless Stainless Steel Tube
GB/T 13296 covers seamless stainless tube for boiler and HX service — cold-drawn or hot-finished — with hydrostatic proof, ultrasonic U2, flattening and flaring where size allows. Inside that standard, 06Cr13 is filed as ferritic. It anchors the low-chromium ferritic end of GB/T 13296.
From pierce/extrude/draw through marking and crate protection, SHH STEEL can produce GB/T 13296 06Cr13 for the sizes and tests on your RFQ. Application sketch: low-pressure heaters, mild condensate coolers, and utility HX where 12% Cr suffices. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr13 before production starts. Corrosion framing beside 06Cr13: modest Cr film for mild aqueous media; chlorides and weld HAZ need care.
On the floor people shorten marks; in QA they must not. 06Cr13 under GB/T 13296 carries specific Table 3 windows and Table 4 floors that a loose “410S-class” note will not enforce. Caution: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change.
Annex A elevated Rp0.2 and Annex B rupture data apply only to named H marks; still match the alloy to the medium. For 06Cr13, that means: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series. Nearby marks: 10Cr17, 008Cr27Mo, 06Cr19Ni10.
Inside this GB/T 13296 series, compare GB/T 13296 10Cr17, GB/T 13296 008Cr27Mo, GB/T 13296 06Cr19Ni10. Hub: GB/T 13296.
When 06Cr13 pipe sits beside plate on the same BOM, link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and GB/T 713.7 S11306 so purchasing does not treat one product form as the other. Flat Chinese grades in-family are indexed at GB/T 4237. Quote 06Cr13 pipe and plate under separate line items.
Chemical Composition of GB/T 13296 06Cr13
For 06Cr13, the melt ticket has to show Table 3 compliance — C ≤0.06, Si ≤1.00, Mn ≤1.00, P ≤0.035, S ≤0.015, Ni ≤0.60, Cr 11.50–13.50. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: modest Cr film for mild aqueous media; chlorides and weld HAZ need care.
Where Mo, Cu, Ti, Nb or N appear, they are intentional levers for 06Cr13, not optional marketing. Confirm them on the MTC line-by-line. Role: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr13 before the order is acknowledged. Application context for 06Cr13 stays low-pressure heaters, mild condensate coolers, and utility HX where 12% Cr suffices.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 06Cr13 | ≤0.06 | ≤1.00 | ≤1.00 | ≤0.035 | ≤0.015 | ≤0.60 | 11.50–13.50 |
Mechanical Properties of GB/T 13296 06Cr13
Do not confuse Table 4 tube tensile floors with pipe or plate standards that share the 410S-class / UNS S11306 alias. For 06Cr13 under 13296 expect Rm min 410 MPa, Rp0.2 min 210 MPa, elongation min 20%, verified per heat/lot rules. Note: filed ferritic in xtd Table 3 note. Tensile sampling follows the batch rules for the ordered test unit of 06Cr13, and retests follow GB/T 2102 when a result sits under the Table 4 floor. This paragraph is locked to 06Cr13 duty: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series.
When wall class changes the ordered tensile specimen orientation, keep the acknowledgement aligned for 06Cr13. Reference density 7.75 kg/dm³; delivery annealed.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 06Cr13 | 410 | 210 | 20 |
Ambient values from GB/T 13296-2023 Table 4 for 06Cr13. Heat treatment (Table 4): 900–1050 °C, air or slow cool. filed ferritic in xtd Table 3 note. Density 7.75 kg/dm³. Delivery: annealed.
Seamless Tube Manufacture of GB/T 13296 06Cr13
For 06Cr13, the mill path is pierce / extrude / draw — never ERW or automatic-arc under GB/T 13296. Delivery is heat-treated and pickled unless overall ground/bored or protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Ferritic heats follow Table 4 anneal bands with air or slow cool as listed — not austenitic solution practice. Do not copy 06Cr19Ni10 furnace charts onto ferritic marks. Seamless W-C and W-H routes are the only valid order paths for 06Cr13 under GB/T 13296.
U-bend and cut-to-length options for 06Cr13 are available by agreement after the straight-tube tests clear. Surface quality rejects cracks, folds, laps, laminations and scabs on ID and OD. Pickling or bright-anneal decisions for 06Cr13 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Weld-shop note tied to 06Cr13: 410S/ferritic fillers; avoid hard HAZ from wrong cool rates.
Manufacture records for 06Cr13 keep heat identity unbroken from melt through final NDT so the MTC can cite one cast for the whole bundle. Hydrostatic pressure or eddy-current class for 06Cr13 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Size practice for 06Cr13 remains straight utility lengths; limited U-bend unless toughness proven.
Dimensions and Tolerances for GB/T 13296 06Cr13
Cut lengths, multiple lengths, and U-bend developed lengths for 06Cr13 need explicit acknowledgement so finishing and crate length match the tubesheet drawing. Caution: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change. Tolerance basis for 06Cr13 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 06Cr13 duty: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series.
Tolerance class follows the manufacture route ordered for 06Cr13; swapping W-C for W-H after acknowledgement without a dimensional review is how fit-up fails at the exchanger shop. Fixed lengths and multiple cut lengths for 06Cr13 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for 06Cr13 remains straight utility lengths; limited U-bend unless toughness proven.
Equivalent Grades for GB/T 13296 06Cr13
Lock 06Cr13 on the PO when the datasheet owner wants GB/T 13296 seamless stainless boiler / heat-exchanger tube. Commercial talk as 410S-class / UNS S11306 is fine in emails; mill paperwork must still show GB/T 13296 06Cr13. This mark sits in the ferritic band of the series. Dual marking is a purchase-order option that still requires every limit that matters for 06Cr13 to be verified on the heat.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 06Cr13 | Governing tube grade for this page |
| Commercial / UNS (body only) | 410S-class / UNS S11306 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Read the notes column literally for 06Cr13: related chemistry is not automatic dual-cert. Cross-check GB/T 13296 10Cr17, GB/T 13296 008Cr27Mo, GB/T 13296 06Cr19Ni10 when Mo, stabilisation, or carbon ceilings change the selection. Hub: GB/T 13296. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (06Cr13).
Heat Treatment and Delivery Condition for GB/T 13296 06Cr13
Stabilisation after solution anneal is available by agreement for Ti/Nb marks; confirm whether 06Cr13 needs that second hold before acknowledging. HT reference: 900–1050 °C, air or slow cool. Recorded furnace charts for 06Cr13 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 06Cr13 duty: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series.
Mixed bundles of different heat-treatment furnace lots of 06Cr13 stay segregated so sampling remains traceable to one Table 4 run. Field heat treatment of 06Cr13 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 06Cr13: modest Cr film for mild aqueous media; chlorides and weld HAZ need care.
Corrosion Resistance of GB/T 13296 06Cr13
Coupon orientation, weld condition, and surface finish for 06Cr13 belong in the corrosion test order so method E or other coupons compare honestly to the installed tube. IGC clause 9 targets austenitic marks; for ferritic 06Cr13, corrosion testing follows the duty file rather than automatic method E. Coupon orientation, weld condition, and surface finish for 06Cr13 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Keep the 06Cr13 caution visible here: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change.
For 06Cr13, specify whether IGC, hardness, or special corrosion coupons are extras beyond the clause 9 default before the heat is melted. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr13 rather than relying on wall thickness alone. This paragraph is locked to 06Cr13 duty: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series.
Applications of GB/T 13296 06Cr13 Seamless Tube
Commissioning dossiers should repeat 06Cr13 beside heat numbers so as-built isometrics stay tied to the same mill certificates. Application thread: low-pressure heaters, mild condensate coolers, and utility HX where 12% Cr suffices. Spool fabricators should copy 06Cr13 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside 06Cr13: modest Cr film for mild aqueous media; chlorides and weld HAZ need care.
Spare-tube stocks of 06Cr13 should keep heat identity so later retubing matches the original corrosion and strength file. Apps: low-pressure heaters, mild condensate coolers, and utility HX where 12% Cr suffices. Commissioning teams benefit when the as-built dossier repeats 06Cr13 beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside 06Cr13: modest Cr film for mild aqueous media; chlorides and weld HAZ need care.
Weldability of GB/T 13296 06Cr13
Repair welding of 06Cr13 must preserve grade identity — a 308 deposit on a 6% Mo tube is a corrosion failure waiting to happen. Note: 410S/ferritic fillers; avoid hard HAZ from wrong cool rates. Procedure qualification for 06Cr13 should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 06Cr13 remains straight utility lengths; limited U-bend unless toughness proven.
Tubesheet joint design for 06Cr13 should state strength weld versus seal weld and any expansion sequence before production welding starts. Consumable lot control and shielding-gas notes for 06Cr13 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 06Cr13: 410S/ferritic fillers; avoid hard HAZ from wrong cool rates.
Surface Finishes for GB/T 13296 06Cr13
06Cr13 under GB/T 13296 typically ships annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series.
| Finish | Typical supply | Order note |
|---|---|---|
| Annealed and pickled | Standard tube mill finish after anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; inspect before polish on ferritic stock |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Do not polish over unresolved defects on 06Cr13; inspection comes before cosmetics. Passivation after pickle or shop welding is good practice in chloride-lean service, but GB/T 13296 acceptance still rests on correct heat treatment. Pack away from carbon-steel contact. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (06Cr13).
Inspection and Testing for GB/T 13296 06Cr13
Hardness by agreement for wall ≥1.7 mm on 06Cr13; grain-size evidence when the mark requires levels 4–7. Apps: low-pressure heaters, mild condensate coolers, and utility HX where 12% Cr suffices. Sampling plans for 06Cr13 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for 06Cr13 stays low-pressure heaters, mild condensate coolers, and utility HX where 12% Cr suffices.
Dimensional reports for 06Cr13 cite Table 1 tolerance basis (W-C vs W-H, min wall vs nominal wall) so receiving inspectors know which band applies. Non-conforming 06Cr13 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Keep the 06Cr13 caution visible here: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change.
Packaging and Shipping for GB/T 13296 06Cr13
U-bend crates for 06Cr13 need radius supports so cold-worked bends do not spring or scar in transit. Caution: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change. Bundle tickets for 06Cr13 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for 06Cr13 remains straight utility lengths; limited U-bend unless toughness proven.
Long-term storage of 06Cr13 should keep bundles dry and off bare soil to protect the pickled surface before installation. Caution: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change. Desiccant and wrap choices for 06Cr13 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 06Cr13 remains straight utility lengths; limited U-bend unless toughness proven.
Packing lists for 06Cr13 cite net/gross weight and crate count so logistics and QA share one document set. Caution: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change. Claims handling for 06Cr13 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 06Cr13 remains straight utility lengths; limited U-bend unless toughness proven.
Why Choose SHH STEEL
Traceability, pickle quality, and size discipline on 06Cr13 are part of the supply promise, not brochure extras. Role: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series. SHH STEEL can produce and supply 06Cr13 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Corrosion framing beside 06Cr13: modest Cr film for mild aqueous media; chlorides and weld HAZ need care.
For 06Cr13, SHH STEEL can produce trial lengths for procedure qualification before bulk release when the project calendar needs it. Apps: low-pressure heaters, mild condensate coolers, and utility HX where 12% Cr suffices. SHH STEEL can make 06Cr13 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Weld-shop note tied to 06Cr13: 410S/ferritic fillers; avoid hard HAZ from wrong cool rates.
Supply Capability
From RFQ to crate, SHH STEEL can produce 06Cr13 as a boiler/HX product — not a repurposed fluid-pipe heat. Size hint: straight utility lengths; limited U-bend unless toughness proven. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr13 when the mill schedule allows. This paragraph is locked to 06Cr13 duty: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 06Cr13 (S11306) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes — SHH STEEL can supply alternate walls for 06Cr13 once design pressure, corrosion allowance, and min-wall rules are clear. Size hint: straight utility lengths; limited U-bend unless toughness proven. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr13 once design pressure and corrosion allowance are clear. Keep the 06Cr13 caution visible here: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change.
Export packing and document sets for 06Cr13 are confirmed on the acknowledgement so customs and site QA see the same grade string. Caution: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change. SHH STEEL can produce trial lengths of 06Cr13 for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to 06Cr13: 410S/ferritic fillers; avoid hard HAZ from wrong cool rates.
FAQ
-
What is GB/T 13296 06Cr13 seamless stainless steel tube used for?
- GB/T 13296 06Cr13 is seamless stainless tube for boilers and heat exchangers — low-pressure heaters, mild condensate coolers, and utility HX where 12% Cr suffices. Role summary: 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series. It is a Chinese product standard grade (S11306), not an automatic ASTM A213 certificate.
-
Is GB/T 13296 06Cr13 seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr13 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 06Cr13?
- 06Cr13 is delivered annealed under GB/T 13296. Table 4 reference: 900–1050 °C, air or slow cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr13 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr13 compare with sister grades 10Cr17, 008Cr27Mo, 06Cr19Ni10?
- 06Cr13 is filed as ferritic. Typical sisters on the same RFQ are 10Cr17, 008Cr27Mo, 06Cr19Ni10. Design caution: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr13?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 410S-class / UNS S11306 the same as ordering 06Cr13?
- No. 410S-class / UNS S11306 is a commercial / UNS cross-walk for body text (unified S11306). The purchase order should lock GB/T 13296 and 06Cr13 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 06Cr13?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr13 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: straight utility lengths; limited U-bend unless toughness proven. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 06Cr13 be welded on site?
- Shop guidance: 410S/ferritic fillers; avoid hard HAZ from wrong cool rates. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr13?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: filed ferritic in xtd — do not heat-treat as martensitic boiler tube without a written schedule change Sister pointers: 10Cr17, 008Cr27Mo, 06Cr19Ni10. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 06Cr13 with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr13 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 06Cr13?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr13 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 06Cr13 is seamless stainless steel tube for boilers and heat exchangers — 12% Cr ferritic tube for mild boiler/HX and utility exchangers at the low-alloy end of the series. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 10Cr17, 008Cr27Mo, 06Cr19Ni10. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.