GB/T 13296 008Cr27Mo Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 008Cr27Mo Seamless Stainless Steel Tube

GB/T 13296 008Cr27Mo seamless stainless steel tube (XM27 / UNS S44627-related, S12791), ferritic, Table 3 cast analysis, Rm min 410 MPa / Rp0.2 min 245 MPa, annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
008Cr27Mo (S12791 / XM27 / UNS S44627-related — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 008Cr27Mo Seamless Stainless Steel Tube

When the approved vendor list and exchanger datasheet say GB/T 13296, the grade mark has to be the Chinese designation. 008Cr27Mo is the full product grade for this ferritic seamless tube. It is the high-purity Mo ferritic mark in this boiler/HX series.

SHH STEEL can supply 008Cr27Mo seamless tube in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the exchanger: ultra-low-carbon high-Cr Mo ferritic tube for chloride-resistant HX without austenitic nickel. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 008Cr27Mo before production starts. Application context for 008Cr27Mo stays chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

Equivalence talk to XM27 / UNS S44627-related belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 13296 008Cr27Mo, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity.

Related ASTM A213 tube pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 10Cr17, 06Cr13, 015Cr20Ni18Mo6CuN. Use thread: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

Inside this GB/T 13296 series, compare GB/T 13296 10Cr17, GB/T 13296 06Cr13, GB/T 13296 015Cr20Ni18Mo6CuN. Hub: GB/T 13296.

For 008Cr27Mo, vertical navigation stays form-specific — open Stainless Steel Pipes and Tubes for pipes/tubes and Stainless Steel Sheets and Plates for sheets/plates, then use GB/T 4237 008Cr27Mo only when the flat form is required. Confirm 008Cr27Mo OD × wall and plate thickness on separate drawings.

Chemical Composition of GB/T 13296 008Cr27Mo

Chemistry control on 008Cr27Mo starts at the ladle. Expect C ≤0.010, Si ≤0.40, Mn ≤0.40, P ≤0.030, S ≤0.015, Cr 25.00–27.50, Mo 0.75–1.50 within Table 3, reported on the inspection document against the heat. Body alias XM27 / UNS S44627-related does not widen those windows. Every ladle analysis for 008Cr27Mo is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Application context for 008Cr27Mo stays chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

Read the table with the family in mind — ferritic — and with caution C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity. Numbers without the matching Table 4 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 008Cr27Mo before the order is acknowledged. Application context for 008Cr27Mo stays chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

Grade C Si Mn P S Cr Mo
008Cr27Mo ≤0.010 ≤0.40 ≤0.40 ≤0.030 ≤0.015 25.00–27.50 0.75–1.50

Mechanical Properties of GB/T 13296 008Cr27Mo

Proof stress and tensile minima for 008Cr27Mo sit at Rm min 410 MPa, Rp0.2 min 245 MPa, elongation min 20%. Flattening and flaring back ductility when size allows. Watch-out: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity. Tensile sampling follows the batch rules for the ordered test unit of 008Cr27Mo, and retests follow GB/T 2102 when a result sits under the Table 4 floor. Application context for 008Cr27Mo stays chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

Batch size limits (D≤76 mm and S≤3 mm: ≤400 tubes; otherwise ≤200) keep sampling honest for 008Cr27Mo. Retests follow GB/T 2102. Density 7.67 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
008Cr27Mo 410 245 20

Ambient values from GB/T 13296-2023 Table 4 for 008Cr27Mo. Heat treatment (Table 4): ≥1150 °C, rapid cool. Density 7.67 kg/dm³. Delivery: annealed.

Seamless Tube Manufacture of GB/T 13296 008Cr27Mo

Seamless is not optional wording for 008Cr27Mo: the standard limits manufacture to W-C or W-H seamless routes for boiler and heat-exchanger tube. Pick W-C when OD precision and U-bend finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 13296 line item. Ferritic heats follow Table 4 anneal bands with air or slow cool as listed — not austenitic solution practice. Do not copy 06Cr19Ni10 furnace charts onto ferritic marks.

SHH STEEL schedules piercing, elongation, and finishing for 008Cr27Mo against the W-C or W-H symbol frozen on the acknowledgement. Ovality and wall eccentricity stay inside 80% of the respective OD and wall tolerances. Pickling or bright-anneal decisions for 008Cr27Mo stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Size practice for 008Cr27Mo remains straight HX tubes; confirm bend radius with ferritic toughness data.

Cold-finish depth of longitudinal marks on 008Cr27Mo is limited to ≤4% of wall and ≤0.2 mm; hot-finish ≤5% and ≤0.4 mm. Apps: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17. Hydrostatic pressure or eddy-current class for 008Cr27Mo is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Size practice for 008Cr27Mo remains straight HX tubes; confirm bend radius with ferritic toughness data.

Dimensions and Tolerances for GB/T 13296 008Cr27Mo

When 008Cr27Mo ships as nominal wall, the note under Table 1 still applies different ± bands for hot and cold routes — do not mix W-C absolute OD tols with W-H percentage thinking. Practice: straight HX tubes; confirm bend radius with ferritic toughness data. Tolerance basis for 008Cr27Mo follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 008Cr27Mo duty: ultra-low-carbon high-Cr Mo ferritic tube for chloride-resistant HX without austenitic nickel.

Fixed lengths of 008Cr27Mo are end-protected so bevels and ID finish survive inland and ocean transit. Random lengths stay inside the usual 2000–12000 mm window unless agreed otherwise. Fixed lengths and multiple cut lengths for 008Cr27Mo are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 008Cr27Mo: matching Mo-ferritic fillers; strict heat input and contamination control.

Equivalent Grades for GB/T 13296 008Cr27Mo

Do not treat XM27 / UNS S44627-related as interchangeable paperwork for GB/T 13296 008Cr27Mo. Chemistry kinship is not acceptance kinship under this product standard. Hydrostatic, NDT, and heat-treatment text diverge across systems even when the cast analysis looks familiar. Dual marking is a purchase-order option that still requires every limit that matters for 008Cr27Mo to be verified on the heat.

System Designation Notes
GB/T 13296 008Cr27Mo Governing tube grade for this page
Commercial / UNS (body only) XM27 / UNS S44627-related (unified S12791) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

When the service outgrows 008Cr27Mo, move to a sister rather than stretching the alias: GB/T 13296 10Cr17, GB/T 13296 06Cr13, GB/T 13296 015Cr20Ni18Mo6CuN. Apps context: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17
– Caution locked in What-is / Corrosion / FAQ: C≤0. Full list under GB/T 13296. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (008Cr27Mo).

Heat Treatment and Delivery Condition for GB/T 13296 008Cr27Mo

For 008Cr27Mo, solution or anneal practice is not a free mill choice — it is the Table 4 band tied to the grade. Delivery: annealed. Role: ultra-low-carbon high-Cr Mo ferritic tube for chloride-resistant HX without austenitic nickel. Recorded furnace charts for 008Cr27Mo should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 008Cr27Mo duty: ultra-low-carbon high-Cr Mo ferritic tube for chloride-resistant HX without austenitic nickel.

When Annex A elevated Rp0.2 is invoked, the certificate for 008Cr27Mo should still show the Table 4 delivery treatment actually performed. Apps: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17. Field heat treatment of 008Cr27Mo after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for 008Cr27Mo stays chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

Corrosion Resistance of GB/T 13296 008Cr27Mo

Pitting, crevice, oxidation, or weld-decay limiters for 008Cr27Mo should be named in the datasheet rather than inferred from the AISI alias alone. Framing: high Cr+Mo ferritic PREN without nickel; toughness and welding need ferritic procedures. Coupon orientation, weld condition, and surface finish for 008Cr27Mo belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Weld-shop note tied to 008Cr27Mo: matching Mo-ferritic fillers; strict heat input and contamination control.

Pickling quality and free-iron cleanliness after fabrication affect startup corrosion of 008Cr27Mo as much as cast chemistry. Role: ultra-low-carbon high-Cr Mo ferritic tube for chloride-resistant HX without austenitic nickel. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 008Cr27Mo rather than relying on wall thickness alone. Corrosion framing beside 008Cr27Mo: high Cr+Mo ferritic PREN without nickel; toughness and welding need ferritic procedures.

Applications of GB/T 13296 008Cr27Mo Seamless Tube

Use 008Cr27Mo on packages that match chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17. Nearby sisters 10Cr17, 06Cr13, 015Cr20Ni18Mo6CuN cover adjacent media or temperature steps. Weld-shop note: matching Mo-ferritic fillers; strict heat input and contamination control. Spool fabricators should copy 008Cr27Mo onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 008Cr27Mo caution visible here: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity.

When the process medium changes mid-project, revisit whether 008Cr27Mo still fits before releasing more heats. Sisters: 10Cr17, 06Cr13, 015Cr20Ni18Mo6CuN. Commissioning teams benefit when the as-built dossier repeats 008Cr27Mo beside heat numbers, linking isometric revisions to the same mill certificates. Keep the 008Cr27Mo caution visible here: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity.

Weldability of GB/T 13296 008Cr27Mo

Consumable selection for 008Cr27Mo follows matching Mo-ferritic fillers; strict heat input and contamination control. Do not improvise under-alloyed fillers on Mo or Cu grades. Role: ultra-low-carbon high-Cr Mo ferritic tube for chloride-resistant HX without austenitic nickel. Procedure qualification for 008Cr27Mo should use the same product form and wall class as production, including the seamless finish that will ship. Corrosion framing beside 008Cr27Mo: high Cr+Mo ferritic PREN without nickel; toughness and welding need ferritic procedures.

Ferrite control and hot-cracking risk for 008Cr27Mo depend on the family chemistry; qualify on production wall, not only on plate coupons. Weld shop: matching Mo-ferritic fillers; strict heat input and contamination control. Consumable lot control and shielding-gas notes for 008Cr27Mo stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 008Cr27Mo: matching Mo-ferritic fillers; strict heat input and contamination control.

Surface Finishes for GB/T 13296 008Cr27Mo

Surface supply for 008Cr27Mo should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless tube, so finish is part of performance, not only appearance. Application framing: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17
– Caution locked in What-is / Corrosion / FAQ: C≤0. Ambiguous “bright tube” language is clarified before finishing slots are booked.

Finish Typical supply Order note
Annealed and pickled Standard tube mill finish after anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; inspect before polish on ferritic stock
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Passivation restores the chromium-rich film after pickling or light fabrication on 008Cr27Mo; it does not replace the heat treatment that sets mechanical properties under GB/T 13296. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.

Inspection and Testing for GB/T 13296 008Cr27Mo

SHH STEEL keeps heat identity for 008Cr27Mo unbroken from melt through bundle tags, including third-party hold points written into the PO. Caution: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity. Sampling plans for 008Cr27Mo keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 008Cr27Mo: matching Mo-ferritic fillers; strict heat input and contamination control.

Certificate lines for 008Cr27Mo must repeat the Chinese grade, unified number, manufacture symbol, and heat treatment actually performed. Caution: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity. Non-conforming 008Cr27Mo lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 008Cr27Mo: matching Mo-ferritic fillers; strict heat input and contamination control.

Packaging and Shipping for GB/T 13296 008Cr27Mo

Desiccant and wrap choices for 008Cr27Mo follow voyage length and storage climate on the shipping order, not a one-size export habit. Apps: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17. Bundle tickets for 008Cr27Mo repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 008Cr27Mo stays chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

Inland trucking of 008Cr27Mo still needs end protection — most ID dents happen between the port and the exchanger shop. Apps: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17. Desiccant and wrap choices for 008Cr27Mo follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 008Cr27Mo caution visible here: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity.

Barcode or stencil extras for 008Cr27Mo are available when the owner’s material system needs them. Apps: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17. Claims handling for 008Cr27Mo starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 008Cr27Mo stays chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

Why Choose SHH STEEL

SHH STEEL can make 008Cr27Mo to a boiler/HX test stack — hydro or E3H, UT U2, flattening/flaring, IGC when required — instead of a generic stainless tube habit. Apps: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17. SHH STEEL can produce and supply 008Cr27Mo against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Application context for 008Cr27Mo stays chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

SHH STEEL can supply 008Cr27Mo with third-party inspection hold points written into the itinerary. Weld-shop note: matching Mo-ferritic fillers; strict heat input and contamination control. SHH STEEL can make 008Cr27Mo to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Application context for 008Cr27Mo stays chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17.

Supply Capability

SHH STEEL can supply 008Cr27Mo with EN 10204 3.1 style documents, IGC when required, and hardness by agreement. Caution: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 008Cr27Mo when the mill schedule allows. Keep the 008Cr27Mo caution visible here: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 008Cr27Mo (S12791)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes: rolling cycles for 008Cr27Mo cover usual 2000–12000 mm lengths; cut-to-length and multiple lengths ship once tests clear. Caution: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity. SHH STEEL can supply alternate walls and W-C/W-H classes for 008Cr27Mo once design pressure and corrosion allowance are clear. Size practice for 008Cr27Mo remains straight HX tubes; confirm bend radius with ferritic toughness data.

SHH STEEL can supply replacement retubing heats of 008Cr27Mo matched to prior certificates when the plant provides heat history. Apps: chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17. SHH STEEL can produce trial lengths of 008Cr27Mo for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside 008Cr27Mo: high Cr+Mo ferritic PREN without nickel; toughness and welding need ferritic procedures.

FAQ

What is GB/T 13296 008Cr27Mo seamless stainless steel tube used for?
GB/T 13296 008Cr27Mo is seamless stainless tube for boilers and heat exchangers — chloride water heaters, condenser tubes preferring ferritic conductivity, and Mo-ferritic upgrades from 10Cr17. Role summary: ultra-low-carbon high-Cr Mo ferritic tube for chloride-resistant HX without austenitic nickel. It is a Chinese product standard grade (S12791), not an automatic ASTM A213 certificate.
Is GB/T 13296 008Cr27Mo seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 008Cr27Mo when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 008Cr27Mo?
008Cr27Mo is delivered annealed under GB/T 13296. Table 4 reference: ≥1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 008Cr27Mo so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 008Cr27Mo compare with sister grades 10Cr17, 06Cr13, 015Cr20Ni18Mo6CuN?
008Cr27Mo is filed as ferritic. Typical sisters on the same RFQ are 10Cr17, 06Cr13, 015Cr20Ni18Mo6CuN. Design caution: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 008Cr27Mo?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is XM27 / UNS S44627-related the same as ordering 008Cr27Mo?
No. XM27 / UNS S44627-related is a commercial / UNS cross-walk for body text (unified S12791). The purchase order should lock GB/T 13296 and 008Cr27Mo so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 008Cr27Mo?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 008Cr27Mo within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: straight HX tubes; confirm bend radius with ferritic toughness data. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 008Cr27Mo be welded on site?
Shop guidance: matching Mo-ferritic fillers; strict heat input and contamination control. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity
When should I choose a higher-Mo or superaustenitic grade instead of 008Cr27Mo?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: C≤0.010 and tight Si/Mn ceilings — ordinary 430 heats fail this identity Sister pointers: 10Cr17, 06Cr13, 015Cr20Ni18Mo6CuN. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 008Cr27Mo with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 008Cr27Mo does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 008Cr27Mo?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 008Cr27Mo when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 008Cr27Mo is seamless stainless steel tube for boilers and heat exchangers — ultra-low-carbon high-Cr Mo ferritic tube for chloride-resistant HX without austenitic nickel. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 10Cr17, 06Cr13, 015Cr20Ni18Mo6CuN. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X