GB/T 13296 06Cr18Ni11Ti Seamless Stainless Steel Tube
What is GB/T 13296 06Cr18Ni11Ti Seamless Stainless Steel Tube
GB/T 13296-2023 is the Chinese national standard for seamless stainless steel tubes for boilers and heat exchangers — replacing the 2013 edition. Grade 06Cr18Ni11Ti (unified number S32168) sits in the austenitic set. Titanium ties up carbon so weld decay is less likely in sulphurous service.
SHH STEEL can produce and supply GB/T 13296 06Cr18Ni11Ti as seamless W-C or W-H tube across the enquiry OD×wall band, heat-treated per Table 4, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service.
Shop language may still say “321 tube,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 13296 and 06Cr18Ni11Ti so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade.
Scope discipline: 06Cr18Ni11Ti is seamless boiler/HX tube under GB/T 13296, not fluid-transport pipe under GB/T 14976 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include 07Cr19Ni11Ti, 06Cr18Ni11Nb, 06Cr19Ni10, 06Cr17Ni12Mo2Ti. Role reminder: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service.
Inside this GB/T 13296 series, compare GB/T 13296 07Cr19Ni11Ti, GB/T 13296 06Cr18Ni11Nb, GB/T 13296 06Cr19Ni10, GB/T 13296 06Cr17Ni12Mo2Ti. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP321.
Chemical Composition of GB/T 13296 06Cr18Ni11Ti
Cast analysis for GB/T 13296 06Cr18Ni11Ti follows Table 3. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 9.00–12.00, Cr 17.00–19.00, Ti 5(C+N)–0.70. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 321 / UNS S32168; unified number S32168. Corrosion thread: stabilisation targets HAZ carbide attack; chloride PREN still tracks Mo-free 18-8.
Chemical limits for 06Cr18Ni11Ti under GB/T 13296-2023 appear in the table underneath. Source priority is the 2023 Table 3 extract (xtd). If your client specification cites a 2013 footnote, send it before the heat is melted. Duty thread: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr18Ni11Ti before the order is acknowledged. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers; preserve Ti strategy across repair welds.
| Grade | C | Si | Mn | P | S | Ni | Cr | Ti |
|---|---|---|---|---|---|---|---|---|
| 06Cr18Ni11Ti | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.015 | 9.00–12.00 | 17.00–19.00 | 5(C+N)–0.70 |
Mechanical Properties of GB/T 13296 06Cr18Ni11Ti
Ambient tensile floors for 06Cr18Ni11Ti come from GB/T 13296 Table 4: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: stabilisation after solution anneal by agreement. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade.
Hardness testing is by agreement for wall ≥1.7 mm; Table 5 bands differ for special marks such as 06Cr18Ni13Si4 and the high-Mo austenitics. Density reference for 06Cr18Ni11Ti is 7.98 kg/dm³. Hydrostatic proof uses P=2SR/D with R at 60% of Table 4 Rp0.2, capped at 20 MPa.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 06Cr18Ni11Ti | 520 | 205 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 06Cr18Ni11Ti. Heat treatment (Table 4): 1010–1150 °C, rapid cool. stabilisation after solution anneal by agreement. Density 7.98 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 06Cr18Ni11Ti
Seamless is not optional wording for 06Cr18Ni11Ti: the standard limits manufacture to W-C or W-H seamless routes for boiler and heat-exchanger tube. Pick W-C when OD precision and U-bend finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 13296 line item. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.
Steelmaking for 06Cr18Ni11Ti is electric-arc or converter with secondary refining, or electroslag remelting. Pickling follows heat treatment unless bright protective-atmosphere practice or overall machining allows omission. Size practice: W-C HX with optional stabilisation treatment by agreement. Pickling or bright-anneal decisions for 06Cr18Ni11Ti stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. This paragraph is locked to 06Cr18Ni11Ti duty: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service.
Eddy-current testing to GB/T 7735 E3H may replace hydrostatic proof when agreed; ultrasonic testing to GB/T 5777 U2 remains a standard acceptance path for 06Cr18Ni11Ti. Role: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. Hydrostatic pressure or eddy-current class for 06Cr18Ni11Ti is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Corrosion framing beside 06Cr18Ni11Ti: stabilisation targets HAZ carbide attack; chloride PREN still tracks Mo-free 18-8.
Dimensions and Tolerances for GB/T 13296 06Cr18Ni11Ti
Dimensions and tolerances for 06Cr18Ni11Ti follow GB/T 13296 Table 1. Usual length is 2000–12000 mm. W-H OD tolerance is ±1.25%D for D≤140 mm and ±1%D above; W-C uses absolute OD bands from ±0.10 mm (D≤25) up through ±0.5%D for D>159 mm. Size hint: W-C HX with optional stabilisation treatment by agreement. Tolerance basis for 06Cr18Ni11Ti follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for 06Cr18Ni11Ti remains W-C HX with optional stabilisation treatment by agreement.
Out-of-roundness and wall unevenness for 06Cr18Ni11Ti shall not exceed 80% of the OD and wall tolerances respectively. Full-length camber ≤0.15% of tube length. Duty: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. Fixed lengths and multiple cut lengths for 06Cr18Ni11Ti are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers; preserve Ti strategy across repair welds.
Equivalent Grades for GB/T 13296 06Cr18Ni11Ti
Lock 06Cr18Ni11Ti on the PO when the datasheet owner wants GB/T 13296 seamless stainless boiler / heat-exchanger tube. Commercial talk as 321 / UNS S32168 is fine in emails; mill paperwork must still show GB/T 13296 06Cr18Ni11Ti. Application framing: refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal
– Caution locked in What-is / Corrosion / FAQ: Ti 5(C+N)–0.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 06Cr18Ni11Ti | Governing tube grade for this page |
| Commercial / UNS (body only) | 321 / UNS S32168 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | 321 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Order discipline for 06Cr18Ni11Ti still points at GB/T 13296, not the brochure alias. Neighbours GB/T 13296 07Cr19Ni11Ti, GB/T 13296 06Cr18Ni11Nb, GB/T 13296 06Cr19Ni10, GB/T 13296 06Cr17Ni12Mo2Ti each carry their own mechanical table. Category hub: GB/T 13296. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (06Cr18Ni11Ti).
Project teams specifying 06Cr18Ni11Ti should the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 3280 06Cr18Ni11Ti. See also the GB/T 4237 hub for related plate designations. Confirm 06Cr18Ni11Ti OD × wall and plate thickness on separate drawings.
Heat Treatment and Delivery Condition for GB/T 13296 06Cr18Ni11Ti
Heat treatment for 06Cr18Ni11Ti follows Table 4: 1010–1150 °C, rapid cool. Delivery condition: solution annealed. SHH STEEL records furnace charts that support the temperature and cool method claimed on the certificate. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni11Ti unless the mark is on the exemption list.
Field heat treatment of 06Cr18Ni11Ti after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni11Ti unless the mark is on the exemption list. Field heat treatment of 06Cr18Ni11Ti after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 06Cr18Ni11Ti caution visible here: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade.
Corrosion Resistance of GB/T 13296 06Cr18Ni11Ti
Corrosion behaviour of 06Cr18Ni11Ti in boiler/HX service: stabilisation targets HAZ carbide attack; chloride PREN still tracks Mo-free 18-8. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni11Ti unless the mark is on the exemption list. Medium risk note: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade.
If operating chlorides, temperature, or under-deposit geometry change after award, reopen the alloy choice for 06Cr18Ni11Ti rather than relying on wall thickness alone. Apps: refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr18Ni11Ti rather than relying on wall thickness alone. This paragraph is locked to 06Cr18Ni11Ti duty: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service.
Applications of GB/T 13296 06Cr18Ni11Ti Seamless Tube
Typical applications for GB/T 13296 06Cr18Ni11Ti: refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal. Duty summary: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. SHH STEEL can produce and supply the sizes and tests those packages need when the mill schedule allows. Spool fabricators should copy 06Cr18Ni11Ti onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 06Cr18Ni11Ti caution visible here: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade.
Spool and bundle fabricators should copy 06Cr18Ni11Ti onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Role: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. Commissioning teams benefit when the as-built dossier repeats 06Cr18Ni11Ti beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 06Cr18Ni11Ti remains W-C HX with optional stabilisation treatment by agreement.
Weldability of GB/T 13296 06Cr18Ni11Ti
Weldability of 06Cr18Ni11Ti: 321/308L fillers; preserve Ti strategy across repair welds. Procedure qualification should use the same product form and wall class as production, including the seamless finish that will ship. Caution: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade. Procedure qualification for 06Cr18Ni11Ti should use the same product form and wall class as production, including the seamless finish that will ship. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers; preserve Ti strategy across repair welds.
Shielding-gas and purge notes for 06Cr18Ni11Ti stay with the WPS package so site crews cannot improvise. Apps: refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal. Consumable lot control and shielding-gas notes for 06Cr18Ni11Ti stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 06Cr18Ni11Ti caution visible here: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade.
Surface Finishes for GB/T 13296 06Cr18Ni11Ti
Surface supply for 06Cr18Ni11Ti should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless tube, so finish is part of performance, not only appearance. Application framing: refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal
– Caution locked in What-is / Corrosion / FAQ: Ti 5(C+N)–0. Ambiguous “bright tube” language is clarified before finishing slots are booked.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
When 06Cr18Ni11Ti ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for solution anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Apps reminder: refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal
– Caution locked in What-is / Corrosion / FAQ: Ti 5(C+N)–0.
Inspection and Testing for GB/T 13296 06Cr18Ni11Ti
Inspection for 06Cr18Ni11Ti includes melt analysis, tensile tests, hydrostatic or eddy-current E3H, ultrasonic U2, and size/straightness checks. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni11Ti unless the mark is on the exemption list. Flattening applies for wall ≤10 mm; flaring for D≤150 mm and wall ≤10 mm.
Non-conforming 06Cr18Ni11Ti lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Documents: GB/T 2102 / EN 10204 3.1 style as ordered. Non-conforming 06Cr18Ni11Ti lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers; preserve Ti strategy across repair welds.
Packaging and Shipping for GB/T 13296 06Cr18Ni11Ti
Packaging for 06Cr18Ni11Ti uses capped ends, wrapped bundles or wooden crates, and waterproof protection matched to the voyage. Bundle tickets repeat grade, heat, size, and quantity. Size hint: W-C HX with optional stabilisation treatment by agreement. Bundle tickets for 06Cr18Ni11Ti repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 06Cr18Ni11Ti: stabilisation targets HAZ carbide attack; chloride PREN still tracks Mo-free 18-8.
Marking on 06Cr18Ni11Ti includes standard, grade, heat number, size, and manufacture symbol so site receiving can match crates to the packing list without opening every wrap. Desiccant and wrap choices for 06Cr18Ni11Ti follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 06Cr18Ni11Ti: stabilisation targets HAZ carbide attack; chloride PREN still tracks Mo-free 18-8.
SHH STEEL can adjust crate schedules for 06Cr18Ni11Ti when staggered retubing deliveries are on the project calendar. Weld-shop note: 321/308L fillers; preserve Ti strategy across repair welds. Claims handling for 06Cr18Ni11Ti starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 06Cr18Ni11Ti stays refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal.
Why Choose SHH STEEL
SHH STEEL can produce and supply GB/T 13296 06Cr18Ni11Ti against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Duty: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. SHH STEEL can produce and supply 06Cr18Ni11Ti against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Size practice for 06Cr18Ni11Ti remains W-C HX with optional stabilisation treatment by agreement.
SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr18Ni11Ti when the mill schedule allows. Sisters on the same hub: 07Cr19Ni11Ti, 06Cr18Ni11Nb, 06Cr19Ni10, 06Cr17Ni12Mo2Ti. SHH STEEL can make 06Cr18Ni11Ti to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Size practice for 06Cr18Ni11Ti remains W-C HX with optional stabilisation treatment by agreement.
Supply Capability
SHH STEEL can produce and supply GB/T 13296 06Cr18Ni11Ti seamless tube to the enquiry size list with Table 3 chemistry, Table 4 heat treatment and tensile floors, and the NDT/hydro stack the datasheet names. Role: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr18Ni11Ti when the mill schedule allows. Keep the 06Cr18Ni11Ti caution visible here: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 06Cr18Ni11Ti (S32168) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes: SHH STEEL can supply 06Cr18Ni11Ti in common HX OD×min-wall bands and boiler straight lengths; non-stock walls and U-bend radii are rolled to order. Confirm W-C versus W-H before booking. Duty: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr18Ni11Ti once design pressure and corrosion allowance are clear. Application context for 06Cr18Ni11Ti stays refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal.
SHH STEEL can produce trial bends and qualification lengths of 06Cr18Ni11Ti ahead of bulk release when the exchanger fabricator needs WPS coupons. Weld-shop: 321/308L fillers; preserve Ti strategy across repair welds. SHH STEEL can produce trial lengths of 06Cr18Ni11Ti for procedure qualification before bulk release when the project calendar needs it. Application context for 06Cr18Ni11Ti stays refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal.
FAQ
-
What is GB/T 13296 06Cr18Ni11Ti seamless stainless steel tube used for?
- GB/T 13296 06Cr18Ni11Ti is seamless stainless tube for boilers and heat exchangers — refinery steam generators, sulphur-plant exchangers, and welded bundles without full PWHT anneal. Role summary: Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. It is a Chinese product standard grade (S32168), not an automatic ASTM A213 certificate.
-
Is GB/T 13296 06Cr18Ni11Ti seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr18Ni11Ti when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 06Cr18Ni11Ti?
- 06Cr18Ni11Ti is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr18Ni11Ti so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr18Ni11Ti compare with sister grades 07Cr19Ni11Ti, 06Cr18Ni11Nb, 06Cr19Ni10?
- 06Cr18Ni11Ti is filed as austenitic. Typical sisters on the same RFQ are 07Cr19Ni11Ti, 06Cr18Ni11Nb, 06Cr19Ni10. Design caution: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr18Ni11Ti?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 321 / UNS S32168 the same as ordering 06Cr18Ni11Ti?
- No. 321 / UNS S32168 is a commercial / UNS cross-walk for body text (unified S32168). The purchase order should lock GB/T 13296 and 06Cr18Ni11Ti so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 06Cr18Ni11Ti?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr18Ni11Ti within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: W-C HX with optional stabilisation treatment by agreement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 06Cr18Ni11Ti be welded on site?
- Shop guidance: 321/308L fillers; preserve Ti strategy across repair welds. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr18Ni11Ti?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Ti 5(C+N)–0.70 is mandatory; a Ti-free 304-class heat is not this grade Sister pointers: 07Cr19Ni11Ti, 06Cr18Ni11Nb, 06Cr19Ni10. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 06Cr18Ni11Ti with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr18Ni11Ti does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 06Cr18Ni11Ti?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr18Ni11Ti when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 06Cr18Ni11Ti is seamless stainless steel tube for boilers and heat exchangers — Ti-stabilised 18-8 austenitic tube for polythionic and weld-decay sensitive boiler/HX service. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 07Cr19Ni11Ti, 06Cr18Ni11Nb, 06Cr19Ni10. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.