GB/T 13296 022Cr17Ni12Mo2 Seamless Stainless Steel Tube
What is GB/T 13296 022Cr17Ni12Mo2 Seamless Stainless Steel Tube
When the approved vendor list and exchanger datasheet say GB/T 13296, the grade mark has to be the Chinese designation. 022Cr17Ni12Mo2 is the full product grade for this austenitic seamless tube. It is the L sister of 06Cr17Ni12Mo2 for as-welded corrosive HX packages.
SHH STEEL can supply 022Cr17Ni12Mo2 seamless tube in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the exchanger: low-carbon Mo austenitic tube for welded HX service in chloride and chemical media. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 022Cr17Ni12Mo2 before production starts. Application context for 022Cr17Ni12Mo2 stays welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers.
Equivalence talk to 316L / UNS S31603 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 13296 022Cr17Ni12Mo2, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors.
Related ASTM A213 tube pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 022Cr19Ni13Mo3, 022Cr18Ni14Mo2Cu2. Use thread: welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers.
Inside this GB/T 13296 series, compare GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 022Cr17Ni12Mo2N, GB/T 13296 022Cr19Ni13Mo3, GB/T 13296 022Cr18Ni14Mo2Cu2. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP316L.
When 022Cr17Ni12Mo2 pipe sits beside plate on the same BOM, Stainless Steel Pipes and Tubes covers the tubular parent, Stainless Steel Sheets and Plates covers flats, and GB/T 3280 022Cr17Ni12Mo2 is the live plate chemistry match — do not merge MTCs. Keep 022Cr17Ni12Mo2 acceptance text on the governing pipe/tube standard.
Chemical Composition of GB/T 13296 022Cr17Ni12Mo2
Chemistry control on 022Cr17Ni12Mo2 starts at the ladle. Expect C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 10.00–14.00, Cr 16.00–18.00, Mo 2.00–3.00 within Table 3, reported on the inspection document against the heat. Body alias 316L / UNS S31603 does not widen those windows. Every ladle analysis for 022Cr17Ni12Mo2 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Corrosion framing beside 022Cr17Ni12Mo2: L-carbon plus Mo: better HAZ behaviour and better PREN than 18-8 L.
Read the table with the family in mind — austenitic — and with caution xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors. Numbers without the matching Table 4 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 022Cr17Ni12Mo2 before the order is acknowledged. Size practice for 022Cr17Ni12Mo2 remains cold-finished thin-wall HX with min-wall ordering.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| 022Cr17Ni12Mo2 | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.015 | 10.00–14.00 | 16.00–18.00 | 2.00–3.00 |
Mechanical Properties of GB/T 13296 022Cr17Ni12Mo2
Proof stress and tensile minima for 022Cr17Ni12Mo2 sit at Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: xtd Table 4 lists Rm≥520 / Rp0.2≥205 for this L grade. Flattening and flaring back ductility when size allows. Watch-out: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors.
Batch size limits (D≤76 mm and S≤3 mm: ≤400 tubes; otherwise ≤200) keep sampling honest for 022Cr17Ni12Mo2. Retests follow GB/T 2102. Density 7.98 kg/dm³.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 022Cr17Ni12Mo2 | 520 | 205 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 022Cr17Ni12Mo2. Heat treatment (Table 4): 1010–1150 °C, rapid cool. xtd Table 4 lists Rm≥520 / Rp0.2≥205 for this L grade. Density 7.98 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 022Cr17Ni12Mo2
SHH STEEL can produce 022Cr17Ni12Mo2 as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 4 heat treatment and pickle (or bright anneal) as ordered. Plain ends are default; bevels by agreement when the tubesheet weld prep needs it. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.
SHH STEEL schedules piercing, elongation, and finishing for 022Cr17Ni12Mo2 against the W-C or W-H symbol frozen on the acknowledgement. Ovality and wall eccentricity stay inside 80% of the respective OD and wall tolerances. Pickling or bright-anneal decisions for 022Cr17Ni12Mo2 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Weld-shop note tied to 022Cr17Ni12Mo2: 316L fillers; low heat input and clean ID purge for U-bend returns.
Cold-finish depth of longitudinal marks on 022Cr17Ni12Mo2 is limited to ≤4% of wall and ≤0.2 mm; hot-finish ≤5% and ≤0.4 mm. Apps: welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers. Hydrostatic pressure or eddy-current class for 022Cr17Ni12Mo2 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Corrosion framing beside 022Cr17Ni12Mo2: L-carbon plus Mo: better HAZ behaviour and better PREN than 18-8 L.
Dimensions and Tolerances for GB/T 13296 022Cr17Ni12Mo2
When 022Cr17Ni12Mo2 ships as nominal wall, the note under Table 1 still applies different ± bands for hot and cold routes — do not mix W-C absolute OD tols with W-H percentage thinking. Practice: cold-finished thin-wall HX with min-wall ordering. Tolerance basis for 022Cr17Ni12Mo2 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 022Cr17Ni12Mo2 caution visible here: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors.
Fixed lengths of 022Cr17Ni12Mo2 are end-protected so bevels and ID finish survive inland and ocean transit. Random lengths stay inside the usual 2000–12000 mm window unless agreed otherwise. Fixed lengths and multiple cut lengths for 022Cr17Ni12Mo2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 022Cr17Ni12Mo2 stays welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers.
Equivalent Grades for GB/T 13296 022Cr17Ni12Mo2
For 022Cr17Ni12Mo2, start with identity under GB/T 13296 and only then walk commercial / UNS aliases. 316L / UNS S31603 is useful in body text; it is not the PO grade by itself. ASTM A213 / A269 related counterparts share a chemistry family at best — wall basis and NDT do not transfer by default.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 022Cr17Ni12Mo2 | Governing tube grade for this page |
| Commercial / UNS (body only) | 316L / UNS S31603 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | 316L chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Order discipline for 022Cr17Ni12Mo2 still points at GB/T 13296, not the brochure alias. Neighbours GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 022Cr17Ni12Mo2N, GB/T 13296 022Cr19Ni13Mo3, GB/T 13296 022Cr18Ni14Mo2Cu2 each carry their own mechanical table. Category hub: GB/T 13296. Dual marking is a purchase-order option that still requires every limit that matters for 022Cr17Ni12Mo2 to be verified on the heat.
Heat Treatment and Delivery Condition for GB/T 13296 022Cr17Ni12Mo2
For 022Cr17Ni12Mo2, solution or anneal practice is not a free mill choice — it is the Table 4 band tied to the grade. Delivery: solution annealed. Role: low-carbon Mo austenitic tube for welded HX service in chloride and chemical media. Recorded furnace charts for 022Cr17Ni12Mo2 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 022Cr17Ni12Mo2 caution visible here: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors.
When Annex A elevated Rp0.2 is invoked, the certificate for 022Cr17Ni12Mo2 should still show the Table 4 delivery treatment actually performed. Apps: welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers. Field heat treatment of 022Cr17Ni12Mo2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 022Cr17Ni12Mo2 remains cold-finished thin-wall HX with min-wall ordering.
Corrosion Resistance of GB/T 13296 022Cr17Ni12Mo2
Pitting, crevice, oxidation, or weld-decay limiters for 022Cr17Ni12Mo2 should be named in the datasheet rather than inferred from the AISI alias alone. Framing: L-carbon plus Mo: better HAZ behaviour and better PREN than 18-8 L. Coupon orientation, weld condition, and surface finish for 022Cr17Ni12Mo2 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Keep the 022Cr17Ni12Mo2 caution visible here: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors.
Pickling quality and free-iron cleanliness after fabrication affect startup corrosion of 022Cr17Ni12Mo2 as much as cast chemistry. Role: low-carbon Mo austenitic tube for welded HX service in chloride and chemical media. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 022Cr17Ni12Mo2 rather than relying on wall thickness alone. Application context for 022Cr17Ni12Mo2 stays welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers.
Applications of GB/T 13296 022Cr17Ni12Mo2 Seamless Tube
Use 022Cr17Ni12Mo2 on packages that match welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers. Nearby sisters 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 022Cr19Ni13Mo3, 022Cr18Ni14Mo2Cu2 cover adjacent media or temperature steps. Weld-shop note: 316L fillers; low heat input and clean ID purge for U-bend returns. Spool fabricators should copy 022Cr17Ni12Mo2 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside 022Cr17Ni12Mo2: L-carbon plus Mo: better HAZ behaviour and better PREN than 18-8 L.
When the process medium changes mid-project, revisit whether 022Cr17Ni12Mo2 still fits before releasing more heats. Sisters: 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 022Cr19Ni13Mo3, 022Cr18Ni14Mo2Cu2. Commissioning teams benefit when the as-built dossier repeats 022Cr17Ni12Mo2 beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside 022Cr17Ni12Mo2: L-carbon plus Mo: better HAZ behaviour and better PREN than 18-8 L.
Weldability of GB/T 13296 022Cr17Ni12Mo2
Consumable selection for 022Cr17Ni12Mo2 follows 316L fillers; low heat input and clean ID purge for U-bend returns. Do not improvise under-alloyed fillers on Mo or Cu grades. Role: low-carbon Mo austenitic tube for welded HX service in chloride and chemical media. Procedure qualification for 022Cr17Ni12Mo2 should use the same product form and wall class as production, including the seamless finish that will ship. Weld-shop note tied to 022Cr17Ni12Mo2: 316L fillers; low heat input and clean ID purge for U-bend returns.
Ferrite control and hot-cracking risk for 022Cr17Ni12Mo2 depend on the family chemistry; qualify on production wall, not only on plate coupons. Weld shop: 316L fillers; low heat input and clean ID purge for U-bend returns. Consumable lot control and shielding-gas notes for 022Cr17Ni12Mo2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 022Cr17Ni12Mo2 duty: low-carbon Mo austenitic tube for welded HX service in chloride and chemical media.
Surface Finishes for GB/T 13296 022Cr17Ni12Mo2
Finish options for 022Cr17Ni12Mo2 follow the ordered heat-treatment route under GB/T 13296. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: solution annealed. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (022Cr17Ni12Mo2).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
For 022Cr17Ni12Mo2, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this tube. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 022Cr17Ni12Mo2.
Inspection and Testing for GB/T 13296 022Cr17Ni12Mo2
SHH STEEL keeps heat identity for 022Cr17Ni12Mo2 unbroken from melt through bundle tags, including third-party hold points written into the PO. Caution: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors. Sampling plans for 022Cr17Ni12Mo2 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 022Cr17Ni12Mo2: 316L fillers; low heat input and clean ID purge for U-bend returns.
Certificate lines for 022Cr17Ni12Mo2 must repeat the Chinese grade, unified number, manufacture symbol, and heat treatment actually performed. Caution: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors. Non-conforming 022Cr17Ni12Mo2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Application context for 022Cr17Ni12Mo2 stays welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers.
Packaging and Shipping for GB/T 13296 022Cr17Ni12Mo2
Desiccant and wrap choices for 022Cr17Ni12Mo2 follow voyage length and storage climate on the shipping order, not a one-size export habit. Apps: welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers. Bundle tickets for 022Cr17Ni12Mo2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 022Cr17Ni12Mo2 stays welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers.
Inland trucking of 022Cr17Ni12Mo2 still needs end protection — most ID dents happen between the port and the exchanger shop. Apps: welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers. Desiccant and wrap choices for 022Cr17Ni12Mo2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 022Cr17Ni12Mo2 caution visible here: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors.
Barcode or stencil extras for 022Cr17Ni12Mo2 are available when the owner’s material system needs them. Apps: welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers. Claims handling for 022Cr17Ni12Mo2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to 022Cr17Ni12Mo2 duty: low-carbon Mo austenitic tube for welded HX service in chloride and chemical media.
Why Choose SHH STEEL
SHH STEEL can make 022Cr17Ni12Mo2 to a boiler/HX test stack — hydro or E3H, UT U2, flattening/flaring, IGC when required — instead of a generic stainless tube habit. Apps: welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers. SHH STEEL can produce and supply 022Cr17Ni12Mo2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Weld-shop note tied to 022Cr17Ni12Mo2: 316L fillers; low heat input and clean ID purge for U-bend returns.
SHH STEEL can supply 022Cr17Ni12Mo2 with third-party inspection hold points written into the itinerary. Weld-shop note: 316L fillers; low heat input and clean ID purge for U-bend returns. SHH STEEL can make 022Cr17Ni12Mo2 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. This paragraph is locked to 022Cr17Ni12Mo2 duty: low-carbon Mo austenitic tube for welded HX service in chloride and chemical media.
Supply Capability
SHH STEEL can supply 022Cr17Ni12Mo2 with EN 10204 3.1 style documents, IGC when required, and hardness by agreement. Caution: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 022Cr17Ni12Mo2 when the mill schedule allows. Application context for 022Cr17Ni12Mo2 stays welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 022Cr17Ni12Mo2 (S31603) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes: rolling cycles for 022Cr17Ni12Mo2 cover usual 2000–12000 mm lengths; cut-to-length and multiple lengths ship once tests clear. Caution: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors. SHH STEEL can supply alternate walls and W-C/W-H classes for 022Cr17Ni12Mo2 once design pressure and corrosion allowance are clear. Keep the 022Cr17Ni12Mo2 caution visible here: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors.
SHH STEEL can supply replacement retubing heats of 022Cr17Ni12Mo2 matched to prior certificates when the plant provides heat history. Apps: welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers. SHH STEEL can produce trial lengths of 022Cr17Ni12Mo2 for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to 022Cr17Ni12Mo2: 316L fillers; low heat input and clean ID purge for U-bend returns.
FAQ
-
What is GB/T 13296 022Cr17Ni12Mo2 seamless stainless steel tube used for?
- GB/T 13296 022Cr17Ni12Mo2 is seamless stainless tube for boilers and heat exchangers — welded tube-to-tubesheet HX, chemical condensers, and food/pharma-adjacent steam exchangers. Role summary: low-carbon Mo austenitic tube for welded HX service in chloride and chemical media. It is a Chinese product standard grade (S31603), not an automatic ASTM A213 certificate.
-
Is GB/T 13296 022Cr17Ni12Mo2 seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 022Cr17Ni12Mo2 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 022Cr17Ni12Mo2?
- 022Cr17Ni12Mo2 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 022Cr17Ni12Mo2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 022Cr17Ni12Mo2 compare with sister grades 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 022Cr19Ni13Mo3?
- 022Cr17Ni12Mo2 is filed as austenitic. Typical sisters on the same RFQ are 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 022Cr19Ni13Mo3. Design caution: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 022Cr17Ni12Mo2?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 316L / UNS S31603 the same as ordering 022Cr17Ni12Mo2?
- No. 316L / UNS S31603 is a commercial / UNS cross-walk for body text (unified S31603). The purchase order should lock GB/T 13296 and 022Cr17Ni12Mo2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 022Cr17Ni12Mo2?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 022Cr17Ni12Mo2 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: cold-finished thin-wall HX with min-wall ordering. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 022Cr17Ni12Mo2 be welded on site?
- Shop guidance: 316L fillers; low heat input and clean ID purge for U-bend returns. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors
-
When should I choose a higher-Mo or superaustenitic grade instead of 022Cr17Ni12Mo2?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: xtd Table 4 prints Rm≥520 / Rp0.2≥205 for this L grade — quote the extract, do not silently copy 14976 L floors Sister pointers: 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 022Cr19Ni13Mo3. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 022Cr17Ni12Mo2 with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 022Cr17Ni12Mo2 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 022Cr17Ni12Mo2?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 022Cr17Ni12Mo2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 022Cr17Ni12Mo2 is seamless stainless steel tube for boilers and heat exchangers — low-carbon Mo austenitic tube for welded HX service in chloride and chemical media. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 022Cr19Ni13Mo3. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.