GB/T 13296 20Cr25Ni20 Seamless Stainless Steel Tube
What is GB/T 13296 20Cr25Ni20 Seamless Stainless Steel Tube
GB/T 13296 covers seamless stainless tube for boiler and HX service — cold-drawn or hot-finished — with hydrostatic proof, ultrasonic U2, flattening and flaring where size allows. Inside that standard, 20Cr25Ni20 is filed as austenitic. It is the high-carbon sister of 06Cr25Ni20 for boiler/HX heat duty.
From pierce/extrude/draw through marking and crate protection, SHH STEEL can produce GB/T 13296 20Cr25Ni20 for the sizes and tests on your RFQ. Application sketch: severe furnace-duty exchangers, high-temperature process coolers, and radiant coils. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 20Cr25Ni20 before production starts. Application context for 20Cr25Ni20 stays severe furnace-duty exchangers, high-temperature process coolers, and radiant coils.
On the floor people shorten marks; in QA they must not. 20Cr25Ni20 under GB/T 13296 carries specific Table 3 windows and Table 4 floors that a loose “310” note will not enforce. Caution: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing.
Annex A elevated Rp0.2 and Annex B rupture data apply only to named H marks; still match the alloy to the medium. For 20Cr25Ni20, that means: higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages. Nearby marks: 06Cr25Ni20, 16Cr23Ni13, 06Cr23Ni13, 07Cr19Ni10.
Inside this GB/T 13296 series, compare GB/T 13296 06Cr25Ni20, GB/T 13296 16Cr23Ni13, GB/T 13296 06Cr23Ni13, GB/T 13296 07Cr19Ni10. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP310S.
When 20Cr25Ni20 pipe sits beside plate on the same BOM, link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and ASTM A240 Type 310S so purchasing does not treat one product form as the other. Do not stretch a 20Cr25Ni20 pipe certificate onto plate.
Chemical Composition of GB/T 13296 20Cr25Ni20
For 20Cr25Ni20, the melt ticket has to show Table 3 compliance — C ≤0.25, Si ≤1.50, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 19.00–22.00, Cr 24.00–26.00. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: top-tier oxidation resistance in this series; aqueous chloride duty usually wants a Mo super-austenitic instead.
Where Mo, Cu, Ti, Nb or N appear, they are intentional levers for 20Cr25Ni20, not optional marketing. Confirm them on the MTC line-by-line. Role: higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 20Cr25Ni20 before the order is acknowledged. Corrosion framing beside 20Cr25Ni20: top-tier oxidation resistance in this series; aqueous chloride duty usually wants a Mo super-austenitic instead.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 20Cr25Ni20 | ≤0.25 | ≤1.50 | ≤2.00 | ≤0.035 | ≤0.015 | 19.00–22.00 | 24.00–26.00 |
UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 20Cr25Ni20 (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 310 / UNS S31000, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 20Cr25Ni20 against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 20Cr25Ni20 before the heat is booked.
Mechanical Properties of GB/T 13296 20Cr25Ni20
Do not confuse Table 4 tube tensile floors with pipe or plate standards that share the 310 / UNS S31000 alias. For 20Cr25Ni20 under 13296 expect Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%, verified per heat/lot rules. Note: UNCERTAIN — provisional; IGC exempt per clause 9 list. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting.
When wall class changes the ordered tensile specimen orientation, keep the acknowledgement aligned for 20Cr25Ni20. Reference density 7.98 kg/dm³; delivery solution annealed.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 20Cr25Ni20 | 520 | 205 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 20Cr25Ni20. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1030–1180 °C, rapid cool. UNCERTAIN — provisional; IGC exempt per clause 9 list. Density 7.98 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 20Cr25Ni20
Seamless is not optional wording for 20Cr25Ni20: the standard limits manufacture to W-C or W-H seamless routes for boiler and heat-exchanger tube. Pick W-C when OD precision and U-bend finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 13296 line item. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.
U-bend and cut-to-length options for 20Cr25Ni20 are available by agreement after the straight-tube tests clear. Surface quality rejects cracks, folds, laps, laminations and scabs on ID and OD. Pickling or bright-anneal decisions for 20Cr25Ni20 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Size practice for 20Cr25Ni20 remains heavy W-H walls where hot finish and oxidation life dominate cost.
Manufacture records for 20Cr25Ni20 keep heat identity unbroken from melt through final NDT so the MTC can cite one cast for the whole bundle. Hydrostatic pressure or eddy-current class for 20Cr25Ni20 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Weld-shop note tied to 20Cr25Ni20: 310H-class fillers; hot-cracking discipline on thick walls.
Dimensions and Tolerances for GB/T 13296 20Cr25Ni20
Cut lengths, multiple lengths, and U-bend developed lengths for 20Cr25Ni20 need explicit acknowledgement so finishing and crate length match the tubesheet drawing. Caution: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing. Tolerance basis for 20Cr25Ni20 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for 20Cr25Ni20 stays severe furnace-duty exchangers, high-temperature process coolers, and radiant coils.
Tolerance class follows the manufacture route ordered for 20Cr25Ni20; swapping W-C for W-H after acknowledgement without a dimensional review is how fit-up fails at the exchanger shop. Fixed lengths and multiple cut lengths for 20Cr25Ni20 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 20Cr25Ni20 caution visible here: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing.
Equivalent Grades for GB/T 13296 20Cr25Ni20
Buyers searching under 310 / UNS S31000 still need the GB/T 13296 20Cr25Ni20 row locked on the acknowledgement. Inside austenitic practice the mechanical table and inspection clauses of GB/T 13296 control acceptance, not a brochure equivalent. Duty context: higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 20Cr25Ni20 | Governing tube grade for this page |
| Commercial / UNS (body only) | 310 / UNS S31000 (unified S31020) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | 310 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Inside this series compare GB/T 13296 06Cr25Ni20, GB/T 13296 16Cr23Ni13, GB/T 13296 06Cr23Ni13, GB/T 13296 07Cr19Ni10 before swapping marks for medium or temperature. Keep this caution visible for 20Cr25Ni20: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing. Hub: GB/T 13296. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (20Cr25Ni20).
Heat Treatment and Delivery Condition for GB/T 13296 20Cr25Ni20
Stabilisation after solution anneal is available by agreement for Ti/Nb marks; confirm whether 20Cr25Ni20 needs that second hold before acknowledging. HT reference: 1030–1180 °C, rapid cool. Recorded furnace charts for 20Cr25Ni20 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside 20Cr25Ni20: top-tier oxidation resistance in this series; aqueous chloride duty usually wants a Mo super-austenitic instead.
Mixed bundles of different heat-treatment furnace lots of 20Cr25Ni20 stay segregated so sampling remains traceable to one Table 4 run. Field heat treatment of 20Cr25Ni20 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 20Cr25Ni20 remains heavy W-H walls where hot finish and oxidation life dominate cost.
Corrosion Resistance of GB/T 13296 20Cr25Ni20
Coupon orientation, weld condition, and surface finish for 20Cr25Ni20 belong in the corrosion test order so method E or other coupons compare honestly to the installed tube. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 20Cr25Ni20 unless the mark is on the exemption list. Coupon orientation, weld condition, and surface finish for 20Cr25Ni20 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Application context for 20Cr25Ni20 stays severe furnace-duty exchangers, high-temperature process coolers, and radiant coils.
For 20Cr25Ni20, specify whether IGC, hardness, or special corrosion coupons are extras beyond the clause 9 default before the heat is melted. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 20Cr25Ni20 rather than relying on wall thickness alone. Application context for 20Cr25Ni20 stays severe furnace-duty exchangers, high-temperature process coolers, and radiant coils.
Applications of GB/T 13296 20Cr25Ni20 Seamless Tube
Commissioning dossiers should repeat 20Cr25Ni20 beside heat numbers so as-built isometrics stay tied to the same mill certificates. Application thread: severe furnace-duty exchangers, high-temperature process coolers, and radiant coils. Spool fabricators should copy 20Cr25Ni20 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 20Cr25Ni20 remains heavy W-H walls where hot finish and oxidation life dominate cost.
Spare-tube stocks of 20Cr25Ni20 should keep heat identity so later retubing matches the original corrosion and strength file. Apps: severe furnace-duty exchangers, high-temperature process coolers, and radiant coils. Commissioning teams benefit when the as-built dossier repeats 20Cr25Ni20 beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to 20Cr25Ni20: 310H-class fillers; hot-cracking discipline on thick walls.
Weldability of GB/T 13296 20Cr25Ni20
Repair welding of 20Cr25Ni20 must preserve grade identity — a 308 deposit on a 6% Mo tube is a corrosion failure waiting to happen. Note: 310H-class fillers; hot-cracking discipline on thick walls. Procedure qualification for 20Cr25Ni20 should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 20Cr25Ni20 caution visible here: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing.
Tubesheet joint design for 20Cr25Ni20 should state strength weld versus seal weld and any expansion sequence before production welding starts. Consumable lot control and shielding-gas notes for 20Cr25Ni20 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 20Cr25Ni20 caution visible here: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing.
Surface Finishes for GB/T 13296 20Cr25Ni20
20Cr25Ni20 under GB/T 13296 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (20Cr25Ni20).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
When 20Cr25Ni20 ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for solution anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (20Cr25Ni20).
Inspection and Testing for GB/T 13296 20Cr25Ni20
Hardness by agreement for wall ≥1.7 mm on 20Cr25Ni20; grain-size evidence when the mark requires levels 4–7. Apps: severe furnace-duty exchangers, high-temperature process coolers, and radiant coils. Sampling plans for 20Cr25Ni20 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to 20Cr25Ni20 duty: higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages.
Dimensional reports for 20Cr25Ni20 cite Table 1 tolerance basis (W-C vs W-H, min wall vs nominal wall) so receiving inspectors know which band applies. Non-conforming 20Cr25Ni20 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 20Cr25Ni20: 310H-class fillers; hot-cracking discipline on thick walls.
Packaging and Shipping for GB/T 13296 20Cr25Ni20
U-bend crates for 20Cr25Ni20 need radius supports so cold-worked bends do not spring or scar in transit. Caution: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing. Bundle tickets for 20Cr25Ni20 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 20Cr25Ni20: top-tier oxidation resistance in this series; aqueous chloride duty usually wants a Mo super-austenitic instead.
Long-term storage of 20Cr25Ni20 should keep bundles dry and off bare soil to protect the pickled surface before installation. Caution: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing. Desiccant and wrap choices for 20Cr25Ni20 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 20Cr25Ni20 remains heavy W-H walls where hot finish and oxidation life dominate cost.
Packing lists for 20Cr25Ni20 cite net/gross weight and crate count so logistics and QA share one document set. Caution: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing. Claims handling for 20Cr25Ni20 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 20Cr25Ni20 stays severe furnace-duty exchangers, high-temperature process coolers, and radiant coils.
Why Choose SHH STEEL
Traceability, pickle quality, and size discipline on 20Cr25Ni20 are part of the supply promise, not brochure extras. Role: higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages. SHH STEEL can produce and supply 20Cr25Ni20 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Keep the 20Cr25Ni20 caution visible here: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing.
For 20Cr25Ni20, SHH STEEL can produce trial lengths for procedure qualification before bulk release when the project calendar needs it. Apps: severe furnace-duty exchangers, high-temperature process coolers, and radiant coils. SHH STEEL can make 20Cr25Ni20 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Weld-shop note tied to 20Cr25Ni20: 310H-class fillers; hot-cracking discipline on thick walls.
Supply Capability
From RFQ to crate, SHH STEEL can produce 20Cr25Ni20 as a boiler/HX product — not a repurposed fluid-pipe heat. Size hint: heavy W-H walls where hot finish and oxidation life dominate cost. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 20Cr25Ni20 when the mill schedule allows. This paragraph is locked to 20Cr25Ni20 duty: higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 20Cr25Ni20 (S31020) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes — SHH STEEL can supply alternate walls for 20Cr25Ni20 once design pressure, corrosion allowance, and min-wall rules are clear. Size hint: heavy W-H walls where hot finish and oxidation life dominate cost. SHH STEEL can supply alternate walls and W-C/W-H classes for 20Cr25Ni20 once design pressure and corrosion allowance are clear. Size practice for 20Cr25Ni20 remains heavy W-H walls where hot finish and oxidation life dominate cost.
Export packing and document sets for 20Cr25Ni20 are confirmed on the acknowledgement so customs and site QA see the same grade string. Caution: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing. SHH STEEL can produce trial lengths of 20Cr25Ni20 for procedure qualification before bulk release when the project calendar needs it. This paragraph is locked to 20Cr25Ni20 duty: higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages.
FAQ
-
What is GB/T 13296 20Cr25Ni20 seamless stainless steel tube used for?
- GB/T 13296 20Cr25Ni20 is seamless stainless tube for boilers and heat exchangers — severe furnace-duty exchangers, high-temperature process coolers, and radiant coils. Role summary: higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages. It is a Chinese product standard grade (S31020), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
-
Is GB/T 13296 20Cr25Ni20 seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 20Cr25Ni20 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 20Cr25Ni20?
- 20Cr25Ni20 is delivered solution annealed under GB/T 13296. Table 4 reference: 1030–1180 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 20Cr25Ni20 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 20Cr25Ni20 compare with sister grades 06Cr25Ni20, 16Cr23Ni13, 06Cr23Ni13?
- 20Cr25Ni20 is filed as austenitic. Typical sisters on the same RFQ are 06Cr25Ni20, 16Cr23Ni13, 06Cr23Ni13. Design caution: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 20Cr25Ni20?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 310 / UNS S31000 the same as ordering 20Cr25Ni20?
- No. 310 / UNS S31000 is a commercial / UNS cross-walk for body text (unified S31020). The purchase order should lock GB/T 13296 and 20Cr25Ni20 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 20Cr25Ni20?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 20Cr25Ni20 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: heavy W-H walls where hot finish and oxidation life dominate cost. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 20Cr25Ni20 be welded on site?
- Shop guidance: 310H-class fillers; hot-cracking discipline on thick walls. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing
-
When should I choose a higher-Mo or superaustenitic grade instead of 20Cr25Ni20?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN vs paid Table 3/4; IGC exempt per clause 9 — still lock heat treatment and grain extras in writing Sister pointers: 06Cr25Ni20, 16Cr23Ni13, 06Cr23Ni13. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 20Cr25Ni20 with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 20Cr25Ni20 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 20Cr25Ni20?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 20Cr25Ni20 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 20Cr25Ni20 is seamless stainless steel tube for boilers and heat exchangers — higher-carbon 25Cr–20Ni heat tube for the toughest oxidation/carburisation boiler and HX packages. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr25Ni20, 16Cr23Ni13, 06Cr23Ni13. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.