GB/T 13296 022Cr19Ni10 Seamless Stainless Steel Tube

GB/T 13296 022Cr19Ni10 seamless stainless steel tube (304L / UNS S30403, S30403), austenitic, Table 3 cast analysis, Rm min 480 MPa / Rp0.2 min 175 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
022Cr19Ni10 (S30403 / 304L / UNS S30403 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 022Cr19Ni10 Seamless Stainless Steel Tube

GB/T 13296 covers seamless stainless tube for boiler and HX service — cold-drawn or hot-finished — with hydrostatic proof, ultrasonic U2, flattening and flaring where size allows. Inside that standard, 022Cr19Ni10 is filed as austenitic. It is the L-carbon sister of 06Cr19Ni10 for boiler/HX packages that weld without post-weld anneal.

From pierce/extrude/draw through marking and crate protection, SHH STEEL can produce GB/T 13296 022Cr19Ni10 for the sizes and tests on your RFQ. Application sketch: welded HX headers, food-adjacent steam lines, condensate coolers, and chloride-mild process exchangers. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 022Cr19Ni10 before production starts. Size practice for 022Cr19Ni10 remains cold-finished small OD for U-bend HX; confirm min-wall vs nominal-wall ordering language.

On the floor people shorten marks; in QA they must not. 022Cr19Ni10 under GB/T 13296 carries specific Table 3 windows and Table 4 floors that a loose “304L” note will not enforce. Caution: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

Annex A elevated Rp0.2 and Annex B rupture data apply only to named H marks; still match the alloy to the medium. For 022Cr19Ni10, that means: low-carbon 18-8 austenitic HX tube chosen when as-welded corrosion resistance matters more than elevated-temperature strength. Nearby marks: 06Cr19Ni10, 022Cr19Ni10N, 06Cr18Ni11Ti, 022Cr17Ni12Mo2.

Inside this GB/T 13296 series, compare GB/T 13296 06Cr19Ni10, GB/T 13296 022Cr19Ni10N, GB/T 13296 06Cr18Ni11Ti, GB/T 13296 022Cr17Ni12Mo2. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP304L.

022Cr19Ni10 sourcing notes should keep forms separate: tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is GB/T 3280 022Cr19Ni10. Keep 022Cr19Ni10 acceptance text on the governing pipe/tube standard.

Chemical Composition of GB/T 13296 022Cr19Ni10

For 022Cr19Ni10, the melt ticket has to show Table 3 compliance — C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 8.00–11.00, Cr 18.00–20.00. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: low carbon slows weld decay; pitting resistance still tracks Mo-free 18-8 behaviour. Every ladle analysis for 022Cr19Ni10 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Size practice for 022Cr19Ni10 remains cold-finished small OD for U-bend HX; confirm min-wall vs nominal-wall ordering language.

Where Mo, Cu, Ti, Nb or N appear, they are intentional levers for 022Cr19Ni10, not optional marketing. Confirm them on the MTC line-by-line. Role: low-carbon 18-8 austenitic HX tube chosen when as-welded corrosion resistance matters more than elevated-temperature strength. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 022Cr19Ni10 before the order is acknowledged. Weld-shop note tied to 022Cr19Ni10: 308L fillers preferred; low heat input and clean purge keep the HAZ honest.

Grade C Si Mn P S Ni Cr
022Cr19Ni10 ≤0.030 ≤1.00 ≤2.00 ≤0.035 ≤0.015 8.00–11.00 18.00–20.00

Mechanical Properties of GB/T 13296 022Cr19Ni10

Do not confuse Table 4 tube tensile floors with pipe or plate standards that share the 304L / UNS S30403 alias. For 022Cr19Ni10 under 13296 expect Rm min 480 MPa, Rp0.2 min 175 MPa, elongation min 35%, verified per heat/lot rules. Tensile sampling follows the batch rules for the ordered test unit of 022Cr19Ni10, and retests follow GB/T 2102 when a result sits under the Table 4 floor. Application context for 022Cr19Ni10 stays welded HX headers, food-adjacent steam lines, condensate coolers, and chloride-mild process exchangers.

When wall class changes the ordered tensile specimen orientation, keep the acknowledgement aligned for 022Cr19Ni10. Reference density 7.9 kg/dm³; delivery solution annealed.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
022Cr19Ni10 480 175 35

Ambient values from GB/T 13296-2023 Table 4 for 022Cr19Ni10. Heat treatment (Table 4): 1010–1150 °C, rapid cool. Density 7.9 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 022Cr19Ni10

For 022Cr19Ni10, the mill path is pierce / extrude / draw — never ERW or automatic-arc under GB/T 13296. Delivery is heat-treated and pickled unless overall ground/bored or protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO. Seamless W-C and W-H routes are the only valid order paths for 022Cr19Ni10 under GB/T 13296.

U-bend and cut-to-length options for 022Cr19Ni10 are available by agreement after the straight-tube tests clear. Surface quality rejects cracks, folds, laps, laminations and scabs on ID and OD. Pickling or bright-anneal decisions for 022Cr19Ni10 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

Manufacture records for 022Cr19Ni10 keep heat identity unbroken from melt through final NDT so the MTC can cite one cast for the whole bundle. Hydrostatic pressure or eddy-current class for 022Cr19Ni10 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Size practice for 022Cr19Ni10 remains cold-finished small OD for U-bend HX; confirm min-wall vs nominal-wall ordering language.

Dimensions and Tolerances for GB/T 13296 022Cr19Ni10

Cut lengths, multiple lengths, and U-bend developed lengths for 022Cr19Ni10 need explicit acknowledgement so finishing and crate length match the tubesheet drawing. Caution: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade. Tolerance basis for 022Cr19Ni10 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

Tolerance class follows the manufacture route ordered for 022Cr19Ni10; swapping W-C for W-H after acknowledgement without a dimensional review is how fit-up fails at the exchanger shop. Fixed lengths and multiple cut lengths for 022Cr19Ni10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 022Cr19Ni10 stays welded HX headers, food-adjacent steam lines, condensate coolers, and chloride-mild process exchangers.

Equivalent Grades for GB/T 13296 022Cr19Ni10

Under GB/T 13296, 022Cr19Ni10 is the governing seamless stainless boiler / heat-exchanger tube designation on this page. Commercial shorthand such as 304L / UNS S30403 helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the GB/T 13296 022Cr19Ni10 line. ASTM A213 / A269 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.

System Designation Notes
GB/T 13296 022Cr19Ni10 Governing tube grade for this page
Commercial / UNS (body only) 304L / UNS S30403 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related 304L chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Order discipline for 022Cr19Ni10 still points at GB/T 13296, not the brochure alias. Neighbours GB/T 13296 06Cr19Ni10, GB/T 13296 022Cr19Ni10N, GB/T 13296 06Cr18Ni11Ti, GB/T 13296 022Cr17Ni12Mo2 each carry their own mechanical table. Category hub: GB/T 13296. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (022Cr19Ni10).

Heat Treatment and Delivery Condition for GB/T 13296 022Cr19Ni10

Stabilisation after solution anneal is available by agreement for Ti/Nb marks; confirm whether 022Cr19Ni10 needs that second hold before acknowledging. HT reference: 1010–1150 °C, rapid cool. Recorded furnace charts for 022Cr19Ni10 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 022Cr19Ni10 duty: low-carbon 18-8 austenitic HX tube chosen when as-welded corrosion resistance matters more than elevated-temperature strength.

Mixed bundles of different heat-treatment furnace lots of 022Cr19Ni10 stay segregated so sampling remains traceable to one Table 4 run. Field heat treatment of 022Cr19Ni10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 022Cr19Ni10 remains cold-finished small OD for U-bend HX; confirm min-wall vs nominal-wall ordering language.

Corrosion Resistance of GB/T 13296 022Cr19Ni10

Coupon orientation, weld condition, and surface finish for 022Cr19Ni10 belong in the corrosion test order so method E or other coupons compare honestly to the installed tube. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 022Cr19Ni10 unless the mark is on the exemption list. Coupon orientation, weld condition, and surface finish for 022Cr19Ni10 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

For 022Cr19Ni10, specify whether IGC, hardness, or special corrosion coupons are extras beyond the clause 9 default before the heat is melted. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 022Cr19Ni10 rather than relying on wall thickness alone. This paragraph is locked to 022Cr19Ni10 duty: low-carbon 18-8 austenitic HX tube chosen when as-welded corrosion resistance matters more than elevated-temperature strength.

Applications of GB/T 13296 022Cr19Ni10 Seamless Tube

Commissioning dossiers should repeat 022Cr19Ni10 beside heat numbers so as-built isometrics stay tied to the same mill certificates. Application thread: welded HX headers, food-adjacent steam lines, condensate coolers, and chloride-mild process exchangers. Spool fabricators should copy 022Cr19Ni10 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 022Cr19Ni10 remains cold-finished small OD for U-bend HX; confirm min-wall vs nominal-wall ordering language.

Spare-tube stocks of 022Cr19Ni10 should keep heat identity so later retubing matches the original corrosion and strength file. Apps: welded HX headers, food-adjacent steam lines, condensate coolers, and chloride-mild process exchangers. Commissioning teams benefit when the as-built dossier repeats 022Cr19Ni10 beside heat numbers, linking isometric revisions to the same mill certificates. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

Weldability of GB/T 13296 022Cr19Ni10

Repair welding of 022Cr19Ni10 must preserve grade identity — a 308 deposit on a 6% Mo tube is a corrosion failure waiting to happen. Note: 308L fillers preferred; low heat input and clean purge keep the HAZ honest. Procedure qualification for 022Cr19Ni10 should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

Tubesheet joint design for 022Cr19Ni10 should state strength weld versus seal weld and any expansion sequence before production welding starts. Consumable lot control and shielding-gas notes for 022Cr19Ni10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 022Cr19Ni10 duty: low-carbon 18-8 austenitic HX tube chosen when as-welded corrosion resistance matters more than elevated-temperature strength.

Surface Finishes for GB/T 13296 022Cr19Ni10

Surface supply for 022Cr19Ni10 should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless tube, so finish is part of performance, not only appearance. Ambiguous “bright tube” language is clarified before finishing slots are booked.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

SHH STEEL sequences pickle, optional passivation, and any agreed polish for 022Cr19Ni10 after the heat-treatment evidence is on the certificate. Free-iron control and packing discipline matter as much as Ra numbers for long tube life in the field. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (022Cr19Ni10).

Inspection and Testing for GB/T 13296 022Cr19Ni10

Hardness by agreement for wall ≥1.7 mm on 022Cr19Ni10; grain-size evidence when the mark requires levels 4–7. Apps: welded HX headers, food-adjacent steam lines, condensate coolers, and chloride-mild process exchangers. Sampling plans for 022Cr19Ni10 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

Dimensional reports for 022Cr19Ni10 cite Table 1 tolerance basis (W-C vs W-H, min wall vs nominal wall) so receiving inspectors know which band applies. Non-conforming 022Cr19Ni10 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Corrosion framing beside 022Cr19Ni10: low carbon slows weld decay; pitting resistance still tracks Mo-free 18-8 behaviour.

Packaging and Shipping for GB/T 13296 022Cr19Ni10

U-bend crates for 022Cr19Ni10 need radius supports so cold-worked bends do not spring or scar in transit. Caution: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade. Bundle tickets for 022Cr19Ni10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

Long-term storage of 022Cr19Ni10 should keep bundles dry and off bare soil to protect the pickled surface before installation. Caution: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade. Desiccant and wrap choices for 022Cr19Ni10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

Packing lists for 022Cr19Ni10 cite net/gross weight and crate count so logistics and QA share one document set. Caution: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade. Claims handling for 022Cr19Ni10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 022Cr19Ni10 stays welded HX headers, food-adjacent steam lines, condensate coolers, and chloride-mild process exchangers.

Why Choose SHH STEEL

Traceability, pickle quality, and size discipline on 022Cr19Ni10 are part of the supply promise, not brochure extras. Role: low-carbon 18-8 austenitic HX tube chosen when as-welded corrosion resistance matters more than elevated-temperature strength. SHH STEEL can produce and supply 022Cr19Ni10 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

For 022Cr19Ni10, SHH STEEL can produce trial lengths for procedure qualification before bulk release when the project calendar needs it. Apps: welded HX headers, food-adjacent steam lines, condensate coolers, and chloride-mild process exchangers. SHH STEEL can make 022Cr19Ni10 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. This paragraph is locked to 022Cr19Ni10 duty: low-carbon 18-8 austenitic HX tube chosen when as-welded corrosion resistance matters more than elevated-temperature strength.

Supply Capability

From RFQ to crate, SHH STEEL can produce 022Cr19Ni10 as a boiler/HX product — not a repurposed fluid-pipe heat. Size hint: cold-finished small OD for U-bend HX; confirm min-wall vs nominal-wall ordering language. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 022Cr19Ni10 when the mill schedule allows. Keep the 022Cr19Ni10 caution visible here: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 022Cr19Ni10 (S30403)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes — SHH STEEL can supply alternate walls for 022Cr19Ni10 once design pressure, corrosion allowance, and min-wall rules are clear. Size hint: cold-finished small OD for U-bend HX; confirm min-wall vs nominal-wall ordering language. SHH STEEL can supply alternate walls and W-C/W-H classes for 022Cr19Ni10 once design pressure and corrosion allowance are clear. Weld-shop note tied to 022Cr19Ni10: 308L fillers preferred; low heat input and clean purge keep the HAZ honest.

Export packing and document sets for 022Cr19Ni10 are confirmed on the acknowledgement so customs and site QA see the same grade string. Caution: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade. SHH STEEL can produce trial lengths of 022Cr19Ni10 for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to 022Cr19Ni10: 308L fillers preferred; low heat input and clean purge keep the HAZ honest.

FAQ

What is GB/T 13296 022Cr19Ni10 seamless stainless steel tube used for?
GB/T 13296 022Cr19Ni10 is seamless stainless tube for boilers and heat exchangers — welded HX headers, food-adjacent steam lines, condensate coolers, and chloride-mild process exchangers. Role summary: low-carbon 18-8 austenitic HX tube chosen when as-welded corrosion resistance matters more than elevated-temperature strength. It is a Chinese product standard grade (S30403), not an automatic ASTM A213 certificate.
Is GB/T 13296 022Cr19Ni10 seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 022Cr19Ni10 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 022Cr19Ni10?
022Cr19Ni10 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 022Cr19Ni10 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 022Cr19Ni10 compare with sister grades 06Cr19Ni10, 022Cr19Ni10N, 06Cr18Ni11Ti?
022Cr19Ni10 is filed as austenitic. Typical sisters on the same RFQ are 06Cr19Ni10, 022Cr19Ni10N, 06Cr18Ni11Ti. Design caution: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 022Cr19Ni10?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 304L / UNS S30403 the same as ordering 022Cr19Ni10?
No. 304L / UNS S30403 is a commercial / UNS cross-walk for body text (unified S30403). The purchase order should lock GB/T 13296 and 022Cr19Ni10 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 022Cr19Ni10?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 022Cr19Ni10 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: cold-finished small OD for U-bend HX; confirm min-wall vs nominal-wall ordering language. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 022Cr19Ni10 be welded on site?
Shop guidance: 308L fillers preferred; low heat input and clean purge keep the HAZ honest. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade
When should I choose a higher-Mo or superaustenitic grade instead of 022Cr19Ni10?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: do not stretch 022Cr19Ni10 into high-temperature creep duty that belongs to 07Cr19Ni10 or a stabilised H grade Sister pointers: 06Cr19Ni10, 022Cr19Ni10N, 06Cr18Ni11Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 022Cr19Ni10 with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 022Cr19Ni10 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 022Cr19Ni10?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 022Cr19Ni10 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 022Cr19Ni10 is seamless stainless steel tube for boilers and heat exchangers — low-carbon 18-8 austenitic HX tube chosen when as-welded corrosion resistance matters more than elevated-temperature strength. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr19Ni10, 022Cr19Ni10N, 06Cr18Ni11Ti. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X