GB/T 13296 022Cr18Ni14Mo2Cu2 Seamless Stainless Steel Tube

GB/T 13296 022Cr18Ni14Mo2Cu2 seamless stainless steel tube (316LCu-class / UNS S31683, S31683), austenitic, Table 3 cast analysis, Rm min 480 MPa / Rp0.2 min 180 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
022Cr18Ni14Mo2Cu2 (S31683 / 316LCu-class / UNS S31683 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 022Cr18Ni14Mo2Cu2 Seamless Stainless Steel Tube

Boiler and heat-exchanger packages written to Chinese product standards look to GB/T 13296-2023 rather than inventing a mill grade from AISI shorthand alone. 022Cr18Ni14Mo2Cu2 is the Table 3/4 Chinese grade name for this austenitic chemistry (S31683). It pairs the 022 carbon ceiling with copper and molybdenum for acid exchangers.

Mill path for 022Cr18Ni14Mo2Cu2: manufacture symbol W-C/W-H, Table 4 heat treatment, Table 3 cast chemistry, Table 4 tensile floors, hydrostatic or eddy-current E3H, ultrasonic U2. SHH STEEL can make and supply the grade to that stack. Typical use: welded sulphuric coolers, sulphate condensers, and acid-plant exchangers. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 022Cr18Ni14Mo2Cu2 before production starts. Application context for 022Cr18Ni14Mo2Cu2 stays welded sulphuric coolers, sulphate condensers, and acid-plant exchangers.

Body text may mention 316LCu-class / UNS S31683 (unified S31683) for cross-reference, but the H1 and order line stay on 022Cr18Ni14Mo2Cu2. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket.

Order the standard the drawing and regulatory file actually require. Inside this 13296 series, compare 06Cr18Ni12Mo2Cu2, 022Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3 before stretching surface finish or wall alone. Duty thread: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service.

Inside this GB/T 13296 series, compare GB/T 13296 06Cr18Ni12Mo2Cu2, GB/T 13296 022Cr17Ni12Mo2, GB/T 13296 015Cr21Ni26Mo5Cu2, GB/T 13296 022Cr19Ni13Mo3. Hub: GB/T 13296.

Project teams specifying 022Cr18Ni14Mo2Cu2 should form hubs stay Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates — no verified plate product page is attached for this chemistry yet. Confirm 022Cr18Ni14Mo2Cu2 OD × wall and plate thickness on separate drawings.

Chemical Composition of GB/T 13296 022Cr18Ni14Mo2Cu2

Table 3 sets the melt limits for 022Cr18Ni14Mo2Cu2. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Highlight band: C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 12.00–16.00, Cr 17.00–19.00, Mo 1.20–2.75. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 3. Alias note: 316LCu-class / UNS S31683.

The composition table below is the cast window SHH STEEL quotes against for 022Cr18Ni14Mo2Cu2. Edition framing is GB/T 13296-2023. Use thread: welded sulphuric coolers, sulphate condensers, and acid-plant exchangers. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 022Cr18Ni14Mo2Cu2 before the order is acknowledged. Corrosion framing beside 022Cr18Ni14Mo2Cu2: L+Cu+Mo stack for welded acid HX.

Grade C Si Mn P S Ni Cr Mo Cu
022Cr18Ni14Mo2Cu2 ≤0.030 ≤1.00 ≤2.00 ≤0.035 ≤0.015 12.00–16.00 17.00–19.00 1.20–2.75 1.00–2.50

UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 022Cr18Ni14Mo2Cu2 (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 316LCu-class / UNS S31683, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 022Cr18Ni14Mo2Cu2 against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 022Cr18Ni14Mo2Cu2 before the heat is booked.

Mechanical Properties of GB/T 13296 022Cr18Ni14Mo2Cu2

Table 4 mechanical acceptance for 022Cr18Ni14Mo2Cu2: Rm min 480 MPa, Rp0.2 min 180 MPa, elongation min 35%. Note: UNCERTAIN — provisional vs paid Table 3/4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Delivery framing: solution annealed. Sampling follows the batch rules for 022Cr18Ni14Mo2Cu2.

Elevated-temperature Annex A Rp0.2 and Annex B 100000 h rupture tables name only selected H marks — check whether 022Cr18Ni14Mo2Cu2 appears before citing those numbers in a design note. Density 7.98 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
022Cr18Ni14Mo2Cu2 480 180 35

Ambient values from GB/T 13296-2023 Table 4 for 022Cr18Ni14Mo2Cu2. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1010–1150 °C, rapid cool. UNCERTAIN — provisional vs paid Table 3/4. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 022Cr18Ni14Mo2Cu2

SHH STEEL can produce 022Cr18Ni14Mo2Cu2 as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 4 heat treatment and pickle (or bright anneal) as ordered. Plain ends are default; bevels by agreement when the tubesheet weld prep needs it. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

After hot or cold working, 022Cr18Ni14Mo2Cu2 is heat-treated per Table 4 and finished to the ordered surface. Straightness limits differ for W-H (≤2.0 mm/m) and W-C (≤1.5 mm/m); full-length bow ≤0.15% of length. Pickling or bright-anneal decisions for 022Cr18Ni14Mo2Cu2 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Weld-shop note tied to 022Cr18Ni14Mo2Cu2: low-C Cu-aware fillers; purge discipline on thin walls.

Straightness, end finish, and marking for 022Cr18Ni14Mo2Cu2 are checked before bundling so tubesheet fit-up crews receive usable lengths. Caution: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket. Hydrostatic pressure or eddy-current class for 022Cr18Ni14Mo2Cu2 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Application context for 022Cr18Ni14Mo2Cu2 stays welded sulphuric coolers, sulphate condensers, and acid-plant exchangers.

Dimensions and Tolerances for GB/T 13296 022Cr18Ni14Mo2Cu2

Minimum-wall ordering is common for HX duty on 022Cr18Ni14Mo2Cu2: W-C min-wall tolerance is +20%S/0 for D≤38 mm and +22%S/0 above; W-H min-wall is +0.90/0 mm for S≤4.0 mm and +25%S/0 above. Confirm nominal-wall versus min-wall language on the PO. Tolerance basis for 022Cr18Ni14Mo2Cu2 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 022Cr18Ni14Mo2Cu2: low-C Cu-aware fillers; purge discipline on thin walls.

Bevel geometry, land, and ID cleanliness notes for 022Cr18Ni14Mo2Cu2 belong on the acknowledgement when automatic welding to the tubesheet is planned. Apps: welded sulphuric coolers, sulphate condensers, and acid-plant exchangers. Fixed lengths and multiple cut lengths for 022Cr18Ni14Mo2Cu2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 022Cr18Ni14Mo2Cu2 stays welded sulphuric coolers, sulphate condensers, and acid-plant exchangers.

Equivalent Grades for GB/T 13296 022Cr18Ni14Mo2Cu2

Cross-references help sourcing 022Cr18Ni14Mo2Cu2, but they do not replace the GB/T 13296 grade line on the enquiry. Family framing here is austenitic; delivery practice from the crib is “solution annealed”. Related ASTM or EN numbers are starting points for engineering comparison, not automatic substitutes. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (022Cr18Ni14Mo2Cu2).

System Designation Notes
GB/T 13296 022Cr18Ni14Mo2Cu2 Governing tube grade for this page
Commercial / UNS (body only) 316LCu-class / UNS S31683 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Inside this series compare GB/T 13296 06Cr18Ni12Mo2Cu2, GB/T 13296 022Cr17Ni12Mo2, GB/T 13296 015Cr21Ni26Mo5Cu2, GB/T 13296 022Cr19Ni13Mo3 before swapping marks for medium or temperature. Keep this caution visible for 022Cr18Ni14Mo2Cu2: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket. Hub: GB/T 13296. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (022Cr18Ni14Mo2Cu2).

Heat Treatment and Delivery Condition for GB/T 13296 022Cr18Ni14Mo2Cu2

Table 4 schedules 022Cr18Ni14Mo2Cu2 at 1010–1150 °C, rapid cool. Protective-atmosphere bright anneal may omit pickle when agreed. Grain-size extras: per family practice. Caution: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket. Recorded furnace charts for 022Cr18Ni14Mo2Cu2 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 022Cr18Ni14Mo2Cu2 duty: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service.

Recorded cool method for 022Cr18Ni14Mo2Cu2 matters as much as peak temperature — rapid cool versus air/slow cool is a family identity issue. Density 7.98 kg/dm³. Field heat treatment of 022Cr18Ni14Mo2Cu2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 022Cr18Ni14Mo2Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket.

Corrosion Resistance of GB/T 13296 022Cr18Ni14Mo2Cu2

Select 022Cr18Ni14Mo2Cu2 when the process side matches this framing: L+Cu+Mo stack for welded acid HX. Sister upgrades on the same hub include 06Cr18Ni12Mo2Cu2, 022Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3. Role: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. Coupon orientation, weld condition, and surface finish for 022Cr18Ni14Mo2Cu2 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Weld-shop note tied to 022Cr18Ni14Mo2Cu2: low-C Cu-aware fillers; purge discipline on thin walls.

Oxidation-first marks and PREN-first marks in this series are not interchangeable — 022Cr18Ni14Mo2Cu2 sits on the L+Cu+Mo stack for welded acid HX side of that split. Caution: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 022Cr18Ni14Mo2Cu2 rather than relying on wall thickness alone. Application context for 022Cr18Ni14Mo2Cu2 stays welded sulphuric coolers, sulphate condensers, and acid-plant exchangers.

Applications of GB/T 13296 022Cr18Ni14Mo2Cu2 Seamless Tube

Exchanger and boiler designers reach for 022Cr18Ni14Mo2Cu2 when: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. Common sketch: welded sulphuric coolers, sulphate condensers, and acid-plant exchangers. Caution on the datasheet: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket. Spool fabricators should copy 022Cr18Ni14Mo2Cu2 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to 022Cr18Ni14Mo2Cu2 duty: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service.

U-bend radius, heat treatment after bending, and tubesheet weld details for 022Cr18Ni14Mo2Cu2 belong in the fabrication specification, not only in the mill PO. Caution: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket. Commissioning teams benefit when the as-built dossier repeats 022Cr18Ni14Mo2Cu2 beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to 022Cr18Ni14Mo2Cu2: low-C Cu-aware fillers; purge discipline on thin walls.

Weldability of GB/T 13296 022Cr18Ni14Mo2Cu2

Shop guidance for 022Cr18Ni14Mo2Cu2: low-C Cu-aware fillers; purge discipline on thin walls. Autogenous orbital welds to tubesheets need clean ID and controlled heat input. Family: austenitic. Procedure qualification for 022Cr18Ni14Mo2Cu2 should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 022Cr18Ni14Mo2Cu2 remains cold-finished acid-HX OD×min wall.

Post-weld heat treatment of 022Cr18Ni14Mo2Cu2 is uncommon for austenitics but may be specified for stabilised marks or ferritic toughness — write it explicitly. Caution: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket. Consumable lot control and shielding-gas notes for 022Cr18Ni14Mo2Cu2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 022Cr18Ni14Mo2Cu2: L+Cu+Mo stack for welded acid HX.

Surface Finishes for GB/T 13296 022Cr18Ni14Mo2Cu2

Finish options for 022Cr18Ni14Mo2Cu2 follow the ordered heat-treatment route under GB/T 13296. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: solution annealed. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (022Cr18Ni14Mo2Cu2).

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Reject grinding burns, embedded free iron, and unrepaired undercut on 022Cr18Ni14Mo2Cu2 before bundles close. Passivation analogues (A967-style) are optional extras — the governing step remains correct heat treatment under GB/T 13296 for this austenitic mark. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 022Cr18Ni14Mo2Cu2.

Inspection and Testing for GB/T 13296 022Cr18Ni14Mo2Cu2

Batch rules for 022Cr18Ni14Mo2Cu2: same grade, heat, size, and heat-treatment lot. Sampling counts follow OD/wall thresholds in the standard. Role: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. Sampling plans for 022Cr18Ni14Mo2Cu2 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 022Cr18Ni14Mo2Cu2: low-C Cu-aware fillers; purge discipline on thin walls.

Witness points for 022Cr18Ni14Mo2Cu2 (hydro, UT, IGC) should be booked before the tubes leave the finishing bay. Duty: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. Non-conforming 022Cr18Ni14Mo2Cu2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Application context for 022Cr18Ni14Mo2Cu2 stays welded sulphuric coolers, sulphate condensers, and acid-plant exchangers.

Packaging and Shipping for GB/T 13296 022Cr18Ni14Mo2Cu2

Export crates for 022Cr18Ni14Mo2Cu2 protect thin-wall HX stock against handling dents that would fail UT or tubesheet fit-up. Role: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. Bundle tickets for 022Cr18Ni14Mo2Cu2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 022Cr18Ni14Mo2Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket.

Claims handling for 022Cr18Ni14Mo2Cu2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Duty: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. Desiccant and wrap choices for 022Cr18Ni14Mo2Cu2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 022Cr18Ni14Mo2Cu2 remains cold-finished acid-HX OD×min wall.

Loose tubes of 022Cr18Ni14Mo2Cu2 are avoided; strapped bundles keep heat lots together for MTC matching. Role: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. Claims handling for 022Cr18Ni14Mo2Cu2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 022Cr18Ni14Mo2Cu2: low-C Cu-aware fillers; purge discipline on thin walls.

Why Choose SHH STEEL

Why buyers stay with SHH STEEL for 022Cr18Ni14Mo2Cu2: written acknowledgements that name W-C/W-H and Table 4 heat treatment before melt, plus MTCs that repeat the Chinese grade. Caution: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket. SHH STEEL can produce and supply 022Cr18Ni14Mo2Cu2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Corrosion framing beside 022Cr18Ni14Mo2Cu2: L+Cu+Mo stack for welded acid HX.

Engineering support for 022Cr18Ni14Mo2Cu2 includes clarifying min-wall versus nominal-wall language and Annex A/B applicability before the heat is melted. Caution: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket. SHH STEEL can make 022Cr18Ni14Mo2Cu2 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Corrosion framing beside 022Cr18Ni14Mo2Cu2: L+Cu+Mo stack for welded acid HX.

Supply Capability

Supply capability for 022Cr18Ni14Mo2Cu2: W-C and W-H seamless routes, pickled or bright, plain or bevelled ends, random or fixed lengths. SHH STEEL can make the grade when melt and finishing slots align. Apps: welded sulphuric coolers, sulphate condensers, and acid-plant exchangers. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 022Cr18Ni14Mo2Cu2 when the mill schedule allows. Corrosion framing beside 022Cr18Ni14Mo2Cu2: L+Cu+Mo stack for welded acid HX.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 022Cr18Ni14Mo2Cu2 (S31683)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes for 022Cr18Ni14Mo2Cu2 centre on cold-finished mid-OD HX tubes and selected hot-finished boiler walls; ask for the current matrix against your datasheet. Apps: welded sulphuric coolers, sulphate condensers, and acid-plant exchangers. SHH STEEL can supply alternate walls and W-C/W-H classes for 022Cr18Ni14Mo2Cu2 once design pressure and corrosion allowance are clear. This paragraph is locked to 022Cr18Ni14Mo2Cu2 duty: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service.

Lead time for 022Cr18Ni14Mo2Cu2 tracks melt booking, finishing, and any third-party holds — send the full test matrix with the RFQ. Role: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. SHH STEEL can produce trial lengths of 022Cr18Ni14Mo2Cu2 for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside 022Cr18Ni14Mo2Cu2: L+Cu+Mo stack for welded acid HX.

FAQ

What is GB/T 13296 022Cr18Ni14Mo2Cu2 seamless stainless steel tube used for?
GB/T 13296 022Cr18Ni14Mo2Cu2 is seamless stainless tube for boilers and heat exchangers — welded sulphuric coolers, sulphate condensers, and acid-plant exchangers. Role summary: low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. It is a Chinese product standard grade (S31683), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
Is GB/T 13296 022Cr18Ni14Mo2Cu2 seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 022Cr18Ni14Mo2Cu2 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 022Cr18Ni14Mo2Cu2?
022Cr18Ni14Mo2Cu2 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 022Cr18Ni14Mo2Cu2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 022Cr18Ni14Mo2Cu2 compare with sister grades 06Cr18Ni12Mo2Cu2, 022Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2?
022Cr18Ni14Mo2Cu2 is filed as austenitic. Typical sisters on the same RFQ are 06Cr18Ni12Mo2Cu2, 022Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2. Design caution: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 022Cr18Ni14Mo2Cu2?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 316LCu-class / UNS S31683 the same as ordering 022Cr18Ni14Mo2Cu2?
No. 316LCu-class / UNS S31683 is a commercial / UNS cross-walk for body text (unified S31683). The purchase order should lock GB/T 13296 and 022Cr18Ni14Mo2Cu2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 022Cr18Ni14Mo2Cu2?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 022Cr18Ni14Mo2Cu2 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: cold-finished acid-HX OD×min wall. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 022Cr18Ni14Mo2Cu2 be welded on site?
Shop guidance: low-C Cu-aware fillers; purge discipline on thin walls. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket
When should I choose a higher-Mo or superaustenitic grade instead of 022Cr18Ni14Mo2Cu2?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN vs paid Table 3/4; L-carbon and Cu must both clear the melt ticket Sister pointers: 06Cr18Ni12Mo2Cu2, 022Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 022Cr18Ni14Mo2Cu2 with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 022Cr18Ni14Mo2Cu2 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 022Cr18Ni14Mo2Cu2?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 022Cr18Ni14Mo2Cu2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 022Cr18Ni14Mo2Cu2 is seamless stainless steel tube for boilers and heat exchangers — low-carbon Cu-Mo austenitic tube for welded reducing-acid HX service. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr18Ni12Mo2Cu2, 022Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X