GB/T 13296 022Cr19Ni13Mo3 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 022Cr19Ni13Mo3 Seamless Stainless Steel Tube

GB/T 13296 022Cr19Ni13Mo3 seamless stainless steel tube (317L / UNS S31703, S31703), austenitic, Table 3 cast analysis, Rm min 480 MPa / Rp0.2 min 175 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
022Cr19Ni13Mo3 (S31703 / 317L / UNS S31703 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 022Cr19Ni13Mo3 Seamless Stainless Steel Tube

When the approved vendor list and exchanger datasheet say GB/T 13296, the grade mark has to be the Chinese designation. 022Cr19Ni13Mo3 is the full product grade for this austenitic seamless tube. It is the L sister of 06Cr19Ni13Mo3 for welded corrosive packages.

SHH STEEL can supply 022Cr19Ni13Mo3 seamless tube in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the exchanger: low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 022Cr19Ni13Mo3 before production starts. Size practice for 022Cr19Ni13Mo3 remains W-C U-bend and straight condenser tubes.

Equivalence talk to 317L / UNS S31703 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 13296 022Cr19Ni13Mo3, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC.

Related ASTM A213 tube pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 06Cr19Ni13Mo3, 022Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN, 022Cr18Ni14Mo2Cu2. Use thread: welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L.

Inside this GB/T 13296 series, compare GB/T 13296 06Cr19Ni13Mo3, GB/T 13296 022Cr17Ni12Mo2, GB/T 13296 015Cr20Ni18Mo6CuN, GB/T 13296 022Cr18Ni14Mo2Cu2. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP317L.

Chemical Composition of GB/T 13296 022Cr19Ni13Mo3

Chemistry control on 022Cr19Ni13Mo3 starts at the ladle. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Expect C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 11.00–15.00, Cr 18.00–20.00, Mo 3.00–4.00 within Table 3, reported on the inspection document against the heat. Body alias 317L / UNS S31703 does not widen those windows.

Read the table with the family in mind — austenitic — and with caution UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC. Numbers without the matching Table 4 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 022Cr19Ni13Mo3 before the order is acknowledged. Corrosion framing beside 022Cr19Ni13Mo3: L-carbon plus 3–4% Mo for HAZ and pitting life.

Grade C Si Mn P S Ni Cr Mo
022Cr19Ni13Mo3 ≤0.030 ≤1.00 ≤2.00 ≤0.035 ≤0.015 11.00–15.00 18.00–20.00 3.00–4.00

UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 022Cr19Ni13Mo3 (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 317L / UNS S31703, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 022Cr19Ni13Mo3 against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 022Cr19Ni13Mo3 before the heat is booked.

Mechanical Properties of GB/T 13296 022Cr19Ni13Mo3

Proof stress and tensile minima for 022Cr19Ni13Mo3 sit at Rm min 480 MPa, Rp0.2 min 175 MPa, elongation min 35%. Note: UNCERTAIN — provisional vs paid Table 3/4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Flattening and flaring back ductility when size allows. Watch-out: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC.

Batch size limits (D≤76 mm and S≤3 mm: ≤400 tubes; otherwise ≤200) keep sampling honest for 022Cr19Ni13Mo3. Retests follow GB/T 2102. Density 7.98 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
022Cr19Ni13Mo3 480 175 35

Ambient values from GB/T 13296-2023 Table 4 for 022Cr19Ni13Mo3. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1010–1150 °C, rapid cool. UNCERTAIN — provisional vs paid Table 3/4. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 022Cr19Ni13Mo3

Seamless is not optional wording for 022Cr19Ni13Mo3: the standard limits manufacture to W-C or W-H seamless routes for boiler and heat-exchanger tube. Pick W-C when OD precision and U-bend finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 13296 line item. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

SHH STEEL schedules piercing, elongation, and finishing for 022Cr19Ni13Mo3 against the W-C or W-H symbol frozen on the acknowledgement. Ovality and wall eccentricity stay inside 80% of the respective OD and wall tolerances. Pickling or bright-anneal decisions for 022Cr19Ni13Mo3 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Keep the 022Cr19Ni13Mo3 caution visible here: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC.

Cold-finish depth of longitudinal marks on 022Cr19Ni13Mo3 is limited to ≤4% of wall and ≤0.2 mm; hot-finish ≤5% and ≤0.4 mm. Apps: welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L. Hydrostatic pressure or eddy-current class for 022Cr19Ni13Mo3 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Size practice for 022Cr19Ni13Mo3 remains W-C U-bend and straight condenser tubes.

Dimensions and Tolerances for GB/T 13296 022Cr19Ni13Mo3

When 022Cr19Ni13Mo3 ships as nominal wall, the note under Table 1 still applies different ± bands for hot and cold routes — do not mix W-C absolute OD tols with W-H percentage thinking. Practice: W-C U-bend and straight condenser tubes. Tolerance basis for 022Cr19Ni13Mo3 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 022Cr19Ni13Mo3 duty: low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service.

Fixed lengths of 022Cr19Ni13Mo3 are end-protected so bevels and ID finish survive inland and ocean transit. Random lengths stay inside the usual 2000–12000 mm window unless agreed otherwise. Fixed lengths and multiple cut lengths for 022Cr19Ni13Mo3 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 022Cr19Ni13Mo3 duty: low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service.

Equivalent Grades for GB/T 13296 022Cr19Ni13Mo3

The table below maps GB/T 13296 022Cr19Ni13Mo3 to commercial aliases and related systems without inventing false one-to-one substitutes. Alias 317L / UNS S31703 stays body-only. Pack caution: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC. Dual marking is a purchase-order option that still requires every limit that matters for 022Cr19Ni13Mo3 to be verified on the heat.

System Designation Notes
GB/T 13296 022Cr19Ni13Mo3 Governing tube grade for this page
Commercial / UNS (body only) 317L / UNS S31703 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related 317L chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

When the service outgrows 022Cr19Ni13Mo3, move to a sister rather than stretching the alias: GB/T 13296 06Cr19Ni13Mo3, GB/T 13296 022Cr17Ni12Mo2, GB/T 13296 015Cr20Ni18Mo6CuN, GB/T 13296 022Cr18Ni14Mo2Cu2. Full list under GB/T 13296. Dual marking is a purchase-order option that still requires every limit that matters for 022Cr19Ni13Mo3 to be verified on the heat. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (022Cr19Ni13Mo3).

Project teams specifying 022Cr19Ni13Mo3 should link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and GB/T 4237 022Cr19Ni13Mo3 so purchasing does not treat one product form as the other. Flat Chinese grades in-family are indexed at GB/T 4237. Confirm 022Cr19Ni13Mo3 OD × wall and plate thickness on separate drawings.

Heat Treatment and Delivery Condition for GB/T 13296 022Cr19Ni13Mo3

For 022Cr19Ni13Mo3, solution or anneal practice is not a free mill choice — it is the Table 4 band tied to the grade. Delivery: solution annealed. Role: low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service. Recorded furnace charts for 022Cr19Ni13Mo3 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 022Cr19Ni13Mo3 caution visible here: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC.

When Annex A elevated Rp0.2 is invoked, the certificate for 022Cr19Ni13Mo3 should still show the Table 4 delivery treatment actually performed. Apps: welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L. Field heat treatment of 022Cr19Ni13Mo3 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 022Cr19Ni13Mo3 caution visible here: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC.

Corrosion Resistance of GB/T 13296 022Cr19Ni13Mo3

Pitting, crevice, oxidation, or weld-decay limiters for 022Cr19Ni13Mo3 should be named in the datasheet rather than inferred from the AISI alias alone. Framing: L-carbon plus 3–4% Mo for HAZ and pitting life. Coupon orientation, weld condition, and surface finish for 022Cr19Ni13Mo3 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Corrosion framing beside 022Cr19Ni13Mo3: L-carbon plus 3–4% Mo for HAZ and pitting life.

Pickling quality and free-iron cleanliness after fabrication affect startup corrosion of 022Cr19Ni13Mo3 as much as cast chemistry. Role: low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 022Cr19Ni13Mo3 rather than relying on wall thickness alone. Application context for 022Cr19Ni13Mo3 stays welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L.

Applications of GB/T 13296 022Cr19Ni13Mo3 Seamless Tube

Use 022Cr19Ni13Mo3 on packages that match welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L. Nearby sisters 06Cr19Ni13Mo3, 022Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN, 022Cr18Ni14Mo2Cu2 cover adjacent media or temperature steps. Weld-shop note: 317L fillers; low heat input on thin walls. Spool fabricators should copy 022Cr19Ni13Mo3 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Weld-shop note tied to 022Cr19Ni13Mo3: 317L fillers; low heat input on thin walls.

When the process medium changes mid-project, revisit whether 022Cr19Ni13Mo3 still fits before releasing more heats. Sisters: 06Cr19Ni13Mo3, 022Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN, 022Cr18Ni14Mo2Cu2. Commissioning teams benefit when the as-built dossier repeats 022Cr19Ni13Mo3 beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 022Cr19Ni13Mo3 stays welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L.

Weldability of GB/T 13296 022Cr19Ni13Mo3

Consumable selection for 022Cr19Ni13Mo3 follows 317L fillers; low heat input on thin walls. Do not improvise under-alloyed fillers on Mo or Cu grades. Role: low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service. Procedure qualification for 022Cr19Ni13Mo3 should use the same product form and wall class as production, including the seamless finish that will ship. Application context for 022Cr19Ni13Mo3 stays welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L.

Ferrite control and hot-cracking risk for 022Cr19Ni13Mo3 depend on the family chemistry; qualify on production wall, not only on plate coupons. Weld shop: 317L fillers; low heat input on thin walls. Consumable lot control and shielding-gas notes for 022Cr19Ni13Mo3 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 022Cr19Ni13Mo3 caution visible here: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC.

Surface Finishes for GB/T 13296 022Cr19Ni13Mo3

Typical GB/T 13296 supply for 022Cr19Ni13Mo3 is a clean pickle after the required heat treatment, with bright anneal reserved for scale-free OD/ID appearance and ground/polished finishes reserved for written roughness targets. Free-iron control starts at the finishing bay, not at commissioning. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 022Cr19Ni13Mo3.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

OD stencil ink on 022Cr19Ni13Mo3 should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC. Close bundles only after free-iron and burn marks are cleared.

Inspection and Testing for GB/T 13296 022Cr19Ni13Mo3

SHH STEEL keeps heat identity for 022Cr19Ni13Mo3 unbroken from melt through bundle tags, including third-party hold points written into the PO. Caution: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC. Sampling plans for 022Cr19Ni13Mo3 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 022Cr19Ni13Mo3: 317L fillers; low heat input on thin walls.

Certificate lines for 022Cr19Ni13Mo3 must repeat the Chinese grade, unified number, manufacture symbol, and heat treatment actually performed. Caution: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC. Non-conforming 022Cr19Ni13Mo3 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Application context for 022Cr19Ni13Mo3 stays welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L.

Packaging and Shipping for GB/T 13296 022Cr19Ni13Mo3

Desiccant and wrap choices for 022Cr19Ni13Mo3 follow voyage length and storage climate on the shipping order, not a one-size export habit. Apps: welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L. Bundle tickets for 022Cr19Ni13Mo3 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 022Cr19Ni13Mo3: L-carbon plus 3–4% Mo for HAZ and pitting life.

Inland trucking of 022Cr19Ni13Mo3 still needs end protection — most ID dents happen between the port and the exchanger shop. Apps: welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L. Desiccant and wrap choices for 022Cr19Ni13Mo3 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 022Cr19Ni13Mo3 caution visible here: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC.

Barcode or stencil extras for 022Cr19Ni13Mo3 are available when the owner’s material system needs them. Apps: welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L. Claims handling for 022Cr19Ni13Mo3 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to 022Cr19Ni13Mo3 duty: low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service.

Why Choose SHH STEEL

SHH STEEL can make 022Cr19Ni13Mo3 to a boiler/HX test stack — hydro or E3H, UT U2, flattening/flaring, IGC when required — instead of a generic stainless tube habit. Apps: welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L. SHH STEEL can produce and supply 022Cr19Ni13Mo3 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. This paragraph is locked to 022Cr19Ni13Mo3 duty: low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service.

SHH STEEL can supply 022Cr19Ni13Mo3 with third-party inspection hold points written into the itinerary. Weld-shop note: 317L fillers; low heat input on thin walls. SHH STEEL can make 022Cr19Ni13Mo3 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Corrosion framing beside 022Cr19Ni13Mo3: L-carbon plus 3–4% Mo for HAZ and pitting life.

Supply Capability

SHH STEEL can supply 022Cr19Ni13Mo3 with EN 10204 3.1 style documents, IGC when required, and hardness by agreement. Caution: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 022Cr19Ni13Mo3 when the mill schedule allows. Corrosion framing beside 022Cr19Ni13Mo3: L-carbon plus 3–4% Mo for HAZ and pitting life.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 022Cr19Ni13Mo3 (S31703)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes: rolling cycles for 022Cr19Ni13Mo3 cover usual 2000–12000 mm lengths; cut-to-length and multiple lengths ship once tests clear. Caution: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC. SHH STEEL can supply alternate walls and W-C/W-H classes for 022Cr19Ni13Mo3 once design pressure and corrosion allowance are clear. Size practice for 022Cr19Ni13Mo3 remains W-C U-bend and straight condenser tubes.

SHH STEEL can supply replacement retubing heats of 022Cr19Ni13Mo3 matched to prior certificates when the plant provides heat history. Apps: welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L. SHH STEEL can produce trial lengths of 022Cr19Ni13Mo3 for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside 022Cr19Ni13Mo3: L-carbon plus 3–4% Mo for HAZ and pitting life.

FAQ

What is GB/T 13296 022Cr19Ni13Mo3 seamless stainless steel tube used for?
GB/T 13296 022Cr19Ni13Mo3 is seamless stainless tube for boilers and heat exchangers — welded chemical condensers, scrubber coolers, and chloride HX that outgrew 316L. Role summary: low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service. It is a Chinese product standard grade (S31703), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
Is GB/T 13296 022Cr19Ni13Mo3 seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 022Cr19Ni13Mo3 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 022Cr19Ni13Mo3?
022Cr19Ni13Mo3 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 022Cr19Ni13Mo3 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 022Cr19Ni13Mo3 compare with sister grades 06Cr19Ni13Mo3, 022Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN?
022Cr19Ni13Mo3 is filed as austenitic. Typical sisters on the same RFQ are 06Cr19Ni13Mo3, 022Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN. Design caution: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 022Cr19Ni13Mo3?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 317L / UNS S31703 the same as ordering 022Cr19Ni13Mo3?
No. 317L / UNS S31703 is a commercial / UNS cross-walk for body text (unified S31703). The purchase order should lock GB/T 13296 and 022Cr19Ni13Mo3 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 022Cr19Ni13Mo3?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 022Cr19Ni13Mo3 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: W-C U-bend and straight condenser tubes. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 022Cr19Ni13Mo3 be welded on site?
Shop guidance: 317L fillers; low heat input on thin walls. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC
When should I choose a higher-Mo or superaustenitic grade instead of 022Cr19Ni13Mo3?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN vs paid Table 3/4; keep Mo and C ceilings visible on the MTC Sister pointers: 06Cr19Ni13Mo3, 022Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 022Cr19Ni13Mo3 with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 022Cr19Ni13Mo3 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 022Cr19Ni13Mo3?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 022Cr19Ni13Mo3 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 022Cr19Ni13Mo3 is seamless stainless steel tube for boilers and heat exchangers — low-carbon higher-Mo austenitic tube for as-welded aggressive chloride HX service. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr19Ni13Mo3, 022Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response