GB/T 13296 015Cr20Ni18Mo6CuN Seamless Stainless Steel Tube

GB/T 13296 015Cr20Ni18Mo6CuN seamless stainless steel tube (254SMO-class / UNS S31254-related, S31252), austenitic, Table 3 cast analysis, Rm min 675 MPa / Rp0.2 min 310 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
015Cr20Ni18Mo6CuN (S31252 / 254SMO-class / UNS S31254-related — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 015Cr20Ni18Mo6CuN Seamless Stainless Steel Tube

Boiler and heat-exchanger packages written to Chinese product standards look to GB/T 13296-2023 rather than inventing a mill grade from AISI shorthand alone. 015Cr20Ni18Mo6CuN is the Table 3/4 Chinese grade name for this austenitic chemistry (S31252). It is the 254SMO-class entry in this boiler/HX tube series.

Mill path for 015Cr20Ni18Mo6CuN: manufacture symbol W-C/W-H, Table 4 heat treatment, Table 3 cast chemistry, Table 4 tensile floors, hydrostatic or eddy-current E3H, ultrasonic U2. SHH STEEL can make and supply the grade to that stack. Typical use: seawater coolers, scrubber condensers, and high-PREN chemical HX. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 015Cr20Ni18Mo6CuN before production starts. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo+N+Cu PREN for crevice and pitting life far above 316/317.

Body text may mention 254SMO-class / UNS S31254-related (unified S31252) for cross-reference, but the H1 and order line stay on 015Cr20Ni18Mo6CuN. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats.

Order the standard the drawing and regulatory file actually require. Inside this 13296 series, compare 022Cr21Ni25Mo7N, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2 before stretching surface finish or wall alone. Duty thread: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers.

Inside this GB/T 13296 series, compare GB/T 13296 022Cr21Ni25Mo7N, GB/T 13296 015Cr21Ni26Mo5Cu2, GB/T 13296 022Cr19Ni13Mo3, GB/T 13296 022Cr17Ni12Mo2. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASME SA213 S31254.

Chemical Composition of GB/T 13296 015Cr20Ni18Mo6CuN

Table 3 sets the melt limits for 015Cr20Ni18Mo6CuN. Highlight band: C ≤0.020, Si ≤0.80, Mn ≤1.00, P ≤0.030, S ≤0.010, Ni 17.50–18.50, Cr 19.50–20.50, Mo 6.00–6.50. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 3. Alias note: 254SMO-class / UNS S31254-related. Every ladle analysis for 015Cr20Ni18Mo6CuN is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. This paragraph is locked to 015Cr20Ni18Mo6CuN duty: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers.

The composition table below is the cast window SHH STEEL quotes against for 015Cr20Ni18Mo6CuN. Edition framing is GB/T 13296-2023. Use thread: seawater coolers, scrubber condensers, and high-PREN chemical HX. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 015Cr20Ni18Mo6CuN before the order is acknowledged. Size practice for 015Cr20Ni18Mo6CuN remains cold-finished thin-wall HX with premium surface notes.

Grade C Si Mn P S Ni Cr Mo Cu N
015Cr20Ni18Mo6CuN ≤0.020 ≤0.80 ≤1.00 ≤0.030 ≤0.010 17.50–18.50 19.50–20.50 6.00–6.50 0.50–1.00 0.18–0.22

Mechanical Properties of GB/T 13296 015Cr20Ni18Mo6CuN

Table 4 mechanical acceptance for 015Cr20Ni18Mo6CuN: Rm min 675 MPa, Rp0.2 min 310 MPa, elongation min 35%. Note: hardness agreement band tighter than common austenitics (Table 5). Delivery framing: solution annealed. Sampling follows the batch rules for 015Cr20Ni18Mo6CuN. Tensile sampling follows the batch rules for the ordered test unit of 015Cr20Ni18Mo6CuN, and retests follow GB/T 2102 when a result sits under the Table 4 floor. Weld-shop note tied to 015Cr20Ni18Mo6CuN: matching super-austenitic fillers; strict heat-input and ferrite control.

Elevated-temperature Annex A Rp0.2 and Annex B 100000 h rupture tables name only selected H marks — check whether 015Cr20Ni18Mo6CuN appears before citing those numbers in a design note. Density 8.1 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
015Cr20Ni18Mo6CuN 675 310 35

Ambient values from GB/T 13296-2023 Table 4 for 015Cr20Ni18Mo6CuN. Heat treatment (Table 4): 1010–1150 °C, rapid cool. hardness agreement band tighter than common austenitics (Table 5). Density 8.1 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 015Cr20Ni18Mo6CuN

Seamless is not optional wording for 015Cr20Ni18Mo6CuN: the standard limits manufacture to W-C or W-H seamless routes for boiler and heat-exchanger tube. Pick W-C when OD precision and U-bend finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 13296 line item. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

After hot or cold working, 015Cr20Ni18Mo6CuN is heat-treated per Table 4 and finished to the ordered surface. Straightness limits differ for W-H (≤2.0 mm/m) and W-C (≤1.5 mm/m); full-length bow ≤0.15% of length. Pickling or bright-anneal decisions for 015Cr20Ni18Mo6CuN stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo+N+Cu PREN for crevice and pitting life far above 316/317.

Straightness, end finish, and marking for 015Cr20Ni18Mo6CuN are checked before bundling so tubesheet fit-up crews receive usable lengths. Caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats. Hydrostatic pressure or eddy-current class for 015Cr20Ni18Mo6CuN is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Weld-shop note tied to 015Cr20Ni18Mo6CuN: matching super-austenitic fillers; strict heat-input and ferrite control.

Dimensions and Tolerances for GB/T 13296 015Cr20Ni18Mo6CuN

Minimum-wall ordering is common for HX duty on 015Cr20Ni18Mo6CuN: W-C min-wall tolerance is +20%S/0 for D≤38 mm and +22%S/0 above; W-H min-wall is +0.90/0 mm for S≤4.0 mm and +25%S/0 above. Confirm nominal-wall versus min-wall language on the PO. Tolerance basis for 015Cr20Ni18Mo6CuN follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 015Cr20Ni18Mo6CuN: matching super-austenitic fillers; strict heat-input and ferrite control.

Bevel geometry, land, and ID cleanliness notes for 015Cr20Ni18Mo6CuN belong on the acknowledgement when automatic welding to the tubesheet is planned. Apps: seawater coolers, scrubber condensers, and high-PREN chemical HX. Fixed lengths and multiple cut lengths for 015Cr20Ni18Mo6CuN are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo+N+Cu PREN for crevice and pitting life far above 316/317.

Equivalent Grades for GB/T 13296 015Cr20Ni18Mo6CuN

The table below maps GB/T 13296 015Cr20Ni18Mo6CuN to commercial aliases and related systems without inventing false one-to-one substitutes. Alias 254SMO-class / UNS S31254-related stays body-only. Pack caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (015Cr20Ni18Mo6CuN).

System Designation Notes
GB/T 13296 015Cr20Ni18Mo6CuN Governing tube grade for this page
Commercial / UNS (body only) 254SMO-class / UNS S31254-related (unified S31252) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related 6Mo / superaustenitic family talk (no identical TP asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

We deliberately avoid inventing a false one-to-one for every foreign system on 015Cr20Ni18Mo6CuN. Use GB/T 13296 022Cr21Ni25Mo7N, GB/T 13296 015Cr21Ni26Mo5Cu2, GB/T 13296 022Cr19Ni13Mo3, GB/T 13296 022Cr17Ni12Mo2 for in-series alternatives, and keep GB/T 13296 as the category landing page. Dual marking is a purchase-order option that still requires every limit that matters for 015Cr20Ni18Mo6CuN to be verified on the heat.

On 015Cr20Ni18Mo6CuN packages that also list flats, keep tubular RFQs under Stainless Steel Pipes and Tubes, flat RFQs under Stainless Steel Sheets and Plates, and pin the plate twin with GB/T 4237 015Cr20Ni18Mo6CuN. Flat Chinese grades in-family are indexed at GB/T 4237. Quote 015Cr20Ni18Mo6CuN pipe and plate under separate line items.

Heat Treatment and Delivery Condition for GB/T 13296 015Cr20Ni18Mo6CuN

Table 4 schedules 015Cr20Ni18Mo6CuN at 1010–1150 °C, rapid cool. Protective-atmosphere bright anneal may omit pickle when agreed. Grain-size extras: per family practice. Caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats. Recorded furnace charts for 015Cr20Ni18Mo6CuN should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo+N+Cu PREN for crevice and pitting life far above 316/317.

Recorded cool method for 015Cr20Ni18Mo6CuN matters as much as peak temperature — rapid cool versus air/slow cool is a family identity issue. Density 8.1 kg/dm³. Field heat treatment of 015Cr20Ni18Mo6CuN after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 015Cr20Ni18Mo6CuN duty: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers.

Corrosion Resistance of GB/T 13296 015Cr20Ni18Mo6CuN

Select 015Cr20Ni18Mo6CuN when the process side matches this framing: high Mo+N+Cu PREN for crevice and pitting life far above 316/317. Sister upgrades on the same hub include 022Cr21Ni25Mo7N, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2. Role: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. Coupon orientation, weld condition, and surface finish for 015Cr20Ni18Mo6CuN belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Application context for 015Cr20Ni18Mo6CuN stays seawater coolers, scrubber condensers, and high-PREN chemical HX.

Oxidation-first marks and PREN-first marks in this series are not interchangeable — 015Cr20Ni18Mo6CuN sits on the high Mo+N+Cu PREN for crevice and pitting life far above 316/317 side of that split. Caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 015Cr20Ni18Mo6CuN rather than relying on wall thickness alone. Application context for 015Cr20Ni18Mo6CuN stays seawater coolers, scrubber condensers, and high-PREN chemical HX.

Applications of GB/T 13296 015Cr20Ni18Mo6CuN Seamless Tube

Exchanger and boiler designers reach for 015Cr20Ni18Mo6CuN when: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. Common sketch: seawater coolers, scrubber condensers, and high-PREN chemical HX. Caution on the datasheet: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats. Spool fabricators should copy 015Cr20Ni18Mo6CuN onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to 015Cr20Ni18Mo6CuN duty: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers.

U-bend radius, heat treatment after bending, and tubesheet weld details for 015Cr20Ni18Mo6CuN belong in the fabrication specification, not only in the mill PO. Caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats. Commissioning teams benefit when the as-built dossier repeats 015Cr20Ni18Mo6CuN beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to 015Cr20Ni18Mo6CuN: matching super-austenitic fillers; strict heat-input and ferrite control.

Weldability of GB/T 13296 015Cr20Ni18Mo6CuN

Shop guidance for 015Cr20Ni18Mo6CuN: matching super-austenitic fillers; strict heat-input and ferrite control. Autogenous orbital welds to tubesheets need clean ID and controlled heat input. Family: austenitic. Procedure qualification for 015Cr20Ni18Mo6CuN should use the same product form and wall class as production, including the seamless finish that will ship. This paragraph is locked to 015Cr20Ni18Mo6CuN duty: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers.

Post-weld heat treatment of 015Cr20Ni18Mo6CuN is uncommon for austenitics but may be specified for stabilised marks or ferritic toughness — write it explicitly. Caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats. Consumable lot control and shielding-gas notes for 015Cr20Ni18Mo6CuN stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo+N+Cu PREN for crevice and pitting life far above 316/317.

Surface Finishes for GB/T 13296 015Cr20Ni18Mo6CuN

Finish options for 015Cr20Ni18Mo6CuN follow the ordered heat-treatment route under GB/T 13296. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: solution annealed. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 015Cr20Ni18Mo6CuN.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Bright or polished callouts for 015Cr20Ni18Mo6CuN never waive heat-treatment proof. After finishing, keep iron-free handling through storage and shipment so GB/T 13296 tube does not leave the yard with free-iron blooms. Caution retained: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats.

Inspection and Testing for GB/T 13296 015Cr20Ni18Mo6CuN

Batch rules for 015Cr20Ni18Mo6CuN: same grade, heat, size, and heat-treatment lot. Sampling counts follow OD/wall thresholds in the standard. Role: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. Sampling plans for 015Cr20Ni18Mo6CuN keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo+N+Cu PREN for crevice and pitting life far above 316/317.

Witness points for 015Cr20Ni18Mo6CuN (hydro, UT, IGC) should be booked before the tubes leave the finishing bay. Duty: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. Non-conforming 015Cr20Ni18Mo6CuN lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Application context for 015Cr20Ni18Mo6CuN stays seawater coolers, scrubber condensers, and high-PREN chemical HX.

Packaging and Shipping for GB/T 13296 015Cr20Ni18Mo6CuN

Export crates for 015Cr20Ni18Mo6CuN protect thin-wall HX stock against handling dents that would fail UT or tubesheet fit-up. Role: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. Bundle tickets for 015Cr20Ni18Mo6CuN repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for 015Cr20Ni18Mo6CuN remains cold-finished thin-wall HX with premium surface notes.

Claims handling for 015Cr20Ni18Mo6CuN starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Duty: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. Desiccant and wrap choices for 015Cr20Ni18Mo6CuN follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 015Cr20Ni18Mo6CuN: matching super-austenitic fillers; strict heat-input and ferrite control.

Loose tubes of 015Cr20Ni18Mo6CuN are avoided; strapped bundles keep heat lots together for MTC matching. Role: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. Claims handling for 015Cr20Ni18Mo6CuN starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 015Cr20Ni18Mo6CuN remains cold-finished thin-wall HX with premium surface notes.

Why Choose SHH STEEL

Why buyers stay with SHH STEEL for 015Cr20Ni18Mo6CuN: written acknowledgements that name W-C/W-H and Table 4 heat treatment before melt, plus MTCs that repeat the Chinese grade. Caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats. SHH STEEL can produce and supply 015Cr20Ni18Mo6CuN against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Size practice for 015Cr20Ni18Mo6CuN remains cold-finished thin-wall HX with premium surface notes.

Engineering support for 015Cr20Ni18Mo6CuN includes clarifying min-wall versus nominal-wall language and Annex A/B applicability before the heat is melted. Caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats. SHH STEEL can make 015Cr20Ni18Mo6CuN to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Weld-shop note tied to 015Cr20Ni18Mo6CuN: matching super-austenitic fillers; strict heat-input and ferrite control.

Supply Capability

Supply capability for 015Cr20Ni18Mo6CuN: W-C and W-H seamless routes, pickled or bright, plain or bevelled ends, random or fixed lengths. SHH STEEL can make the grade when melt and finishing slots align. Apps: seawater coolers, scrubber condensers, and high-PREN chemical HX. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 015Cr20Ni18Mo6CuN when the mill schedule allows. Keep the 015Cr20Ni18Mo6CuN caution visible here: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 015Cr20Ni18Mo6CuN (S31252)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes for 015Cr20Ni18Mo6CuN centre on cold-finished mid-OD HX tubes and selected hot-finished boiler walls; ask for the current matrix against your datasheet. Apps: seawater coolers, scrubber condensers, and high-PREN chemical HX. SHH STEEL can supply alternate walls and W-C/W-H classes for 015Cr20Ni18Mo6CuN once design pressure and corrosion allowance are clear. Keep the 015Cr20Ni18Mo6CuN caution visible here: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats.

Lead time for 015Cr20Ni18Mo6CuN tracks melt booking, finishing, and any third-party holds — send the full test matrix with the RFQ. Role: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. SHH STEEL can produce trial lengths of 015Cr20Ni18Mo6CuN for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to 015Cr20Ni18Mo6CuN: matching super-austenitic fillers; strict heat-input and ferrite control.

FAQ

What is GB/T 13296 015Cr20Ni18Mo6CuN seamless stainless steel tube used for?
GB/T 13296 015Cr20Ni18Mo6CuN is seamless stainless tube for boilers and heat exchangers — seawater coolers, scrubber condensers, and high-PREN chemical HX. Role summary: 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. It is a Chinese product standard grade (S31252), not an automatic ASTM A213 certificate.
Is GB/T 13296 015Cr20Ni18Mo6CuN seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 015Cr20Ni18Mo6CuN when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 015Cr20Ni18Mo6CuN?
015Cr20Ni18Mo6CuN is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 015Cr20Ni18Mo6CuN so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 015Cr20Ni18Mo6CuN compare with sister grades 022Cr21Ni25Mo7N, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3?
015Cr20Ni18Mo6CuN is filed as austenitic. Typical sisters on the same RFQ are 022Cr21Ni25Mo7N, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3. Design caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 015Cr20Ni18Mo6CuN?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 254SMO-class / UNS S31254-related the same as ordering 015Cr20Ni18Mo6CuN?
No. 254SMO-class / UNS S31254-related is a commercial / UNS cross-walk for body text (unified S31252). The purchase order should lock GB/T 13296 and 015Cr20Ni18Mo6CuN so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 015Cr20Ni18Mo6CuN?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 015Cr20Ni18Mo6CuN within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: cold-finished thin-wall HX with premium surface notes. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 015Cr20Ni18Mo6CuN be welded on site?
Shop guidance: matching super-austenitic fillers; strict heat-input and ferrite control. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats
When should I choose a higher-Mo or superaustenitic grade instead of 015Cr20Ni18Mo6CuN?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: hardness Table 5 band is tighter; chemistry windows are narrow — no “close enough” 317 heats Sister pointers: 022Cr21Ni25Mo7N, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 015Cr20Ni18Mo6CuN with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 015Cr20Ni18Mo6CuN does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 015Cr20Ni18Mo6CuN?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 015Cr20Ni18Mo6CuN when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 015Cr20Ni18Mo6CuN is seamless stainless steel tube for boilers and heat exchangers — 6% Mo super-austenitic HX tube for severe chloride and seawater-adjacent exchangers. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr21Ni25Mo7N, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X