GB/T 13296 07Cr17Ni12Mo2 Seamless Stainless Steel Tube
What is GB/T 13296 07Cr17Ni12Mo2 Seamless Stainless Steel Tube
When the approved vendor list and exchanger datasheet say GB/T 13296, the grade mark has to be the Chinese designation. 07Cr17Ni12Mo2 is the full product grade for this austenitic seamless tube. Clause 9 lists this mark with the H-grade IGC exemptions and grain-size rule.
SHH STEEL can supply 07Cr17Ni12Mo2 seamless tube in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the exchanger: carbon-aware Mo austenitic tube for elevated-temperature boiler/HX duty needing molybdenum. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 07Cr17Ni12Mo2 before production starts. This paragraph is locked to 07Cr17Ni12Mo2 duty: carbon-aware Mo austenitic tube for elevated-temperature boiler/HX duty needing molybdenum.
Equivalence talk to 316H / UNS S31609 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 13296 07Cr17Ni12Mo2, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory.
Related ASTM A213 tube pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti, 07Cr18Ni11Nb. Use thread: high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service.
Inside this GB/T 13296 series, compare GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 07Cr19Ni10, GB/T 13296 07Cr19Ni11Ti, GB/T 13296 07Cr18Ni11Nb. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP316H.
Buyers comparing 07Cr17Ni12Mo2 tubulars with sheet/plate can link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and GB/T 4237 07Cr17Ni12Mo2 so purchasing does not treat one product form as the other. Flat Chinese grades in-family are indexed at GB/T 4237. Quote 07Cr17Ni12Mo2 pipe and plate under separate line items.
Chemical Composition of GB/T 13296 07Cr17Ni12Mo2
Chemistry control on 07Cr17Ni12Mo2 starts at the ladle. Expect C 0.04–0.10, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 10.00–14.00, Cr 16.00–18.00, Mo 2.00–3.00 within Table 3, reported on the inspection document against the heat. Body alias 316H / UNS S31609 does not widen those windows. Every ladle analysis for 07Cr17Ni12Mo2 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Size practice for 07Cr17Ni12Mo2 remains straight boiler lengths, often W-H.
Read the table with the family in mind — austenitic — and with caution xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory. Numbers without the matching Table 4 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 07Cr17Ni12Mo2 before the order is acknowledged. Keep the 07Cr17Ni12Mo2 caution visible here: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| 07Cr17Ni12Mo2 | 0.04–0.10 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.015 | 10.00–14.00 | 16.00–18.00 | 2.00–3.00 |
Mechanical Properties of GB/T 13296 07Cr17Ni12Mo2
Proof stress and tensile minima for 07Cr17Ni12Mo2 sit at Rm min 480 MPa, Rp0.2 min 175 MPa, elongation min 35%. Note: xtd Table 4 lists Rm≥480 / Rp0.2≥175 for this H grade as printed. Flattening and flaring back ductility when size allows. Watch-out: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory.
Batch size limits (D≤76 mm and S≤3 mm: ≤400 tubes; otherwise ≤200) keep sampling honest for 07Cr17Ni12Mo2. Retests follow GB/T 2102. Density 8.0 kg/dm³.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 07Cr17Ni12Mo2 | 480 | 175 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 07Cr17Ni12Mo2. Heat treatment (Table 4): 1010–1150 °C, rapid cool. xtd Table 4 lists Rm≥480 / Rp0.2≥175 for this H grade as printed. Density 8.0 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 07Cr17Ni12Mo2
GB/T 13296 manufactures 07Cr17Ni12Mo2 as seamless tube only — cold-drawn or cold-rolled (symbol W-C) or hot-rolled / extruded (symbol W-H). SHH STEEL confirms the manufacture symbol on the acknowledgement before piercing or drawing starts; welded tube is outside this standard. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.
SHH STEEL schedules piercing, elongation, and finishing for 07Cr17Ni12Mo2 against the W-C or W-H symbol frozen on the acknowledgement. Ovality and wall eccentricity stay inside 80% of the respective OD and wall tolerances. Pickling or bright-anneal decisions for 07Cr17Ni12Mo2 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. This paragraph is locked to 07Cr17Ni12Mo2 duty: carbon-aware Mo austenitic tube for elevated-temperature boiler/HX duty needing molybdenum.
Cold-finish depth of longitudinal marks on 07Cr17Ni12Mo2 is limited to ≤4% of wall and ≤0.2 mm; hot-finish ≤5% and ≤0.4 mm. Apps: high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service. Hydrostatic pressure or eddy-current class for 07Cr17Ni12Mo2 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Weld-shop note tied to 07Cr17Ni12Mo2: 316H-oriented fillers; grain control on the product certificate.
Dimensions and Tolerances for GB/T 13296 07Cr17Ni12Mo2
When 07Cr17Ni12Mo2 ships as nominal wall, the note under Table 1 still applies different ± bands for hot and cold routes — do not mix W-C absolute OD tols with W-H percentage thinking. Practice: straight boiler lengths, often W-H. Tolerance basis for 07Cr17Ni12Mo2 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for 07Cr17Ni12Mo2 remains straight boiler lengths, often W-H.
Fixed lengths of 07Cr17Ni12Mo2 are end-protected so bevels and ID finish survive inland and ocean transit. Random lengths stay inside the usual 2000–12000 mm window unless agreed otherwise. Fixed lengths and multiple cut lengths for 07Cr17Ni12Mo2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for 07Cr17Ni12Mo2 remains straight boiler lengths, often W-H.
Equivalent Grades for GB/T 13296 07Cr17Ni12Mo2
Equivalence language around 07Cr17Ni12Mo2 is often looser than a tube purchase order can afford. GB/T 13296 07Cr17Ni12Mo2 governs this article; 316H / UNS S31609 is body-only framing for catalogues and dual-cert talk, not a substitute mark on the MTC. Keep the GB/T 13296 symbol unless a written dual-cert plan lists both standards with separate test scopes.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 07Cr17Ni12Mo2 | Governing tube grade for this page |
| Commercial / UNS (body only) | 316H / UNS S31609 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Read the notes column literally for 07Cr17Ni12Mo2: related chemistry is not automatic dual-cert. Cross-check GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 07Cr19Ni10, GB/T 13296 07Cr19Ni11Ti, GB/T 13296 07Cr18Ni11Nb when Mo, stabilisation, or carbon ceilings change the selection. Hub: GB/T 13296. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (07Cr17Ni12Mo2).
Heat Treatment and Delivery Condition for GB/T 13296 07Cr17Ni12Mo2
For 07Cr17Ni12Mo2, solution or anneal practice is not a free mill choice — it is the Table 4 band tied to the grade. Delivery: solution annealed. Role: carbon-aware Mo austenitic tube for elevated-temperature boiler/HX duty needing molybdenum. Recorded furnace charts for 07Cr17Ni12Mo2 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous/chloride life; elevated-temperature strength is the H-carbon story.
When Annex A elevated Rp0.2 is invoked, the certificate for 07Cr17Ni12Mo2 should still show the Table 4 delivery treatment actually performed. Apps: high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service. Field heat treatment of 07Cr17Ni12Mo2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 07Cr17Ni12Mo2: 316H-oriented fillers; grain control on the product certificate.
Corrosion Resistance of GB/T 13296 07Cr17Ni12Mo2
Pitting, crevice, oxidation, or weld-decay limiters for 07Cr17Ni12Mo2 should be named in the datasheet rather than inferred from the AISI alias alone. Framing: Mo helps aqueous/chloride life; elevated-temperature strength is the H-carbon story. Coupon orientation, weld condition, and surface finish for 07Cr17Ni12Mo2 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous/chloride life; elevated-temperature strength is the H-carbon story.
Pickling quality and free-iron cleanliness after fabrication affect startup corrosion of 07Cr17Ni12Mo2 as much as cast chemistry. Role: carbon-aware Mo austenitic tube for elevated-temperature boiler/HX duty needing molybdenum. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 07Cr17Ni12Mo2 rather than relying on wall thickness alone. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous/chloride life; elevated-temperature strength is the H-carbon story.
Applications of GB/T 13296 07Cr17Ni12Mo2 Seamless Tube
Use 07Cr17Ni12Mo2 on packages that match high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service. Nearby sisters 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti, 07Cr18Ni11Nb cover adjacent media or temperature steps. Weld-shop note: 316H-oriented fillers; grain control on the product certificate. Spool fabricators should copy 07Cr17Ni12Mo2 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Application context for 07Cr17Ni12Mo2 stays high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service.
When the process medium changes mid-project, revisit whether 07Cr17Ni12Mo2 still fits before releasing more heats. Sisters: 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti, 07Cr18Ni11Nb. Commissioning teams benefit when the as-built dossier repeats 07Cr17Ni12Mo2 beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous/chloride life; elevated-temperature strength is the H-carbon story.
Weldability of GB/T 13296 07Cr17Ni12Mo2
Consumable selection for 07Cr17Ni12Mo2 follows 316H-oriented fillers; grain control on the product certificate. Do not improvise under-alloyed fillers on Mo or Cu grades. Role: carbon-aware Mo austenitic tube for elevated-temperature boiler/HX duty needing molybdenum. Procedure qualification for 07Cr17Ni12Mo2 should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 07Cr17Ni12Mo2 caution visible here: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory.
Ferrite control and hot-cracking risk for 07Cr17Ni12Mo2 depend on the family chemistry; qualify on production wall, not only on plate coupons. Weld shop: 316H-oriented fillers; grain control on the product certificate. Consumable lot control and shielding-gas notes for 07Cr17Ni12Mo2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous/chloride life; elevated-temperature strength is the H-carbon story.
Surface Finishes for GB/T 13296 07Cr17Ni12Mo2
On 07Cr17Ni12Mo2, cosmetics never outrank correct heat treatment. Passivation and polish are sequenced after the anneal that qualifies the tube. Duty locked here: carbon-aware Mo austenitic tube for elevated-temperature boiler/HX duty needing molybdenum. Name which surface carries each finish callout. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (07Cr17Ni12Mo2).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Passivation restores the chromium-rich film after pickling or light fabrication on 07Cr17Ni12Mo2; it does not replace the heat treatment that sets mechanical properties under GB/T 13296. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.
Inspection and Testing for GB/T 13296 07Cr17Ni12Mo2
SHH STEEL keeps heat identity for 07Cr17Ni12Mo2 unbroken from melt through bundle tags, including third-party hold points written into the PO. Caution: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory. Sampling plans for 07Cr17Ni12Mo2 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for 07Cr17Ni12Mo2 stays high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service.
Certificate lines for 07Cr17Ni12Mo2 must repeat the Chinese grade, unified number, manufacture symbol, and heat treatment actually performed. Caution: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory. Non-conforming 07Cr17Ni12Mo2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Application context for 07Cr17Ni12Mo2 stays high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service.
Packaging and Shipping for GB/T 13296 07Cr17Ni12Mo2
Desiccant and wrap choices for 07Cr17Ni12Mo2 follow voyage length and storage climate on the shipping order, not a one-size export habit. Apps: high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service. Bundle tickets for 07Cr17Ni12Mo2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 07Cr17Ni12Mo2: 316H-oriented fillers; grain control on the product certificate.
Inland trucking of 07Cr17Ni12Mo2 still needs end protection — most ID dents happen between the port and the exchanger shop. Apps: high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service. Desiccant and wrap choices for 07Cr17Ni12Mo2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 07Cr17Ni12Mo2: 316H-oriented fillers; grain control on the product certificate.
Barcode or stencil extras for 07Cr17Ni12Mo2 are available when the owner’s material system needs them. Apps: high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service. Claims handling for 07Cr17Ni12Mo2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 07Cr17Ni12Mo2 remains straight boiler lengths, often W-H.
Why Choose SHH STEEL
SHH STEEL can make 07Cr17Ni12Mo2 to a boiler/HX test stack — hydro or E3H, UT U2, flattening/flaring, IGC when required — instead of a generic stainless tube habit. Apps: high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service. SHH STEEL can produce and supply 07Cr17Ni12Mo2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Keep the 07Cr17Ni12Mo2 caution visible here: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory.
SHH STEEL can supply 07Cr17Ni12Mo2 with third-party inspection hold points written into the itinerary. Weld-shop note: 316H-oriented fillers; grain control on the product certificate. SHH STEEL can make 07Cr17Ni12Mo2 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Weld-shop note tied to 07Cr17Ni12Mo2: 316H-oriented fillers; grain control on the product certificate.
Supply Capability
SHH STEEL can supply 07Cr17Ni12Mo2 with EN 10204 3.1 style documents, IGC when required, and hardness by agreement. Caution: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 07Cr17Ni12Mo2 when the mill schedule allows. Keep the 07Cr17Ni12Mo2 caution visible here: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 07Cr17Ni12Mo2 (S31609) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes: rolling cycles for 07Cr17Ni12Mo2 cover usual 2000–12000 mm lengths; cut-to-length and multiple lengths ship once tests clear. Caution: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory. SHH STEEL can supply alternate walls and W-C/W-H classes for 07Cr17Ni12Mo2 once design pressure and corrosion allowance are clear. Application context for 07Cr17Ni12Mo2 stays high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service.
SHH STEEL can supply replacement retubing heats of 07Cr17Ni12Mo2 matched to prior certificates when the plant provides heat history. Apps: high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service. SHH STEEL can produce trial lengths of 07Cr17Ni12Mo2 for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous/chloride life; elevated-temperature strength is the H-carbon story.
FAQ
-
What is GB/T 13296 07Cr17Ni12Mo2 seamless stainless steel tube used for?
- GB/T 13296 07Cr17Ni12Mo2 is seamless stainless tube for boilers and heat exchangers — high-temperature chemical HX, steam coils in mildly corrosive flue, and creep-conscious Mo service. Role summary: carbon-aware Mo austenitic tube for elevated-temperature boiler/HX duty needing molybdenum. It is a Chinese product standard grade (S31609), not an automatic ASTM A213 certificate.
-
Is GB/T 13296 07Cr17Ni12Mo2 seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 07Cr17Ni12Mo2 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 07Cr17Ni12Mo2?
- 07Cr17Ni12Mo2 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 07Cr17Ni12Mo2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 07Cr17Ni12Mo2 compare with sister grades 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti?
- 07Cr17Ni12Mo2 is filed as austenitic. Typical sisters on the same RFQ are 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti. Design caution: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 07Cr17Ni12Mo2?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 316H / UNS S31609 the same as ordering 07Cr17Ni12Mo2?
- No. 316H / UNS S31609 is a commercial / UNS cross-walk for body text (unified S31609). The purchase order should lock GB/T 13296 and 07Cr17Ni12Mo2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 07Cr17Ni12Mo2?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 07Cr17Ni12Mo2 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: straight boiler lengths, often W-H. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 07Cr17Ni12Mo2 be welded on site?
- Shop guidance: 316H-oriented fillers; grain control on the product certificate. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory
-
When should I choose a higher-Mo or superaustenitic grade instead of 07Cr17Ni12Mo2?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: xtd Table 4 lists Rm≥480 / Rp0.2≥175 as printed; IGC exempt with grain-size 4–7 mandatory Sister pointers: 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 07Cr17Ni12Mo2 with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 07Cr17Ni12Mo2 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 07Cr17Ni12Mo2?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 07Cr17Ni12Mo2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 07Cr17Ni12Mo2 is seamless stainless steel tube for boilers and heat exchangers — carbon-aware Mo austenitic tube for elevated-temperature boiler/HX duty needing molybdenum. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.