GB/T 13296 07Cr18Ni11Nb Seamless Stainless Steel Tube

GB/T 13296 07Cr18Ni11Nb seamless stainless steel tube (347H / UNS S34779, S34779), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
07Cr18Ni11Nb (S34779 / 347H / UNS S34779 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 07Cr18Ni11Nb Seamless Stainless Steel Tube

Boiler and heat-exchanger packages written to Chinese product standards look to GB/T 13296-2023 rather than inventing a mill grade from AISI shorthand alone. 07Cr18Ni11Nb is the Table 3/4 Chinese grade name for this austenitic chemistry (S34779). Annex A/B name this mark beside 07Cr19Ni10 and 07Cr19Ni11Ti.

Mill path for 07Cr18Ni11Nb: manufacture symbol W-C/W-H, Table 4 heat treatment, Table 3 cast chemistry, Table 4 tensile floors, hydrostatic or eddy-current E3H, ultrasonic U2. SHH STEEL can make and supply the grade to that stack. Typical use: high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 07Cr18Ni11Nb before production starts. Weld-shop note tied to 07Cr18Ni11Nb: 347H-oriented fillers; grain-size evidence on the MTC.

Body text may mention 347H / UNS S34779 (unified S34779) for cross-reference, but the H1 and order line stay on 07Cr18Ni11Nb. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10.

Order the standard the drawing and regulatory file actually require. Inside this 13296 series, compare 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10, 07Cr17Ni12Mo2 before stretching surface finish or wall alone. Duty thread: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty.

Inside this GB/T 13296 series, compare GB/T 13296 06Cr18Ni11Nb, GB/T 13296 07Cr19Ni11Ti, GB/T 13296 07Cr19Ni10, GB/T 13296 07Cr17Ni12Mo2. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP347H.

For 07Cr18Ni11Nb dual-form buying, the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 4237 07Cr18Ni11Nb. See also the GB/T 4237 hub for related plate designations. Quote 07Cr18Ni11Nb pipe and plate under separate line items.

Chemical Composition of GB/T 13296 07Cr18Ni11Nb

Table 3 sets the melt limits for 07Cr18Ni11Nb. Highlight band: C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 9.00–12.00, Cr 17.00–19.00, Nb 8C–1.10. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 3. Alias note: 347H / UNS S34779. Every ladle analysis for 07Cr18Ni11Nb is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Keep the 07Cr18Ni11Nb caution visible here: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10.

The composition table below is the cast window SHH STEEL quotes against for 07Cr18Ni11Nb. Edition framing is GB/T 13296-2023. Use thread: high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 07Cr18Ni11Nb before the order is acknowledged. This paragraph is locked to 07Cr18Ni11Nb duty: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty.

Grade C Si Mn P S Ni Cr Nb
07Cr18Ni11Nb ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.015 9.00–12.00 17.00–19.00 8C–1.10

Mechanical Properties of GB/T 13296 07Cr18Ni11Nb

Table 4 mechanical acceptance for 07Cr18Ni11Nb: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: Annex A/B elevated data; grain size 4–7; C ceiling ≤0.08 per xtd Table 3 (not a 0.04–0.10 floor row). Delivery framing: solution annealed. Sampling follows the batch rules for 07Cr18Ni11Nb. Tensile sampling follows the batch rules for the ordered test unit of 07Cr18Ni11Nb, and retests follow GB/T 2102 when a result sits under the Table 4 floor. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus H product framing for hot sulphurous duty.

Elevated-temperature Annex A Rp0.2 and Annex B 100000 h rupture tables name only selected H marks — check whether 07Cr18Ni11Nb appears before citing those numbers in a design note. Density 8.03 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
07Cr18Ni11Nb 520 205 35

Ambient values from GB/T 13296-2023 Table 4 for 07Cr18Ni11Nb. Heat treatment (Table 4): W-H ≥1050 °C rapid cool; W-C ≥1100 °C rapid cool. Annex A/B elevated data; grain size 4–7; C ceiling ≤0.08 per xtd Table 3 (not a 0.04–0.10 floor row). Density 8.03 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 07Cr18Ni11Nb

GB/T 13296 manufactures 07Cr18Ni11Nb as seamless tube only — cold-drawn or cold-rolled (symbol W-C) or hot-rolled / extruded (symbol W-H). SHH STEEL confirms the manufacture symbol on the acknowledgement before piercing or drawing starts; welded tube is outside this standard. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

After hot or cold working, 07Cr18Ni11Nb is heat-treated per Table 4 and finished to the ordered surface. Straightness limits differ for W-H (≤2.0 mm/m) and W-C (≤1.5 mm/m); full-length bow ≤0.15% of length. Pickling or bright-anneal decisions for 07Cr18Ni11Nb stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. This paragraph is locked to 07Cr18Ni11Nb duty: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty.

Straightness, end finish, and marking for 07Cr18Ni11Nb are checked before bundling so tubesheet fit-up crews receive usable lengths. Caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10. Hydrostatic pressure or eddy-current class for 07Cr18Ni11Nb is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Application context for 07Cr18Ni11Nb stays high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages.

Dimensions and Tolerances for GB/T 13296 07Cr18Ni11Nb

Minimum-wall ordering is common for HX duty on 07Cr18Ni11Nb: W-C min-wall tolerance is +20%S/0 for D≤38 mm and +22%S/0 above; W-H min-wall is +0.90/0 mm for S≤4.0 mm and +25%S/0 above. Confirm nominal-wall versus min-wall language on the PO. Tolerance basis for 07Cr18Ni11Nb follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus H product framing for hot sulphurous duty.

Bevel geometry, land, and ID cleanliness notes for 07Cr18Ni11Nb belong on the acknowledgement when automatic welding to the tubesheet is planned. Apps: high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages. Fixed lengths and multiple cut lengths for 07Cr18Ni11Nb are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 07Cr18Ni11Nb caution visible here: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10.

Equivalent Grades for GB/T 13296 07Cr18Ni11Nb

The table below maps GB/T 13296 07Cr18Ni11Nb to commercial aliases and related systems without inventing false one-to-one substitutes. Alias 347H / UNS S34779 stays body-only. Pack caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (07Cr18Ni11Nb).

System Designation Notes
GB/T 13296 07Cr18Ni11Nb Governing tube grade for this page
Commercial / UNS (body only) 347H / UNS S34779 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Order discipline for 07Cr18Ni11Nb still points at GB/T 13296, not the brochure alias. Neighbours GB/T 13296 06Cr18Ni11Nb, GB/T 13296 07Cr19Ni11Ti, GB/T 13296 07Cr19Ni10, GB/T 13296 07Cr17Ni12Mo2 each carry their own mechanical table. Category hub: GB/T 13296. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (07Cr18Ni11Nb).

Heat Treatment and Delivery Condition for GB/T 13296 07Cr18Ni11Nb

Table 4 schedules 07Cr18Ni11Nb at W-H ≥1050 °C rapid cool; W-C ≥1100 °C rapid cool. Protective-atmosphere bright anneal may omit pickle when agreed. Grain-size extras: per family practice. Caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10. Recorded furnace charts for 07Cr18Ni11Nb should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for 07Cr18Ni11Nb stays high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages.

Recorded cool method for 07Cr18Ni11Nb matters as much as peak temperature — rapid cool versus air/slow cool is a family identity issue. Density 8.03 kg/dm³. Field heat treatment of 07Cr18Ni11Nb after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 07Cr18Ni11Nb remains route-specific solution minima (W-H ≥1050 °C / W-C ≥1100 °C).

Corrosion Resistance of GB/T 13296 07Cr18Ni11Nb

Select 07Cr18Ni11Nb when the process side matches this framing: Nb stabilisation plus H product framing for hot sulphurous duty. Sister upgrades on the same hub include 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10, 07Cr17Ni12Mo2. Role: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. Coupon orientation, weld condition, and surface finish for 07Cr18Ni11Nb belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus H product framing for hot sulphurous duty.

Oxidation-first marks and PREN-first marks in this series are not interchangeable — 07Cr18Ni11Nb sits on the Nb stabilisation plus H product framing for hot sulphurous duty side of that split. Caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 07Cr18Ni11Nb rather than relying on wall thickness alone. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus H product framing for hot sulphurous duty.

Applications of GB/T 13296 07Cr18Ni11Nb Seamless Tube

Exchanger and boiler designers reach for 07Cr18Ni11Nb when: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. Common sketch: high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages. Caution on the datasheet: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10. Spool fabricators should copy 07Cr18Ni11Nb onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 07Cr18Ni11Nb remains route-specific solution minima (W-H ≥1050 °C / W-C ≥1100 °C).

U-bend radius, heat treatment after bending, and tubesheet weld details for 07Cr18Ni11Nb belong in the fabrication specification, not only in the mill PO. Caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10. Commissioning teams benefit when the as-built dossier repeats 07Cr18Ni11Nb beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 07Cr18Ni11Nb remains route-specific solution minima (W-H ≥1050 °C / W-C ≥1100 °C).

Weldability of GB/T 13296 07Cr18Ni11Nb

Shop guidance for 07Cr18Ni11Nb: 347H-oriented fillers; grain-size evidence on the MTC. Autogenous orbital welds to tubesheets need clean ID and controlled heat input. Family: austenitic. Procedure qualification for 07Cr18Ni11Nb should use the same product form and wall class as production, including the seamless finish that will ship. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus H product framing for hot sulphurous duty.

Post-weld heat treatment of 07Cr18Ni11Nb is uncommon for austenitics but may be specified for stabilised marks or ferritic toughness — write it explicitly. Caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10. Consumable lot control and shielding-gas notes for 07Cr18Ni11Nb stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 07Cr18Ni11Nb duty: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty.

Surface Finishes for GB/T 13296 07Cr18Ni11Nb

Iron-free handling after pickle matters for 07Cr18Ni11Nb — carbon-steel strapping stains show up later as rust blooms on finished tube. Standard route is solution annealed and pickled when HT is specified; polish scope must name the surface. Apps: high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

OD stencil ink on 07Cr18Ni11Nb should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0. Close bundles only after free-iron and burn marks are cleared. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (07Cr18Ni11Nb).

Inspection and Testing for GB/T 13296 07Cr18Ni11Nb

Batch rules for 07Cr18Ni11Nb: same grade, heat, size, and heat-treatment lot. Sampling counts follow OD/wall thresholds in the standard. Role: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. Sampling plans for 07Cr18Ni11Nb keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 07Cr18Ni11Nb: 347H-oriented fillers; grain-size evidence on the MTC.

Witness points for 07Cr18Ni11Nb (hydro, UT, IGC) should be booked before the tubes leave the finishing bay. Duty: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. Non-conforming 07Cr18Ni11Nb lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Keep the 07Cr18Ni11Nb caution visible here: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10.

Packaging and Shipping for GB/T 13296 07Cr18Ni11Nb

Export crates for 07Cr18Ni11Nb protect thin-wall HX stock against handling dents that would fail UT or tubesheet fit-up. Role: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. Bundle tickets for 07Cr18Ni11Nb repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 07Cr18Ni11Nb duty: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty.

Claims handling for 07Cr18Ni11Nb starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Duty: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. Desiccant and wrap choices for 07Cr18Ni11Nb follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus H product framing for hot sulphurous duty.

Loose tubes of 07Cr18Ni11Nb are avoided; strapped bundles keep heat lots together for MTC matching. Role: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. Claims handling for 07Cr18Ni11Nb starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 07Cr18Ni11Nb: 347H-oriented fillers; grain-size evidence on the MTC.

Why Choose SHH STEEL

Why buyers stay with SHH STEEL for 07Cr18Ni11Nb: written acknowledgements that name W-C/W-H and Table 4 heat treatment before melt, plus MTCs that repeat the Chinese grade. Caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10. SHH STEEL can produce and supply 07Cr18Ni11Nb against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Application context for 07Cr18Ni11Nb stays high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages.

Engineering support for 07Cr18Ni11Nb includes clarifying min-wall versus nominal-wall language and Annex A/B applicability before the heat is melted. Caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10. SHH STEEL can make 07Cr18Ni11Nb to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. This paragraph is locked to 07Cr18Ni11Nb duty: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty.

Supply Capability

Supply capability for 07Cr18Ni11Nb: W-C and W-H seamless routes, pickled or bright, plain or bevelled ends, random or fixed lengths. SHH STEEL can make the grade when melt and finishing slots align. Apps: high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 07Cr18Ni11Nb when the mill schedule allows. Weld-shop note tied to 07Cr18Ni11Nb: 347H-oriented fillers; grain-size evidence on the MTC.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 07Cr18Ni11Nb (S34779)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes for 07Cr18Ni11Nb centre on cold-finished mid-OD HX tubes and selected hot-finished boiler walls; ask for the current matrix against your datasheet. Apps: high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages. SHH STEEL can supply alternate walls and W-C/W-H classes for 07Cr18Ni11Nb once design pressure and corrosion allowance are clear. Application context for 07Cr18Ni11Nb stays high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages.

Lead time for 07Cr18Ni11Nb tracks melt booking, finishing, and any third-party holds — send the full test matrix with the RFQ. Role: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. SHH STEEL can produce trial lengths of 07Cr18Ni11Nb for procedure qualification before bulk release when the project calendar needs it. Size practice for 07Cr18Ni11Nb remains route-specific solution minima (W-H ≥1050 °C / W-C ≥1100 °C).

FAQ

What is GB/T 13296 07Cr18Ni11Nb seamless stainless steel tube used for?
GB/T 13296 07Cr18Ni11Nb is seamless stainless tube for boilers and heat exchangers — high-temperature refinery exchangers, Annex A/B referenced steam coils, creep-rupture packages. Role summary: Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. It is a Chinese product standard grade (S34779), not an automatic ASTM A213 certificate.
Is GB/T 13296 07Cr18Ni11Nb seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 07Cr18Ni11Nb when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 07Cr18Ni11Nb?
07Cr18Ni11Nb is delivered solution annealed under GB/T 13296. Table 4 reference: W-H ≥1050 °C rapid cool; W-C ≥1100 °C rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark.
How does 07Cr18Ni11Nb compare with sister grades 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10?
07Cr18Ni11Nb is filed as austenitic. Typical sisters on the same RFQ are 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10. Design caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10 Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 07Cr18Ni11Nb?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 347H / UNS S34779 the same as ordering 07Cr18Ni11Nb?
No. 347H / UNS S34779 is a commercial / UNS cross-walk for body text (unified S34779). The purchase order should lock GB/T 13296 and 07Cr18Ni11Nb so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 07Cr18Ni11Nb?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 07Cr18Ni11Nb within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: route-specific solution minima (W-H ≥1050 °C / W-C ≥1100 °C). Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 07Cr18Ni11Nb be welded on site?
Shop guidance: 347H-oriented fillers; grain-size evidence on the MTC. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10
When should I choose a higher-Mo or superaustenitic grade instead of 07Cr18Ni11Nb?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: IGC exempt with grain-size 4–7; xtd Table 3 shows C≤0.08 (not a 0.04–0.10 floor row) with Nb 8C–1.10 Sister pointers: 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 07Cr18Ni11Nb with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 07Cr18Ni11Nb does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 07Cr18Ni11Nb?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 07Cr18Ni11Nb when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 07Cr18Ni11Nb is seamless stainless steel tube for boilers and heat exchangers — Nb-stabilised elevated-temperature austenitic tube for creep-conscious stabilised boiler/HX duty. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response