GB/T 13296 06Cr17Ni12Mo2 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr17Ni12Mo2 Seamless Stainless Steel Tube

GB/T 13296 06Cr17Ni12Mo2 seamless stainless steel tube (316 / UNS S31608, S31608), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr17Ni12Mo2 (S31608 / 316 / UNS S31608 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 06Cr17Ni12Mo2 Seamless Stainless Steel Tube

When the approved vendor list and exchanger datasheet say GB/T 13296, the grade mark has to be the Chinese designation. 06Cr17Ni12Mo2 is the full product grade for this austenitic seamless tube. It is the Chinese 316-class mark buyers reach for when 18-8 pitting life runs out.

SHH STEEL can supply 06Cr17Ni12Mo2 seamless tube in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the exchanger: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr17Ni12Mo2 before production starts. Corrosion framing beside 06Cr17Ni12Mo2: Mo lifts pitting and crevice resistance versus 06Cr19Ni10; still not a 6% Mo super-austenitic.

Equivalence talk to 316 / UNS S31608 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 13296 06Cr17Ni12Mo2, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister.

Related ASTM A213 tube pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 022Cr17Ni12Mo2, 07Cr17Ni12Mo2, 06Cr17Ni12Mo2Ti, 06Cr19Ni13Mo3. Use thread: seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers.

Inside this GB/T 13296 series, compare GB/T 13296 022Cr17Ni12Mo2, GB/T 13296 07Cr17Ni12Mo2, GB/T 13296 06Cr17Ni12Mo2Ti, GB/T 13296 06Cr19Ni13Mo3. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP316.

Beside this 06Cr17Ni12Mo2 page, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is GB/T 3280 06Cr17Ni12Mo2. Do not stretch a 06Cr17Ni12Mo2 pipe certificate onto plate.

Chemical Composition of GB/T 13296 06Cr17Ni12Mo2

Chemistry control on 06Cr17Ni12Mo2 starts at the ladle. Expect C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 10.00–14.00, Cr 16.00–18.00, Mo 2.00–3.00 within Table 3, reported on the inspection document against the heat. Body alias 316 / UNS S31608 does not widen those windows. Every ladle analysis for 06Cr17Ni12Mo2 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Size practice for 06Cr17Ni12Mo2 remains W-C HX U-bend stock and straight condenser tubes.

Read the table with the family in mind — austenitic — and with caution as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister. Numbers without the matching Table 4 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr17Ni12Mo2 before the order is acknowledged. Weld-shop note tied to 06Cr17Ni12Mo2: 316/316L fillers; control ferrite and heat input on corrosive duties.

Grade C Si Mn P S Ni Cr Mo
06Cr17Ni12Mo2 ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.015 10.00–14.00 16.00–18.00 2.00–3.00

Mechanical Properties of GB/T 13296 06Cr17Ni12Mo2

Proof stress and tensile minima for 06Cr17Ni12Mo2 sit at Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Flattening and flaring back ductility when size allows. Watch-out: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister. Tensile sampling follows the batch rules for the ordered test unit of 06Cr17Ni12Mo2, and retests follow GB/T 2102 when a result sits under the Table 4 floor. Size practice for 06Cr17Ni12Mo2 remains W-C HX U-bend stock and straight condenser tubes.

Batch size limits (D≤76 mm and S≤3 mm: ≤400 tubes; otherwise ≤200) keep sampling honest for 06Cr17Ni12Mo2. Retests follow GB/T 2102. Density 7.98 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
06Cr17Ni12Mo2 520 205 35

Ambient values from GB/T 13296-2023 Table 4 for 06Cr17Ni12Mo2. Heat treatment (Table 4): 1010–1150 °C, rapid cool. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 06Cr17Ni12Mo2

For 06Cr17Ni12Mo2, the mill path is pierce / extrude / draw — never ERW or automatic-arc under GB/T 13296. Delivery is heat-treated and pickled unless overall ground/bored or protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO. Seamless W-C and W-H routes are the only valid order paths for 06Cr17Ni12Mo2 under GB/T 13296.

SHH STEEL schedules piercing, elongation, and finishing for 06Cr17Ni12Mo2 against the W-C or W-H symbol frozen on the acknowledgement. Ovality and wall eccentricity stay inside 80% of the respective OD and wall tolerances. Pickling or bright-anneal decisions for 06Cr17Ni12Mo2 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Application context for 06Cr17Ni12Mo2 stays seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers.

Cold-finish depth of longitudinal marks on 06Cr17Ni12Mo2 is limited to ≤4% of wall and ≤0.2 mm; hot-finish ≤5% and ≤0.4 mm. Apps: seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers. Hydrostatic pressure or eddy-current class for 06Cr17Ni12Mo2 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Keep the 06Cr17Ni12Mo2 caution visible here: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister.

Dimensions and Tolerances for GB/T 13296 06Cr17Ni12Mo2

When 06Cr17Ni12Mo2 ships as nominal wall, the note under Table 1 still applies different ± bands for hot and cold routes — do not mix W-C absolute OD tols with W-H percentage thinking. Practice: W-C HX U-bend stock and straight condenser tubes. Tolerance basis for 06Cr17Ni12Mo2 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 06Cr17Ni12Mo2 duty: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8.

Fixed lengths of 06Cr17Ni12Mo2 are end-protected so bevels and ID finish survive inland and ocean transit. Random lengths stay inside the usual 2000–12000 mm window unless agreed otherwise. Fixed lengths and multiple cut lengths for 06Cr17Ni12Mo2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 06Cr17Ni12Mo2 caution visible here: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister.

Equivalent Grades for GB/T 13296 06Cr17Ni12Mo2

Lock 06Cr17Ni12Mo2 on the PO when the datasheet owner wants GB/T 13296 seamless stainless boiler / heat-exchanger tube. Commercial talk as 316 / UNS S31608 is fine in emails; mill paperwork must still show GB/T 13296 06Cr17Ni12Mo2. Application framing: seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers
– Caution locked in What-is / Corrosion / FAQ: as-welded corrosive service near 0.

System Designation Notes
GB/T 13296 06Cr17Ni12Mo2 Governing tube grade for this page
Commercial / UNS (body only) 316 / UNS S31608 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related 316 chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Inside this series compare GB/T 13296 022Cr17Ni12Mo2, GB/T 13296 07Cr17Ni12Mo2, GB/T 13296 06Cr17Ni12Mo2Ti, GB/T 13296 06Cr19Ni13Mo3 before swapping marks for medium or temperature. Keep this caution visible for 06Cr17Ni12Mo2: as-welded corrosive service near 0. Hub: GB/T 13296. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (06Cr17Ni12Mo2).

Heat Treatment and Delivery Condition for GB/T 13296 06Cr17Ni12Mo2

For 06Cr17Ni12Mo2, solution or anneal practice is not a free mill choice — it is the Table 4 band tied to the grade. Delivery: solution annealed. Role: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8. Recorded furnace charts for 06Cr17Ni12Mo2 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to 06Cr17Ni12Mo2: 316/316L fillers; control ferrite and heat input on corrosive duties.

When Annex A elevated Rp0.2 is invoked, the certificate for 06Cr17Ni12Mo2 should still show the Table 4 delivery treatment actually performed. Apps: seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers. Field heat treatment of 06Cr17Ni12Mo2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 06Cr17Ni12Mo2 caution visible here: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister.

Corrosion Resistance of GB/T 13296 06Cr17Ni12Mo2

Pitting, crevice, oxidation, or weld-decay limiters for 06Cr17Ni12Mo2 should be named in the datasheet rather than inferred from the AISI alias alone. Framing: Mo lifts pitting and crevice resistance versus 06Cr19Ni10; still not a 6% Mo super-austenitic. Coupon orientation, weld condition, and surface finish for 06Cr17Ni12Mo2 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. This paragraph is locked to 06Cr17Ni12Mo2 duty: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8.

Pickling quality and free-iron cleanliness after fabrication affect startup corrosion of 06Cr17Ni12Mo2 as much as cast chemistry. Role: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr17Ni12Mo2 rather than relying on wall thickness alone. Application context for 06Cr17Ni12Mo2 stays seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers.

Applications of GB/T 13296 06Cr17Ni12Mo2 Seamless Tube

Use 06Cr17Ni12Mo2 on packages that match seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers. Nearby sisters 022Cr17Ni12Mo2, 07Cr17Ni12Mo2, 06Cr17Ni12Mo2Ti, 06Cr19Ni13Mo3 cover adjacent media or temperature steps. Weld-shop note: 316/316L fillers; control ferrite and heat input on corrosive duties. Spool fabricators should copy 06Cr17Ni12Mo2 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to 06Cr17Ni12Mo2 duty: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8.

When the process medium changes mid-project, revisit whether 06Cr17Ni12Mo2 still fits before releasing more heats. Sisters: 022Cr17Ni12Mo2, 07Cr17Ni12Mo2, 06Cr17Ni12Mo2Ti, 06Cr19Ni13Mo3. Commissioning teams benefit when the as-built dossier repeats 06Cr17Ni12Mo2 beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside 06Cr17Ni12Mo2: Mo lifts pitting and crevice resistance versus 06Cr19Ni10; still not a 6% Mo super-austenitic.

Weldability of GB/T 13296 06Cr17Ni12Mo2

Consumable selection for 06Cr17Ni12Mo2 follows 316/316L fillers; control ferrite and heat input on corrosive duties. Do not improvise under-alloyed fillers on Mo or Cu grades. Role: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8. Procedure qualification for 06Cr17Ni12Mo2 should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 06Cr17Ni12Mo2 caution visible here: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister.

Ferrite control and hot-cracking risk for 06Cr17Ni12Mo2 depend on the family chemistry; qualify on production wall, not only on plate coupons. Weld shop: 316/316L fillers; control ferrite and heat input on corrosive duties. Consumable lot control and shielding-gas notes for 06Cr17Ni12Mo2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 06Cr17Ni12Mo2: 316/316L fillers; control ferrite and heat input on corrosive duties.

Surface Finishes for GB/T 13296 06Cr17Ni12Mo2

Welded or heavily formed 06Cr17Ni12Mo2 may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to GB/T 13296 seamless stainless boiler / heat-exchanger tube. Caution: as-welded corrosive service near 0. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (06Cr17Ni12Mo2).

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Passivation restores the chromium-rich film after pickling or light fabrication on 06Cr17Ni12Mo2; it does not replace the heat treatment that sets mechanical properties under GB/T 13296. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.

Inspection and Testing for GB/T 13296 06Cr17Ni12Mo2

SHH STEEL keeps heat identity for 06Cr17Ni12Mo2 unbroken from melt through bundle tags, including third-party hold points written into the PO. Caution: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister. Sampling plans for 06Cr17Ni12Mo2 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 06Cr17Ni12Mo2 caution visible here: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister.

Certificate lines for 06Cr17Ni12Mo2 must repeat the Chinese grade, unified number, manufacture symbol, and heat treatment actually performed. Caution: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister. Non-conforming 06Cr17Ni12Mo2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 06Cr17Ni12Mo2: 316/316L fillers; control ferrite and heat input on corrosive duties.

Packaging and Shipping for GB/T 13296 06Cr17Ni12Mo2

Desiccant and wrap choices for 06Cr17Ni12Mo2 follow voyage length and storage climate on the shipping order, not a one-size export habit. Apps: seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers. Bundle tickets for 06Cr17Ni12Mo2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 06Cr17Ni12Mo2: 316/316L fillers; control ferrite and heat input on corrosive duties.

Inland trucking of 06Cr17Ni12Mo2 still needs end protection — most ID dents happen between the port and the exchanger shop. Apps: seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers. Desiccant and wrap choices for 06Cr17Ni12Mo2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 06Cr17Ni12Mo2: 316/316L fillers; control ferrite and heat input on corrosive duties.

Barcode or stencil extras for 06Cr17Ni12Mo2 are available when the owner’s material system needs them. Apps: seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers. Claims handling for 06Cr17Ni12Mo2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to 06Cr17Ni12Mo2 duty: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8.

Why Choose SHH STEEL

SHH STEEL can make 06Cr17Ni12Mo2 to a boiler/HX test stack — hydro or E3H, UT U2, flattening/flaring, IGC when required — instead of a generic stainless tube habit. Apps: seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers. SHH STEEL can produce and supply 06Cr17Ni12Mo2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Weld-shop note tied to 06Cr17Ni12Mo2: 316/316L fillers; control ferrite and heat input on corrosive duties.

SHH STEEL can supply 06Cr17Ni12Mo2 with third-party inspection hold points written into the itinerary. Weld-shop note: 316/316L fillers; control ferrite and heat input on corrosive duties. SHH STEEL can make 06Cr17Ni12Mo2 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Application context for 06Cr17Ni12Mo2 stays seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers.

Supply Capability

SHH STEEL can supply 06Cr17Ni12Mo2 with EN 10204 3.1 style documents, IGC when required, and hardness by agreement. Caution: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr17Ni12Mo2 when the mill schedule allows. Size practice for 06Cr17Ni12Mo2 remains W-C HX U-bend stock and straight condenser tubes.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 06Cr17Ni12Mo2 (S31608)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes: rolling cycles for 06Cr17Ni12Mo2 cover usual 2000–12000 mm lengths; cut-to-length and multiple lengths ship once tests clear. Caution: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr17Ni12Mo2 once design pressure and corrosion allowance are clear. Application context for 06Cr17Ni12Mo2 stays seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers.

SHH STEEL can supply replacement retubing heats of 06Cr17Ni12Mo2 matched to prior certificates when the plant provides heat history. Apps: seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers. SHH STEEL can produce trial lengths of 06Cr17Ni12Mo2 for procedure qualification before bulk release when the project calendar needs it. This paragraph is locked to 06Cr17Ni12Mo2 duty: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8.

FAQ

What is GB/T 13296 06Cr17Ni12Mo2 seamless stainless steel tube used for?
GB/T 13296 06Cr17Ni12Mo2 is seamless stainless tube for boilers and heat exchangers — seawater-cooled exchangers (with design caution), chemical condensers, and boiler blowdown coolers. Role summary: Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8. It is a Chinese product standard grade (S31608), not an automatic ASTM A213 certificate.
Is GB/T 13296 06Cr17Ni12Mo2 seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr17Ni12Mo2 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 06Cr17Ni12Mo2?
06Cr17Ni12Mo2 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr17Ni12Mo2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr17Ni12Mo2 compare with sister grades 022Cr17Ni12Mo2, 07Cr17Ni12Mo2, 06Cr17Ni12Mo2Ti?
06Cr17Ni12Mo2 is filed as austenitic. Typical sisters on the same RFQ are 022Cr17Ni12Mo2, 07Cr17Ni12Mo2, 06Cr17Ni12Mo2Ti. Design caution: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr17Ni12Mo2?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 316 / UNS S31608 the same as ordering 06Cr17Ni12Mo2?
No. 316 / UNS S31608 is a commercial / UNS cross-walk for body text (unified S31608). The purchase order should lock GB/T 13296 and 06Cr17Ni12Mo2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 06Cr17Ni12Mo2?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr17Ni12Mo2 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: W-C HX U-bend stock and straight condenser tubes. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 06Cr17Ni12Mo2 be welded on site?
Shop guidance: 316/316L fillers; control ferrite and heat input on corrosive duties. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr17Ni12Mo2?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: as-welded corrosive service near 0.08% C still prefers 022Cr17Ni12Mo2 or Ti-stabilised sister Sister pointers: 022Cr17Ni12Mo2, 07Cr17Ni12Mo2, 06Cr17Ni12Mo2Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 06Cr17Ni12Mo2 with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr17Ni12Mo2 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 06Cr17Ni12Mo2?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr17Ni12Mo2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 06Cr17Ni12Mo2 is seamless stainless steel tube for boilers and heat exchangers — Mo-bearing austenitic HX tube for chloride-bearing waters and process condensates that outgrow 18-8. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr17Ni12Mo2, 07Cr17Ni12Mo2, 06Cr17Ni12Mo2Ti. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X