GB/T 13296 022Cr19Ni10N Seamless Stainless Steel Tube

GB/T 13296 022Cr19Ni10N seamless stainless steel tube (304LN / UNS S30453, S30453), austenitic, Table 3 cast analysis, Rm min 550 MPa / Rp0.2 min 245 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
022Cr19Ni10N (S30453 / 304LN / UNS S30453 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 022Cr19Ni10N Seamless Stainless Steel Tube

GB/T 13296 covers seamless stainless tube for boiler and HX service — cold-drawn or hot-finished — with hydrostatic proof, ultrasonic U2, flattening and flaring where size allows. Inside that standard, 022Cr19Ni10N is filed as austenitic. It pairs the 022 carbon ceiling with an intentional nitrogen band for boiler/HX work.

From pierce/extrude/draw through marking and crate protection, SHH STEEL can produce GB/T 13296 022Cr19Ni10N for the sizes and tests on your RFQ. Application sketch: welded HX bundles under higher design pressure where Mo is still not justified. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 022Cr19Ni10N before production starts. Keep the 022Cr19Ni10N caution visible here: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat.

On the floor people shorten marks; in QA they must not. 022Cr19Ni10N under GB/T 13296 carries specific Table 3 windows and Table 4 floors that a loose “304LN” note will not enforce. Caution: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat.

Annex A elevated Rp0.2 and Annex B rupture data apply only to named H marks; still match the alloy to the medium. For 022Cr19Ni10N, that means: low-carbon nitrogen-bearing 18-8 tube combining weld-decay resistance with a higher strength floor. Nearby marks: 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N, 06Cr19Ni10.

Inside this GB/T 13296 series, compare GB/T 13296 022Cr19Ni10, GB/T 13296 06Cr19Ni10N, GB/T 13296 022Cr17Ni12Mo2N, GB/T 13296 06Cr19Ni10. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP304L.

Project teams specifying 022Cr19Ni10N should the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 4237 022Cr19Ni10N. Quote 022Cr19Ni10N pipe and plate under separate line items.

Chemical Composition of GB/T 13296 022Cr19Ni10N

For 022Cr19Ni10N, the melt ticket has to show Table 3 compliance — C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 8.00–11.00, Cr 18.00–20.00, N 0.10–0.16. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: L-carbon plus N: better HAZ behaviour than standard 304-class, still Mo-free pitting resistance.

Where Mo, Cu, Ti, Nb or N appear, they are intentional levers for 022Cr19Ni10N, not optional marketing. Confirm them on the MTC line-by-line. Role: low-carbon nitrogen-bearing 18-8 tube combining weld-decay resistance with a higher strength floor. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 022Cr19Ni10N before the order is acknowledged. Corrosion framing beside 022Cr19Ni10N: L-carbon plus N: better HAZ behaviour than standard 304-class, still Mo-free pitting resistance.

Grade C Si Mn P S Ni Cr N
022Cr19Ni10N ≤0.030 ≤1.00 ≤2.00 ≤0.035 ≤0.015 8.00–11.00 18.00–20.00 0.10–0.16

UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 022Cr19Ni10N (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 304LN / UNS S30453, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 022Cr19Ni10N against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 022Cr19Ni10N before the heat is booked.

Mechanical Properties of GB/T 13296 022Cr19Ni10N

Do not confuse Table 4 tube tensile floors with pipe or plate standards that share the 304LN / UNS S30453 alias. For 022Cr19Ni10N under 13296 expect Rm min 550 MPa, Rp0.2 min 245 MPa, elongation min 35%, verified per heat/lot rules. Note: UNCERTAIN — provisional vs paid Table 3/4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting.

When wall class changes the ordered tensile specimen orientation, keep the acknowledgement aligned for 022Cr19Ni10N. Reference density 7.93 kg/dm³; delivery solution annealed.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
022Cr19Ni10N 550 245 35

Ambient values from GB/T 13296-2023 Table 4 for 022Cr19Ni10N. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1010–1150 °C, rapid cool. UNCERTAIN — provisional vs paid Table 3/4. Density 7.93 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 022Cr19Ni10N

Seamless is not optional wording for 022Cr19Ni10N: the standard limits manufacture to W-C or W-H seamless routes for boiler and heat-exchanger tube. Pick W-C when OD precision and U-bend finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 13296 line item. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

U-bend and cut-to-length options for 022Cr19Ni10N are available by agreement after the straight-tube tests clear. Surface quality rejects cracks, folds, laps, laminations and scabs on ID and OD. Pickling or bright-anneal decisions for 022Cr19Ni10N stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Keep the 022Cr19Ni10N caution visible here: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat.

Manufacture records for 022Cr19Ni10N keep heat identity unbroken from melt through final NDT so the MTC can cite one cast for the whole bundle. Hydrostatic pressure or eddy-current class for 022Cr19Ni10N is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Corrosion framing beside 022Cr19Ni10N: L-carbon plus N: better HAZ behaviour than standard 304-class, still Mo-free pitting resistance.

Dimensions and Tolerances for GB/T 13296 022Cr19Ni10N

Cut lengths, multiple lengths, and U-bend developed lengths for 022Cr19Ni10N need explicit acknowledgement so finishing and crate length match the tubesheet drawing. Caution: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat. Tolerance basis for 022Cr19Ni10N follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 022Cr19Ni10N: 308L fillers; control dilution so N benefit is not washed out.

Tolerance class follows the manufacture route ordered for 022Cr19Ni10N; swapping W-C for W-H after acknowledgement without a dimensional review is how fit-up fails at the exchanger shop. Fixed lengths and multiple cut lengths for 022Cr19Ni10N are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 022Cr19Ni10N stays welded HX bundles under higher design pressure where Mo is still not justified.

Equivalent Grades for GB/T 13296 022Cr19Ni10N

Do not treat 304LN / UNS S30453 as interchangeable paperwork for GB/T 13296 022Cr19Ni10N. Chemistry kinship is not acceptance kinship under this product standard. Hydrostatic, NDT, and heat-treatment text diverge across systems even when the cast analysis looks familiar. Dual marking is a purchase-order option that still requires every limit that matters for 022Cr19Ni10N to be verified on the heat.

System Designation Notes
GB/T 13296 022Cr19Ni10N Governing tube grade for this page
Commercial / UNS (body only) 304LN / UNS S30453 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

When the service outgrows 022Cr19Ni10N, move to a sister rather than stretching the alias: GB/T 13296 022Cr19Ni10, GB/T 13296 06Cr19Ni10N, GB/T 13296 022Cr17Ni12Mo2N, GB/T 13296 06Cr19Ni10. Full list under GB/T 13296. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (022Cr19Ni10N).

Heat Treatment and Delivery Condition for GB/T 13296 022Cr19Ni10N

Stabilisation after solution anneal is available by agreement for Ti/Nb marks; confirm whether 022Cr19Ni10N needs that second hold before acknowledging. HT reference: 1010–1150 °C, rapid cool. Recorded furnace charts for 022Cr19Ni10N should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 022Cr19Ni10N duty: low-carbon nitrogen-bearing 18-8 tube combining weld-decay resistance with a higher strength floor.

Mixed bundles of different heat-treatment furnace lots of 022Cr19Ni10N stay segregated so sampling remains traceable to one Table 4 run. Field heat treatment of 022Cr19Ni10N after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 022Cr19Ni10N: 308L fillers; control dilution so N benefit is not washed out.

Corrosion Resistance of GB/T 13296 022Cr19Ni10N

Coupon orientation, weld condition, and surface finish for 022Cr19Ni10N belong in the corrosion test order so method E or other coupons compare honestly to the installed tube. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 022Cr19Ni10N unless the mark is on the exemption list. Coupon orientation, weld condition, and surface finish for 022Cr19Ni10N belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Weld-shop note tied to 022Cr19Ni10N: 308L fillers; control dilution so N benefit is not washed out.

For 022Cr19Ni10N, specify whether IGC, hardness, or special corrosion coupons are extras beyond the clause 9 default before the heat is melted. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 022Cr19Ni10N rather than relying on wall thickness alone. Keep the 022Cr19Ni10N caution visible here: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat.

Applications of GB/T 13296 022Cr19Ni10N Seamless Tube

Commissioning dossiers should repeat 022Cr19Ni10N beside heat numbers so as-built isometrics stay tied to the same mill certificates. Application thread: welded HX bundles under higher design pressure where Mo is still not justified. Spool fabricators should copy 022Cr19Ni10N onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 022Cr19Ni10N remains cold-finished HX OD×min wall with clear dual L+N marking.

Spare-tube stocks of 022Cr19Ni10N should keep heat identity so later retubing matches the original corrosion and strength file. Apps: welded HX bundles under higher design pressure where Mo is still not justified. Commissioning teams benefit when the as-built dossier repeats 022Cr19Ni10N beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside 022Cr19Ni10N: L-carbon plus N: better HAZ behaviour than standard 304-class, still Mo-free pitting resistance.

Weldability of GB/T 13296 022Cr19Ni10N

Repair welding of 022Cr19Ni10N must preserve grade identity — a 308 deposit on a 6% Mo tube is a corrosion failure waiting to happen. Note: 308L fillers; control dilution so N benefit is not washed out. Procedure qualification for 022Cr19Ni10N should use the same product form and wall class as production, including the seamless finish that will ship. Application context for 022Cr19Ni10N stays welded HX bundles under higher design pressure where Mo is still not justified.

Tubesheet joint design for 022Cr19Ni10N should state strength weld versus seal weld and any expansion sequence before production welding starts. Consumable lot control and shielding-gas notes for 022Cr19Ni10N stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 022Cr19Ni10N: 308L fillers; control dilution so N benefit is not washed out.

Surface Finishes for GB/T 13296 022Cr19Ni10N

Iron-free handling after pickle matters for 022Cr19Ni10N — carbon-steel strapping stains show up later as rust blooms on finished tube. Standard route is solution annealed and pickled when HT is specified; polish scope must name the surface. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 022Cr19Ni10N.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

OD stencil ink on 022Cr19Ni10N should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat. Close bundles only after free-iron and burn marks are cleared.

Inspection and Testing for GB/T 13296 022Cr19Ni10N

Hardness by agreement for wall ≥1.7 mm on 022Cr19Ni10N; grain-size evidence when the mark requires levels 4–7. Apps: welded HX bundles under higher design pressure where Mo is still not justified. Sampling plans for 022Cr19Ni10N keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Size practice for 022Cr19Ni10N remains cold-finished HX OD×min wall with clear dual L+N marking.

Dimensional reports for 022Cr19Ni10N cite Table 1 tolerance basis (W-C vs W-H, min wall vs nominal wall) so receiving inspectors know which band applies. Non-conforming 022Cr19Ni10N lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Size practice for 022Cr19Ni10N remains cold-finished HX OD×min wall with clear dual L+N marking.

Packaging and Shipping for GB/T 13296 022Cr19Ni10N

U-bend crates for 022Cr19Ni10N need radius supports so cold-worked bends do not spring or scar in transit. Caution: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat. Bundle tickets for 022Cr19Ni10N repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 022Cr19Ni10N stays welded HX bundles under higher design pressure where Mo is still not justified.

Long-term storage of 022Cr19Ni10N should keep bundles dry and off bare soil to protect the pickled surface before installation. Caution: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat. Desiccant and wrap choices for 022Cr19Ni10N follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for 022Cr19Ni10N stays welded HX bundles under higher design pressure where Mo is still not justified.

Packing lists for 022Cr19Ni10N cite net/gross weight and crate count so logistics and QA share one document set. Caution: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat. Claims handling for 022Cr19Ni10N starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 022Cr19Ni10N stays welded HX bundles under higher design pressure where Mo is still not justified.

Why Choose SHH STEEL

Traceability, pickle quality, and size discipline on 022Cr19Ni10N are part of the supply promise, not brochure extras. Role: low-carbon nitrogen-bearing 18-8 tube combining weld-decay resistance with a higher strength floor. SHH STEEL can produce and supply 022Cr19Ni10N against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. This paragraph is locked to 022Cr19Ni10N duty: low-carbon nitrogen-bearing 18-8 tube combining weld-decay resistance with a higher strength floor.

For 022Cr19Ni10N, SHH STEEL can produce trial lengths for procedure qualification before bulk release when the project calendar needs it. Apps: welded HX bundles under higher design pressure where Mo is still not justified. SHH STEEL can make 022Cr19Ni10N to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Corrosion framing beside 022Cr19Ni10N: L-carbon plus N: better HAZ behaviour than standard 304-class, still Mo-free pitting resistance.

Supply Capability

From RFQ to crate, SHH STEEL can produce 022Cr19Ni10N as a boiler/HX product — not a repurposed fluid-pipe heat. Size hint: cold-finished HX OD×min wall with clear dual L+N marking. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 022Cr19Ni10N when the mill schedule allows. Corrosion framing beside 022Cr19Ni10N: L-carbon plus N: better HAZ behaviour than standard 304-class, still Mo-free pitting resistance.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 022Cr19Ni10N (S30453)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes — SHH STEEL can supply alternate walls for 022Cr19Ni10N once design pressure, corrosion allowance, and min-wall rules are clear. Size hint: cold-finished HX OD×min wall with clear dual L+N marking. SHH STEEL can supply alternate walls and W-C/W-H classes for 022Cr19Ni10N once design pressure and corrosion allowance are clear. Keep the 022Cr19Ni10N caution visible here: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat.

Export packing and document sets for 022Cr19Ni10N are confirmed on the acknowledgement so customs and site QA see the same grade string. Caution: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat. SHH STEEL can produce trial lengths of 022Cr19Ni10N for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside 022Cr19Ni10N: L-carbon plus N: better HAZ behaviour than standard 304-class, still Mo-free pitting resistance.

FAQ

What is GB/T 13296 022Cr19Ni10N seamless stainless steel tube used for?
GB/T 13296 022Cr19Ni10N is seamless stainless tube for boilers and heat exchangers — welded HX bundles under higher design pressure where Mo is still not justified. Role summary: low-carbon nitrogen-bearing 18-8 tube combining weld-decay resistance with a higher strength floor. It is a Chinese product standard grade (S30453), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
Is GB/T 13296 022Cr19Ni10N seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 022Cr19Ni10N when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 022Cr19Ni10N?
022Cr19Ni10N is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 022Cr19Ni10N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 022Cr19Ni10N compare with sister grades 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N?
022Cr19Ni10N is filed as austenitic. Typical sisters on the same RFQ are 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N. Design caution: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 022Cr19Ni10N?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 304LN / UNS S30453 the same as ordering 022Cr19Ni10N?
No. 304LN / UNS S30453 is a commercial / UNS cross-walk for body text (unified S30453). The purchase order should lock GB/T 13296 and 022Cr19Ni10N so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 022Cr19Ni10N?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 022Cr19Ni10N within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: cold-finished HX OD×min wall with clear dual L+N marking. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 022Cr19Ni10N be welded on site?
Shop guidance: 308L fillers; control dilution so N benefit is not washed out. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat
When should I choose a higher-Mo or superaustenitic grade instead of 022Cr19Ni10N?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN vs paid Table 3/4 — confirm melt windows and tensile floors before melting the heat Sister pointers: 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 022Cr19Ni10N with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 022Cr19Ni10N does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 022Cr19Ni10N?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 022Cr19Ni10N when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 022Cr19Ni10N is seamless stainless steel tube for boilers and heat exchangers — low-carbon nitrogen-bearing 18-8 tube combining weld-decay resistance with a higher strength floor. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X