GB/T 13296 06Cr19Ni13Mo3 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr19Ni13Mo3 Seamless Stainless Steel Tube

GB/T 13296 06Cr19Ni13Mo3 seamless stainless steel tube (317 / UNS S31708, S31708), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr19Ni13Mo3 (S31708 / 317 / UNS S31708 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 06Cr19Ni13Mo3 Seamless Stainless Steel Tube

When the approved vendor list and exchanger datasheet say GB/T 13296, the grade mark has to be the Chinese designation. 06Cr19Ni13Mo3 is the full product grade for this austenitic seamless tube. It is the 317-class step-up inside this boiler/HX series.

SHH STEEL can supply 06Cr19Ni13Mo3 seamless tube in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the exchanger: higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr19Ni13Mo3 before production starts. This paragraph is locked to 06Cr19Ni13Mo3 duty: higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough.

Equivalence talk to 317 / UNS S31708 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 13296 06Cr19Ni13Mo3, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade.

Related ASTM A213 tube pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN, 06Cr18Ni12Mo2Cu2. Use thread: aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316.

Inside this GB/T 13296 series, compare GB/T 13296 022Cr19Ni13Mo3, GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 015Cr20Ni18Mo6CuN, GB/T 13296 06Cr18Ni12Mo2Cu2. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP317L.

On 06Cr19Ni13Mo3 packages that also list flats, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is GB/T 4237 06Cr19Ni13Mo3. Confirm 06Cr19Ni13Mo3 OD × wall and plate thickness on separate drawings.

Chemical Composition of GB/T 13296 06Cr19Ni13Mo3

Chemistry control on 06Cr19Ni13Mo3 starts at the ladle. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Expect C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 11.00–15.00, Cr 18.00–20.00, Mo 3.00–4.00 within Table 3, reported on the inspection document against the heat. Body alias 317 / UNS S31708 does not widen those windows.

Read the table with the family in mind — austenitic — and with caution UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade. Numbers without the matching Table 4 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr19Ni13Mo3 before the order is acknowledged. Corrosion framing beside 06Cr19Ni13Mo3: 3–4% Mo lifts PREN clearly above 06Cr17Ni12Mo2.

Grade C Si Mn P S Ni Cr Mo
06Cr19Ni13Mo3 ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.015 11.00–15.00 18.00–20.00 3.00–4.00

UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 06Cr19Ni13Mo3 (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 317 / UNS S31708, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 06Cr19Ni13Mo3 against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 06Cr19Ni13Mo3 before the heat is booked.

Mechanical Properties of GB/T 13296 06Cr19Ni13Mo3

Proof stress and tensile minima for 06Cr19Ni13Mo3 sit at Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: UNCERTAIN — provisional vs paid Table 3/4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Flattening and flaring back ductility when size allows. Watch-out: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade.

Batch size limits (D≤76 mm and S≤3 mm: ≤400 tubes; otherwise ≤200) keep sampling honest for 06Cr19Ni13Mo3. Retests follow GB/T 2102. Density 7.98 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
06Cr19Ni13Mo3 520 205 35

Ambient values from GB/T 13296-2023 Table 4 for 06Cr19Ni13Mo3. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1010–1150 °C, rapid cool. UNCERTAIN — provisional vs paid Table 3/4. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 06Cr19Ni13Mo3

GB/T 13296 manufactures 06Cr19Ni13Mo3 as seamless tube only — cold-drawn or cold-rolled (symbol W-C) or hot-rolled / extruded (symbol W-H). SHH STEEL confirms the manufacture symbol on the acknowledgement before piercing or drawing starts; welded tube is outside this standard. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

SHH STEEL schedules piercing, elongation, and finishing for 06Cr19Ni13Mo3 against the W-C or W-H symbol frozen on the acknowledgement. Ovality and wall eccentricity stay inside 80% of the respective OD and wall tolerances. Pickling or bright-anneal decisions for 06Cr19Ni13Mo3 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Application context for 06Cr19Ni13Mo3 stays aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316.

Cold-finish depth of longitudinal marks on 06Cr19Ni13Mo3 is limited to ≤4% of wall and ≤0.2 mm; hot-finish ≤5% and ≤0.4 mm. Apps: aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316. Hydrostatic pressure or eddy-current class for 06Cr19Ni13Mo3 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Weld-shop note tied to 06Cr19Ni13Mo3: 317/317L fillers; match Mo in the weld metal.

Dimensions and Tolerances for GB/T 13296 06Cr19Ni13Mo3

When 06Cr19Ni13Mo3 ships as nominal wall, the note under Table 1 still applies different ± bands for hot and cold routes — do not mix W-C absolute OD tols with W-H percentage thinking. Practice: cold-finished HX OD with Mo called on both tube and weld procedure. Tolerance basis for 06Cr19Ni13Mo3 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 06Cr19Ni13Mo3 duty: higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough.

Fixed lengths of 06Cr19Ni13Mo3 are end-protected so bevels and ID finish survive inland and ocean transit. Random lengths stay inside the usual 2000–12000 mm window unless agreed otherwise. Fixed lengths and multiple cut lengths for 06Cr19Ni13Mo3 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 06Cr19Ni13Mo3 stays aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316.

Equivalent Grades for GB/T 13296 06Cr19Ni13Mo3

Cross-references help sourcing 06Cr19Ni13Mo3, but they do not replace the GB/T 13296 grade line on the enquiry. Family framing here is austenitic; delivery practice from the crib is “solution annealed”. Related ASTM or EN numbers are starting points for engineering comparison, not automatic substitutes. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (06Cr19Ni13Mo3).

System Designation Notes
GB/T 13296 06Cr19Ni13Mo3 Governing tube grade for this page
Commercial / UNS (body only) 317 / UNS S31708 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related 317 chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Order discipline for 06Cr19Ni13Mo3 still points at GB/T 13296, not the brochure alias. Neighbours GB/T 13296 022Cr19Ni13Mo3, GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 015Cr20Ni18Mo6CuN, GB/T 13296 06Cr18Ni12Mo2Cu2 each carry their own mechanical table. Category hub: GB/T 13296. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (06Cr19Ni13Mo3).

Heat Treatment and Delivery Condition for GB/T 13296 06Cr19Ni13Mo3

For 06Cr19Ni13Mo3, solution or anneal practice is not a free mill choice — it is the Table 4 band tied to the grade. Delivery: solution annealed. Role: higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough. Recorded furnace charts for 06Cr19Ni13Mo3 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 06Cr19Ni13Mo3 caution visible here: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade.

When Annex A elevated Rp0.2 is invoked, the certificate for 06Cr19Ni13Mo3 should still show the Table 4 delivery treatment actually performed. Apps: aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316. Field heat treatment of 06Cr19Ni13Mo3 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 06Cr19Ni13Mo3 caution visible here: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade.

Corrosion Resistance of GB/T 13296 06Cr19Ni13Mo3

Pitting, crevice, oxidation, or weld-decay limiters for 06Cr19Ni13Mo3 should be named in the datasheet rather than inferred from the AISI alias alone. Framing: 3–4% Mo lifts PREN clearly above 06Cr17Ni12Mo2. Coupon orientation, weld condition, and surface finish for 06Cr19Ni13Mo3 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Corrosion framing beside 06Cr19Ni13Mo3: 3–4% Mo lifts PREN clearly above 06Cr17Ni12Mo2.

Pickling quality and free-iron cleanliness after fabrication affect startup corrosion of 06Cr19Ni13Mo3 as much as cast chemistry. Role: higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr19Ni13Mo3 rather than relying on wall thickness alone. Keep the 06Cr19Ni13Mo3 caution visible here: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade.

Applications of GB/T 13296 06Cr19Ni13Mo3 Seamless Tube

Use 06Cr19Ni13Mo3 on packages that match aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316. Nearby sisters 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN, 06Cr18Ni12Mo2Cu2 cover adjacent media or temperature steps. Weld-shop note: 317/317L fillers; match Mo in the weld metal. Spool fabricators should copy 06Cr19Ni13Mo3 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Application context for 06Cr19Ni13Mo3 stays aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316.

When the process medium changes mid-project, revisit whether 06Cr19Ni13Mo3 still fits before releasing more heats. Sisters: 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN, 06Cr18Ni12Mo2Cu2. Commissioning teams benefit when the as-built dossier repeats 06Cr19Ni13Mo3 beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 06Cr19Ni13Mo3 remains cold-finished HX OD with Mo called on both tube and weld procedure.

Weldability of GB/T 13296 06Cr19Ni13Mo3

Consumable selection for 06Cr19Ni13Mo3 follows 317/317L fillers; match Mo in the weld metal. Do not improvise under-alloyed fillers on Mo or Cu grades. Role: higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough. Procedure qualification for 06Cr19Ni13Mo3 should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 06Cr19Ni13Mo3 remains cold-finished HX OD with Mo called on both tube and weld procedure.

Ferrite control and hot-cracking risk for 06Cr19Ni13Mo3 depend on the family chemistry; qualify on production wall, not only on plate coupons. Weld shop: 317/317L fillers; match Mo in the weld metal. Consumable lot control and shielding-gas notes for 06Cr19Ni13Mo3 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 06Cr19Ni13Mo3: 3–4% Mo lifts PREN clearly above 06Cr17Ni12Mo2.

Surface Finishes for GB/T 13296 06Cr19Ni13Mo3

Pickled mill finish covers most RFQs for 06Cr19Ni13Mo3. Bright anneal, grind, or polish only when the enquiry writes a measurable target and names OD, ID, or both. Pack caution carried into finish control: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Passivation restores the chromium-rich film after pickling or light fabrication on 06Cr19Ni13Mo3; it does not replace the heat treatment that sets mechanical properties under GB/T 13296. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.

Inspection and Testing for GB/T 13296 06Cr19Ni13Mo3

SHH STEEL keeps heat identity for 06Cr19Ni13Mo3 unbroken from melt through bundle tags, including third-party hold points written into the PO. Caution: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade. Sampling plans for 06Cr19Ni13Mo3 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 06Cr19Ni13Mo3 caution visible here: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade.

Certificate lines for 06Cr19Ni13Mo3 must repeat the Chinese grade, unified number, manufacture symbol, and heat treatment actually performed. Caution: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade. Non-conforming 06Cr19Ni13Mo3 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 06Cr19Ni13Mo3: 317/317L fillers; match Mo in the weld metal.

Packaging and Shipping for GB/T 13296 06Cr19Ni13Mo3

Desiccant and wrap choices for 06Cr19Ni13Mo3 follow voyage length and storage climate on the shipping order, not a one-size export habit. Apps: aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316. Bundle tickets for 06Cr19Ni13Mo3 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for 06Cr19Ni13Mo3 remains cold-finished HX OD with Mo called on both tube and weld procedure.

Inland trucking of 06Cr19Ni13Mo3 still needs end protection — most ID dents happen between the port and the exchanger shop. Apps: aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316. Desiccant and wrap choices for 06Cr19Ni13Mo3 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. This paragraph is locked to 06Cr19Ni13Mo3 duty: higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough.

Barcode or stencil extras for 06Cr19Ni13Mo3 are available when the owner’s material system needs them. Apps: aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316. Claims handling for 06Cr19Ni13Mo3 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 06Cr19Ni13Mo3 stays aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316.

Why Choose SHH STEEL

SHH STEEL can make 06Cr19Ni13Mo3 to a boiler/HX test stack — hydro or E3H, UT U2, flattening/flaring, IGC when required — instead of a generic stainless tube habit. Apps: aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316. SHH STEEL can produce and supply 06Cr19Ni13Mo3 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Corrosion framing beside 06Cr19Ni13Mo3: 3–4% Mo lifts PREN clearly above 06Cr17Ni12Mo2.

SHH STEEL can supply 06Cr19Ni13Mo3 with third-party inspection hold points written into the itinerary. Weld-shop note: 317/317L fillers; match Mo in the weld metal. SHH STEEL can make 06Cr19Ni13Mo3 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. This paragraph is locked to 06Cr19Ni13Mo3 duty: higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough.

Supply Capability

SHH STEEL can supply 06Cr19Ni13Mo3 with EN 10204 3.1 style documents, IGC when required, and hardness by agreement. Caution: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr19Ni13Mo3 when the mill schedule allows. Weld-shop note tied to 06Cr19Ni13Mo3: 317/317L fillers; match Mo in the weld metal.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 06Cr19Ni13Mo3 (S31708)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes: rolling cycles for 06Cr19Ni13Mo3 cover usual 2000–12000 mm lengths; cut-to-length and multiple lengths ship once tests clear. Caution: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr19Ni13Mo3 once design pressure and corrosion allowance are clear. Corrosion framing beside 06Cr19Ni13Mo3: 3–4% Mo lifts PREN clearly above 06Cr17Ni12Mo2.

SHH STEEL can supply replacement retubing heats of 06Cr19Ni13Mo3 matched to prior certificates when the plant provides heat history. Apps: aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316. SHH STEEL can produce trial lengths of 06Cr19Ni13Mo3 for procedure qualification before bulk release when the project calendar needs it. Size practice for 06Cr19Ni13Mo3 remains cold-finished HX OD with Mo called on both tube and weld procedure.

FAQ

What is GB/T 13296 06Cr19Ni13Mo3 seamless stainless steel tube used for?
GB/T 13296 06Cr19Ni13Mo3 is seamless stainless tube for boilers and heat exchangers — aggressive chloride condensers, bleach-adjacent coolers, and chemical HX upgrades from 316. Role summary: higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough. It is a Chinese product standard grade (S31708), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
Is GB/T 13296 06Cr19Ni13Mo3 seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr19Ni13Mo3 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 06Cr19Ni13Mo3?
06Cr19Ni13Mo3 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr19Ni13Mo3 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr19Ni13Mo3 compare with sister grades 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN?
06Cr19Ni13Mo3 is filed as austenitic. Typical sisters on the same RFQ are 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN. Design caution: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr19Ni13Mo3?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 317 / UNS S31708 the same as ordering 06Cr19Ni13Mo3?
No. 317 / UNS S31708 is a commercial / UNS cross-walk for body text (unified S31708). The purchase order should lock GB/T 13296 and 06Cr19Ni13Mo3 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 06Cr19Ni13Mo3?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr19Ni13Mo3 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: cold-finished HX OD with Mo called on both tube and weld procedure. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 06Cr19Ni13Mo3 be welded on site?
Shop guidance: 317/317L fillers; match Mo in the weld metal. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr19Ni13Mo3?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN vs paid Table 3/4; do not accept a 316 heat as a silent Mo upgrade Sister pointers: 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 06Cr19Ni13Mo3 with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr19Ni13Mo3 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 06Cr19Ni13Mo3?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr19Ni13Mo3 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 06Cr19Ni13Mo3 is seamless stainless steel tube for boilers and heat exchangers — higher-Mo austenitic HX tube when 2% Mo 316-class PREN is no longer enough. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X