GB/T 13296 07Cr19Ni11Ti Seamless Stainless Steel Tube
What is GB/T 13296 07Cr19Ni11Ti Seamless Stainless Steel Tube
GB/T 13296-2023 is the Chinese national standard for seamless stainless steel tubes for boilers and heat exchangers — replacing the 2013 edition. Grade 07Cr19Ni11Ti (unified number S32169) sits in the austenitic set. Table 4 splits hot-finished and cold-finished minimum solution temperatures for this mark.
SHH STEEL can produce and supply GB/T 13296 07Cr19Ni11Ti as seamless W-C or W-H tube across the enquiry OD×wall band, heat-treated per Table 4, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 07Cr19Ni11Ti before production starts. Corrosion framing beside 07Cr19Ni11Ti: stabilisation plus H-carbon for hot sulphurous duty.
Shop language may still say “321H tube,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 13296 and 07Cr19Ni11Ti so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti.
Scope discipline: 07Cr19Ni11Ti is seamless boiler/HX tube under GB/T 13296, not fluid-transport pipe under GB/T 14976 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include 06Cr18Ni11Ti, 07Cr18Ni11Nb, 07Cr19Ni10, 07Cr17Ni12Mo2. Role reminder: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty.
Inside this GB/T 13296 series, compare GB/T 13296 06Cr18Ni11Ti, GB/T 13296 07Cr18Ni11Nb, GB/T 13296 07Cr19Ni10, GB/T 13296 07Cr17Ni12Mo2. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP321H.
Project teams specifying 07Cr19Ni11Ti should link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and GB/T 4237 07Cr19Ni11Ti so purchasing does not treat one product form as the other. Confirm 07Cr19Ni11Ti OD × wall and plate thickness on separate drawings.
Chemical Composition of GB/T 13296 07Cr19Ni11Ti
Cast analysis for GB/T 13296 07Cr19Ni11Ti follows Table 3. Key windows on a typical certificate include C 0.04–0.10, Si ≤0.75, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 9.00–13.00, Cr 17.00–19.00, Ti 4(C+N)–0.70. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 321H / UNS S32169; unified number S32169. Corrosion thread: stabilisation plus H-carbon for hot sulphurous duty.
Chemical limits for 07Cr19Ni11Ti under GB/T 13296-2023 appear in the table underneath. Source priority is the 2023 Table 3 extract (xtd). If your client specification cites a 2013 footnote, send it before the heat is melted. Duty thread: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 07Cr19Ni11Ti before the order is acknowledged. This paragraph is locked to 07Cr19Ni11Ti duty: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty.
| Grade | C | Si | Mn | P | S | Ni | Cr | Ti |
|---|---|---|---|---|---|---|---|---|
| 07Cr19Ni11Ti | 0.04–0.10 | ≤0.75 | ≤2.00 | ≤0.035 | ≤0.015 | 9.00–13.00 | 17.00–19.00 | 4(C+N)–0.70 |
Mechanical Properties of GB/T 13296 07Cr19Ni11Ti
Ambient tensile floors for 07Cr19Ni11Ti come from GB/T 13296 Table 4: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: Annex A/B elevated data apply; grain size 4–7. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti.
Hardness testing is by agreement for wall ≥1.7 mm; Table 5 bands differ for special marks such as 06Cr18Ni13Si4 and the high-Mo austenitics. Density reference for 07Cr19Ni11Ti is 7.98 kg/dm³. Hydrostatic proof uses P=2SR/D with R at 60% of Table 4 Rp0.2, capped at 20 MPa.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 07Cr19Ni11Ti | 520 | 205 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 07Cr19Ni11Ti. Heat treatment (Table 4): W-H ≥1050 °C rapid cool; W-C ≥1100 °C rapid cool. Annex A/B elevated data apply; grain size 4–7. Density 7.98 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 07Cr19Ni11Ti
For 07Cr19Ni11Ti, the mill path is pierce / extrude / draw — never ERW or automatic-arc under GB/T 13296. Delivery is heat-treated and pickled unless overall ground/bored or protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO. Seamless W-C and W-H routes are the only valid order paths for 07Cr19Ni11Ti under GB/T 13296.
Steelmaking for 07Cr19Ni11Ti is electric-arc or converter with secondary refining, or electroslag remelting. Pickling follows heat treatment unless bright protective-atmosphere practice or overall machining allows omission. Size practice: straight W-H/W-C with route-specific solution temperatures per Table 4. Pickling or bright-anneal decisions for 07Cr19Ni11Ti stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Application context for 07Cr19Ni11Ti stays high-temperature refinery HX, creep-conscious stabilised steam coils, Annex A/B referenced service.
Eddy-current testing to GB/T 7735 E3H may replace hydrostatic proof when agreed; ultrasonic testing to GB/T 5777 U2 remains a standard acceptance path for 07Cr19Ni11Ti. Role: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. Hydrostatic pressure or eddy-current class for 07Cr19Ni11Ti is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Keep the 07Cr19Ni11Ti caution visible here: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti.
Dimensions and Tolerances for GB/T 13296 07Cr19Ni11Ti
Dimensions and tolerances for 07Cr19Ni11Ti follow GB/T 13296 Table 1. Usual length is 2000–12000 mm. W-H OD tolerance is ±1.25%D for D≤140 mm and ±1%D above; W-C uses absolute OD bands from ±0.10 mm (D≤25) up through ±0.5%D for D>159 mm. Size hint: straight W-H/W-C with route-specific solution temperatures per Table 4.
Out-of-roundness and wall unevenness for 07Cr19Ni11Ti shall not exceed 80% of the OD and wall tolerances respectively. Full-length camber ≤0.15% of tube length. Duty: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. Fixed lengths and multiple cut lengths for 07Cr19Ni11Ti are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 07Cr19Ni11Ti stays high-temperature refinery HX, creep-conscious stabilised steam coils, Annex A/B referenced service.
Equivalent Grades for GB/T 13296 07Cr19Ni11Ti
European and ASTM marks may sit near 321H / UNS S32169, yet GB/T 13296 hydrostatic and heat-treatment text for 07Cr19Ni11Ti still diverge. Keep 07Cr19Ni11Ti as the governing symbol. Caution retained from pack notes: IGC exempt with grain-size 4–7; Si ceiling ≤0. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (07Cr19Ni11Ti).
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 07Cr19Ni11Ti | Governing tube grade for this page |
| Commercial / UNS (body only) | 321H / UNS S32169 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Inside this series compare GB/T 13296 06Cr18Ni11Ti, GB/T 13296 07Cr18Ni11Nb, GB/T 13296 07Cr19Ni10, GB/T 13296 07Cr17Ni12Mo2 before swapping marks for medium or temperature. Keep this caution visible for 07Cr19Ni11Ti: IGC exempt with grain-size 4–7; Si ceiling ≤0. Hub: GB/T 13296. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (07Cr19Ni11Ti).
Heat Treatment and Delivery Condition for GB/T 13296 07Cr19Ni11Ti
Heat treatment for 07Cr19Ni11Ti follows Table 4: W-H ≥1050 °C rapid cool; W-C ≥1100 °C rapid cool. Delivery condition: solution annealed. SHH STEEL records furnace charts that support the temperature and cool method claimed on the certificate. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 07Cr19Ni11Ti unless the mark is on the exemption list.
Field heat treatment of 07Cr19Ni11Ti after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 07Cr19Ni11Ti unless the mark is on the exemption list. Field heat treatment of 07Cr19Ni11Ti after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 07Cr19Ni11Ti: 321H-oriented fillers; grain control on the certificate.
Corrosion Resistance of GB/T 13296 07Cr19Ni11Ti
Corrosion behaviour of 07Cr19Ni11Ti in boiler/HX service: stabilisation plus H-carbon for hot sulphurous duty. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 07Cr19Ni11Ti unless the mark is on the exemption list. Medium risk note: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti.
If operating chlorides, temperature, or under-deposit geometry change after award, reopen the alloy choice for 07Cr19Ni11Ti rather than relying on wall thickness alone. Apps: high-temperature refinery HX, creep-conscious stabilised steam coils, Annex A/B referenced service. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 07Cr19Ni11Ti rather than relying on wall thickness alone. This paragraph is locked to 07Cr19Ni11Ti duty: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty.
Applications of GB/T 13296 07Cr19Ni11Ti Seamless Tube
Typical applications for GB/T 13296 07Cr19Ni11Ti: high-temperature refinery HX, creep-conscious stabilised steam coils, Annex A/B referenced service. Duty summary: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. SHH STEEL can produce and supply the sizes and tests those packages need when the mill schedule allows. Spool fabricators should copy 07Cr19Ni11Ti onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 07Cr19Ni11Ti caution visible here: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti.
Spool and bundle fabricators should copy 07Cr19Ni11Ti onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Role: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. Commissioning teams benefit when the as-built dossier repeats 07Cr19Ni11Ti beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 07Cr19Ni11Ti remains straight W-H/W-C with route-specific solution temperatures per Table 4.
Weldability of GB/T 13296 07Cr19Ni11Ti
Weldability of 07Cr19Ni11Ti: 321H-oriented fillers; grain control on the certificate. Procedure qualification should use the same product form and wall class as production, including the seamless finish that will ship. Caution: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti. Procedure qualification for 07Cr19Ni11Ti should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 07Cr19Ni11Ti remains straight W-H/W-C with route-specific solution temperatures per Table 4.
Shielding-gas and purge notes for 07Cr19Ni11Ti stay with the WPS package so site crews cannot improvise. Apps: high-temperature refinery HX, creep-conscious stabilised steam coils, Annex A/B referenced service. Consumable lot control and shielding-gas notes for 07Cr19Ni11Ti stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Application context for 07Cr19Ni11Ti stays high-temperature refinery HX, creep-conscious stabilised steam coils, Annex A/B referenced service.
Surface Finishes for GB/T 13296 07Cr19Ni11Ti
07Cr19Ni11Ti under GB/T 13296 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (07Cr19Ni11Ti).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
For 07Cr19Ni11Ti, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this tube. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (07Cr19Ni11Ti).
Inspection and Testing for GB/T 13296 07Cr19Ni11Ti
Inspection for 07Cr19Ni11Ti includes melt analysis, tensile tests, hydrostatic or eddy-current E3H, ultrasonic U2, and size/straightness checks. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 07Cr19Ni11Ti unless the mark is on the exemption list. Flattening applies for wall ≤10 mm; flaring for D≤150 mm and wall ≤10 mm.
Non-conforming 07Cr19Ni11Ti lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Documents: GB/T 2102 / EN 10204 3.1 style as ordered. Non-conforming 07Cr19Ni11Ti lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Application context for 07Cr19Ni11Ti stays high-temperature refinery HX, creep-conscious stabilised steam coils, Annex A/B referenced service.
Packaging and Shipping for GB/T 13296 07Cr19Ni11Ti
Packaging for 07Cr19Ni11Ti uses capped ends, wrapped bundles or wooden crates, and waterproof protection matched to the voyage. Bundle tickets repeat grade, heat, size, and quantity. Size hint: straight W-H/W-C with route-specific solution temperatures per Table 4. Bundle tickets for 07Cr19Ni11Ti repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 07Cr19Ni11Ti: 321H-oriented fillers; grain control on the certificate.
Marking on 07Cr19Ni11Ti includes standard, grade, heat number, size, and manufacture symbol so site receiving can match crates to the packing list without opening every wrap. Desiccant and wrap choices for 07Cr19Ni11Ti follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 07Cr19Ni11Ti: stabilisation plus H-carbon for hot sulphurous duty.
SHH STEEL can adjust crate schedules for 07Cr19Ni11Ti when staggered retubing deliveries are on the project calendar. Weld-shop note: 321H-oriented fillers; grain control on the certificate. Claims handling for 07Cr19Ni11Ti starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 07Cr19Ni11Ti stays high-temperature refinery HX, creep-conscious stabilised steam coils, Annex A/B referenced service.
Why Choose SHH STEEL
SHH STEEL can produce and supply GB/T 13296 07Cr19Ni11Ti against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Duty: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. SHH STEEL can produce and supply 07Cr19Ni11Ti against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Keep the 07Cr19Ni11Ti caution visible here: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti.
SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 07Cr19Ni11Ti when the mill schedule allows. Sisters on the same hub: 06Cr18Ni11Ti, 07Cr18Ni11Nb, 07Cr19Ni10, 07Cr17Ni12Mo2. SHH STEEL can make 07Cr19Ni11Ti to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Weld-shop note tied to 07Cr19Ni11Ti: 321H-oriented fillers; grain control on the certificate.
Supply Capability
SHH STEEL can produce and supply GB/T 13296 07Cr19Ni11Ti seamless tube to the enquiry size list with Table 3 chemistry, Table 4 heat treatment and tensile floors, and the NDT/hydro stack the datasheet names. Role: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 07Cr19Ni11Ti when the mill schedule allows. Keep the 07Cr19Ni11Ti caution visible here: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 07Cr19Ni11Ti (S32169) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes: SHH STEEL can supply 07Cr19Ni11Ti in common HX OD×min-wall bands and boiler straight lengths; non-stock walls and U-bend radii are rolled to order. Confirm W-C versus W-H before booking. Duty: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. SHH STEEL can supply alternate walls and W-C/W-H classes for 07Cr19Ni11Ti once design pressure and corrosion allowance are clear. This paragraph is locked to 07Cr19Ni11Ti duty: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty.
SHH STEEL can produce trial bends and qualification lengths of 07Cr19Ni11Ti ahead of bulk release when the exchanger fabricator needs WPS coupons. Weld-shop: 321H-oriented fillers; grain control on the certificate. SHH STEEL can produce trial lengths of 07Cr19Ni11Ti for procedure qualification before bulk release when the project calendar needs it. Size practice for 07Cr19Ni11Ti remains straight W-H/W-C with route-specific solution temperatures per Table 4.
FAQ
-
What is GB/T 13296 07Cr19Ni11Ti seamless stainless steel tube used for?
- GB/T 13296 07Cr19Ni11Ti is seamless stainless tube for boilers and heat exchangers — high-temperature refinery HX, creep-conscious stabilised steam coils, Annex A/B referenced service. Role summary: carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. It is a Chinese product standard grade (S32169), not an automatic ASTM A213 certificate.
-
Is GB/T 13296 07Cr19Ni11Ti seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 07Cr19Ni11Ti when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 07Cr19Ni11Ti?
- 07Cr19Ni11Ti is delivered solution annealed under GB/T 13296. Table 4 reference: W-H ≥1050 °C rapid cool; W-C ≥1100 °C rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark.
-
How does 07Cr19Ni11Ti compare with sister grades 06Cr18Ni11Ti, 07Cr18Ni11Nb, 07Cr19Ni10?
- 07Cr19Ni11Ti is filed as austenitic. Typical sisters on the same RFQ are 06Cr18Ni11Ti, 07Cr18Ni11Nb, 07Cr19Ni10. Design caution: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 07Cr19Ni11Ti?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 321H / UNS S32169 the same as ordering 07Cr19Ni11Ti?
- No. 321H / UNS S32169 is a commercial / UNS cross-walk for body text (unified S32169). The purchase order should lock GB/T 13296 and 07Cr19Ni11Ti so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 07Cr19Ni11Ti?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 07Cr19Ni11Ti within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: straight W-H/W-C with route-specific solution temperatures per Table 4. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 07Cr19Ni11Ti be welded on site?
- Shop guidance: 321H-oriented fillers; grain control on the certificate. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti
-
When should I choose a higher-Mo or superaustenitic grade instead of 07Cr19Ni11Ti?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: IGC exempt with grain-size 4–7; Si ceiling ≤0.75 and Ti 4(C+N)–0.70 differ from 06Cr18Ni11Ti Sister pointers: 06Cr18Ni11Ti, 07Cr18Ni11Nb, 07Cr19Ni10. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 07Cr19Ni11Ti with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 07Cr19Ni11Ti does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 07Cr19Ni11Ti?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 07Cr19Ni11Ti when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 07Cr19Ni11Ti is seamless stainless steel tube for boilers and heat exchangers — carbon-floor Ti-stabilised austenitic tube for elevated-temperature stabilised boiler/HX duty. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr18Ni11Ti, 07Cr18Ni11Nb, 07Cr19Ni10. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.