GB/T 13296 015Cr21Ni26Mo5Cu2 Seamless Stainless Steel Tube
What is GB/T 13296 015Cr21Ni26Mo5Cu2 Seamless Stainless Steel Tube
GB/T 13296-2023 is the Chinese national standard for seamless stainless steel tubes for boilers and heat exchangers — replacing the 2013 edition. Grade 015Cr21Ni26Mo5Cu2 (unified number S39042) sits in the austenitic set. It sits with the high-alloy Cu-Mo set for acid heat-exchange packages.
SHH STEEL can produce and supply GB/T 13296 015Cr21Ni26Mo5Cu2 as seamless W-C or W-H tube across the enquiry OD×wall band, heat-treated per Table 4, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers.
Shop language may still say “904L-class tube,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 13296 and 015Cr21Ni26Mo5Cu2 so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark.
Scope discipline: 015Cr21Ni26Mo5Cu2 is seamless boiler/HX tube under GB/T 13296, not fluid-transport pipe under GB/T 14976 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include 015Cr20Ni18Mo6CuN, 022Cr21Ni25Mo7N, 022Cr18Ni14Mo2Cu2, 022Cr19Ni13Mo3. Role reminder: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers.
Inside this GB/T 13296 series, compare GB/T 13296 015Cr20Ni18Mo6CuN, GB/T 13296 022Cr21Ni25Mo7N, GB/T 13296 022Cr18Ni14Mo2Cu2, GB/T 13296 022Cr19Ni13Mo3. Hub: GB/T 13296.
Chemical Composition of GB/T 13296 015Cr21Ni26Mo5Cu2
Cast analysis for GB/T 13296 015Cr21Ni26Mo5Cu2 follows Table 3. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Key windows on a typical certificate include C ≤0.020, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 23.00–28.00, Cr 19.00–23.00, Mo 4.00–5.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 904L-class / UNS N08904-related; unified number S39042. Corrosion thread: Cu+Mo+high Ni for reducing-acid and chloride crossover duties.
Chemical limits for 015Cr21Ni26Mo5Cu2 under GB/T 13296-2023 appear in the table underneath. Source priority is the 2023 Table 3 extract (xtd). If your client specification cites a 2013 footnote, send it before the heat is melted. Duty thread: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 015Cr21Ni26Mo5Cu2 before the order is acknowledged. Corrosion framing beside 015Cr21Ni26Mo5Cu2: Cu+Mo+high Ni for reducing-acid and chloride crossover duties.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo | Cu | N |
|---|---|---|---|---|---|---|---|---|---|---|
| 015Cr21Ni26Mo5Cu2 | ≤0.020 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.015 | 23.00–28.00 | 19.00–23.00 | 4.00–5.00 | 1.00–2.00 | ≤0.10 |
UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 015Cr21Ni26Mo5Cu2 (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 904L-class / UNS N08904-related, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 015Cr21Ni26Mo5Cu2 against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 015Cr21Ni26Mo5Cu2 before the heat is booked.
Mechanical Properties of GB/T 13296 015Cr21Ni26Mo5Cu2
Ambient tensile floors for 015Cr21Ni26Mo5Cu2 come from GB/T 13296 Table 4: Rm min 490 MPa, Rp0.2 min 220 MPa, elongation min 35%. Note: UNCERTAIN — provisional vs paid Table 3/4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark.
Hardness testing is by agreement for wall ≥1.7 mm; Table 5 bands differ for special marks such as 06Cr18Ni13Si4 and the high-Mo austenitics. Density reference for 015Cr21Ni26Mo5Cu2 is 8.05 kg/dm³. Hydrostatic proof uses P=2SR/D with R at 60% of Table 4 Rp0.2, capped at 20 MPa.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 015Cr21Ni26Mo5Cu2 | 490 | 220 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 015Cr21Ni26Mo5Cu2. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1065–1150 °C, rapid cool. UNCERTAIN — provisional vs paid Table 3/4. Density 8.05 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 015Cr21Ni26Mo5Cu2
For 015Cr21Ni26Mo5Cu2, the mill path is pierce / extrude / draw — never ERW or automatic-arc under GB/T 13296. Delivery is heat-treated and pickled unless overall ground/bored or protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO. Seamless W-C and W-H routes are the only valid order paths for 015Cr21Ni26Mo5Cu2 under GB/T 13296.
Steelmaking for 015Cr21Ni26Mo5Cu2 is electric-arc or converter with secondary refining, or electroslag remelting. Pickling follows heat treatment unless bright protective-atmosphere practice or overall machining allows omission. Size practice: W-C acid-HX stock with alloy surcharge clarity on the quote. Pickling or bright-anneal decisions for 015Cr21Ni26Mo5Cu2 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark.
Eddy-current testing to GB/T 7735 E3H may replace hydrostatic proof when agreed; ultrasonic testing to GB/T 5777 U2 remains a standard acceptance path for 015Cr21Ni26Mo5Cu2. Role: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. Hydrostatic pressure or eddy-current class for 015Cr21Ni26Mo5Cu2 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Application context for 015Cr21Ni26Mo5Cu2 stays sulphuric acid coolers, mixed-acid condensers, and high-alloy chemical HX.
Dimensions and Tolerances for GB/T 13296 015Cr21Ni26Mo5Cu2
Dimensions and tolerances for 015Cr21Ni26Mo5Cu2 follow GB/T 13296 Table 1. Usual length is 2000–12000 mm. W-H OD tolerance is ±1.25%D for D≤140 mm and ±1%D above; W-C uses absolute OD bands from ±0.10 mm (D≤25) up through ±0.5%D for D>159 mm. Size hint: W-C acid-HX stock with alloy surcharge clarity on the quote.
Out-of-roundness and wall unevenness for 015Cr21Ni26Mo5Cu2 shall not exceed 80% of the OD and wall tolerances respectively. Full-length camber ≤0.15% of tube length. Duty: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. Fixed lengths and multiple cut lengths for 015Cr21Ni26Mo5Cu2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 015Cr21Ni26Mo5Cu2 duty: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers.
Equivalent Grades for GB/T 13296 015Cr21Ni26Mo5Cu2
Buyers searching under 904L-class / UNS N08904-related still need the GB/T 13296 015Cr21Ni26Mo5Cu2 row locked on the acknowledgement. Inside austenitic practice the mechanical table and inspection clauses of GB/T 13296 control acceptance, not a brochure equivalent. Duty context: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 015Cr21Ni26Mo5Cu2 | Governing tube grade for this page |
| Commercial / UNS (body only) | 904L-class / UNS N08904-related (unified S39042) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | 904L-family related marks | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
We deliberately avoid inventing a false one-to-one for every foreign system on 015Cr21Ni26Mo5Cu2. Use GB/T 13296 015Cr20Ni18Mo6CuN, GB/T 13296 022Cr21Ni25Mo7N, GB/T 13296 022Cr18Ni14Mo2Cu2, GB/T 13296 022Cr19Ni13Mo3 for in-series alternatives, and keep GB/T 13296 as the category landing page. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (015Cr21Ni26Mo5Cu2).
Buyers comparing 015Cr21Ni26Mo5Cu2 tubulars with sheet/plate can the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 4237 015Cr21Ni26Mo5Cu2. See also the GB/T 4237 hub for related plate designations. Keep 015Cr21Ni26Mo5Cu2 acceptance text on the governing pipe/tube standard.
Heat Treatment and Delivery Condition for GB/T 13296 015Cr21Ni26Mo5Cu2
Heat treatment for 015Cr21Ni26Mo5Cu2 follows Table 4: 1065–1150 °C, rapid cool. Delivery condition: solution annealed. SHH STEEL records furnace charts that support the temperature and cool method claimed on the certificate. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 015Cr21Ni26Mo5Cu2 unless the mark is on the exemption list.
Field heat treatment of 015Cr21Ni26Mo5Cu2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 015Cr21Ni26Mo5Cu2 unless the mark is on the exemption list. Field heat treatment of 015Cr21Ni26Mo5Cu2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 015Cr21Ni26Mo5Cu2: Cu+Mo+high Ni for reducing-acid and chloride crossover duties.
Corrosion Resistance of GB/T 13296 015Cr21Ni26Mo5Cu2
Corrosion behaviour of 015Cr21Ni26Mo5Cu2 in boiler/HX service: Cu+Mo+high Ni for reducing-acid and chloride crossover duties. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 015Cr21Ni26Mo5Cu2 unless the mark is on the exemption list. Medium risk note: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark.
If operating chlorides, temperature, or under-deposit geometry change after award, reopen the alloy choice for 015Cr21Ni26Mo5Cu2 rather than relying on wall thickness alone. Apps: sulphuric acid coolers, mixed-acid condensers, and high-alloy chemical HX. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 015Cr21Ni26Mo5Cu2 rather than relying on wall thickness alone. Size practice for 015Cr21Ni26Mo5Cu2 remains W-C acid-HX stock with alloy surcharge clarity on the quote.
Applications of GB/T 13296 015Cr21Ni26Mo5Cu2 Seamless Tube
Typical applications for GB/T 13296 015Cr21Ni26Mo5Cu2: sulphuric acid coolers, mixed-acid condensers, and high-alloy chemical HX. Duty summary: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. SHH STEEL can produce and supply the sizes and tests those packages need when the mill schedule allows. Spool fabricators should copy 015Cr21Ni26Mo5Cu2 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark.
Spool and bundle fabricators should copy 015Cr21Ni26Mo5Cu2 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Role: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. Commissioning teams benefit when the as-built dossier repeats 015Cr21Ni26Mo5Cu2 beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 015Cr21Ni26Mo5Cu2 stays sulphuric acid coolers, mixed-acid condensers, and high-alloy chemical HX.
Weldability of GB/T 13296 015Cr21Ni26Mo5Cu2
Weldability of 015Cr21Ni26Mo5Cu2: 904L/matching fillers; low heat input. Procedure qualification should use the same product form and wall class as production, including the seamless finish that will ship. Caution: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark. Procedure qualification for 015Cr21Ni26Mo5Cu2 should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark.
Shielding-gas and purge notes for 015Cr21Ni26Mo5Cu2 stay with the WPS package so site crews cannot improvise. Apps: sulphuric acid coolers, mixed-acid condensers, and high-alloy chemical HX. Consumable lot control and shielding-gas notes for 015Cr21Ni26Mo5Cu2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 015Cr21Ni26Mo5Cu2: 904L/matching fillers; low heat input.
Surface Finishes for GB/T 13296 015Cr21Ni26Mo5Cu2
015Cr21Ni26Mo5Cu2 under GB/T 13296 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (015Cr21Ni26Mo5Cu2).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
For 015Cr21Ni26Mo5Cu2, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this tube. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (015Cr21Ni26Mo5Cu2).
Inspection and Testing for GB/T 13296 015Cr21Ni26Mo5Cu2
Inspection for 015Cr21Ni26Mo5Cu2 includes melt analysis, tensile tests, hydrostatic or eddy-current E3H, ultrasonic U2, and size/straightness checks. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 015Cr21Ni26Mo5Cu2 unless the mark is on the exemption list. Flattening applies for wall ≤10 mm; flaring for D≤150 mm and wall ≤10 mm.
Non-conforming 015Cr21Ni26Mo5Cu2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Documents: GB/T 2102 / EN 10204 3.1 style as ordered. Non-conforming 015Cr21Ni26Mo5Cu2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. This paragraph is locked to 015Cr21Ni26Mo5Cu2 duty: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers.
Packaging and Shipping for GB/T 13296 015Cr21Ni26Mo5Cu2
Packaging for 015Cr21Ni26Mo5Cu2 uses capped ends, wrapped bundles or wooden crates, and waterproof protection matched to the voyage. Bundle tickets repeat grade, heat, size, and quantity. Size hint: W-C acid-HX stock with alloy surcharge clarity on the quote. Bundle tickets for 015Cr21Ni26Mo5Cu2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 015Cr21Ni26Mo5Cu2 duty: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers.
Marking on 015Cr21Ni26Mo5Cu2 includes standard, grade, heat number, size, and manufacture symbol so site receiving can match crates to the packing list without opening every wrap. Desiccant and wrap choices for 015Cr21Ni26Mo5Cu2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 015Cr21Ni26Mo5Cu2: 904L/matching fillers; low heat input.
SHH STEEL can adjust crate schedules for 015Cr21Ni26Mo5Cu2 when staggered retubing deliveries are on the project calendar. Weld-shop note: 904L/matching fillers; low heat input. Claims handling for 015Cr21Ni26Mo5Cu2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 015Cr21Ni26Mo5Cu2: Cu+Mo+high Ni for reducing-acid and chloride crossover duties.
Why Choose SHH STEEL
SHH STEEL can produce and supply GB/T 13296 015Cr21Ni26Mo5Cu2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Duty: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. SHH STEEL can produce and supply 015Cr21Ni26Mo5Cu2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Weld-shop note tied to 015Cr21Ni26Mo5Cu2: 904L/matching fillers; low heat input.
SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 015Cr21Ni26Mo5Cu2 when the mill schedule allows. Sisters on the same hub: 015Cr20Ni18Mo6CuN, 022Cr21Ni25Mo7N, 022Cr18Ni14Mo2Cu2, 022Cr19Ni13Mo3. SHH STEEL can make 015Cr21Ni26Mo5Cu2 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark.
Supply Capability
SHH STEEL can produce and supply GB/T 13296 015Cr21Ni26Mo5Cu2 seamless tube to the enquiry size list with Table 3 chemistry, Table 4 heat treatment and tensile floors, and the NDT/hydro stack the datasheet names. Role: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 015Cr21Ni26Mo5Cu2 when the mill schedule allows. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 015Cr21Ni26Mo5Cu2 (S39042) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes: SHH STEEL can supply 015Cr21Ni26Mo5Cu2 in common HX OD×min-wall bands and boiler straight lengths; non-stock walls and U-bend radii are rolled to order. Confirm W-C versus W-H before booking. Duty: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. SHH STEEL can supply alternate walls and W-C/W-H classes for 015Cr21Ni26Mo5Cu2 once design pressure and corrosion allowance are clear. Corrosion framing beside 015Cr21Ni26Mo5Cu2: Cu+Mo+high Ni for reducing-acid and chloride crossover duties.
SHH STEEL can produce trial bends and qualification lengths of 015Cr21Ni26Mo5Cu2 ahead of bulk release when the exchanger fabricator needs WPS coupons. Weld-shop: 904L/matching fillers; low heat input. SHH STEEL can produce trial lengths of 015Cr21Ni26Mo5Cu2 for procedure qualification before bulk release when the project calendar needs it. Application context for 015Cr21Ni26Mo5Cu2 stays sulphuric acid coolers, mixed-acid condensers, and high-alloy chemical HX.
FAQ
-
What is GB/T 13296 015Cr21Ni26Mo5Cu2 seamless stainless steel tube used for?
- GB/T 13296 015Cr21Ni26Mo5Cu2 is seamless stainless tube for boilers and heat exchangers — sulphuric acid coolers, mixed-acid condensers, and high-alloy chemical HX. Role summary: Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. It is a Chinese product standard grade (S39042), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
-
Is GB/T 13296 015Cr21Ni26Mo5Cu2 seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 015Cr21Ni26Mo5Cu2 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 015Cr21Ni26Mo5Cu2?
- 015Cr21Ni26Mo5Cu2 is delivered solution annealed under GB/T 13296. Table 4 reference: 1065–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 015Cr21Ni26Mo5Cu2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 015Cr21Ni26Mo5Cu2 compare with sister grades 015Cr20Ni18Mo6CuN, 022Cr21Ni25Mo7N, 022Cr18Ni14Mo2Cu2?
- 015Cr21Ni26Mo5Cu2 is filed as austenitic. Typical sisters on the same RFQ are 015Cr20Ni18Mo6CuN, 022Cr21Ni25Mo7N, 022Cr18Ni14Mo2Cu2. Design caution: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 015Cr21Ni26Mo5Cu2?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 904L-class / UNS N08904-related the same as ordering 015Cr21Ni26Mo5Cu2?
- No. 904L-class / UNS N08904-related is a commercial / UNS cross-walk for body text (unified S39042). The purchase order should lock GB/T 13296 and 015Cr21Ni26Mo5Cu2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 015Cr21Ni26Mo5Cu2?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 015Cr21Ni26Mo5Cu2 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: W-C acid-HX stock with alloy surcharge clarity on the quote. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 015Cr21Ni26Mo5Cu2 be welded on site?
- Shop guidance: 904L/matching fillers; low heat input. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark
-
When should I choose a higher-Mo or superaustenitic grade instead of 015Cr21Ni26Mo5Cu2?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN vs paid Table 3/4; do not accept a 316Cu heat as this mark Sister pointers: 015Cr20Ni18Mo6CuN, 022Cr21Ni25Mo7N, 022Cr18Ni14Mo2Cu2. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 015Cr21Ni26Mo5Cu2 with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 015Cr21Ni26Mo5Cu2 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 015Cr21Ni26Mo5Cu2?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 015Cr21Ni26Mo5Cu2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 015Cr21Ni26Mo5Cu2 is seamless stainless steel tube for boilers and heat exchangers — Cu-Mo super-austenitic / 904L-class HX tube for sulphuric and mixed-acid coolers. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 015Cr20Ni18Mo6CuN, 022Cr21Ni25Mo7N, 022Cr18Ni14Mo2Cu2. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.