GB/T 13296 06Cr18Ni12Mo2Cu2 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr18Ni12Mo2Cu2 Seamless Stainless Steel Tube

GB/T 13296 06Cr18Ni12Mo2Cu2 seamless stainless steel tube (316Cu-class / UNS S31688, S31688), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr18Ni12Mo2Cu2 (S31688 / 316Cu-class / UNS S31688 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 06Cr18Ni12Mo2Cu2 Seamless Stainless Steel Tube

When the approved vendor list and exchanger datasheet say GB/T 13296, the grade mark has to be the Chinese designation. 06Cr18Ni12Mo2Cu2 is the full product grade for this austenitic seamless tube. Copper is the intentional lever for reducing-acid heat-exchange duty.

SHH STEEL can supply 06Cr18Ni12Mo2Cu2 seamless tube in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the exchanger: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr18Ni12Mo2Cu2 before production starts. Weld-shop note tied to 06Cr18Ni12Mo2Cu2: matching Cu-bearing or 316L fillers per WPS qualification.

Equivalence talk to 316Cu-class / UNS S31688 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 13296 06Cr18Ni12Mo2Cu2, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade.

Related ASTM A213 tube pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3, 015Cr21Ni26Mo5Cu2. Use thread: sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades.

Inside this GB/T 13296 series, compare GB/T 13296 022Cr18Ni14Mo2Cu2, GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 015Cr21Ni26Mo5Cu2, GB/T 13296 06Cr19Ni13Mo3. Hub: GB/T 13296.

Project teams specifying 06Cr18Ni12Mo2Cu2 should the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 4237 06Cr18Ni12Mo2Cu2. Confirm 06Cr18Ni12Mo2Cu2 OD × wall and plate thickness on separate drawings.

Chemical Composition of GB/T 13296 06Cr18Ni12Mo2Cu2

Chemistry control on 06Cr18Ni12Mo2Cu2 starts at the ladle. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Expect C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 10.00–14.00, Cr 16.00–18.00, Mo 1.20–2.75 within Table 3, reported on the inspection document against the heat. Body alias 316Cu-class / UNS S31688 does not widen those windows.

Read the table with the family in mind — austenitic — and with caution UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade. Numbers without the matching Table 4 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr18Ni12Mo2Cu2 before the order is acknowledged. This paragraph is locked to 06Cr18Ni12Mo2Cu2 duty: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media.

Grade C Si Mn P S Ni Cr Mo Cu
06Cr18Ni12Mo2Cu2 ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.015 10.00–14.00 16.00–18.00 1.20–2.75 1.00–2.50

UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 06Cr18Ni12Mo2Cu2 (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 316Cu-class / UNS S31688, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 06Cr18Ni12Mo2Cu2 against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 06Cr18Ni12Mo2Cu2 before the heat is booked.

Mechanical Properties of GB/T 13296 06Cr18Ni12Mo2Cu2

Proof stress and tensile minima for 06Cr18Ni12Mo2Cu2 sit at Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: UNCERTAIN — provisional vs paid Table 3/4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Flattening and flaring back ductility when size allows. Watch-out: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade.

Batch size limits (D≤76 mm and S≤3 mm: ≤400 tubes; otherwise ≤200) keep sampling honest for 06Cr18Ni12Mo2Cu2. Retests follow GB/T 2102. Density 7.98 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
06Cr18Ni12Mo2Cu2 520 205 35

Ambient values from GB/T 13296-2023 Table 4 for 06Cr18Ni12Mo2Cu2. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1010–1150 °C, rapid cool. UNCERTAIN — provisional vs paid Table 3/4. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 06Cr18Ni12Mo2Cu2

For 06Cr18Ni12Mo2Cu2, the mill path is pierce / extrude / draw — never ERW or automatic-arc under GB/T 13296. Delivery is heat-treated and pickled unless overall ground/bored or protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO. Seamless W-C and W-H routes are the only valid order paths for 06Cr18Ni12Mo2Cu2 under GB/T 13296.

SHH STEEL schedules piercing, elongation, and finishing for 06Cr18Ni12Mo2Cu2 against the W-C or W-H symbol frozen on the acknowledgement. Ovality and wall eccentricity stay inside 80% of the respective OD and wall tolerances. Pickling or bright-anneal decisions for 06Cr18Ni12Mo2Cu2 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Application context for 06Cr18Ni12Mo2Cu2 stays sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades.

Cold-finish depth of longitudinal marks on 06Cr18Ni12Mo2Cu2 is limited to ≤4% of wall and ≤0.2 mm; hot-finish ≤5% and ≤0.4 mm. Apps: sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades. Hydrostatic pressure or eddy-current class for 06Cr18Ni12Mo2Cu2 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Corrosion framing beside 06Cr18Ni12Mo2Cu2: Cu plus Mo helps reducing-acid and sulphate attack beyond plain 316.

Dimensions and Tolerances for GB/T 13296 06Cr18Ni12Mo2Cu2

When 06Cr18Ni12Mo2Cu2 ships as nominal wall, the note under Table 1 still applies different ± bands for hot and cold routes — do not mix W-C absolute OD tols with W-H percentage thinking. Practice: straight and U-bend HX with acid-duty surface finish notes. Tolerance basis for 06Cr18Ni12Mo2Cu2 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 06Cr18Ni12Mo2Cu2 duty: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media.

Fixed lengths of 06Cr18Ni12Mo2Cu2 are end-protected so bevels and ID finish survive inland and ocean transit. Random lengths stay inside the usual 2000–12000 mm window unless agreed otherwise. Fixed lengths and multiple cut lengths for 06Cr18Ni12Mo2Cu2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 06Cr18Ni12Mo2Cu2 duty: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media.

Equivalent Grades for GB/T 13296 06Cr18Ni12Mo2Cu2

Identity first: GB/T 13296 06Cr18Ni12Mo2Cu2 is the HX/boiler tube grade for this page. 316Cu-class / UNS S31688 helps buyers who think in AISI/UNS labels. Role: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media. Foreign product standards remain separate documents. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (06Cr18Ni12Mo2Cu2).

System Designation Notes
GB/T 13296 06Cr18Ni12Mo2Cu2 Governing tube grade for this page
Commercial / UNS (body only) 316Cu-class / UNS S31688 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

We deliberately avoid inventing a false one-to-one for every foreign system on 06Cr18Ni12Mo2Cu2. Use GB/T 13296 022Cr18Ni14Mo2Cu2, GB/T 13296 06Cr17Ni12Mo2, GB/T 13296 06Cr19Ni13Mo3, GB/T 13296 015Cr21Ni26Mo5Cu2 for in-series alternatives, and keep GB/T 13296 as the category landing page. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (06Cr18Ni12Mo2Cu2).

Heat Treatment and Delivery Condition for GB/T 13296 06Cr18Ni12Mo2Cu2

For 06Cr18Ni12Mo2Cu2, solution or anneal practice is not a free mill choice — it is the Table 4 band tied to the grade. Delivery: solution annealed. Role: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media. Recorded furnace charts for 06Cr18Ni12Mo2Cu2 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 06Cr18Ni12Mo2Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade.

When Annex A elevated Rp0.2 is invoked, the certificate for 06Cr18Ni12Mo2Cu2 should still show the Table 4 delivery treatment actually performed. Apps: sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades. Field heat treatment of 06Cr18Ni12Mo2Cu2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for 06Cr18Ni12Mo2Cu2 stays sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades.

Corrosion Resistance of GB/T 13296 06Cr18Ni12Mo2Cu2

Pitting, crevice, oxidation, or weld-decay limiters for 06Cr18Ni12Mo2Cu2 should be named in the datasheet rather than inferred from the AISI alias alone. Framing: Cu plus Mo helps reducing-acid and sulphate attack beyond plain 316. Coupon orientation, weld condition, and surface finish for 06Cr18Ni12Mo2Cu2 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Application context for 06Cr18Ni12Mo2Cu2 stays sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades.

Pickling quality and free-iron cleanliness after fabrication affect startup corrosion of 06Cr18Ni12Mo2Cu2 as much as cast chemistry. Role: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr18Ni12Mo2Cu2 rather than relying on wall thickness alone. This paragraph is locked to 06Cr18Ni12Mo2Cu2 duty: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media.

Applications of GB/T 13296 06Cr18Ni12Mo2Cu2 Seamless Tube

Use 06Cr18Ni12Mo2Cu2 on packages that match sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades. Nearby sisters 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3, 015Cr21Ni26Mo5Cu2 cover adjacent media or temperature steps. Weld-shop note: matching Cu-bearing or 316L fillers per WPS qualification. Spool fabricators should copy 06Cr18Ni12Mo2Cu2 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 06Cr18Ni12Mo2Cu2 remains straight and U-bend HX with acid-duty surface finish notes.

When the process medium changes mid-project, revisit whether 06Cr18Ni12Mo2Cu2 still fits before releasing more heats. Sisters: 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3, 015Cr21Ni26Mo5Cu2. Commissioning teams benefit when the as-built dossier repeats 06Cr18Ni12Mo2Cu2 beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 06Cr18Ni12Mo2Cu2 stays sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades.

Weldability of GB/T 13296 06Cr18Ni12Mo2Cu2

Consumable selection for 06Cr18Ni12Mo2Cu2 follows matching Cu-bearing or 316L fillers per WPS qualification. Do not improvise under-alloyed fillers on Mo or Cu grades. Role: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media. Procedure qualification for 06Cr18Ni12Mo2Cu2 should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 06Cr18Ni12Mo2Cu2 remains straight and U-bend HX with acid-duty surface finish notes.

Ferrite control and hot-cracking risk for 06Cr18Ni12Mo2Cu2 depend on the family chemistry; qualify on production wall, not only on plate coupons. Weld shop: matching Cu-bearing or 316L fillers per WPS qualification. Consumable lot control and shielding-gas notes for 06Cr18Ni12Mo2Cu2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 06Cr18Ni12Mo2Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade.

Surface Finishes for GB/T 13296 06Cr18Ni12Mo2Cu2

On 06Cr18Ni12Mo2Cu2, cosmetics never outrank correct heat treatment. Passivation and polish are sequenced after the anneal that qualifies the tube. Duty locked here: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media. Name which surface carries each finish callout. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 06Cr18Ni12Mo2Cu2.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Bright or polished callouts for 06Cr18Ni12Mo2Cu2 never waive heat-treatment proof. After finishing, keep iron-free handling through storage and shipment so GB/T 13296 tube does not leave the yard with free-iron blooms. Caution retained: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade.

Inspection and Testing for GB/T 13296 06Cr18Ni12Mo2Cu2

SHH STEEL keeps heat identity for 06Cr18Ni12Mo2Cu2 unbroken from melt through bundle tags, including third-party hold points written into the PO. Caution: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade. Sampling plans for 06Cr18Ni12Mo2Cu2 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to 06Cr18Ni12Mo2Cu2 duty: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media.

Certificate lines for 06Cr18Ni12Mo2Cu2 must repeat the Chinese grade, unified number, manufacture symbol, and heat treatment actually performed. Caution: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade. Non-conforming 06Cr18Ni12Mo2Cu2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. This paragraph is locked to 06Cr18Ni12Mo2Cu2 duty: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media.

Packaging and Shipping for GB/T 13296 06Cr18Ni12Mo2Cu2

Desiccant and wrap choices for 06Cr18Ni12Mo2Cu2 follow voyage length and storage climate on the shipping order, not a one-size export habit. Apps: sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades. Bundle tickets for 06Cr18Ni12Mo2Cu2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for 06Cr18Ni12Mo2Cu2 remains straight and U-bend HX with acid-duty surface finish notes.

Inland trucking of 06Cr18Ni12Mo2Cu2 still needs end protection — most ID dents happen between the port and the exchanger shop. Apps: sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades. Desiccant and wrap choices for 06Cr18Ni12Mo2Cu2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. This paragraph is locked to 06Cr18Ni12Mo2Cu2 duty: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media.

Barcode or stencil extras for 06Cr18Ni12Mo2Cu2 are available when the owner’s material system needs them. Apps: sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades. Claims handling for 06Cr18Ni12Mo2Cu2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 06Cr18Ni12Mo2Cu2 remains straight and U-bend HX with acid-duty surface finish notes.

Why Choose SHH STEEL

SHH STEEL can make 06Cr18Ni12Mo2Cu2 to a boiler/HX test stack — hydro or E3H, UT U2, flattening/flaring, IGC when required — instead of a generic stainless tube habit. Apps: sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades. SHH STEEL can produce and supply 06Cr18Ni12Mo2Cu2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Keep the 06Cr18Ni12Mo2Cu2 caution visible here: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade.

SHH STEEL can supply 06Cr18Ni12Mo2Cu2 with third-party inspection hold points written into the itinerary. Weld-shop note: matching Cu-bearing or 316L fillers per WPS qualification. SHH STEEL can make 06Cr18Ni12Mo2Cu2 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Weld-shop note tied to 06Cr18Ni12Mo2Cu2: matching Cu-bearing or 316L fillers per WPS qualification.

Supply Capability

SHH STEEL can supply 06Cr18Ni12Mo2Cu2 with EN 10204 3.1 style documents, IGC when required, and hardness by agreement. Caution: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr18Ni12Mo2Cu2 when the mill schedule allows. Size practice for 06Cr18Ni12Mo2Cu2 remains straight and U-bend HX with acid-duty surface finish notes.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 06Cr18Ni12Mo2Cu2 (S31688)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes: rolling cycles for 06Cr18Ni12Mo2Cu2 cover usual 2000–12000 mm lengths; cut-to-length and multiple lengths ship once tests clear. Caution: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr18Ni12Mo2Cu2 once design pressure and corrosion allowance are clear. Weld-shop note tied to 06Cr18Ni12Mo2Cu2: matching Cu-bearing or 316L fillers per WPS qualification.

SHH STEEL can supply replacement retubing heats of 06Cr18Ni12Mo2Cu2 matched to prior certificates when the plant provides heat history. Apps: sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades. SHH STEEL can produce trial lengths of 06Cr18Ni12Mo2Cu2 for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to 06Cr18Ni12Mo2Cu2: matching Cu-bearing or 316L fillers per WPS qualification.

FAQ

What is GB/T 13296 06Cr18Ni12Mo2Cu2 seamless stainless steel tube used for?
GB/T 13296 06Cr18Ni12Mo2Cu2 is seamless stainless tube for boilers and heat exchangers — sulphuric-acid coolers, sulphate process condensers, and reducing-acid HX upgrades. Role summary: Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media. It is a Chinese product standard grade (S31688), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
Is GB/T 13296 06Cr18Ni12Mo2Cu2 seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr18Ni12Mo2Cu2 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 06Cr18Ni12Mo2Cu2?
06Cr18Ni12Mo2Cu2 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr18Ni12Mo2Cu2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr18Ni12Mo2Cu2 compare with sister grades 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2?
06Cr18Ni12Mo2Cu2 is filed as austenitic. Typical sisters on the same RFQ are 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2. Design caution: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr18Ni12Mo2Cu2?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 316Cu-class / UNS S31688 the same as ordering 06Cr18Ni12Mo2Cu2?
No. 316Cu-class / UNS S31688 is a commercial / UNS cross-walk for body text (unified S31688). The purchase order should lock GB/T 13296 and 06Cr18Ni12Mo2Cu2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 06Cr18Ni12Mo2Cu2?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr18Ni12Mo2Cu2 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: straight and U-bend HX with acid-duty surface finish notes. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 06Cr18Ni12Mo2Cu2 be welded on site?
Shop guidance: matching Cu-bearing or 316L fillers per WPS qualification. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr18Ni12Mo2Cu2?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN vs paid Table 3/4; Cu band is identity — missing Cu is a different grade Sister pointers: 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 06Cr18Ni12Mo2Cu2 with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr18Ni12Mo2Cu2 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 06Cr18Ni12Mo2Cu2?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr18Ni12Mo2Cu2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 06Cr18Ni12Mo2Cu2 is seamless stainless steel tube for boilers and heat exchangers — Cu-bearing Mo austenitic tube aimed at reducing-acid and sulphate HX media. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 015Cr21Ni26Mo5Cu2. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X