GB/T 13296 06Cr23Ni13 Seamless Stainless Steel Tube
What is GB/T 13296 06Cr23Ni13 Seamless Stainless Steel Tube
GB/T 13296-2023 is the Chinese national standard for seamless stainless steel tubes for boilers and heat exchangers — replacing the 2013 edition. Grade 06Cr23Ni13 (unified number S30908) sits in the austenitic set. It is the low-carbon 309S-class sister inside the GB/T 13296 heat set.
SHH STEEL can produce and supply GB/T 13296 06Cr23Ni13 as seamless W-C or W-H tube across the enquiry OD×wall band, heat-treated per Table 4, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils.
Shop language may still say “309S tube,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 13296 and 06Cr23Ni13 so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy.
Scope discipline: 06Cr23Ni13 is seamless boiler/HX tube under GB/T 13296, not fluid-transport pipe under GB/T 14976 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include 16Cr23Ni13, 06Cr25Ni20, 20Cr25Ni20, 06Cr19Ni10. Role reminder: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils.
Inside this GB/T 13296 series, compare GB/T 13296 16Cr23Ni13, GB/T 13296 06Cr25Ni20, GB/T 13296 20Cr25Ni20, GB/T 13296 06Cr19Ni10. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP309S.
On 06Cr23Ni13 packages that also list flats, open Stainless Steel Pipes and Tubes for pipes/tubes and Stainless Steel Sheets and Plates for sheets/plates, then use GB/T 4237 06Cr23Ni13 only when the flat form is required. Chinese plate series context: GB/T 4237. Confirm 06Cr23Ni13 OD × wall and plate thickness on separate drawings.
Chemical Composition of GB/T 13296 06Cr23Ni13
Cast analysis for GB/T 13296 06Cr23Ni13 follows Table 3. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 12.00–15.00, Cr 22.00–24.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 309S / UNS S30908; unified number S30908. Corrosion thread: higher Cr/Ni improve oxidation scaling resistance versus 18-8; aqueous chloride PREN is not the selling point.
Chemical limits for 06Cr23Ni13 under GB/T 13296-2023 appear in the table underneath. Source priority is the 2023 Table 3 extract (xtd). If your client specification cites a 2013 footnote, send it before the heat is melted. Duty thread: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr23Ni13 before the order is acknowledged. This paragraph is locked to 06Cr23Ni13 duty: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 06Cr23Ni13 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.015 | 12.00–15.00 | 22.00–24.00 |
UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 06Cr23Ni13 (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 309S / UNS S30908, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 06Cr23Ni13 against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 06Cr23Ni13 before the heat is booked.
Mechanical Properties of GB/T 13296 06Cr23Ni13
Ambient tensile floors for 06Cr23Ni13 come from GB/T 13296 Table 4: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: UNCERTAIN — provisional vs paid Table 3/4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy.
Hardness testing is by agreement for wall ≥1.7 mm; Table 5 bands differ for special marks such as 06Cr18Ni13Si4 and the high-Mo austenitics. Density reference for 06Cr23Ni13 is 7.98 kg/dm³. Hydrostatic proof uses P=2SR/D with R at 60% of Table 4 Rp0.2, capped at 20 MPa.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A min (%) |
|---|---|---|---|
| 06Cr23Ni13 | 520 | 205 | 35 |
Ambient values from GB/T 13296-2023 Table 4 for 06Cr23Ni13. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1030–1150 °C, rapid cool. UNCERTAIN — provisional vs paid Table 3/4. Density 7.98 kg/dm³. Delivery: solution annealed.
Seamless Tube Manufacture of GB/T 13296 06Cr23Ni13
For 06Cr23Ni13, the mill path is pierce / extrude / draw — never ERW or automatic-arc under GB/T 13296. Delivery is heat-treated and pickled unless overall ground/bored or protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO. Seamless W-C and W-H routes are the only valid order paths for 06Cr23Ni13 under GB/T 13296.
Steelmaking for 06Cr23Ni13 is electric-arc or converter with secondary refining, or electroslag remelting. Pickling follows heat treatment unless bright protective-atmosphere practice or overall machining allows omission. Size practice: W-H thicker walls for furnace-duty straight lengths. Pickling or bright-anneal decisions for 06Cr23Ni13 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Weld-shop note tied to 06Cr23Ni13: 309/309L-class fillers; watch sigma risk on long high-temperature exposure.
Eddy-current testing to GB/T 7735 E3H may replace hydrostatic proof when agreed; ultrasonic testing to GB/T 5777 U2 remains a standard acceptance path for 06Cr23Ni13. Role: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. Hydrostatic pressure or eddy-current class for 06Cr23Ni13 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Keep the 06Cr23Ni13 caution visible here: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy.
Dimensions and Tolerances for GB/T 13296 06Cr23Ni13
Dimensions and tolerances for 06Cr23Ni13 follow GB/T 13296 Table 1. Usual length is 2000–12000 mm. W-H OD tolerance is ±1.25%D for D≤140 mm and ±1%D above; W-C uses absolute OD bands from ±0.10 mm (D≤25) up through ±0.5%D for D>159 mm. Size hint: W-H thicker walls for furnace-duty straight lengths. Tolerance basis for 06Cr23Ni13 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for 06Cr23Ni13 remains W-H thicker walls for furnace-duty straight lengths.
Out-of-roundness and wall unevenness for 06Cr23Ni13 shall not exceed 80% of the OD and wall tolerances respectively. Full-length camber ≤0.15% of tube length. Duty: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. Fixed lengths and multiple cut lengths for 06Cr23Ni13 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 06Cr23Ni13 stays high-temperature air heaters, reformer transfer lines companion tubes, and oxidising flue-gas exchangers.
Equivalent Grades for GB/T 13296 06Cr23Ni13
Buyers searching under 309S / UNS S30908 still need the GB/T 13296 06Cr23Ni13 row locked on the acknowledgement. Inside austenitic practice the mechanical table and inspection clauses of GB/T 13296 control acceptance, not a brochure equivalent. Duty context: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils.
| System | Designation | Notes |
|---|---|---|
| GB/T 13296 | 06Cr23Ni13 | Governing tube grade for this page |
| Commercial / UNS (body only) | 309S / UNS S30908 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A213 / A269 related | related chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Inside this series compare GB/T 13296 16Cr23Ni13, GB/T 13296 06Cr25Ni20, GB/T 13296 20Cr25Ni20, GB/T 13296 06Cr19Ni10 before swapping marks for medium or temperature. Keep this caution visible for 06Cr23Ni13: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy. Hub: GB/T 13296. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (06Cr23Ni13).
Heat Treatment and Delivery Condition for GB/T 13296 06Cr23Ni13
Heat treatment for 06Cr23Ni13 follows Table 4: 1030–1150 °C, rapid cool. Delivery condition: solution annealed. SHH STEEL records furnace charts that support the temperature and cool method claimed on the certificate. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr23Ni13 unless the mark is on the exemption list.
Field heat treatment of 06Cr23Ni13 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr23Ni13 unless the mark is on the exemption list. Field heat treatment of 06Cr23Ni13 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 06Cr23Ni13: higher Cr/Ni improve oxidation scaling resistance versus 18-8; aqueous chloride PREN is not the selling point.
Corrosion Resistance of GB/T 13296 06Cr23Ni13
Corrosion behaviour of 06Cr23Ni13 in boiler/HX service: higher Cr/Ni improve oxidation scaling resistance versus 18-8; aqueous chloride PREN is not the selling point. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr23Ni13 unless the mark is on the exemption list. Medium risk note: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy.
If operating chlorides, temperature, or under-deposit geometry change after award, reopen the alloy choice for 06Cr23Ni13 rather than relying on wall thickness alone. Apps: high-temperature air heaters, reformer transfer lines companion tubes, and oxidising flue-gas exchangers. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr23Ni13 rather than relying on wall thickness alone. Keep the 06Cr23Ni13 caution visible here: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy.
Applications of GB/T 13296 06Cr23Ni13 Seamless Tube
Typical applications for GB/T 13296 06Cr23Ni13: high-temperature air heaters, reformer transfer lines companion tubes, and oxidising flue-gas exchangers. Duty summary: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. SHH STEEL can produce and supply the sizes and tests those packages need when the mill schedule allows. Spool fabricators should copy 06Cr23Ni13 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to 06Cr23Ni13 duty: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils.
Spool and bundle fabricators should copy 06Cr23Ni13 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Role: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. Commissioning teams benefit when the as-built dossier repeats 06Cr23Ni13 beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 06Cr23Ni13 remains W-H thicker walls for furnace-duty straight lengths.
Weldability of GB/T 13296 06Cr23Ni13
Weldability of 06Cr23Ni13: 309/309L-class fillers; watch sigma risk on long high-temperature exposure. Procedure qualification should use the same product form and wall class as production, including the seamless finish that will ship. Caution: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy. Procedure qualification for 06Cr23Ni13 should use the same product form and wall class as production, including the seamless finish that will ship. Corrosion framing beside 06Cr23Ni13: higher Cr/Ni improve oxidation scaling resistance versus 18-8; aqueous chloride PREN is not the selling point.
Shielding-gas and purge notes for 06Cr23Ni13 stay with the WPS package so site crews cannot improvise. Apps: high-temperature air heaters, reformer transfer lines companion tubes, and oxidising flue-gas exchangers. Consumable lot control and shielding-gas notes for 06Cr23Ni13 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 06Cr23Ni13: 309/309L-class fillers; watch sigma risk on long high-temperature exposure.
Surface Finishes for GB/T 13296 06Cr23Ni13
Finish options for 06Cr23Ni13 follow the ordered heat-treatment route under GB/T 13296. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: solution annealed. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 06Cr23Ni13.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Passivation restores the chromium-rich film after pickling or light fabrication on 06Cr23Ni13; it does not replace the heat treatment that sets mechanical properties under GB/T 13296. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.
Inspection and Testing for GB/T 13296 06Cr23Ni13
Inspection for 06Cr23Ni13 includes melt analysis, tensile tests, hydrostatic or eddy-current E3H, ultrasonic U2, and size/straightness checks. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr23Ni13 unless the mark is on the exemption list. Flattening applies for wall ≤10 mm; flaring for D≤150 mm and wall ≤10 mm.
Non-conforming 06Cr23Ni13 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Documents: GB/T 2102 / EN 10204 3.1 style as ordered. Non-conforming 06Cr23Ni13 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Application context for 06Cr23Ni13 stays high-temperature air heaters, reformer transfer lines companion tubes, and oxidising flue-gas exchangers.
Packaging and Shipping for GB/T 13296 06Cr23Ni13
Packaging for 06Cr23Ni13 uses capped ends, wrapped bundles or wooden crates, and waterproof protection matched to the voyage. Bundle tickets repeat grade, heat, size, and quantity. Size hint: W-H thicker walls for furnace-duty straight lengths. Bundle tickets for 06Cr23Ni13 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 06Cr23Ni13 caution visible here: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy.
Marking on 06Cr23Ni13 includes standard, grade, heat number, size, and manufacture symbol so site receiving can match crates to the packing list without opening every wrap. Desiccant and wrap choices for 06Cr23Ni13 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 06Cr23Ni13: higher Cr/Ni improve oxidation scaling resistance versus 18-8; aqueous chloride PREN is not the selling point.
SHH STEEL can adjust crate schedules for 06Cr23Ni13 when staggered retubing deliveries are on the project calendar. Weld-shop note: 309/309L-class fillers; watch sigma risk on long high-temperature exposure. Claims handling for 06Cr23Ni13 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 06Cr23Ni13: higher Cr/Ni improve oxidation scaling resistance versus 18-8; aqueous chloride PREN is not the selling point.
Why Choose SHH STEEL
SHH STEEL can produce and supply GB/T 13296 06Cr23Ni13 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Duty: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. SHH STEEL can produce and supply 06Cr23Ni13 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Keep the 06Cr23Ni13 caution visible here: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy.
SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr23Ni13 when the mill schedule allows. Sisters on the same hub: 16Cr23Ni13, 06Cr25Ni20, 20Cr25Ni20, 06Cr19Ni10. SHH STEEL can make 06Cr23Ni13 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Application context for 06Cr23Ni13 stays high-temperature air heaters, reformer transfer lines companion tubes, and oxidising flue-gas exchangers.
Supply Capability
SHH STEEL can produce and supply GB/T 13296 06Cr23Ni13 seamless tube to the enquiry size list with Table 3 chemistry, Table 4 heat treatment and tensile floors, and the NDT/hydro stack the datasheet names. Role: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr23Ni13 when the mill schedule allows. Size practice for 06Cr23Ni13 remains W-H thicker walls for furnace-duty straight lengths.
| Item | Capability |
|---|---|
| Standard | GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger |
| Grade | 06Cr23Ni13 (S30908) |
| Product form | Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm |
| Tests | Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9 |
Stock / Available sizes
Stock / Available sizes: SHH STEEL can supply 06Cr23Ni13 in common HX OD×min-wall bands and boiler straight lengths; non-stock walls and U-bend radii are rolled to order. Confirm W-C versus W-H before booking. Duty: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr23Ni13 once design pressure and corrosion allowance are clear. Keep the 06Cr23Ni13 caution visible here: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy.
SHH STEEL can produce trial bends and qualification lengths of 06Cr23Ni13 ahead of bulk release when the exchanger fabricator needs WPS coupons. Weld-shop: 309/309L-class fillers; watch sigma risk on long high-temperature exposure. SHH STEEL can produce trial lengths of 06Cr23Ni13 for procedure qualification before bulk release when the project calendar needs it. Size practice for 06Cr23Ni13 remains W-H thicker walls for furnace-duty straight lengths.
FAQ
-
What is GB/T 13296 06Cr23Ni13 seamless stainless steel tube used for?
- GB/T 13296 06Cr23Ni13 is seamless stainless tube for boilers and heat exchangers — high-temperature air heaters, reformer transfer lines companion tubes, and oxidising flue-gas exchangers. Role summary: 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. It is a Chinese product standard grade (S30908), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
-
Is GB/T 13296 06Cr23Ni13 seamless only, or does it cover welded tube?
- Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr23Ni13 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
-
What heat treatment applies to 06Cr23Ni13?
- 06Cr23Ni13 is delivered solution annealed under GB/T 13296. Table 4 reference: 1030–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr23Ni13 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr23Ni13 compare with sister grades 16Cr23Ni13, 06Cr25Ni20, 20Cr25Ni20?
- 06Cr23Ni13 is filed as austenitic. Typical sisters on the same RFQ are 16Cr23Ni13, 06Cr25Ni20, 20Cr25Ni20. Design caution: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr23Ni13?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 309S / UNS S30908 the same as ordering 06Cr23Ni13?
- No. 309S / UNS S30908 is a commercial / UNS cross-walk for body text (unified S30908). The purchase order should lock GB/T 13296 and 06Cr23Ni13 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 13296 06Cr23Ni13?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr23Ni13 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: W-H thicker walls for furnace-duty straight lengths. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
-
How should 06Cr23Ni13 be welded on site?
- Shop guidance: 309/309L-class fillers; watch sigma risk on long high-temperature exposure. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr23Ni13?
- Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN chem/mech vs paid Table 3/4; do not dual-cert as 16Cr23Ni13 without matching carbon strategy Sister pointers: 16Cr23Ni13, 06Cr25Ni20, 20Cr25Ni20. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 13296 06Cr23Ni13 with ASTM A213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr23Ni13 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for 06Cr23Ni13?
- Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr23Ni13 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 13296 06Cr23Ni13 is seamless stainless steel tube for boilers and heat exchangers — 22Cr–13Ni heat-resisting austenitic tube for oxidation-prone HX and furnace-adjacent coils. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 16Cr23Ni13, 06Cr25Ni20, 20Cr25Ni20. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.