GB/T 13296 022Cr21Ni25Mo7N Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 022Cr21Ni25Mo7N Seamless Stainless Steel Tube

GB/T 13296 022Cr21Ni25Mo7N seamless stainless steel tube (AL-6XN-class / UNS N08367-related, S38367), austenitic, Table 3 cast analysis, Rm min 690 MPa / Rp0.2 min 310 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
022Cr21Ni25Mo7N (S38367 / AL-6XN-class / UNS N08367-related — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 022Cr21Ni25Mo7N Seamless Stainless Steel Tube

When the approved vendor list and exchanger datasheet say GB/T 13296, the grade mark has to be the Chinese designation. 022Cr21Ni25Mo7N is the full product grade for this austenitic seamless tube. Table 4 sets a distinctly higher solution floor and tensile pair for this mark.

SHH STEEL can supply 022Cr21Ni25Mo7N seamless tube in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the exchanger: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 022Cr21Ni25Mo7N before production starts. This paragraph is locked to 022Cr21Ni25Mo7N duty: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series.

Equivalence talk to AL-6XN-class / UNS N08367-related belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 13296 022Cr21Ni25Mo7N, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking.

Related ASTM A213 tube pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 015Cr20Ni18Mo6CuN, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2. Use thread: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers.

Inside this GB/T 13296 series, compare GB/T 13296 015Cr20Ni18Mo6CuN, GB/T 13296 015Cr21Ni26Mo5Cu2, GB/T 13296 022Cr19Ni13Mo3, GB/T 13296 022Cr17Ni12Mo2. Hub: GB/T 13296.

When 022Cr21Ni25Mo7N pipe sits beside plate on the same BOM, Stainless Steel Pipes and Tubes covers the tubular parent, Stainless Steel Sheets and Plates covers flats, and GB/T 4237 022Cr21Ni25Mo7N is the live plate chemistry match — do not merge MTCs. Chinese plate series context: GB/T 4237. Quote 022Cr21Ni25Mo7N pipe and plate under separate line items.

Chemical Composition of GB/T 13296 022Cr21Ni25Mo7N

Chemistry control on 022Cr21Ni25Mo7N starts at the ladle. Expect C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 23.50–25.50, Cr 20.00–22.00, Mo 6.00–7.00 within Table 3, reported on the inspection document against the heat. Body alias AL-6XN-class / UNS N08367-related does not widen those windows. Every ladle analysis for 022Cr21Ni25Mo7N is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Application context for 022Cr21Ni25Mo7N stays severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers.

Read the table with the family in mind — austenitic — and with caution solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking. Numbers without the matching Table 4 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 022Cr21Ni25Mo7N before the order is acknowledged. Keep the 022Cr21Ni25Mo7N caution visible here: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking.

Grade C Si Mn P S Ni Cr Mo N
022Cr21Ni25Mo7N ≤0.030 ≤1.00 ≤2.00 ≤0.035 ≤0.015 23.50–25.50 20.00–22.00 6.00–7.00 0.18–0.25

Mechanical Properties of GB/T 13296 022Cr21Ni25Mo7N

Proof stress and tensile minima for 022Cr21Ni25Mo7N sit at Rm min 690 MPa, Rp0.2 min 310 MPa, elongation min 35%. Flattening and flaring back ductility when size allows. Watch-out: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking. Tensile sampling follows the batch rules for the ordered test unit of 022Cr21Ni25Mo7N, and retests follow GB/T 2102 when a result sits under the Table 4 floor. Application context for 022Cr21Ni25Mo7N stays severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers.

Batch size limits (D≤76 mm and S≤3 mm: ≤400 tubes; otherwise ≤200) keep sampling honest for 022Cr21Ni25Mo7N. Retests follow GB/T 2102. Density 8.06 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
022Cr21Ni25Mo7N 690 310 35

Ambient values from GB/T 13296-2023 Table 4 for 022Cr21Ni25Mo7N. Heat treatment (Table 4): ≥1110 °C, rapid cool. Density 8.06 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 022Cr21Ni25Mo7N

SHH STEEL can produce 022Cr21Ni25Mo7N as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 4 heat treatment and pickle (or bright anneal) as ordered. Plain ends are default; bevels by agreement when the tubesheet weld prep needs it. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

SHH STEEL schedules piercing, elongation, and finishing for 022Cr21Ni25Mo7N against the W-C or W-H symbol frozen on the acknowledgement. Ovality and wall eccentricity stay inside 80% of the respective OD and wall tolerances. Pickling or bright-anneal decisions for 022Cr21Ni25Mo7N stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Keep the 022Cr21Ni25Mo7N caution visible here: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking.

Cold-finish depth of longitudinal marks on 022Cr21Ni25Mo7N is limited to ≤4% of wall and ≤0.2 mm; hot-finish ≤5% and ≤0.4 mm. Apps: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers. Hydrostatic pressure or eddy-current class for 022Cr21Ni25Mo7N is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Application context for 022Cr21Ni25Mo7N stays severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers.

Dimensions and Tolerances for GB/T 13296 022Cr21Ni25Mo7N

When 022Cr21Ni25Mo7N ships as nominal wall, the note under Table 1 still applies different ± bands for hot and cold routes — do not mix W-C absolute OD tols with W-H percentage thinking. Practice: premium cold-finished HX OD with elevated solution practice. Tolerance basis for 022Cr21Ni25Mo7N follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 022Cr21Ni25Mo7N duty: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series.

Fixed lengths of 022Cr21Ni25Mo7N are end-protected so bevels and ID finish survive inland and ocean transit. Random lengths stay inside the usual 2000–12000 mm window unless agreed otherwise. Fixed lengths and multiple cut lengths for 022Cr21Ni25Mo7N are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside 022Cr21Ni25Mo7N: Mo 6–7% plus N for top PREN in this GB/T 13296 set.

Equivalent Grades for GB/T 13296 022Cr21Ni25Mo7N

Under GB/T 13296, 022Cr21Ni25Mo7N is the governing seamless stainless boiler / heat-exchanger tube designation on this page. Commercial shorthand such as AL-6XN-class / UNS N08367-related helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the GB/T 13296 022Cr21Ni25Mo7N line. ASTM A213 / A269 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.

System Designation Notes
GB/T 13296 022Cr21Ni25Mo7N Governing tube grade for this page
Commercial / UNS (body only) AL-6XN-class / UNS N08367-related (unified S38367) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

When the service outgrows 022Cr21Ni25Mo7N, move to a sister rather than stretching the alias: GB/T 13296 015Cr20Ni18Mo6CuN, GB/T 13296 015Cr21Ni26Mo5Cu2, GB/T 13296 022Cr19Ni13Mo3, GB/T 13296 022Cr17Ni12Mo2. Apps context: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers
– Caution locked in What-is / Corrosion / FAQ: solution temperature ≥1110 °C; Rm≥690 / Rp0. Full list under GB/T 13296.

Heat Treatment and Delivery Condition for GB/T 13296 022Cr21Ni25Mo7N

For 022Cr21Ni25Mo7N, solution or anneal practice is not a free mill choice — it is the Table 4 band tied to the grade. Delivery: solution annealed. Role: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series. Recorded furnace charts for 022Cr21Ni25Mo7N should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Size practice for 022Cr21Ni25Mo7N remains premium cold-finished HX OD with elevated solution practice.

When Annex A elevated Rp0.2 is invoked, the certificate for 022Cr21Ni25Mo7N should still show the Table 4 delivery treatment actually performed. Apps: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers. Field heat treatment of 022Cr21Ni25Mo7N after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 022Cr21Ni25Mo7N: matching high-Mo fillers; rigorous purge and heat-input control.

Corrosion Resistance of GB/T 13296 022Cr21Ni25Mo7N

Pitting, crevice, oxidation, or weld-decay limiters for 022Cr21Ni25Mo7N should be named in the datasheet rather than inferred from the AISI alias alone. Framing: Mo 6–7% plus N for top PREN in this GB/T 13296 set. Coupon orientation, weld condition, and surface finish for 022Cr21Ni25Mo7N belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Size practice for 022Cr21Ni25Mo7N remains premium cold-finished HX OD with elevated solution practice.

Pickling quality and free-iron cleanliness after fabrication affect startup corrosion of 022Cr21Ni25Mo7N as much as cast chemistry. Role: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 022Cr21Ni25Mo7N rather than relying on wall thickness alone. Application context for 022Cr21Ni25Mo7N stays severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers.

Applications of GB/T 13296 022Cr21Ni25Mo7N Seamless Tube

Use 022Cr21Ni25Mo7N on packages that match severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers. Nearby sisters 015Cr20Ni18Mo6CuN, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2 cover adjacent media or temperature steps. Weld-shop note: matching high-Mo fillers; rigorous purge and heat-input control. Spool fabricators should copy 022Cr21Ni25Mo7N onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Weld-shop note tied to 022Cr21Ni25Mo7N: matching high-Mo fillers; rigorous purge and heat-input control.

When the process medium changes mid-project, revisit whether 022Cr21Ni25Mo7N still fits before releasing more heats. Sisters: 015Cr20Ni18Mo6CuN, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2. Commissioning teams benefit when the as-built dossier repeats 022Cr21Ni25Mo7N beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to 022Cr21Ni25Mo7N: matching high-Mo fillers; rigorous purge and heat-input control.

Weldability of GB/T 13296 022Cr21Ni25Mo7N

Consumable selection for 022Cr21Ni25Mo7N follows matching high-Mo fillers; rigorous purge and heat-input control. Do not improvise under-alloyed fillers on Mo or Cu grades. Role: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series. Procedure qualification for 022Cr21Ni25Mo7N should use the same product form and wall class as production, including the seamless finish that will ship. Weld-shop note tied to 022Cr21Ni25Mo7N: matching high-Mo fillers; rigorous purge and heat-input control.

Ferrite control and hot-cracking risk for 022Cr21Ni25Mo7N depend on the family chemistry; qualify on production wall, not only on plate coupons. Weld shop: matching high-Mo fillers; rigorous purge and heat-input control. Consumable lot control and shielding-gas notes for 022Cr21Ni25Mo7N stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 022Cr21Ni25Mo7N remains premium cold-finished HX OD with elevated solution practice.

Surface Finishes for GB/T 13296 022Cr21Ni25Mo7N

Iron-free handling after pickle matters for 022Cr21Ni25Mo7N — carbon-steel strapping stains show up later as rust blooms on finished tube. Standard route is solution annealed and pickled when HT is specified; polish scope must name the surface. Apps: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers
– Caution locked in What-is / Corrosion / FAQ: solution temperature ≥1110 °C; Rm≥690 / Rp0.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Do not polish over unresolved defects on 022Cr21Ni25Mo7N; inspection comes before cosmetics. Passivation after pickle or shop welding is good practice in chloride-lean service, but GB/T 13296 acceptance still rests on correct heat treatment. Pack away from carbon-steel contact. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 022Cr21Ni25Mo7N.

Inspection and Testing for GB/T 13296 022Cr21Ni25Mo7N

SHH STEEL keeps heat identity for 022Cr21Ni25Mo7N unbroken from melt through bundle tags, including third-party hold points written into the PO. Caution: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking. Sampling plans for 022Cr21Ni25Mo7N keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Size practice for 022Cr21Ni25Mo7N remains premium cold-finished HX OD with elevated solution practice.

Certificate lines for 022Cr21Ni25Mo7N must repeat the Chinese grade, unified number, manufacture symbol, and heat treatment actually performed. Caution: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking. Non-conforming 022Cr21Ni25Mo7N lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. This paragraph is locked to 022Cr21Ni25Mo7N duty: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series.

Packaging and Shipping for GB/T 13296 022Cr21Ni25Mo7N

Desiccant and wrap choices for 022Cr21Ni25Mo7N follow voyage length and storage climate on the shipping order, not a one-size export habit. Apps: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers. Bundle tickets for 022Cr21Ni25Mo7N repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 022Cr21Ni25Mo7N duty: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series.

Inland trucking of 022Cr21Ni25Mo7N still needs end protection — most ID dents happen between the port and the exchanger shop. Apps: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers. Desiccant and wrap choices for 022Cr21Ni25Mo7N follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 022Cr21Ni25Mo7N remains premium cold-finished HX OD with elevated solution practice.

Barcode or stencil extras for 022Cr21Ni25Mo7N are available when the owner’s material system needs them. Apps: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers. Claims handling for 022Cr21Ni25Mo7N starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 022Cr21Ni25Mo7N: matching high-Mo fillers; rigorous purge and heat-input control.

Why Choose SHH STEEL

SHH STEEL can make 022Cr21Ni25Mo7N to a boiler/HX test stack — hydro or E3H, UT U2, flattening/flaring, IGC when required — instead of a generic stainless tube habit. Apps: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers. SHH STEEL can produce and supply 022Cr21Ni25Mo7N against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Weld-shop note tied to 022Cr21Ni25Mo7N: matching high-Mo fillers; rigorous purge and heat-input control.

SHH STEEL can supply 022Cr21Ni25Mo7N with third-party inspection hold points written into the itinerary. Weld-shop note: matching high-Mo fillers; rigorous purge and heat-input control. SHH STEEL can make 022Cr21Ni25Mo7N to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. This paragraph is locked to 022Cr21Ni25Mo7N duty: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series.

Supply Capability

SHH STEEL can supply 022Cr21Ni25Mo7N with EN 10204 3.1 style documents, IGC when required, and hardness by agreement. Caution: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 022Cr21Ni25Mo7N when the mill schedule allows. Corrosion framing beside 022Cr21Ni25Mo7N: Mo 6–7% plus N for top PREN in this GB/T 13296 set.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 022Cr21Ni25Mo7N (S38367)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes: rolling cycles for 022Cr21Ni25Mo7N cover usual 2000–12000 mm lengths; cut-to-length and multiple lengths ship once tests clear. Caution: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking. SHH STEEL can supply alternate walls and W-C/W-H classes for 022Cr21Ni25Mo7N once design pressure and corrosion allowance are clear. This paragraph is locked to 022Cr21Ni25Mo7N duty: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series.

SHH STEEL can supply replacement retubing heats of 022Cr21Ni25Mo7N matched to prior certificates when the plant provides heat history. Apps: severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers. SHH STEEL can produce trial lengths of 022Cr21Ni25Mo7N for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside 022Cr21Ni25Mo7N: Mo 6–7% plus N for top PREN in this GB/T 13296 set.

FAQ

What is GB/T 13296 022Cr21Ni25Mo7N seamless stainless steel tube used for?
GB/T 13296 022Cr21Ni25Mo7N is seamless stainless tube for boilers and heat exchangers — severe seawater exchangers, bleach coolers, and high-PREN scrubber condensers. Role summary: high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series. It is a Chinese product standard grade (S38367), not an automatic ASTM A213 certificate.
Is GB/T 13296 022Cr21Ni25Mo7N seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 022Cr21Ni25Mo7N when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 022Cr21Ni25Mo7N?
022Cr21Ni25Mo7N is delivered solution annealed under GB/T 13296. Table 4 reference: ≥1110 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 022Cr21Ni25Mo7N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 022Cr21Ni25Mo7N compare with sister grades 015Cr20Ni18Mo6CuN, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3?
022Cr21Ni25Mo7N is filed as austenitic. Typical sisters on the same RFQ are 015Cr20Ni18Mo6CuN, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3. Design caution: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 022Cr21Ni25Mo7N?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is AL-6XN-class / UNS N08367-related the same as ordering 022Cr21Ni25Mo7N?
No. AL-6XN-class / UNS N08367-related is a commercial / UNS cross-walk for body text (unified S38367). The purchase order should lock GB/T 13296 and 022Cr21Ni25Mo7N so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 022Cr21Ni25Mo7N?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 022Cr21Ni25Mo7N within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: premium cold-finished HX OD with elevated solution practice. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 022Cr21Ni25Mo7N be welded on site?
Shop guidance: matching high-Mo fillers; rigorous purge and heat-input control. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking
When should I choose a higher-Mo or superaustenitic grade instead of 022Cr21Ni25Mo7N?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: solution temperature ≥1110 °C; Rm≥690 / Rp0.2≥310 — do not mix with 6% Mo neighbour without checking Sister pointers: 015Cr20Ni18Mo6CuN, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 022Cr21Ni25Mo7N with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 022Cr21Ni25Mo7N does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 022Cr21Ni25Mo7N?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 022Cr21Ni25Mo7N when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 022Cr21Ni25Mo7N is seamless stainless steel tube for boilers and heat exchangers — high-Mo nitrogen super-austenitic tube for the most aggressive chloride HX duties in this series. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 015Cr20Ni18Mo6CuN, 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X