GB/T 13296 06Cr25Ni20 Seamless Stainless Steel Tube | GB/T 13296 Stainless Steel Tube - SHH STEEL

GB/T 13296 06Cr25Ni20 Seamless Stainless Steel Tube

GB/T 13296 06Cr25Ni20 seamless stainless steel tube (310S / UNS S31008, S31008), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr25Ni20 (S31008 / 310S / UNS S31008 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 06Cr25Ni20 Seamless Stainless Steel Tube

GB/T 13296 covers seamless stainless tube for boiler and HX service — cold-drawn or hot-finished — with hydrostatic proof, ultrasonic U2, flattening and flaring where size allows. Inside that standard, 06Cr25Ni20 is filed as austenitic. It is the 310S-class workhorse for Chinese boiler/HX oxidation duty.

From pierce/extrude/draw through marking and crate protection, SHH STEEL can produce GB/T 13296 06Cr25Ni20 for the sizes and tests on your RFQ. Application sketch: high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr25Ni20 before production starts. Weld-shop note tied to 06Cr25Ni20: 310/310S fillers; control heat input against hot cracking.

On the floor people shorten marks; in QA they must not. 06Cr25Ni20 under GB/T 13296 carries specific Table 3 windows and Table 4 floors that a loose “310S” note will not enforce. Caution: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO.

Annex A elevated Rp0.2 and Annex B rupture data apply only to named H marks; still match the alloy to the medium. For 06Cr25Ni20, that means: 25Cr–20Ni heat-resisting austenitic tube for severe oxidation and carburising HX environments. Nearby marks: 20Cr25Ni20, 06Cr23Ni13, 16Cr23Ni13, 06Cr19Ni10.

Inside this GB/T 13296 series, compare GB/T 13296 20Cr25Ni20, GB/T 13296 06Cr23Ni13, GB/T 13296 16Cr23Ni13, GB/T 13296 06Cr19Ni10. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP310S.

Buyers comparing 06Cr25Ni20 tubulars with sheet/plate can the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 3280 06Cr25Ni20. See also the GB/T 4237 hub for related plate designations. Do not stretch a 06Cr25Ni20 pipe certificate onto plate.

Chemical Composition of GB/T 13296 06Cr25Ni20

For 06Cr25Ni20, the melt ticket has to show Table 3 compliance — C ≤0.08, Si ≤1.50, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 19.00–22.00, Cr 24.00–26.00. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: excellent oxidation resistance; aqueous pitting still needs Mo or super-austenitic thinking.

Where Mo, Cu, Ti, Nb or N appear, they are intentional levers for 06Cr25Ni20, not optional marketing. Confirm them on the MTC line-by-line. Role: 25Cr–20Ni heat-resisting austenitic tube for severe oxidation and carburising HX environments. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 06Cr25Ni20 before the order is acknowledged. Size practice for 06Cr25Ni20 remains hot-finished boiler OD bands with oxidation allowance discussed separately from corrosion allowance.

Grade C Si Mn P S Ni Cr
06Cr25Ni20 ≤0.08 ≤1.50 ≤2.00 ≤0.035 ≤0.015 19.00–22.00 24.00–26.00

UNCERTAIN: Public xtd Table 3 extract omits a numbered row for 06Cr25Ni20 (series numbering gaps). Provisional melt windows above follow GB/T 20878 / sibling GB practice for 310S / UNS S31008, with sulphur tightened toward the boiler-tube austenitic pattern where that pattern applies. SHH STEEL will not melt 06Cr25Ni20 against these provisional digits once a purchaser supplies paid Table 3 text that differs — confirm the paid GB/T 13296-2023 Table 3 line for 06Cr25Ni20 before the heat is booked.

Mechanical Properties of GB/T 13296 06Cr25Ni20

Do not confuse Table 4 tube tensile floors with pipe or plate standards that share the 310S / UNS S31008 alias. For 06Cr25Ni20 under 13296 expect Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%, verified per heat/lot rules. Note: UNCERTAIN — provisional vs paid Table 3/4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting.

When wall class changes the ordered tensile specimen orientation, keep the acknowledgement aligned for 06Cr25Ni20. Reference density 7.98 kg/dm³; delivery solution annealed.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
06Cr25Ni20 520 205 35

Ambient values from GB/T 13296-2023 Table 4 for 06Cr25Ni20. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1030–1180 °C, rapid cool. UNCERTAIN — provisional vs paid Table 3/4. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 06Cr25Ni20

SHH STEEL can produce 06Cr25Ni20 as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 4 heat treatment and pickle (or bright anneal) as ordered. Plain ends are default; bevels by agreement when the tubesheet weld prep needs it. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

U-bend and cut-to-length options for 06Cr25Ni20 are available by agreement after the straight-tube tests clear. Surface quality rejects cracks, folds, laps, laminations and scabs on ID and OD. Pickling or bright-anneal decisions for 06Cr25Ni20 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Application context for 06Cr25Ni20 stays high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers.

Manufacture records for 06Cr25Ni20 keep heat identity unbroken from melt through final NDT so the MTC can cite one cast for the whole bundle. Hydrostatic pressure or eddy-current class for 06Cr25Ni20 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. This paragraph is locked to 06Cr25Ni20 duty: 25Cr–20Ni heat-resisting austenitic tube for severe oxidation and carburising HX environments.

Dimensions and Tolerances for GB/T 13296 06Cr25Ni20

Cut lengths, multiple lengths, and U-bend developed lengths for 06Cr25Ni20 need explicit acknowledgement so finishing and crate length match the tubesheet drawing. Caution: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO. Tolerance basis for 06Cr25Ni20 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 06Cr25Ni20 duty: 25Cr–20Ni heat-resisting austenitic tube for severe oxidation and carburising HX environments.

Tolerance class follows the manufacture route ordered for 06Cr25Ni20; swapping W-C for W-H after acknowledgement without a dimensional review is how fit-up fails at the exchanger shop. Fixed lengths and multiple cut lengths for 06Cr25Ni20 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 06Cr25Ni20: 310/310S fillers; control heat input against hot cracking.

Equivalent Grades for GB/T 13296 06Cr25Ni20

Equivalence language around 06Cr25Ni20 is often looser than a tube purchase order can afford. GB/T 13296 06Cr25Ni20 governs this article; 310S / UNS S31008 is body-only framing for catalogues and dual-cert talk, not a substitute mark on the MTC. Keep the GB/T 13296 symbol unless a written dual-cert plan lists both standards with separate test scopes.

System Designation Notes
GB/T 13296 06Cr25Ni20 Governing tube grade for this page
Commercial / UNS (body only) 310S / UNS S31008 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related related chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Order discipline for 06Cr25Ni20 still points at GB/T 13296, not the brochure alias. Neighbours GB/T 13296 20Cr25Ni20, GB/T 13296 06Cr23Ni13, GB/T 13296 16Cr23Ni13, GB/T 13296 06Cr19Ni10 each carry their own mechanical table. Category hub: GB/T 13296. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (06Cr25Ni20).

Heat Treatment and Delivery Condition for GB/T 13296 06Cr25Ni20

Stabilisation after solution anneal is available by agreement for Ti/Nb marks; confirm whether 06Cr25Ni20 needs that second hold before acknowledging. HT reference: 1030–1180 °C, rapid cool. Recorded furnace charts for 06Cr25Ni20 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for 06Cr25Ni20 stays high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers.

Mixed bundles of different heat-treatment furnace lots of 06Cr25Ni20 stay segregated so sampling remains traceable to one Table 4 run. Field heat treatment of 06Cr25Ni20 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 06Cr25Ni20: excellent oxidation resistance; aqueous pitting still needs Mo or super-austenitic thinking.

Corrosion Resistance of GB/T 13296 06Cr25Ni20

Coupon orientation, weld condition, and surface finish for 06Cr25Ni20 belong in the corrosion test order so method E or other coupons compare honestly to the installed tube. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr25Ni20 unless the mark is on the exemption list. Coupon orientation, weld condition, and surface finish for 06Cr25Ni20 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Corrosion framing beside 06Cr25Ni20: excellent oxidation resistance; aqueous pitting still needs Mo or super-austenitic thinking.

For 06Cr25Ni20, specify whether IGC, hardness, or special corrosion coupons are extras beyond the clause 9 default before the heat is melted. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr25Ni20 rather than relying on wall thickness alone. Weld-shop note tied to 06Cr25Ni20: 310/310S fillers; control heat input against hot cracking.

Applications of GB/T 13296 06Cr25Ni20 Seamless Tube

Commissioning dossiers should repeat 06Cr25Ni20 beside heat numbers so as-built isometrics stay tied to the same mill certificates. Application thread: high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers. Spool fabricators should copy 06Cr25Ni20 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 06Cr25Ni20 remains hot-finished boiler OD bands with oxidation allowance discussed separately from corrosion allowance.

Spare-tube stocks of 06Cr25Ni20 should keep heat identity so later retubing matches the original corrosion and strength file. Apps: high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers. Commissioning teams benefit when the as-built dossier repeats 06Cr25Ni20 beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside 06Cr25Ni20: excellent oxidation resistance; aqueous pitting still needs Mo or super-austenitic thinking.

Weldability of GB/T 13296 06Cr25Ni20

Repair welding of 06Cr25Ni20 must preserve grade identity — a 308 deposit on a 6% Mo tube is a corrosion failure waiting to happen. Note: 310/310S fillers; control heat input against hot cracking. Procedure qualification for 06Cr25Ni20 should use the same product form and wall class as production, including the seamless finish that will ship. This paragraph is locked to 06Cr25Ni20 duty: 25Cr–20Ni heat-resisting austenitic tube for severe oxidation and carburising HX environments.

Tubesheet joint design for 06Cr25Ni20 should state strength weld versus seal weld and any expansion sequence before production welding starts. Consumable lot control and shielding-gas notes for 06Cr25Ni20 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 06Cr25Ni20: 310/310S fillers; control heat input against hot cracking.

Surface Finishes for GB/T 13296 06Cr25Ni20

Pickled mill finish covers most RFQs for 06Cr25Ni20. Bright anneal, grind, or polish only when the enquiry writes a measurable target and names OD, ID, or both. Pack caution carried into finish control: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 06Cr25Ni20.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

For 06Cr25Ni20, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this tube. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (06Cr25Ni20).

Inspection and Testing for GB/T 13296 06Cr25Ni20

Hardness by agreement for wall ≥1.7 mm on 06Cr25Ni20; grain-size evidence when the mark requires levels 4–7. Apps: high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers. Sampling plans for 06Cr25Ni20 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside 06Cr25Ni20: excellent oxidation resistance; aqueous pitting still needs Mo or super-austenitic thinking.

Dimensional reports for 06Cr25Ni20 cite Table 1 tolerance basis (W-C vs W-H, min wall vs nominal wall) so receiving inspectors know which band applies. Non-conforming 06Cr25Ni20 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Keep the 06Cr25Ni20 caution visible here: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO.

Packaging and Shipping for GB/T 13296 06Cr25Ni20

U-bend crates for 06Cr25Ni20 need radius supports so cold-worked bends do not spring or scar in transit. Caution: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO. Bundle tickets for 06Cr25Ni20 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 06Cr25Ni20 duty: 25Cr–20Ni heat-resisting austenitic tube for severe oxidation and carburising HX environments.

Long-term storage of 06Cr25Ni20 should keep bundles dry and off bare soil to protect the pickled surface before installation. Caution: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO. Desiccant and wrap choices for 06Cr25Ni20 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for 06Cr25Ni20 stays high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers.

Packing lists for 06Cr25Ni20 cite net/gross weight and crate count so logistics and QA share one document set. Caution: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO. Claims handling for 06Cr25Ni20 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 06Cr25Ni20 remains hot-finished boiler OD bands with oxidation allowance discussed separately from corrosion allowance.

Why Choose SHH STEEL

Traceability, pickle quality, and size discipline on 06Cr25Ni20 are part of the supply promise, not brochure extras. Role: 25Cr–20Ni heat-resisting austenitic tube for severe oxidation and carburising HX environments. SHH STEEL can produce and supply 06Cr25Ni20 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Corrosion framing beside 06Cr25Ni20: excellent oxidation resistance; aqueous pitting still needs Mo or super-austenitic thinking.

For 06Cr25Ni20, SHH STEEL can produce trial lengths for procedure qualification before bulk release when the project calendar needs it. Apps: high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers. SHH STEEL can make 06Cr25Ni20 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Application context for 06Cr25Ni20 stays high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers.

Supply Capability

From RFQ to crate, SHH STEEL can produce 06Cr25Ni20 as a boiler/HX product — not a repurposed fluid-pipe heat. Size hint: hot-finished boiler OD bands with oxidation allowance discussed separately from corrosion allowance. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr25Ni20 when the mill schedule allows. Size practice for 06Cr25Ni20 remains hot-finished boiler OD bands with oxidation allowance discussed separately from corrosion allowance.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 06Cr25Ni20 (S31008)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes — SHH STEEL can supply alternate walls for 06Cr25Ni20 once design pressure, corrosion allowance, and min-wall rules are clear. Size hint: hot-finished boiler OD bands with oxidation allowance discussed separately from corrosion allowance. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr25Ni20 once design pressure and corrosion allowance are clear. Size practice for 06Cr25Ni20 remains hot-finished boiler OD bands with oxidation allowance discussed separately from corrosion allowance.

Export packing and document sets for 06Cr25Ni20 are confirmed on the acknowledgement so customs and site QA see the same grade string. Caution: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO. SHH STEEL can produce trial lengths of 06Cr25Ni20 for procedure qualification before bulk release when the project calendar needs it. Application context for 06Cr25Ni20 stays high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers.

FAQ

What is GB/T 13296 06Cr25Ni20 seamless stainless steel tube used for?
GB/T 13296 06Cr25Ni20 is seamless stainless tube for boilers and heat exchangers — high-temperature process gas coolers, radiant-section companion tubes, and oxidising waste-heat exchangers. Role summary: 25Cr–20Ni heat-resisting austenitic tube for severe oxidation and carburising HX environments. It is a Chinese product standard grade (S31008), not an automatic ASTM A213 certificate. Chem/mech for this mark is flagged UNCERTAIN versus paid Table 3/4 — confirm before melt.
Is GB/T 13296 06Cr25Ni20 seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr25Ni20 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 06Cr25Ni20?
06Cr25Ni20 is delivered solution annealed under GB/T 13296. Table 4 reference: 1030–1180 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr25Ni20 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr25Ni20 compare with sister grades 20Cr25Ni20, 06Cr23Ni13, 16Cr23Ni13?
06Cr25Ni20 is filed as austenitic. Typical sisters on the same RFQ are 20Cr25Ni20, 06Cr23Ni13, 16Cr23Ni13. Design caution: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr25Ni20?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 310S / UNS S31008 the same as ordering 06Cr25Ni20?
No. 310S / UNS S31008 is a commercial / UNS cross-walk for body text (unified S31008). The purchase order should lock GB/T 13296 and 06Cr25Ni20 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 06Cr25Ni20?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr25Ni20 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: hot-finished boiler OD bands with oxidation allowance discussed separately from corrosion allowance. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 06Cr25Ni20 be welded on site?
Shop guidance: 310/310S fillers; control heat input against hot cracking. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr25Ni20?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: UNCERTAIN vs paid Table 3/4; distinguish clearly from higher-carbon 20Cr25Ni20 on the PO Sister pointers: 20Cr25Ni20, 06Cr23Ni13, 16Cr23Ni13. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 06Cr25Ni20 with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr25Ni20 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 06Cr25Ni20?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr25Ni20 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 06Cr25Ni20 is seamless stainless steel tube for boilers and heat exchangers — 25Cr–20Ni heat-resisting austenitic tube for severe oxidation and carburising HX environments. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 20Cr25Ni20, 06Cr23Ni13, 16Cr23Ni13. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X