GB/T 13296 07Cr19Ni10 Seamless Stainless Steel Tube

GB/T 13296 07Cr19Ni10 seamless stainless steel tube (304H / UNS S30409, S30409), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
07Cr19Ni10 (S30409 / 304H / UNS S30409 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 07Cr19Ni10 Seamless Stainless Steel Tube

Boiler and heat-exchanger packages written to Chinese product standards look to GB/T 13296-2023 rather than inventing a mill grade from AISI shorthand alone. 07Cr19Ni10 is the Table 3/4 Chinese grade name for this austenitic chemistry (S30409). Annex A elevated Rp0.2 and Annex B 100000 h rupture tables name this mark explicitly.

Mill path for 07Cr19Ni10: manufacture symbol W-C/W-H, Table 4 heat treatment, Table 3 cast chemistry, Table 4 tensile floors, hydrostatic or eddy-current E3H, ultrasonic U2. SHH STEEL can make and supply the grade to that stack. Typical use: superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter.

Body text may mention 304H / UNS S30409 (unified S30409) for cross-reference, but the H1 and order line stay on 07Cr19Ni10. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived.

Order the standard the drawing and regulatory file actually require. Inside this 13296 series, compare 06Cr19Ni10, 07Cr19Ni11Ti, 07Cr18Ni11Nb, 07Cr17Ni12Mo2 before stretching surface finish or wall alone. Duty thread: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data.

Inside this GB/T 13296 series, compare GB/T 13296 06Cr19Ni10, GB/T 13296 07Cr19Ni11Ti, GB/T 13296 07Cr18Ni11Nb, GB/T 13296 07Cr17Ni12Mo2. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP304H.

Chemical Composition of GB/T 13296 07Cr19Ni10

Table 3 sets the melt limits for 07Cr19Ni10. Highlight band: C 0.04–0.10, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 8.00–11.00, Cr 18.00–20.00. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 3. Alias note: 304H / UNS S30409. Every ladle analysis for 07Cr19Ni10 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Keep the 07Cr19Ni10 caution visible here: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived.

The composition table below is the cast window SHH STEEL quotes against for 07Cr19Ni10. Edition framing is GB/T 13296-2023. Use thread: superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for 07Cr19Ni10 before the order is acknowledged. This paragraph is locked to 07Cr19Ni10 duty: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data.

Grade C Si Mn P S Ni Cr
07Cr19Ni10 0.04–0.10 ≤1.00 ≤2.00 ≤0.035 ≤0.015 8.00–11.00 18.00–20.00

Mechanical Properties of GB/T 13296 07Cr19Ni10

Table 4 mechanical acceptance for 07Cr19Ni10: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: Annex A elevated Rp0.2 and Annex B 100000 h rupture data apply to this mark. Delivery framing: solution annealed. Sampling follows the batch rules for 07Cr19Ni10. Tensile sampling follows the batch rules for the ordered test unit of 07Cr19Ni10, and retests follow GB/T 2102 when a result sits under the Table 4 floor. This paragraph is locked to 07Cr19Ni10 duty: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data.

Elevated-temperature Annex A Rp0.2 and Annex B 100000 h rupture tables name only selected H marks — check whether 07Cr19Ni10 appears before citing those numbers in a design note. Density 7.9 kg/dm³.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
07Cr19Ni10 520 205 35

Ambient values from GB/T 13296-2023 Table 4 for 07Cr19Ni10. Heat treatment (Table 4): 1010–1150 °C, rapid cool. Annex A elevated Rp0.2 and Annex B 100000 h rupture data apply to this mark. Density 7.9 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 07Cr19Ni10

SHH STEEL can produce 07Cr19Ni10 as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 4 heat treatment and pickle (or bright anneal) as ordered. Plain ends are default; bevels by agreement when the tubesheet weld prep needs it. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

After hot or cold working, 07Cr19Ni10 is heat-treated per Table 4 and finished to the ordered surface. Straightness limits differ for W-H (≤2.0 mm/m) and W-C (≤1.5 mm/m); full-length bow ≤0.15% of length. Pickling or bright-anneal decisions for 07Cr19Ni10 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Size practice for 07Cr19Ni10 remains straight boiler lengths and thicker W-H walls where hot finish is economical.

Straightness, end finish, and marking for 07Cr19Ni10 are checked before bundling so tubesheet fit-up crews receive usable lengths. Caution: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived. Hydrostatic pressure or eddy-current class for 07Cr19Ni10 is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Weld-shop note tied to 07Cr19Ni10: 308H-class thinking; match carbon strategy and grain control to the H product.

Dimensions and Tolerances for GB/T 13296 07Cr19Ni10

Minimum-wall ordering is common for HX duty on 07Cr19Ni10: W-C min-wall tolerance is +20%S/0 for D≤38 mm and +22%S/0 above; W-H min-wall is +0.90/0 mm for S≤4.0 mm and +25%S/0 above. Confirm nominal-wall versus min-wall language on the PO. Tolerance basis for 07Cr19Ni10 follows the W-C or W-H route ordered, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside 07Cr19Ni10: oxidation and creep framing dominate over aqueous pitting upgrades; chloride HX media may still need Mo.

Bevel geometry, land, and ID cleanliness notes for 07Cr19Ni10 belong on the acknowledgement when automatic welding to the tubesheet is planned. Apps: superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter. Fixed lengths and multiple cut lengths for 07Cr19Ni10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 07Cr19Ni10 duty: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data.

Equivalent Grades for GB/T 13296 07Cr19Ni10

Identity first: GB/T 13296 07Cr19Ni10 is the HX/boiler tube grade for this page. 304H / UNS S30409 helps buyers who think in AISI/UNS labels. Role: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. Foreign product standards remain separate documents.

System Designation Notes
GB/T 13296 07Cr19Ni10 Governing tube grade for this page
Commercial / UNS (body only) 304H / UNS S30409 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

We deliberately avoid inventing a false one-to-one for every foreign system on 07Cr19Ni10. Use GB/T 13296 06Cr19Ni10, GB/T 13296 07Cr19Ni11Ti, GB/T 13296 07Cr18Ni11Nb, GB/T 13296 07Cr17Ni12Mo2 for in-series alternatives, and keep GB/T 13296 as the category landing page. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (07Cr19Ni10).

For 07Cr19Ni10, vertical navigation stays form-specific — tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is GB/T 4237 07Cr19Ni10. See also the GB/T 4237 hub for related plate designations. Confirm 07Cr19Ni10 OD × wall and plate thickness on separate drawings.

Heat Treatment and Delivery Condition for GB/T 13296 07Cr19Ni10

Table 4 schedules 07Cr19Ni10 at 1010–1150 °C, rapid cool. Protective-atmosphere bright anneal may omit pickle when agreed. Grain-size extras: per family practice. Caution: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived. Recorded furnace charts for 07Cr19Ni10 should support the Table 4 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 07Cr19Ni10 caution visible here: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived.

Recorded cool method for 07Cr19Ni10 matters as much as peak temperature — rapid cool versus air/slow cool is a family identity issue. Density 7.9 kg/dm³. Field heat treatment of 07Cr19Ni10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 07Cr19Ni10: 308H-class thinking; match carbon strategy and grain control to the H product.

Corrosion Resistance of GB/T 13296 07Cr19Ni10

Select 07Cr19Ni10 when the process side matches this framing: oxidation and creep framing dominate over aqueous pitting upgrades; chloride HX media may still need Mo. Sister upgrades on the same hub include 06Cr19Ni10, 07Cr19Ni11Ti, 07Cr18Ni11Nb, 07Cr17Ni12Mo2. Role: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. Coupon orientation, weld condition, and surface finish for 07Cr19Ni10 belong in the corrosion test order so clause 9 results can be compared to the installed tube honestly. Size practice for 07Cr19Ni10 remains straight boiler lengths and thicker W-H walls where hot finish is economical.

Oxidation-first marks and PREN-first marks in this series are not interchangeable — 07Cr19Ni10 sits on the oxidation and creep framing dominate over aqueous pitting upgrades; chloride HX media may still need Mo side of that split. Caution: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived.

Applications of GB/T 13296 07Cr19Ni10 Seamless Tube

Exchanger and boiler designers reach for 07Cr19Ni10 when: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. Common sketch: superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter. Caution on the datasheet: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived.

U-bend radius, heat treatment after bending, and tubesheet weld details for 07Cr19Ni10 belong in the fabrication specification, not only in the mill PO. Caution: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived. Commissioning teams benefit when the as-built dossier repeats 07Cr19Ni10 beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 07Cr19Ni10 remains straight boiler lengths and thicker W-H walls where hot finish is economical.

Weldability of GB/T 13296 07Cr19Ni10

Shop guidance for 07Cr19Ni10: 308H-class thinking; match carbon strategy and grain control to the H product. Autogenous orbital welds to tubesheets need clean ID and controlled heat input. Family: austenitic. Procedure qualification for 07Cr19Ni10 should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 07Cr19Ni10 remains straight boiler lengths and thicker W-H walls where hot finish is economical.

Post-weld heat treatment of 07Cr19Ni10 is uncommon for austenitics but may be specified for stabilised marks or ferritic toughness — write it explicitly. Caution: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived. Consumable lot control and shielding-gas notes for 07Cr19Ni10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Application context for 07Cr19Ni10 stays superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter.

Surface Finishes for GB/T 13296 07Cr19Ni10

Surface supply for 07Cr19Ni10 should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless tube, so finish is part of performance, not only appearance. Application framing: superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter. Ambiguous “bright tube” language is clarified before finishing slots are booked.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

When 07Cr19Ni10 ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for solution anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Apps reminder: superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter.

Inspection and Testing for GB/T 13296 07Cr19Ni10

Batch rules for 07Cr19Ni10: same grade, heat, size, and heat-treatment lot. Sampling counts follow OD/wall thresholds in the standard. Role: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. Sampling plans for 07Cr19Ni10 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 07Cr19Ni10 caution visible here: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived.

Witness points for 07Cr19Ni10 (hydro, UT, IGC) should be booked before the tubes leave the finishing bay. Duty: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. Non-conforming 07Cr19Ni10 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 07Cr19Ni10: 308H-class thinking; match carbon strategy and grain control to the H product.

Packaging and Shipping for GB/T 13296 07Cr19Ni10

Export crates for 07Cr19Ni10 protect thin-wall HX stock against handling dents that would fail UT or tubesheet fit-up. Role: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. Bundle tickets for 07Cr19Ni10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 07Cr19Ni10 caution visible here: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived.

Claims handling for 07Cr19Ni10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Duty: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. Desiccant and wrap choices for 07Cr19Ni10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 07Cr19Ni10 caution visible here: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived.

Loose tubes of 07Cr19Ni10 are avoided; strapped bundles keep heat lots together for MTC matching. Role: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. Claims handling for 07Cr19Ni10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to 07Cr19Ni10 duty: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data.

Why Choose SHH STEEL

SHH STEEL can produce and supply GB/T 13296 07Cr19Ni10. Why buyers stay with SHH STEEL for 07Cr19Ni10: written acknowledgements that name W-C/W-H and Table 4 heat treatment before melt, plus MTCs that repeat the Chinese grade. Caution: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived.

Engineering support for 07Cr19Ni10 includes clarifying min-wall versus nominal-wall language and Annex A/B applicability before the heat is melted. Caution: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived. SHH STEEL can make 07Cr19Ni10 to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. Corrosion framing beside 07Cr19Ni10: oxidation and creep framing dominate over aqueous pitting upgrades; chloride HX media may still need Mo.

Supply Capability

Supply capability for 07Cr19Ni10: W-C and W-H seamless routes, pickled or bright, plain or bevelled ends, random or fixed lengths. SHH STEEL can make the grade when melt and finishing slots align. Apps: superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 07Cr19Ni10 when the mill schedule allows. Corrosion framing beside 07Cr19Ni10: oxidation and creep framing dominate over aqueous pitting upgrades; chloride HX media may still need Mo.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 07Cr19Ni10 (S30409)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes for 07Cr19Ni10 centre on cold-finished mid-OD HX tubes and selected hot-finished boiler walls; ask for the current matrix against your datasheet. Apps: superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter. SHH STEEL can supply alternate walls and W-C/W-H classes for 07Cr19Ni10 once design pressure and corrosion allowance are clear. Size practice for 07Cr19Ni10 remains straight boiler lengths and thicker W-H walls where hot finish is economical.

Lead time for 07Cr19Ni10 tracks melt booking, finishing, and any third-party holds — send the full test matrix with the RFQ. Role: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. SHH STEEL can produce trial lengths of 07Cr19Ni10 for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside 07Cr19Ni10: oxidation and creep framing dominate over aqueous pitting upgrades; chloride HX media may still need Mo.

FAQ

What is GB/T 13296 07Cr19Ni10 seamless stainless steel tube used for?
GB/T 13296 07Cr19Ni10 is seamless stainless tube for boilers and heat exchangers — superheater/reheater companion tubes, high-temperature steam coils, and HX bundles where creep rupture notes matter. Role summary: carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. It is a Chinese product standard grade (S30409), not an automatic ASTM A213 certificate.
Is GB/T 13296 07Cr19Ni10 seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 07Cr19Ni10 when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 07Cr19Ni10?
07Cr19Ni10 is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 07Cr19Ni10 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 07Cr19Ni10 compare with sister grades 06Cr19Ni10, 07Cr19Ni11Ti, 07Cr18Ni11Nb?
07Cr19Ni10 is filed as austenitic. Typical sisters on the same RFQ are 06Cr19Ni10, 07Cr19Ni11Ti, 07Cr18Ni11Nb. Design caution: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 07Cr19Ni10?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 304H / UNS S30409 the same as ordering 07Cr19Ni10?
No. 304H / UNS S30409 is a commercial / UNS cross-walk for body text (unified S30409). The purchase order should lock GB/T 13296 and 07Cr19Ni10 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 07Cr19Ni10?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 07Cr19Ni10 within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: straight boiler lengths and thicker W-H walls where hot finish is economical. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 07Cr19Ni10 be welded on site?
Shop guidance: 308H-class thinking; match carbon strategy and grain control to the H product. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived
When should I choose a higher-Mo or superaustenitic grade instead of 07Cr19Ni10?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: IGC is exempt for this mark under clause 9, but grain-size 4–7 still applies — do not skip grain control because IGC is waived Sister pointers: 06Cr19Ni10, 07Cr19Ni11Ti, 07Cr18Ni11Nb. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 07Cr19Ni10 with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 07Cr19Ni10 does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 07Cr19Ni10?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 07Cr19Ni10 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 07Cr19Ni10 is seamless stainless steel tube for boilers and heat exchangers — carbon-floor 18-8 austenitic tube aimed at elevated-temperature boiler/HX duty with Annex A/B reference data. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr19Ni10, 07Cr19Ni11Ti, 07Cr18Ni11Nb. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X