GB/T 13296 06Cr19Ni10N Seamless Stainless Steel Tube

GB/T 13296 06Cr19Ni10N seamless stainless steel tube (304N / UNS S30458, S30458), austenitic, Table 3 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr19Ni10N (S30458 / 304N / UNS S30458 — body alias)
Standard
GB/T 13296-2023
Product form
Seamless stainless steel tube (W-C / W-H), delivery solution annealed
Size
OD × wall per Table 1; usual length 2000–12000 mm; min-wall or nominal-wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 13296 06Cr19Ni10N Seamless Stainless Steel Tube

GB/T 13296-2023 is the Chinese national standard for seamless stainless steel tubes for boilers and heat exchangers — replacing the 2013 edition. Grade 06Cr19Ni10N (unified number S30458) sits in the austenitic set. Nitrogen is the intentional lever that separates this mark from ordinary 06Cr19Ni10.

SHH STEEL can produce and supply GB/T 13296 06Cr19Ni10N as seamless W-C or W-H tube across the enquiry OD×wall band, heat-treated per Table 4, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades.

Shop language may still say “304N tube,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 13296 and 06Cr19Ni10N so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute.

Scope discipline: 06Cr19Ni10N is seamless boiler/HX tube under GB/T 13296, not fluid-transport pipe under GB/T 14976 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N, 022Cr19Ni10. Role reminder: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades.

Inside this GB/T 13296 series, compare GB/T 13296 06Cr19Ni10, GB/T 13296 022Cr19Ni10N, GB/T 13296 06Cr17Ni12Mo2N, GB/T 13296 022Cr19Ni10. Hub: GB/T 13296. ASTM/ASME related boiler/HX tube pages (not interchangeable by default): ASTM A213 TP304.

For 06Cr19Ni10N, vertical navigation stays form-specific — open Stainless Steel Pipes and Tubes for pipes/tubes and Stainless Steel Sheets and Plates for sheets/plates, then use GB/T 4237 06Cr19Ni10N only when the flat form is required. Chinese plate series context: GB/T 4237. Quote 06Cr19Ni10N pipe and plate under separate line items.

Chemical Composition of GB/T 13296 06Cr19Ni10N

Cast analysis for GB/T 13296 06Cr19Ni10N follows Table 3. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.015, Ni 8.00–11.00, Cr 18.00–20.00, N 0.10–0.16. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 304N / UNS S30458; unified number S30458. Corrosion thread: corrosion stays in the Mo-free 18-8 family; N helps strength more than PREN.

Chemical limits for 06Cr19Ni10N under GB/T 13296-2023 appear in the table underneath. Source priority is the 2023 Table 3 extract (xtd). If your client specification cites a 2013 footnote, send it before the heat is melted. Duty thread: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades.

Grade C Si Mn P S Ni Cr N
06Cr19Ni10N ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.015 8.00–11.00 18.00–20.00 0.10–0.16

Mechanical Properties of GB/T 13296 06Cr19Ni10N

Ambient tensile floors for 06Cr19Ni10N come from GB/T 13296 Table 4: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation min 35%. Note: Rm/Rp floors for N-grade not separately printed in xtd Table 4 excerpt for seq 5 — ambient row follows neighbouring 06Cr19Ni10 extract; confirm paid Table 4. UNCERTAIN versus the paid GB/T 13296-2023 Table 3/4 text — the figures below are provisional from the xtd excerpt merge and sibling GB windows; confirm before melting. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute.

Hardness testing is by agreement for wall ≥1.7 mm; Table 5 bands differ for special marks such as 06Cr18Ni13Si4 and the high-Mo austenitics. Density reference for 06Cr19Ni10N is 7.93 kg/dm³. Hydrostatic proof uses P=2SR/D with R at 60% of Table 4 Rp0.2, capped at 20 MPa.

Grade Rm min (MPa) Rp0.2 min (MPa) A min (%)
06Cr19Ni10N 520 205 35

Ambient values from GB/T 13296-2023 Table 4 for 06Cr19Ni10N. UNCERTAIN tensile/HT versus paid Table 4 where flagged — confirm before design lock. Heat treatment (Table 4): 1010–1150 °C, rapid cool. Rm/Rp floors for N-grade not separately printed in xtd Table 4 excerpt for seq 5 — ambient row follows neighbouring 06Cr19Ni10 extract; confirm paid Table 4. Density 7.93 kg/dm³. Delivery: solution annealed.

Seamless Tube Manufacture of GB/T 13296 06Cr19Ni10N

GB/T 13296 manufactures 06Cr19Ni10N as seamless tube only — cold-drawn or cold-rolled (symbol W-C) or hot-rolled / extruded (symbol W-H). SHH STEEL confirms the manufacture symbol on the acknowledgement before piercing or drawing starts; welded tube is outside this standard. Austenitic heats take solution annealing with rapid cool per Table 4; route-specific minima (for example W-H versus W-C on some Ti/Nb H marks) must match the manufacture symbol on the PO.

Steelmaking for 06Cr19Ni10N is electric-arc or converter with secondary refining, or electroslag remelting. Pickling follows heat treatment unless bright protective-atmosphere practice or overall machining allows omission. Size practice: mid OD W-C where tensile floors drive wall selection. Pickling or bright-anneal decisions for 06Cr19Ni10N stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive HX duties. Application context for 06Cr19Ni10N stays higher-pressure HX shellside tubes, steam coils needing a strength bump, and weight-sensitive bundles.

Eddy-current testing to GB/T 7735 E3H may replace hydrostatic proof when agreed; ultrasonic testing to GB/T 5777 U2 remains a standard acceptance path for 06Cr19Ni10N. Role: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. Hydrostatic pressure or eddy-current class for 06Cr19Ni10N is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Corrosion framing beside 06Cr19Ni10N: corrosion stays in the Mo-free 18-8 family; N helps strength more than PREN.

Dimensions and Tolerances for GB/T 13296 06Cr19Ni10N

Dimensions and tolerances for 06Cr19Ni10N follow GB/T 13296 Table 1. Usual length is 2000–12000 mm. W-H OD tolerance is ±1.25%D for D≤140 mm and ±1%D above; W-C uses absolute OD bands from ±0.10 mm (D≤25) up through ±0.5%D for D>159 mm. Size hint: mid OD W-C where tensile floors drive wall selection.

Out-of-roundness and wall unevenness for 06Cr19Ni10N shall not exceed 80% of the OD and wall tolerances respectively. Full-length camber ≤0.15% of tube length. Duty: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. Fixed lengths and multiple cut lengths for 06Cr19Ni10N are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 06Cr19Ni10N: 308/308L with N-aware procedures; avoid under-matched soft fillers on strength-critical joints.

Equivalent Grades for GB/T 13296 06Cr19Ni10N

GB/T 13296 does not make 304N / UNS S30458 a drop-in certificate for 06Cr19Ni10N. Use the commercial name in dual-cert talk, then verify every Table limit that matters for this tube. Sisters in the series are comparison pages, not interchangeable stock codes. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (06Cr19Ni10N).

System Designation Notes
GB/T 13296 06Cr19Ni10N Governing tube grade for this page
Commercial / UNS (body only) 304N / UNS S30458 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A269 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Inside this series compare GB/T 13296 06Cr19Ni10, GB/T 13296 022Cr19Ni10N, GB/T 13296 06Cr17Ni12Mo2N, GB/T 13296 022Cr19Ni10 before swapping marks for medium or temperature. Confirm chemistry windows on the 06Cr19Ni10N MTC before dual-cert claims. Hub: GB/T 13296. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (06Cr19Ni10N).

Heat Treatment and Delivery Condition for GB/T 13296 06Cr19Ni10N

Heat treatment for 06Cr19Ni10N follows Table 4: 1010–1150 °C, rapid cool. Delivery condition: solution annealed. SHH STEEL records furnace charts that support the temperature and cool method claimed on the certificate. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr19Ni10N unless the mark is on the exemption list.

Field heat treatment of 06Cr19Ni10N after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr19Ni10N unless the mark is on the exemption list. Field heat treatment of 06Cr19Ni10N after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 06Cr19Ni10N caution visible here: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute.

Corrosion Resistance of GB/T 13296 06Cr19Ni10N

Corrosion behaviour of 06Cr19Ni10N in boiler/HX service: corrosion stays in the Mo-free 18-8 family; N helps strength more than PREN. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr19Ni10N unless the mark is on the exemption list. Medium risk note: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute.

If operating chlorides, temperature, or under-deposit geometry change after award, reopen the alloy choice for 06Cr19Ni10N rather than relying on wall thickness alone. Apps: higher-pressure HX shellside tubes, steam coils needing a strength bump, and weight-sensitive bundles. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr19Ni10N rather than relying on wall thickness alone. Weld-shop note tied to 06Cr19Ni10N: 308/308L with N-aware procedures; avoid under-matched soft fillers on strength-critical joints.

Applications of GB/T 13296 06Cr19Ni10N Seamless Tube

Typical applications for GB/T 13296 06Cr19Ni10N: higher-pressure HX shellside tubes, steam coils needing a strength bump, and weight-sensitive bundles. Duty summary: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. SHH STEEL can produce and supply the sizes and tests those packages need when the mill schedule allows.

Spool and bundle fabricators should copy 06Cr19Ni10N onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Role: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. Commissioning teams benefit when the as-built dossier repeats 06Cr19Ni10N beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 06Cr19Ni10N stays higher-pressure HX shellside tubes, steam coils needing a strength bump, and weight-sensitive bundles.

Weldability of GB/T 13296 06Cr19Ni10N

Weldability of 06Cr19Ni10N: 308/308L with N-aware procedures; avoid under-matched soft fillers on strength-critical joints. Procedure qualification should use the same product form and wall class as production, including the seamless finish that will ship. Caution: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute. Procedure qualification for 06Cr19Ni10N should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 06Cr19Ni10N caution visible here: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute.

Shielding-gas and purge notes for 06Cr19Ni10N stay with the WPS package so site crews cannot improvise. Apps: higher-pressure HX shellside tubes, steam coils needing a strength bump, and weight-sensitive bundles. Consumable lot control and shielding-gas notes for 06Cr19Ni10N stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 06Cr19Ni10N: corrosion stays in the Mo-free 18-8 family; N helps strength more than PREN.

Surface Finishes for GB/T 13296 06Cr19Ni10N

06Cr19Ni10N under GB/T 13296 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (06Cr19Ni10N).

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Reject grinding burns, embedded free iron, and unrepaired undercut on 06Cr19Ni10N before bundles close. Passivation analogues (A967-style) are optional extras — the governing step remains correct heat treatment under GB/T 13296 for this austenitic mark. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (06Cr19Ni10N).

Inspection and Testing for GB/T 13296 06Cr19Ni10N

Inspection for 06Cr19Ni10N includes melt analysis, tensile tests, hydrostatic or eddy-current E3H, ultrasonic U2, and size/straightness checks. Clause 9 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr19Ni10N unless the mark is on the exemption list. Flattening applies for wall ≤10 mm; flaring for D≤150 mm and wall ≤10 mm.

Non-conforming 06Cr19Ni10N lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Documents: GB/T 2102 / EN 10204 3.1 style as ordered. Non-conforming 06Cr19Ni10N lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 06Cr19Ni10N: 308/308L with N-aware procedures; avoid under-matched soft fillers on strength-critical joints.

Packaging and Shipping for GB/T 13296 06Cr19Ni10N

Packaging for 06Cr19Ni10N uses capped ends, wrapped bundles or wooden crates, and waterproof protection matched to the voyage. Bundle tickets repeat grade, heat, size, and quantity. Size hint: mid OD W-C where tensile floors drive wall selection. Bundle tickets for 06Cr19Ni10N repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for 06Cr19Ni10N remains mid OD W-C where tensile floors drive wall selection.

Marking on 06Cr19Ni10N includes standard, grade, heat number, size, and manufacture symbol so site receiving can match crates to the packing list without opening every wrap. Desiccant and wrap choices for 06Cr19Ni10N follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 06Cr19Ni10N caution visible here: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute.

SHH STEEL can adjust crate schedules for 06Cr19Ni10N when staggered retubing deliveries are on the project calendar. Weld-shop note: 308/308L with N-aware procedures; avoid under-matched soft fillers on strength-critical joints. Claims handling for 06Cr19Ni10N starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 06Cr19Ni10N remains mid OD W-C where tensile floors drive wall selection.

Why Choose SHH STEEL

SHH STEEL can produce and supply GB/T 13296 06Cr19Ni10N against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. Duty: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. SHH STEEL can produce and supply 06Cr19Ni10N against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade. This paragraph is locked to 06Cr19Ni10N duty: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades.

SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr19Ni10N when the mill schedule allows. Sisters on the same hub: 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N, 022Cr19Ni10. SHH STEEL can make 06Cr19Ni10N to a written acknowledgement that names W-C/W-H and Table 4 heat treatment before melt. This paragraph is locked to 06Cr19Ni10N duty: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades.

Supply Capability

SHH STEEL can produce and supply GB/T 13296 06Cr19Ni10N seamless tube to the enquiry size list with Table 3 chemistry, Table 4 heat treatment and tensile floors, and the NDT/hydro stack the datasheet names. Role: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. SHH STEEL can produce and supply cut lengths, U-bends, and ordered annex tests for 06Cr19Ni10N when the mill schedule allows. This paragraph is locked to 06Cr19Ni10N duty: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades.

Item Capability
Standard GB/T 13296-2023 seamless stainless steel tubes for boiler and heat exchanger
Grade 06Cr19Ni10N (S30458)
Product form Seamless tube only — cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × min wall (or nominal wall) per Table 1; usual length 2000–12000 mm
Tests Hydrostatic (or ET E3H), UT U2, flattening/flaring when size allows, IGC per clause 9

Stock / Available sizes

Stock / Available sizes: SHH STEEL can supply 06Cr19Ni10N in common HX OD×min-wall bands and boiler straight lengths; non-stock walls and U-bend radii are rolled to order. Confirm W-C versus W-H before booking. Duty: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. SHH STEEL can supply alternate walls and W-C/W-H classes for 06Cr19Ni10N once design pressure and corrosion allowance are clear. Weld-shop note tied to 06Cr19Ni10N: 308/308L with N-aware procedures; avoid under-matched soft fillers on strength-critical joints.

SHH STEEL can produce trial bends and qualification lengths of 06Cr19Ni10N ahead of bulk release when the exchanger fabricator needs WPS coupons. Weld-shop: 308/308L with N-aware procedures; avoid under-matched soft fillers on strength-critical joints. SHH STEEL can produce trial lengths of 06Cr19Ni10N for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside 06Cr19Ni10N: corrosion stays in the Mo-free 18-8 family; N helps strength more than PREN.

FAQ

What is GB/T 13296 06Cr19Ni10N seamless stainless steel tube used for?
GB/T 13296 06Cr19Ni10N is seamless stainless tube for boilers and heat exchangers — higher-pressure HX shellside tubes, steam coils needing a strength bump, and weight-sensitive bundles. Role summary: nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. It is a Chinese product standard grade (S30458), not an automatic ASTM A213 certificate.
Is GB/T 13296 06Cr19Ni10N seamless only, or does it cover welded tube?
Seamless only. Manufacture is limited to cold-drawn/rolled (W-C) or hot-rolled/extruded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr19Ni10N when the mill can meet the ordered size and tests. Welded tube belongs under other standards, not 13296.
What heat treatment applies to 06Cr19Ni10N?
06Cr19Ni10N is delivered solution annealed under GB/T 13296. Table 4 reference: 1010–1150 °C, rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Grain-size or IGC extras follow clause 9 for this mark. Keep the purchase order locked to GB/T 13296 and 06Cr19Ni10N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr19Ni10N compare with sister grades 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N?
06Cr19Ni10N is filed as austenitic. Typical sisters on the same RFQ are 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N. Design caution: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute Pick the sister when the medium or temperature outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr19Ni10N?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic test (or replacing ET E3H), ultrasonic U2, appearance, flattening/flaring when size allows, and every IGC or hardness test actually performed. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 304N / UNS S30458 the same as ordering 06Cr19Ni10N?
No. 304N / UNS S30458 is a commercial / UNS cross-walk for body text (unified S30458). The purchase order should lock GB/T 13296 and 06Cr19Ni10N so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 13296 06Cr19Ni10N?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr19Ni10N within Table 1 practice, with min-wall or nominal-wall options by agreement. Size context: mid OD W-C where tensile floors drive wall selection. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Usual length 2000–12000 mm.
How should 06Cr19Ni10N be welded on site?
Shop guidance: 308/308L with N-aware procedures; avoid under-matched soft fillers on strength-critical joints. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr19Ni10N?
Move when chloride pitting, crevice attack, reducing-acid risk, or oxidation life exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: N band 0.10–0.16 is mandatory identity — a plain 06Cr19Ni10 heat is not a quiet substitute Sister pointers: 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 13296 06Cr19Ni10N with ASTM A213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 13296 06Cr19Ni10N does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for 06Cr19Ni10N?
Pickled after heat treatment is the usual boiler/HX supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr19Ni10N when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 13296 06Cr19Ni10N is seamless stainless steel tube for boilers and heat exchangers — nitrogen-strengthened 18-8 austenitic tube when higher proof stress is wanted without jumping to Mo grades. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N. Related ASTM A213 pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X