EN 10296-2 1.4003 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4003 Welded Stainless Steel Tube

EN 10296-2 1.4003 / X2CrNi12 welded stainless general-purpose tube (3Cr12 / 1.4003 utility ferritic), ferritic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 280 MPa, Rm min 450 MPa, A long. min 20%, delivery +A. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4003 / X2CrNi12 (3Cr12 / 1.4003 utility ferritic — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +A as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4003 Welded Stainless Steel Tube

EN 10296-2:2005 (BS EN 10296-2:2005) is the European product standard for welded circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10217-7, and not for seamless general-purpose tube under EN 10297-2. Steel number 1.4003 is listed as X2CrNi12 in the ferritic corrosion-resisting set. When a drawing still says “3Cr12 welded tube” without a European product standard, EN 10296-2 1.4003 is the general-purpose welded designation that carries the Ni-bearing 12%Cr analysis into the MTC. Filler/shop note for 1.4003: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming.

SHH STEEL can make and supply EN 10296-2 1.4003 / X2CrNi12 as welded general-purpose tube across commodity structural and light mechanical OD×wall on W1A/W2A-class descaled routes (ferritic symbols exclude W0/W1/W2), annealed or solution annealed as the grade tables and order require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Filler/shop note for 1.4003: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming.

On the shop floor people still say “3Cr12 / 1.4003 utility ferritic tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4003, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: Ni-bearing 12%Cr weldable ferritic welded tube for structural and utility mechanical duty where nickel cost of 18-8 is not justified. Typical duties include bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”. Design caution: not a chloride-service austenitic substitute — pitting and HAZ toughness stay limited versus 18-8; keep wall and forming within ferritic practice, and remember W0/W1/W2 symbols are not for ferritic grades Filler/shop note for 1.4003: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming.

Do not treat an EN 10296-2 1.4003 MTC as automatic clearance for pressure equipment — EN 10217-7 is the welded pressure home. Likewise, seamless pressure tube lives under EN 10216-5 and seamless general-purpose under EN 10297-2. Match the product standard to the duty before dual-marking talk begins. Use thread: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”.

Inside this welded general-purpose series, compare EN 10296-2 1.4512, EN 10296-2 1.4016, EN 10296-2 1.4509. Hub: EN 10296-2.

Chemical Composition of EN 10296-2 1.4003

Buying 3Cr12 / 1.4003 utility ferritic-family welded tube without locking 1.4003 invites silent chemistry drift. Under EN 10296-2 the cast must satisfy X2CrNi12; highlight elements for this grade include C ≤0.030, Cr 10.5–12.5, Ni 0.30–1.00, N ≤0.030, Si ≤1.00, S ≤0.015. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Duty thread: Ni-bearing 12%Cr weldable ferritic welded tube for structural and utility mechanical duty where nickel cost of 18-8 is not justified.

Use the cast table for 1.4003 as the contractual chemistry window for welded general-purpose duty — role reminder: Ni-bearing 12%Cr weldable ferritic welded tube for structural and utility mechanical duty where nickel cost of 18-8 is not justified. Do not substitute a sister analysis from 1.4512, 1.4016, 1.4509 without rewriting the steel number on the order. Primary application sketch: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”.

Steel C Si Mn P S Cr Ni N
1.4003 / X2CrNi12 ≤0.030 ≤1.00 ≤1.50 ≤0.040 ≤0.015 10.5–12.5 0.30–1.00 ≤0.030

Mechanical Properties of EN 10296-2 1.4003

Table mechanical floors for 1.4003 / X2CrNi12 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 280 MPa, Rp1.0 min 290 MPa, Rm min 450 MPa, longitudinal elongation min 20%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Caution thread: not a chloride-service austenitic substitute — pitting and HAZ toughness stay limited versus 18-8; keep wall and forming within ferritic practice, and remember W0/W1/W2 symbols are not for ferritic grades.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+A 280 290 450 min 20 18 No

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4003 / X2CrNi12. Guideline solution/anneal band (Annex B): 700–750 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4003

Ferritic welded 1.4003 (X2CrNi12) is produced from strip or plate, longitudinally welded, then delivered +AR or +A per 7.2.2. Grain-growth control during anneal matters for toughness and forming when +A is ordered. Annex A process-route symbols for ferritic 1.4003 exclude W0, W1 and W2. Typical ordered routes are W1A/W2A-class heat-treated descaled finishes, WCA/WCR cold-worked recrystallised welds, and WG/WP when ground or polished roughness is written into the purchase order (bead-worked appends “b”). Weld thread: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming.

Ferritic 1.4003 under EN 10296-2 may be delivered as-welded (+AR) or annealed (+A) at the manufacturer’s discretion unless the order locks +A. Annex B annealing guidance sits near 700–750 °C with water, air or gas cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Forming and expansion trials should respect ferritic elongation floors rather than austenitic shop habits. Caution thread: not a chloride-service austenitic substitute — pitting and HAZ toughness stay limited versus 18-8; keep wall and forming within ferritic practice, and remember W0/W1/W2 symbols are not for ferritic grades.

When dual documentation against EN 10217-7 is requested for the same 1.4003 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Use thread: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”.

Dimensions and Tolerances for EN 10296-2 1.4003

Order EN 10296-2 1.4003 by outside diameter D and wall thickness T for steel name X2CrNi12. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Commodity structural and light mechanical od×wall on w1a/w2a-class descaled routes (ferritic symbols exclude w0/w1/w2). Weld thread: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming.

Length supply for 1.4003 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Duty thread: Ni-bearing 12%Cr weldable ferritic welded tube for structural and utility mechanical duty where nickel cost of 18-8 is not justified.

Equivalent Grades for EN 10296-2 1.4003

Do not treat ASTM welded or seamless pages as drop-in equals for EN 10296-2 1.4003 / X2CrNi12. Wall bases, mechanical tables, and optional tests differ. Body alias 3Cr12 / 1.4003 utility ferritic is fine in BOM notes; H1 and order line stay on the steel number. Compare 1.4512, 1.4016, 1.4509 when the medium outgrows this analysis. Size context for 1.4003: commodity structural and light mechanical OD×wall on W1A/W2A-class descaled routes (ferritic symbols exclude W0/W1/W2).

Heat Treatment and Delivery Condition for EN 10296-2 1.4003

Ferritic 1.4003 under EN 10296-2 may be delivered as-welded (+AR) or annealed (+A) at the manufacturer’s discretion unless the order locks +A. Annex B annealing guidance sits near 700–750 °C with water, air or gas cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Delivery framing on the certificate for 1.4003 should match the ordered +AR/+A/+AT symbol — alias 3Cr12 / 1.4003 utility ferritic alone is not enough. Corrosion thread: chromium passive film for dry and mildly wet atmospheres; nickel addition aids weldability versus plain 12%Cr but does not create Mo-class chloride resistance.

Hot-working temperature bands in Annex B for X2CrNi12 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Weld thread: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming.

Corrosion Resistance of EN 10296-2 1.4003

For 1.4003 / X2CrNi12, read corrosion through the ferritic corrosion-resisting lens rather than a generic “stainless” slogan. Plain-language summary: chromium passive film for dry and mildly wet atmospheres; nickel addition aids weldability versus plain 12%Cr but does not create Mo-class chloride resistance. IGC Options follow EN ISO 3651-2 where the tables say Yes — and still do not replace medium-specific design. Caution: not a chloride-service austenitic substitute — pitting and HAZ toughness stay limited versus 18-8; keep wall and forming within ferritic practice, and remember W0/W1/W2 symbols are not for ferritic grades Primary application sketch: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”.

SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4003. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Corrosion thread: chromium passive film for dry and mildly wet atmospheres; nickel addition aids weldability versus plain 12%Cr but does not create Mo-class chloride resistance.

Applications of EN 10296-2 1.4003 Tube

Typical field use for 3Cr12 / 1.4003 utility ferritic-named welded tube under steel number 1.4003: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”. Keep pressure seamless talk on EN 10216-5 pages when that standard is the regulatory home. Primary application sketch: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”.

Skip 1.4003 when the specification locks a different family — for example forcing ferritic 1.4003 into severe chloride process duty, or forcing a heat-resisting number into aqueous chloride service. Sister conversation inside EN 10296-2: 1.4512, 1.4016, 1.4509. Size context for 1.4003: commodity structural and light mechanical OD×wall on W1A/W2A-class descaled routes (ferritic symbols exclude W0/W1/W2).

Weldability of EN 10296-2 1.4003

Even though 1.4003 is already a welded tube product, site joints still need a WPS matched to X2CrNi12. Filler and heat-input guidance: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming. Alias on the shop traveler may say 3Cr12 / 1.4003 utility ferritic; the WPS should cite the steel number. Primary application sketch: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”.

Filler selection should match or over-alloy the base X2CrNi12 chemistry as the WPS demands. Heat input, interpass temperature, and shielding practice follow the family — austenitic, ferritic, duplex, or heat-resisting — not a single shop habit. Corrosion thread: chromium passive film for dry and mildly wet atmospheres; nickel addition aids weldability versus plain 12%Cr but does not create Mo-class chloride resistance.

Surface Finishes for EN 10296-2 1.4003

Interior Ra limits, electropolish, or special protection for X2CrNi12 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4003 when the mill can measure and report the finish. Duty thread: Ni-bearing 12%Cr weldable ferritic welded tube for structural and utility mechanical duty where nickel cost of 18-8 is not justified.

For 1.4003, export and coastal routes need extra wrap discipline on W*R/WCR/WG/WP finishes. Size context: commodity structural and light mechanical OD×wall on W1A/W2A-class descaled routes (ferritic symbols exclude W0/W1/W2). SHH STEEL confirms sleeve, paper, or plastic protection against the ordered Annex A symbol before dispatch.

Inspection and Testing for EN 10296-2 1.4003

Specific inspection applies to EN 10296-2 1.4003 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Weld thread: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming.

Inspection intensity on 1.4003 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: Ni-bearing 12%Cr weldable ferritic welded tube for structural and utility mechanical duty where nickel cost of 18-8 is not justified. Filler/shop note for 1.4003: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming.

Packaging and Shipping for EN 10296-2 1.4003

SHH STEEL ships EN 10296-2 1.4003 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled W1A/W2A engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Caution thread: not a chloride-service austenitic substitute — pitting and HAZ toughness stay limited versus 18-8; keep wall and forming within ferritic practice, and remember W0/W1/W2 symbols are not for ferritic grades.

When cut lengths and special ends are part of the 1.4003 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Size context for 1.4003: commodity structural and light mechanical OD×wall on W1A/W2A-class descaled routes (ferritic symbols exclude W0/W1/W2).

Export packing lists for 1.4003 / X2CrNi12 cross-reference heat numbers to bundle IDs so the EN 10204 3.1 document matches without opening every crate. SHH STEEL aligns packaging with the order text before dispatch and can photograph bundle marks on request for project files that still say 3Cr12 / 1.4003 utility ferritic in the email subject. Use thread: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10296-2 1.4003 as welded general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “3Cr12 / 1.4003 utility ferritic tube” label on whatever is in the rack. We keep pressure talk honest: when PED welded pressure acceptance is required, we point you to EN 10217-7 for the same chemistry family where it exists. Use thread: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”.

Why this mill page exists: honest EN 10296-2 1.4003 welded supply with Annex A and delivery-condition clarity — not a generic 3Cr12 / 1.4003 utility ferritic rack pull. Sisters on the same RFQ conversation: 1.4512, 1.4016, 1.4509. Use thread: bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”.

Supply Capability

SHH STEEL can produce and supply EN 10296-2 1.4003 welded stainless steel tube against the edition, delivery condition, Annex A symbol, and Options named on your enquiry. The capability table and Stock / Available sizes enquiry map below frame a first-pass size list for X2CrNi12 — role: Ni-bearing 12%Cr weldable ferritic welded tube for structural and utility mechanical duty where nickel cost of 18-8 is not justified. Family filing for 1.4003 is ferritic corrosion-resisting.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4003 / X2CrNi12
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +A
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

For X2CrNi12, tell us which Annex A symbol and whether +AT (or +A/+AR) is locked before we hold strip. Caution that shapes size choice: not a chloride-service austenitic substitute — pitting and HAZ toughness stay limited versus 18-8; keep wall and forming within ferritic practice, and remember W0/W1/W2 symbols are not for ferritic grades Filler/shop note for 1.4003: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming.

Trial lengths of 1.4003 / X2CrNi12 help fabricators prove forming and weld procedures before a production heat. Sisters often sampled on the same RFQ: 1.4512, 1.4016, 1.4509. SHH STEEL can produce and supply those trials when strip slots allow. Corrosion thread: chromium passive film for dry and mildly wet atmospheres; nickel addition aids weldability versus plain 12%Cr but does not create Mo-class chloride resistance.

FAQ

What is EN 10296-2 1.4003 welded stainless steel tube used for?
EN 10296-2 1.4003 (X2CrNi12) is welded tube for mechanical and general engineering — bus-frame and light structural welded tube, utility handrails, agricultural equipment lines, and mild aqueous mechanical fabrications that still say “3Cr12”. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: Ni-bearing 12%Cr weldable ferritic welded tube for structural and utility mechanical duty where nickel cost of 18-8 is not justified.
Is EN 10296-2 1.4003 the same as EN 10216-5 1.4003?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4003 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4003 / X2CrNi12?
Delivery framing for 1.4003 is +A under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 700–750 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4003?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4003 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4003 compare with sister grades 1.4512, 1.4016, 1.4509?
1.4003 / X2CrNi12 is filed as ferritic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4512, 1.4016, 1.4509. Design caution: not a chloride-service austenitic substitute — pitting and HAZ toughness stay limited versus 18-8; keep wall and forming within ferritic practice, and remember W0/W1/W2 symbols are not for ferritic grades Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4003 tube on site?
1.4003 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: low-to-moderate heat input with matching or overlying ferritic fillers; mill welded seam already exists — fabricator joints still need ferritic WPS discipline and optional post-weld anneal after heavy forming. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4003?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4003?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4003 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: commodity structural and light mechanical OD×wall on W1A/W2A-class descaled routes (ferritic symbols exclude W0/W1/W2). Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 3Cr12 / 1.4003 utility ferritic belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 3Cr12 / 1.4003 utility ferritic in body text and BOM notes, but lock EN 10296-2 and 1.4003 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4003?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: not a chloride-service austenitic substitute — pitting and HAZ toughness stay limited versus 18-8; keep wall and forming within ferritic practice, and remember W0/W1/W2 symbols are not for ferritic grades Sister pointers: 1.4512, 1.4016, 1.4509. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4003 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4003 is filed as ferritic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4003 (X2CrNi12) is welded stainless tube for mechanical and general engineering — Ni-bearing 12%Cr weldable ferritic welded tube for structural and utility mechanical duty where nickel cost of 18-8 is not justified. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4512, 1.4016, 1.4509. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X