EN 10296-2 1.4550 Welded Stainless Steel Tube
What is EN 10296-2 1.4550 Welded Stainless Steel Tube
EN 10296-2 covers welded stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4550 is the austenitic corrosion-resisting grade X6CrNiNb18-10, commercially discussed as 347. When the spec literally names Nb-stabilised 347 welded tube, EN 10296-2 1.4550 is the general-purpose welded designation that belongs on the order line. Family filing for 1.4550 is austenitic corrosion-resisting.
SHH STEEL can make and supply EN 10296-2 1.4550 / X6CrNiNb18-10 as welded general-purpose tube across process welded OD×wall on W1A/W2A routes with +AT when ordered, annealed or solution annealed as the grade tables and order require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Family filing for 1.4550 is austenitic corrosion-resisting.
On the shop floor people still say “347 tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4550, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty. Typical duties include process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named. Design caution: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8 Primary application sketch: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named.
EN 10296-2 is welded product only for this series. When a seamless general-purpose twin is required, look to EN 10297-2 rather than forcing a seamless claim onto a 10296-2 order. When PED pressure welded acceptance is mandatory, use EN 10217-7 for the same chemistry family where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Duty thread: niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty.
Inside this welded general-purpose series, compare EN 10296-2 1.4541, EN 10296-2 1.4307, EN 10296-2 1.4301. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4550. ASTM/ASME related product pages (not interchangeable by default): A269 TP347, A213 TP347.
Chemical Composition of EN 10296-2 1.4550
Every 1.4550 heat under EN 10296-2 must meet the cast (ladle) analysis for X6CrNiNb18-10 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Caution thread: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8.
The table below reproduces public BSSA EN 10296-2 chemical limits for 1.4550 / X6CrNiNb18-10, cross-checked against the EN 10296-2:2005 grade list. Values are maximum unless a range is shown. Commercial talk still says 347, but only the steel-number cast windows below belong on the MTC for this austenitic corrosion-resisting welded tube. Weld thread: 347/308L-class fillers; control heat input on fabricator joints after the mill longitudinal weld.
| Steel | C | Si | Mn | P | S | Cr | Ni | Nb |
|---|---|---|---|---|---|---|---|---|
| 1.4550 / X6CrNiNb18-10 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.015 | 17.0–19.0 | 9.0–12.0 | 10×C–1.00 |
Mechanical Properties of EN 10296-2 1.4550
Table mechanical floors for 1.4550 / X6CrNiNb18-10 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 205 MPa, Rp1.0 min 240 MPa, Rm min 510 MPa, longitudinal elongation min 35%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Caution thread: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 205 | 240 | 510 min | 35 | 30 | Yes |
Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4550 / X6CrNiNb18-10. Guideline solution/anneal band (Annex B): 1020–1100 °C; cooling: water, air or gas.
Welded Tube Manufacture for EN 10296-2 1.4550
EN 10296-2 does not offer a seamless route for 1.4550. Tube in X6CrNiNb18-10 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. Order EN 10296-2 1.4550 with an Annex A surface/process symbol — W0 when as-welded is acceptable, W1A/W2A for metallically clean heat-treated descaled tube, W1R/W2R when bright heat treatment is required, WCA/WCR when the weld must be scarcely recognizable, and WG/WP when ground or polished roughness is written into the purchase order. Size context for 1.4550: process welded OD×wall on W1A/W2A routes with +AT when ordered.
For austenitic 1.4550, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4550 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1020–1100 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Caution thread: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8.
State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4550. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Use thread: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named.
Dimensions and Tolerances for EN 10296-2 1.4550
Dimensional orders for 1.4550 name OD × wall, length tolerance, delivery condition, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Process welded od×wall on w1a/w2a routes with +at when ordered. Size context for 1.4550: process welded OD×wall on W1A/W2A routes with +AT when ordered.
For precision mechanical or decorative duty on 1.4550, cold-rolled W2/W2A/W2R and WCA/WCR routes are the usual conversation; heavier walls may start from hot-rolled strip. Agree bead-worked “b” suffixes when smoothed welds are mandatory. Duty thread: niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty.
Equivalent Grades for EN 10296-2 1.4550
Equivalence talk for 1.4550 starts with X6CrNiNb18-10: that is the EN steel name for welded general-purpose tube under this Part 2. Buyers who only write 347 still need the steel number and EN 10296-2 on the PO. Sister grades often quoted alongside this duty: 1.4541, 1.4307, 1.4301. Design caution stays: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8 Family filing for 1.4550 is austenitic corrosion-resisting.
Heat Treatment and Delivery Condition for EN 10296-2 1.4550
Austenitic 1.4550 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1020–1100 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Apps that usually decide +AT versus +AR for this number: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named. Filler/shop note for 1.4550: 347/308L-class fillers; control heat input on fabricator joints after the mill longitudinal weld.
Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4550, restore the delivery condition agreed on the order before corrosive or load-bearing service. Corrosion thread: Nb stabilisation for as-welded IGC and elevated mild service; same Mo-free aqueous limits as sister 18-8 grades.
Corrosion Resistance of EN 10296-2 1.4550
For 1.4550 / X6CrNiNb18-10, read corrosion through the austenitic corrosion-resisting lens rather than a generic “stainless” slogan. Plain-language summary: Nb stabilisation for as-welded IGC and elevated mild service; same Mo-free aqueous limits as sister 18-8 grades. IGC Options follow EN ISO 3651-2 where the tables say Yes — and still do not replace medium-specific design. Caution: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8 Primary application sketch: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named.
SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4550. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Duty thread: niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty.
Applications of EN 10296-2 1.4550 Tube
Typical field use for 347-named welded tube under steel number 1.4550: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named. Keep pressure seamless talk on EN 10216-5 pages when that standard is the regulatory home. Filler/shop note for 1.4550: 347/308L-class fillers; control heat input on fabricator joints after the mill longitudinal weld.
Skip 1.4550 when the specification locks a different family — for example forcing ferritic 1.4550 into severe chloride process duty, or forcing a heat-resisting number into aqueous chloride service. Sister conversation inside EN 10296-2: 1.4541, 1.4307, 1.4301. Duty thread: niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty.
Weldability of EN 10296-2 1.4550
Weldability of EN 10296-2 1.4550 covers both the mill longitudinal seam and downstream fabricator joints. Practical shop note: 347/308L-class fillers; control heat input on fabricator joints after the mill longitudinal weld. Caution that shapes WPS choices: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8 Primary application sketch: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named.
Filler selection should match or over-alloy the base X6CrNiNb18-10 chemistry as the WPS demands. Heat input, interpass temperature, and shielding practice follow the family — austenitic, ferritic, duplex, or heat-resisting — not a single shop habit. Corrosion thread: Nb stabilisation for as-welded IGC and elevated mild service; same Mo-free aqueous limits as sister 18-8 grades.
Surface Finishes for EN 10296-2 1.4550
For 1.4550, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Use thread: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named.
Descaled 1.4550 engineering finishes still get caps and separators; bright X6CrNiNb18-10 OD never rides bare under carbon-steel strapping. Packaging notes on the order should repeat the Annex A symbol so warehouse staff do not treat every bundle as the same 347 commodity. Caution thread: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8.
Inspection and Testing for EN 10296-2 1.4550
SHH STEEL EN 10204 3.1 documents for 1.4550 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a leak-test or NDT line unless that Option was executed. Duty thread: niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty.
For X6CrNiNb18-10 under EN 10296-2, technological Options and IGC (where tabulated) belong on the enquiry checklist beside OD × wall. SHH STEEL correlates marking on 1.4550 bundles to the EN 10204 3.1 document so heat identity survives transit. Caution reminder: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8 Filler/shop note for 1.4550: 347/308L-class fillers; control heat input on fabricator joints after the mill longitudinal weld.
Packaging and Shipping for EN 10296-2 1.4550
Export packing for 1.4550 / X6CrNiNb18-10 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavier descaled bundles use spacers to stop fretting in transit. Corrosion thread: Nb stabilisation for as-welded IGC and elevated mild service; same Mo-free aqueous limits as sister 18-8 grades.
Marking typically includes manufacturer identity, dimensions, EN 10296-2, steel name or number 1.4550, cast/code, inspection mark, delivery-condition symbol, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging bright or polished surfaces. Duty thread: niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty.
Ocean-freight wrap for X6CrNiNb18-10 repeats cast/code on tags inside and outside the wrap. Duty thread for why identity matters: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named. Filler/shop note for 1.4550: 347/308L-class fillers; control heat input on fabricator joints after the mill longitudinal weld.
Why Choose SHH STEEL
SHH STEEL can produce and supply EN 10296-2 1.4550 as welded general-purpose tube when you need a mill partner who will not blur EN 10296-2 with EN 10217-7 or EN 10216-5 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty.
SHH STEEL will not stretch X6CrNiNb18-10 into a medium it cannot defend. Typical right-fit duties: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named. When those duties slip toward a sister, we say so before the quote hardens. Primary application sketch: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named.
Supply Capability
Supply capability for 1.4550 / X6CrNiNb18-10 is enquiry-led: SHH STEEL can produce and supply welded general-purpose tube with the Annex A finish and +AR/+A/+AT condition you name. Size hint: process welded OD×wall on W1A/W2A routes with +AT when ordered. Primary application sketch: process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named.
| Item | Capability |
|---|---|
| Standard | EN 10296-2:2005 welded general-purpose |
| Steel | 1.4550 / X6CrNiNb18-10 |
| Product form | Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–12.7 mm within welded family practice (other by agreement) |
Stock / Available sizes
Enquiry-oriented Stock / Available sizes map for EN 10296-2 1.4550 — not a frozen warehouse SKU list with tonnages. Availability tracks mill heats of X6CrNiNb18-10, strip/plate starting stock, and welding/finishing slots for the ordered Annex A symbol; send the OD × wall list, delivery-condition preference, and any Optional tests tied to process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named. Filler/shop note for 1.4550: 347/308L-class fillers; control heat input on fabricator joints after the mill longitudinal weld.
Trial lengths of 1.4550 / X6CrNiNb18-10 help fabricators prove forming and weld procedures before a production heat. Sisters often sampled on the same RFQ: 1.4541, 1.4307, 1.4301. SHH STEEL can produce and supply those trials when strip slots allow. Weld thread: 347/308L-class fillers; control heat input on fabricator joints after the mill longitudinal weld.
FAQ
-
What is EN 10296-2 1.4550 welded stainless steel tube used for?
- EN 10296-2 1.4550 (X6CrNiNb18-10) is welded tube for mechanical and general engineering — process heaters, exhaust gas lines, and chemical transfer fabrications where Nb stabilisation is named. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty.
-
Is EN 10296-2 1.4550 the same as EN 10216-5 1.4550?
- Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4550 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4550 / X6CrNiNb18-10?
- Delivery framing for 1.4550 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1020–1100 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4550?
- SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4550 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4550 compare with sister grades 1.4541, 1.4307, 1.4301?
- 1.4550 / X6CrNiNb18-10 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4541, 1.4307, 1.4301. Design caution: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8 Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
How should fabricators weld EN 10296-2 1.4550 tube on site?
- 1.4550 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 347/308L-class fillers; control heat input on fabricator joints after the mill longitudinal weld. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4550?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10296-2 1.4550?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4550 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: process welded OD×wall on W1A/W2A routes with +AT when ordered. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 347 belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 347 in body text and BOM notes, but lock EN 10296-2 and 1.4550 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4550?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: Nb stabilisation is not a Mo upgrade — chloride PREN still tracks Mo-free 18-8 Sister pointers: 1.4541, 1.4307, 1.4301. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10296-2 1.4550 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4550 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10296-2 1.4550 (X6CrNiNb18-10) is welded stainless tube for mechanical and general engineering — niobium-stabilised 18-8 welded tube parallel to Ti-stabilised 1.4541 for as-welded and elevated-temperature mechanical duty. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4541, 1.4307, 1.4301. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.