EN 10296-2 1.4436 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4436 Welded Stainless Steel Tube

EN 10296-2 1.4436 / X3CrNiMo17-13-3 welded stainless general-purpose tube (316 high-Mo), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 205 MPa, Rm min 510 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4436 / X3CrNiMo17-13-3 (316 high-Mo — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4436 Welded Stainless Steel Tube

If the purchase file still names only a commercial alias such as 316 high-Mo without a product standard, the mill cannot know whether general-purpose welded acceptance or pressure-tube acceptance applies. EN 10296-2 plus steel number 1.4436 (X3CrNiMo17-13-3) selects welded tube for mechanical and general engineering. EN 10296-2 1.4436 locks the higher-Mo X3CrNiMo17-13-3 analysis for welded general-purpose tube when commodity 316 Mo is underspecified. Family filing for 1.4436 is austenitic corrosion-resisting.

SHH STEEL can make and supply EN 10296-2 1.4436 / X3CrNiMo17-13-3 as welded general-purpose tube across process welded OD×wall on descaled heat-treated Annex A routes, annealed or solution annealed as the grade tables and order require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Filler/shop note for 1.4436: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned.

On the shop floor people still say “316 high-Mo tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4436, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401. Typical duties include chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316. Design caution: standard-carbon band — prefer low-carbon 1.4432/1.4435 for corrosive as-welded fabricator joints when IGC is critical Primary application sketch: chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316.

EN 10296-2 is welded product only for this series. When a seamless general-purpose twin is required, look to EN 10297-2 rather than forcing a seamless claim onto a 10296-2 order. When PED pressure welded acceptance is mandatory, use EN 10217-7 for the same chemistry family where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Size context for 1.4436: process welded OD×wall on descaled heat-treated Annex A routes.

Inside this welded general-purpose series, compare EN 10296-2 1.4401, EN 10296-2 1.4432, EN 10296-2 1.4571. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4436. ASTM/ASME related product pages (not interchangeable by default): A269 TP316.

Chemical Composition of EN 10296-2 1.4436

Buying 316 high-Mo-family welded tube without locking 1.4436 invites silent chemistry drift. Under EN 10296-2 the cast must satisfy X3CrNiMo17-13-3; highlight elements for this grade include C ≤0.05, Cr 16.5–18.5, Ni 10.5–13.0, Mo 2.50–3.00, N ≤0.11, Si ≤1.00. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Use thread: chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316.

Use the cast table for 1.4436 as the contractual chemistry window for welded general-purpose duty — role reminder: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401. Do not substitute a sister analysis from 1.4401, 1.4432, 1.4571 without rewriting the steel number on the order. Primary application sketch: chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316.

Steel C Si Mn P S Cr Mo Ni N
1.4436 / X3CrNiMo17-13-3 ≤0.05 ≤1.00 ≤2.00 ≤0.045 ≤0.015 16.5–18.5 2.50–3.00 10.5–13.0 ≤0.11

Mechanical Properties of EN 10296-2 1.4436

Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4436 order. General-purpose Table values for this number read: Rp0.2 min 205 MPa, Rp1.0 min 240 MPa, Rm min 510 MPa, longitudinal elongation min 40%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Duty thread: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 205 240 510 min 40 30 Yes* (normally not sensitised)

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4436 / X3CrNiMo17-13-3. Guideline solution/anneal band (Annex B): 1030–1110 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4436

EN 10296-2 does not offer a seamless route for 1.4436. Tube in X3CrNiMo17-13-3 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. For 1.4436, SHH STEEL aligns the Annex A symbol to the duty: W0 for as-welded economy, W1A/W2A for descaled engineering tube, W2R/WCR for brighter OD, and WG/WP when a measured roughness target is part of the order text. Corrosion thread: higher Mo versus 1.4401 for chloride pitting margin; IGC after welding tracks carbon like other non-L 316-family grades.

For austenitic 1.4436, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4436 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1030–1110 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Corrosion thread: higher Mo versus 1.4401 for chloride pitting margin; IGC after welding tracks carbon like other non-L 316-family grades.

State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4436. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Duty thread: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401.

Dimensions and Tolerances for EN 10296-2 1.4436

Dimensional orders for 1.4436 name OD × wall, length tolerance, delivery condition, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Process welded od×wall on descaled heat-treated annex a routes. Weld thread: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned.

Tolerance classes on diameter and wall follow the EN 10296-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Use thread: chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316.

Equivalent Grades for EN 10296-2 1.4436

Do not treat ASTM welded or seamless pages as drop-in equals for EN 10296-2 1.4436 / X3CrNiMo17-13-3. Wall bases, mechanical tables, and optional tests differ. Body alias 316 high-Mo is fine in BOM notes; H1 and order line stay on the steel number. Compare 1.4401, 1.4432, 1.4571 when the medium outgrows this analysis. Corrosion thread: higher Mo versus 1.4401 for chloride pitting margin; IGC after welding tracks carbon like other non-L 316-family grades.

Heat Treatment and Delivery Condition for EN 10296-2 1.4436

Austenitic 1.4436 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1030–1110 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Apps that usually decide +AT versus +AR for this number: chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316. Family filing for 1.4436 is austenitic corrosion-resisting.

Hot-working temperature bands in Annex B for X3CrNiMo17-13-3 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Size context for 1.4436: process welded OD×wall on descaled heat-treated Annex A routes.

Corrosion Resistance of EN 10296-2 1.4436

For 1.4436 / X3CrNiMo17-13-3, read corrosion through the austenitic corrosion-resisting lens rather than a generic “stainless” slogan. Plain-language summary: higher Mo versus 1.4401 for chloride pitting margin; IGC after welding tracks carbon like other non-L 316-family grades. IGC Options follow EN ISO 3651-2 where the tables say Yes — and still do not replace medium-specific design. Caution: standard-carbon band — prefer low-carbon 1.4432/1.4435 for corrosive as-welded fabricator joints when IGC is critical Family filing for 1.4436 is austenitic corrosion-resisting.

Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4401, 1.4432, 1.4571 when the medium outgrows this number rather than hoping surface finish alone will hold. Duty thread: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401.

Applications of EN 10296-2 1.4436 Tube

Buyers pick EN 10296-2 1.4436 / X3CrNiMo17-13-3 when the duty list looks like this: chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316. That is welded general-purpose work — not a silent PED pressure shell. Role in one line: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401. Filler/shop note for 1.4436: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned.

Typical BOM language pairs EN 10296-2 1.4436 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “316 high-Mo” substitutions do not creep in. Duty thread: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401.

Weldability of EN 10296-2 1.4436

1.4436 / X3CrNiMo17-13-3 arrives as a longitudinally welded product under EN 10296-2, and fabricators still add circumferential and attachment welds on mechanical assemblies. Shop guidance: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Filler/shop note for 1.4436: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: standard-carbon band — prefer low-carbon 1.4432/1.4435 for corrosive as-welded fabricator joints when IGC is critical Primary application sketch: chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316.

Surface Finishes for EN 10296-2 1.4436

For 1.4436, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Duty thread: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401.

Descaled 1.4436 engineering finishes still get caps and separators; bright X3CrNiMo17-13-3 OD never rides bare under carbon-steel strapping. Packaging notes on the order should repeat the Annex A symbol so warehouse staff do not treat every bundle as the same 316 high-Mo commodity. Use thread: chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316.

Inspection and Testing for EN 10296-2 1.4436

SHH STEEL EN 10204 3.1 documents for 1.4436 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a leak-test or NDT line unless that Option was executed. Caution thread: standard-carbon band — prefer low-carbon 1.4432/1.4435 for corrosive as-welded fabricator joints when IGC is critical.

For X3CrNiMo17-13-3 under EN 10296-2, technological Options and IGC (where tabulated) belong on the enquiry checklist beside OD × wall. SHH STEEL correlates marking on 1.4436 bundles to the EN 10204 3.1 document so heat identity survives transit. Caution reminder: standard-carbon band — prefer low-carbon 1.4432/1.4435 for corrosive as-welded fabricator joints when IGC is critical Filler/shop note for 1.4436: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned.

Packaging and Shipping for EN 10296-2 1.4436

Export packing for 1.4436 / X3CrNiMo17-13-3 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavier descaled bundles use spacers to stop fretting in transit. Caution thread: standard-carbon band — prefer low-carbon 1.4432/1.4435 for corrosive as-welded fabricator joints when IGC is critical.

Marking typically includes manufacturer identity, dimensions, EN 10296-2, steel name or number 1.4436, cast/code, inspection mark, delivery-condition symbol, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging bright or polished surfaces. Duty thread: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401.

For 1.4436, packing-list discipline matters when multiple sisters (1.4401, 1.4432, 1.4571) ship on the same vessel — wrong bundle cards create wrong field installs. SHH STEEL can produce and supply photographed mark sets when the EPC file demands them. Corrosion thread: higher Mo versus 1.4401 for chloride pitting margin; IGC after welding tracks carbon like other non-L 316-family grades.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10296-2 1.4436 as welded general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “316 high-Mo tube” label on whatever is in the rack. We keep pressure talk honest: when PED welded pressure acceptance is required, we point you to EN 10217-7 for the same chemistry family where it exists. Weld thread: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned.

Why this mill page exists: honest EN 10296-2 1.4436 welded supply with Annex A and delivery-condition clarity — not a generic 316 high-Mo rack pull. Sisters on the same RFQ conversation: 1.4401, 1.4432, 1.4571. Weld thread: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned.

Supply Capability

SHH STEEL can produce and supply EN 10296-2 1.4436 welded stainless steel tube against the edition, delivery condition, Annex A symbol, and Options named on your enquiry. The capability table and Stock / Available sizes enquiry map below frame a first-pass size list for X3CrNiMo17-13-3 — role: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401. Filler/shop note for 1.4436: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4436 / X3CrNiMo17-13-3
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

Stock / Available sizes for 1.4436 means RFQ bands, not published tonnages. Typical conversation starts around commodity-to-process welded OD with walls suited to austenitic corrosion-resisting practice. Alias on emails may still say 316 high-Mo; the acknowledgement must say 1.4436. Corrosion thread: higher Mo versus 1.4401 for chloride pitting margin; IGC after welding tracks carbon like other non-L 316-family grades.

When the project needs both decorative WP and engineering W2A on 1.4436, say so up front — finishing slots differ. Apps that usually drive the mix: chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316. Filler/shop note for 1.4436: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned.

FAQ

What is EN 10296-2 1.4436 welded stainless steel tube used for?
EN 10296-2 1.4436 (X3CrNiMo17-13-3) is welded tube for mechanical and general engineering — chemical process lines, coastal utilities, and orders that name X3CrNiMo17-13-3 rather than commodity 316. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401.
Is EN 10296-2 1.4436 the same as EN 10216-5 1.4436?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4436 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4436 / X3CrNiMo17-13-3?
Delivery framing for 1.4436 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1030–1110 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4436?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4436 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4436 compare with sister grades 1.4401, 1.4432, 1.4571?
1.4436 / X3CrNiMo17-13-3 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4401, 1.4432, 1.4571. Design caution: standard-carbon band — prefer low-carbon 1.4432/1.4435 for corrosive as-welded fabricator joints when IGC is critical Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4436 tube on site?
1.4436 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 316/316L-class fillers; prefer L fillers when as-welded corrosive service is planned. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4436?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4436?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4436 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: process welded OD×wall on descaled heat-treated Annex A routes. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 316 high-Mo belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 316 high-Mo in body text and BOM notes, but lock EN 10296-2 and 1.4436 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4436?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: standard-carbon band — prefer low-carbon 1.4432/1.4435 for corrosive as-welded fabricator joints when IGC is critical Sister pointers: 1.4401, 1.4432, 1.4571. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4436 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4436 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4436 (X3CrNiMo17-13-3) is welded stainless tube for mechanical and general engineering — higher-Mo 316-family austenitic welded tube (Mo 2.5–3.0) for mechanical duty needing more Mo than 1.4401. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4401, 1.4432, 1.4571. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X