EN 10296-2 1.4571 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4571 Welded Stainless Steel Tube

EN 10296-2 1.4571 / X6CrNiMoTi17-12-2 welded stainless general-purpose tube (316Ti), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 210 MPa, Rm min 510 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4571 / X6CrNiMoTi17-12-2 (316Ti — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4571 Welded Stainless Steel Tube

EN 10296-2:2005 (BS EN 10296-2:2005) is the European product standard for welded circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10217-7, and not for seamless general-purpose tube under EN 10297-2. Steel number 1.4571 is listed as X6CrNiMoTi17-12-2 in the austenitic corrosion-resisting set. When the drawing insists on Ti-stabilised 316Ti welded tube, EN 10296-2 1.4571 locks X6CrNiMoTi17-12-2 onto the general-purpose welded MTC. Family filing for 1.4571 is austenitic corrosion-resisting.

SHH STEEL can make and supply EN 10296-2 1.4571 / X6CrNiMoTi17-12-2 as welded general-purpose tube across process welded OD×wall common in European 316Ti catalogues, annealed or solution annealed as the grade tables and order require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Filler/shop note for 1.4571: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints.

On the shop floor people still say “316Ti tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4571, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service. Typical duties include chemical plant mechanical lines, heat-transfer loops with chlorides, and European projects that prefer 316Ti over 316L carbon control. Design caution: stabilisation helps as-welded IGC but Mo floor is still commodity 2–2.5% — severe chlorides need higher-Mo or duplex sisters Filler/shop note for 1.4571: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints.

Scope discipline matters: 1.4571 under EN 10296-2 is welded general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Corrosion thread: Mo plus Ti stabilisation for as-welded chloride and elevated mild chemical duty.

Inside this welded general-purpose series, compare EN 10296-2 1.4404, EN 10296-2 1.4401, EN 10296-2 1.4435. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4571. ASTM/ASME related product pages (not interchangeable by default): A269 TP316L.

Chemical Composition of EN 10296-2 1.4571

Every 1.4571 heat under EN 10296-2 must meet the cast (ladle) analysis for X6CrNiMoTi17-12-2 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Duty thread: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service.

Use the cast table for 1.4571 as the contractual chemistry window for welded general-purpose duty — role reminder: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service. Do not substitute a sister analysis from 1.4404, 1.4401, 1.4435 without rewriting the steel number on the order. Family filing for 1.4571 is austenitic corrosion-resisting.

Steel C Si Mn P S Cr Mo Ni Ti
1.4571 / X6CrNiMoTi17-12-2 ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.015 16.5–18.5 2.00–2.50 10.5–13.5 5×C–0.70

Mechanical Properties of EN 10296-2 1.4571

Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4571 order. General-purpose Table values for this number read: Rp0.2 min 210 MPa, Rp1.0 min 245 MPa, Rm min 510 MPa, longitudinal elongation min 35%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Corrosion thread: Mo plus Ti stabilisation for as-welded chloride and elevated mild chemical duty.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 210 245 510 min 35 30 Yes

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4571 / X6CrNiMoTi17-12-2. Guideline solution/anneal band (Annex B): 1030–1110 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4571

EN 10296-2 does not offer a seamless route for 1.4571. Tube in X6CrNiMoTi17-12-2 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. Annex A process-route symbols for welded 1.4571 include W0 (as-welded), W1/W1A/W1R (hot-rolled strip routes), W2/W2A/W2R (cold-rolled strip routes), WCA/WCR (cold-worked recrystallised weld), and WG/WP (ground/polished). Bead-worked conditions append “b” (for example W2Ab). Use thread: chemical plant mechanical lines, heat-transfer loops with chlorides, and European projects that prefer 316Ti over 316L carbon control.

For austenitic 1.4571, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4571 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1030–1110 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Size context for 1.4571: process welded OD×wall common in European 316Ti catalogues.

State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4571. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Corrosion thread: Mo plus Ti stabilisation for as-welded chloride and elevated mild chemical duty.

Dimensions and Tolerances for EN 10296-2 1.4571

Order EN 10296-2 1.4571 by outside diameter D and wall thickness T for steel name X6CrNiMoTi17-12-2. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Process welded od×wall common in european 316ti catalogues. Duty thread: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service.

Length supply for 1.4571 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Corrosion thread: Mo plus Ti stabilisation for as-welded chloride and elevated mild chemical duty.

Equivalent Grades for EN 10296-2 1.4571

1.4571 / X6CrNiMoTi17-12-2 is the EN 10296-2 designation for this chemistry as welded general-purpose tube. Commercial alias 316Ti appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this welded general-purpose series, compare sisters 1.4404, 1.4401, 1.4435. Hook for buyers still using only the 316Ti alias: lock EN 10296-2 1.4571 on the order line. Duty thread: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service.

Heat Treatment and Delivery Condition for EN 10296-2 1.4571

Austenitic 1.4571 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1030–1110 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Delivery framing on the certificate for 1.4571 should match the ordered +AR/+A/+AT symbol — alias 316Ti alone is not enough. Size context for 1.4571: process welded OD×wall common in European 316Ti catalogues.

Hot-working temperature bands in Annex B for X6CrNiMoTi17-12-2 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Corrosion thread: Mo plus Ti stabilisation for as-welded chloride and elevated mild chemical duty.

Corrosion Resistance of EN 10296-2 1.4571

316Ti-family marketing claims do not override EN 10296-2 tabulated IGC notes for 1.4571. Corrosion thread: Mo plus Ti stabilisation for as-welded chloride and elevated mild chemical duty. Move to sisters 1.4404, 1.4401, 1.4435 when the medium outgrows this analysis.

Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4404, 1.4401, 1.4435 when the medium outgrows this number rather than hoping surface finish alone will hold. Size context for 1.4571: process welded OD×wall common in European 316Ti catalogues.

Applications of EN 10296-2 1.4571 Tube

Buyers pick EN 10296-2 1.4571 / X6CrNiMoTi17-12-2 when the duty list looks like this: chemical plant mechanical lines, heat-transfer loops with chlorides, and European projects that prefer 316Ti over 316L carbon control. That is welded general-purpose work — not a silent PED pressure shell. Role in one line: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service. Filler/shop note for 1.4571: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints.

Skip 1.4571 when the specification locks a different family — for example forcing ferritic 1.4571 into severe chloride process duty, or forcing a heat-resisting number into aqueous chloride service. Sister conversation inside EN 10296-2: 1.4404, 1.4401, 1.4435. Size context for 1.4571: process welded OD×wall common in European 316Ti catalogues.

Weldability of EN 10296-2 1.4571

Even though 1.4571 is already a welded tube product, site joints still need a WPS matched to X6CrNiMoTi17-12-2. Filler and heat-input guidance: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints. Alias on the shop traveler may say 316Ti; the WPS should cite the steel number. Family filing for 1.4571 is austenitic corrosion-resisting.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: stabilisation helps as-welded IGC but Mo floor is still commodity 2–2.5% — severe chlorides need higher-Mo or duplex sisters Filler/shop note for 1.4571: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints.

Surface Finishes for EN 10296-2 1.4571

Interior Ra limits, electropolish, or special protection for X6CrNiMoTi17-12-2 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4571 when the mill can measure and report the finish. Caution thread: stabilisation helps as-welded IGC but Mo floor is still commodity 2–2.5% — severe chlorides need higher-Mo or duplex sisters.

Descaled 1.4571 engineering finishes still get caps and separators; bright X6CrNiMoTi17-12-2 OD never rides bare under carbon-steel strapping. Packaging notes on the order should repeat the Annex A symbol so warehouse staff do not treat every bundle as the same 316Ti commodity. Caution thread: stabilisation helps as-welded IGC but Mo floor is still commodity 2–2.5% — severe chlorides need higher-Mo or duplex sisters.

Inspection and Testing for EN 10296-2 1.4571

NDT and technological-test intensity on 1.4571 is Option-driven under EN 10296-2 — leak, flattening, drift expanding, bend, or NDT methods are selected at enquiry. That is a different framing from EN 10217-7 pressure categories; copy the Options you need. Duty thread: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service.

Inspection intensity on 1.4571 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service. Primary application sketch: chemical plant mechanical lines, heat-transfer loops with chlorides, and European projects that prefer 316Ti over 316L carbon control.

Packaging and Shipping for EN 10296-2 1.4571

Export packing for 1.4571 / X6CrNiMoTi17-12-2 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavier descaled bundles use spacers to stop fretting in transit. Weld thread: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints.

For 1.4571, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Weld thread: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints.

For 1.4571, packing-list discipline matters when multiple sisters (1.4404, 1.4401, 1.4435) ship on the same vessel — wrong bundle cards create wrong field installs. SHH STEEL can produce and supply photographed mark sets when the EPC file demands them. Corrosion thread: Mo plus Ti stabilisation for as-welded chloride and elevated mild chemical duty.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10296-2 1.4571 as welded general-purpose tube when you need a mill partner who will not blur EN 10296-2 with EN 10217-7 or EN 10216-5 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service.

SHH STEEL will not stretch X6CrNiMoTi17-12-2 into a medium it cannot defend. Typical right-fit duties: chemical plant mechanical lines, heat-transfer loops with chlorides, and European projects that prefer 316Ti over 316L carbon control. When those duties slip toward a sister, we say so before the quote hardens. Family filing for 1.4571 is austenitic corrosion-resisting.

Supply Capability

Supply capability for 1.4571 / X6CrNiMoTi17-12-2 is enquiry-led: SHH STEEL can produce and supply welded general-purpose tube with the Annex A finish and +AR/+A/+AT condition you name. Size hint: process welded OD×wall common in European 316Ti catalogues. Filler/shop note for 1.4571: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4571 / X6CrNiMoTi17-12-2
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

Enquiry-oriented Stock / Available sizes map for EN 10296-2 1.4571 — not a frozen warehouse SKU list with tonnages. Availability tracks mill heats of X6CrNiMoTi17-12-2, strip/plate starting stock, and welding/finishing slots for the ordered Annex A symbol; send the OD × wall list, delivery-condition preference, and any Optional tests tied to chemical plant mechanical lines, heat-transfer loops with chlorides, and European projects that prefer 316Ti over 316L carbon control. Primary application sketch: chemical plant mechanical lines, heat-transfer loops with chlorides, and European projects that prefer 316Ti over 316L carbon control.

When the project needs both decorative WP and engineering W2A on 1.4571, say so up front — finishing slots differ. Apps that usually drive the mix: chemical plant mechanical lines, heat-transfer loops with chlorides, and European projects that prefer 316Ti over 316L carbon control. Filler/shop note for 1.4571: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints.

FAQ

What is EN 10296-2 1.4571 welded stainless steel tube used for?
EN 10296-2 1.4571 (X6CrNiMoTi17-12-2) is welded tube for mechanical and general engineering — chemical plant mechanical lines, heat-transfer loops with chlorides, and European projects that prefer 316Ti over 316L carbon control. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service.
Is EN 10296-2 1.4571 the same as EN 10216-5 1.4571?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4571 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4571 / X6CrNiMoTi17-12-2?
Delivery framing for 1.4571 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1030–1110 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4571?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4571 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4571 compare with sister grades 1.4404, 1.4401, 1.4435?
1.4571 / X6CrNiMoTi17-12-2 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4404, 1.4401, 1.4435. Design caution: stabilisation helps as-welded IGC but Mo floor is still commodity 2–2.5% — severe chlorides need higher-Mo or duplex sisters Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4571 tube on site?
1.4571 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 316Ti/316L-class fillers per WPS; avoid procedures that leave sensitised HAZ on fabricator joints. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4571?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4571?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4571 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: process welded OD×wall common in European 316Ti catalogues. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 316Ti belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 316Ti in body text and BOM notes, but lock EN 10296-2 and 1.4571 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4571?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: stabilisation helps as-welded IGC but Mo floor is still commodity 2–2.5% — severe chlorides need higher-Mo or duplex sisters Sister pointers: 1.4404, 1.4401, 1.4435. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4571 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4571 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4571 (X6CrNiMoTi17-12-2) is welded stainless tube for mechanical and general engineering — Ti-stabilised Mo-bearing austenitic welded tube for as-welded chloride and elevated-temperature mechanical service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4404, 1.4401, 1.4435. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X