EN 10296-2 1.4526 / X6CrMoNb17-1 welded stainless general-purpose tube (436 / Mo-Nb ferritic), ferritic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 280 MPa, Rm min 480 MPa, A long. min 25%, delivery +A. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4526 / X6CrMoNb17-1 (436 / Mo-Nb ferritic — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +A as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4526 Welded Stainless Steel Tube

Mechanical, decorative, and general engineering projects that need welded stainless tube under a European product standard look to EN 10296-2:2005 — Part 2 of EN 10296 — rather than a PED pressure Part 7 page or an ASTM tubing habit alone. 1.4526 / X6CrMoNb17-1 sits in the ferritic corrosion-resisting tables. If the exhaust BOM says “436 welded tube,” lock EN 10296-2 1.4526 so X6CrMoNb17-1 chemistry and welded general-purpose acceptance ride together. Family filing for 1.4526 is ferritic corrosion-resisting.

SHH STEEL can make and supply EN 10296-2 1.4526 / X6CrMoNb17-1 as welded general-purpose tube across thin-wall welded exhaust and light mechanical OD bands, annealed or solution annealed as the grade tables and order require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Filler/shop note for 1.4526: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified.

On the shop floor people still say “436 / Mo-Nb ferritic tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4526, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty. Typical duties include automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry. Design caution: Nb/Mo ferritic still lacks austenitic toughness and chloride margins — not a silent swap for 1.4404 in process chlorides Primary application sketch: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry.

Scope discipline matters: 1.4526 under EN 10296-2 is welded general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Duty thread: Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty.

Inside this welded general-purpose series, compare EN 10296-2 1.4521, EN 10296-2 1.4509, EN 10296-2 1.4510. Hub: EN 10296-2.

Chemical Composition of EN 10296-2 1.4526

Cast analysis for EN 10296-2 1.4526 follows the X6CrMoNb17-1 limits published for this standard’s corrosion- or heat-resisting tables. Key windows on a typical certificate include C ≤0.08, Cr 16.0–18.0, Mo 0.80–1.40, N ≤0.040, Nb 7×(C+N)+0.10–1.00, Si ≤1.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Weld thread: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified.

Use the cast table for 1.4526 as the contractual chemistry window for welded general-purpose duty — role reminder: Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty. Do not substitute a sister analysis from 1.4521, 1.4509, 1.4510 without rewriting the steel number on the order. Filler/shop note for 1.4526: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified.

Steel C Si Mn P S Cr Mo N Nb
1.4526 / X6CrMoNb17-1 ≤0.08 ≤1.00 ≤1.00 ≤0.040 ≤0.015 16.0–18.0 0.80–1.40 ≤0.040 7×(C+N)+0.10–1.00

Mechanical Properties of EN 10296-2 1.4526

Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4526 order. General-purpose Table values for this number read: Rp0.2 min 280 MPa, Rp1.0 min 290 MPa, Rm min 480 MPa, longitudinal elongation min 25%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Duty thread: Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+A 280 290 480 min 25 23 Yes

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4526 / X6CrMoNb17-1. Guideline solution/anneal band (Annex B): 820–880 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4526

Ferritic welded 1.4526 (X6CrMoNb17-1) is produced from strip or plate, longitudinally welded, then delivered +AR or +A per 7.2.2. Grain-growth control during anneal matters for toughness and forming when +A is ordered. Order EN 10296-2 1.4526 with an Annex A surface/process symbol suited to ferritic tube — heat-treated descaled W1A/W2A analogues, WCA/WCR when the weld must be scarcely recognizable, and WG/WP only with a written OD/ID roughness scope. W0/W1/W2 are not applicable to ferritic steels. Caution thread: Nb/Mo ferritic still lacks austenitic toughness and chloride margins — not a silent swap for 1.4404 in process chlorides.

Ferritic 1.4526 under EN 10296-2 may be delivered as-welded (+AR) or annealed (+A) at the manufacturer’s discretion unless the order locks +A. Annex B annealing guidance sits near 820–880 °C with water, air or gas cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Forming and expansion trials should respect ferritic elongation floors rather than austenitic shop habits. Weld thread: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified.

State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4526. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Duty thread: Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty.

Dimensions and Tolerances for EN 10296-2 1.4526

SHH STEEL aligns OD × wall, tolerance class, and process-route symbol for 1.4526 / X6CrMoNb17-1 before strip forming and welding slots are locked. Thin-wall welded exhaust and light mechanical od bands. Size context for 1.4526: thin-wall welded exhaust and light mechanical OD bands.

Tolerance classes on diameter and wall follow the EN 10296-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Corrosion thread: Mo aids pitting versus plain 430; Nb stabilisation supports as-welded behaviour in many exhaust-gas condensates.

Equivalent Grades for EN 10296-2 1.4526

Do not treat ASTM welded or seamless pages as drop-in equals for EN 10296-2 1.4526 / X6CrMoNb17-1. Wall bases, mechanical tables, and optional tests differ. Body alias 436 / Mo-Nb ferritic is fine in BOM notes; H1 and order line stay on the steel number. Compare 1.4521, 1.4509, 1.4510 when the medium outgrows this analysis. Use thread: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry.

Heat Treatment and Delivery Condition for EN 10296-2 1.4526

Ferritic 1.4526 under EN 10296-2 may be delivered as-welded (+AR) or annealed (+A) at the manufacturer’s discretion unless the order locks +A. Annex B annealing guidance sits near 820–880 °C with water, air or gas cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Delivery framing on the certificate for 1.4526 should match the ordered +AR/+A/+AT symbol — alias 436 / Mo-Nb ferritic alone is not enough. Size context for 1.4526: thin-wall welded exhaust and light mechanical OD bands.

Hot-working temperature bands in Annex B for X6CrMoNb17-1 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Weld thread: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified.

Corrosion Resistance of EN 10296-2 1.4526

For 1.4526 / X6CrMoNb17-1, read corrosion through the ferritic corrosion-resisting lens rather than a generic “stainless” slogan. Plain-language summary: Mo aids pitting versus plain 430; Nb stabilisation supports as-welded behaviour in many exhaust-gas condensates. IGC Options follow EN ISO 3651-2 where the tables say Yes — and still do not replace medium-specific design. Caution: Nb/Mo ferritic still lacks austenitic toughness and chloride margins — not a silent swap for 1.4404 in process chlorides Family filing for 1.4526 is ferritic corrosion-resisting.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4526 is filed as ferritic corrosion-resisting — pick tests that match that filing. Weld thread: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified.

Applications of EN 10296-2 1.4526 Tube

Applications of EN 10296-2 1.4526 tube centre on mechanical, decorative, and general engineering rather than PED pressure shells: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry. Role summary: Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists and is live. Primary application sketch: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry.

It is the wrong first choice when a seamless product form is mandatory (use EN 10297-2 or EN 10216-5 as applicable), when PED pressure welded acceptance is locked to EN 10217-7 alone, or when the medium clearly needs a sister such as 1.4521. Caution thread: Nb/Mo ferritic still lacks austenitic toughness and chloride margins — not a silent swap for 1.4404 in process chlorides.

Weldability of EN 10296-2 1.4526

Weldability of EN 10296-2 1.4526 covers both the mill longitudinal seam and downstream fabricator joints. Practical shop note: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified. Caution that shapes WPS choices: Nb/Mo ferritic still lacks austenitic toughness and chloride margins — not a silent swap for 1.4404 in process chlorides Family filing for 1.4526 is ferritic corrosion-resisting.

When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Use thread: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry.

Surface Finishes for EN 10296-2 1.4526

For 1.4526, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Weld thread: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified.

Special measures to protect 1.4526 / X6CrMoNb17-1 during delivery or storage may be agreed at enquiry. Bright and polished tubes take sleeve or paper wrap; descaled engineering finishes still need end caps and dry bundling so chloride-bearing dirt does not sit on the OD in transit — especially important for 436 / Mo-Nb ferritic-family decorative or hygienic OD. Weld thread: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified.

Inspection and Testing for EN 10296-2 1.4526

SHH STEEL EN 10204 3.1 documents for 1.4526 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a leak-test or NDT line unless that Option was executed. Caution thread: Nb/Mo ferritic still lacks austenitic toughness and chloride margins — not a silent swap for 1.4404 in process chlorides.

IGC testing for 1.4526, when required, follows EN ISO 3651-2 as referenced by the grade tables. Hardness, flattening, drift expanding, or bend tests are applied when the order invokes them. Marking typically includes manufacturer identity, dimensions, EN 10296-2, steel name or number 1.4526, cast/code, delivery-condition symbol, and inspection correlation — not a bare 436 / Mo-Nb ferritic stencil alone. Corrosion thread: Mo aids pitting versus plain 430; Nb stabilisation supports as-welded behaviour in many exhaust-gas condensates.

Packaging and Shipping for EN 10296-2 1.4526

SHH STEEL ships EN 10296-2 1.4526 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled W1A/W2A engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Duty thread: Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty.

Marking typically includes manufacturer identity, dimensions, EN 10296-2, steel name or number 1.4526, cast/code, inspection mark, delivery-condition symbol, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging bright or polished surfaces. Size context for 1.4526: thin-wall welded exhaust and light mechanical OD bands.

Ocean-freight wrap for X6CrMoNb17-1 repeats cast/code on tags inside and outside the wrap. Duty thread for why identity matters: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry. Family filing for 1.4526 is ferritic corrosion-resisting.

Why Choose SHH STEEL

SHH STEEL can produce and supply X6CrMoNb17-1 as EN 10296-2 1.4526 welded tube with honest scope boundaries. General engineering welded acceptance is what this page sells; pressure welded, seamless pressure, and seamless general-purpose sisters are separate standards with separate MTCs. Duty thread: Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty.

SHH STEEL will not stretch X6CrMoNb17-1 into a medium it cannot defend. Typical right-fit duties: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry. When those duties slip toward a sister, we say so before the quote hardens. Primary application sketch: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry.

Supply Capability

Supply capability for 1.4526 / X6CrMoNb17-1 is enquiry-led: SHH STEEL can produce and supply welded general-purpose tube with the Annex A finish and +AR/+A/+AT condition you name. Size hint: thin-wall welded exhaust and light mechanical OD bands. Filler/shop note for 1.4526: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4526 / X6CrMoNb17-1
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +A
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

Stock / Available sizes for 1.4526 means RFQ bands, not published tonnages. Typical conversation starts around commodity-to-process welded OD with walls suited to ferritic corrosion-resisting practice. Alias on emails may still say 436 / Mo-Nb ferritic; the acknowledgement must say 1.4526. Corrosion thread: Mo aids pitting versus plain 430; Nb stabilisation supports as-welded behaviour in many exhaust-gas condensates.

When the project needs both decorative WP and engineering W2A on 1.4526, say so up front — finishing slots differ. Apps that usually drive the mix: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry. Primary application sketch: automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry.

FAQ

What is EN 10296-2 1.4526 welded stainless steel tube used for?
EN 10296-2 1.4526 (X6CrMoNb17-1) is welded tube for mechanical and general engineering — automotive exhaust systems, muffler and resonator tubing, and mild aqueous ferritic lines naming 436-class chemistry. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty.
Is EN 10296-2 1.4526 the same as EN 10216-5 1.4526?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4526 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4526 / X6CrMoNb17-1?
Delivery framing for 1.4526 is +A under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 820–880 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4526?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4526 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4526 compare with sister grades 1.4521, 1.4509, 1.4510?
1.4526 / X6CrMoNb17-1 is filed as ferritic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4521, 1.4509, 1.4510. Design caution: Nb/Mo ferritic still lacks austenitic toughness and chloride margins — not a silent swap for 1.4404 in process chlorides Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4526 tube on site?
1.4526 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: ferritic fillers, low heat input; mill seam plus fabricator joints — anneal when ductility after forming is specified. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4526?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4526?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4526 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: thin-wall welded exhaust and light mechanical OD bands. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 436 / Mo-Nb ferritic belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 436 / Mo-Nb ferritic in body text and BOM notes, but lock EN 10296-2 and 1.4526 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4526?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: Nb/Mo ferritic still lacks austenitic toughness and chloride margins — not a silent swap for 1.4404 in process chlorides Sister pointers: 1.4521, 1.4509, 1.4510. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4526 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4526 is filed as ferritic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4526 (X6CrMoNb17-1) is welded stainless tube for mechanical and general engineering — Mo-Nb stabilised 17%Cr ferritic welded tube for exhaust and mild aqueous mechanical duty. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4521, 1.4509, 1.4510. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X