EN 10296-2 1.4833 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4833 Welded Stainless Steel Tube

EN 10296-2 1.4833 / X12CrNi23-13 welded stainless general-purpose tube (309S), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 210 MPa, Rm min 500 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4833 / X12CrNi23-13 (309S — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4833 Welded Stainless Steel Tube

Mechanical, decorative, and general engineering projects that need welded stainless tube under a European product standard look to EN 10296-2:2005 — Part 2 of EN 10296 — rather than a PED pressure Part 7 page or an ASTM tubing habit alone. 1.4833 / X12CrNi23-13 sits in the austenitic heat-resisting tables. If the file still says “309S welded tube” for heat service, EN 10296-2 1.4833 locks X12CrNi23-13 under welded general-purpose acceptance. Filler/shop note for 1.4833: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

SHH STEEL can produce and supply EN 10296-2 1.4833 welded stainless steel tube — longitudinal welded from strip or plate on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, flattening, drift expanding, bend, and non-destructive testing Options). Size context for 1.4833: furnace and heat-shield welded OD on +AT routes.

On the shop floor people still say “309S tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4833, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty. Typical duties include furnace parts, heat shields, radiant-section adjacent hardware, and high-temperature mechanical tubing in oxidising gases. Design caution: heat-resisting grade — aqueous chloride process is the wrong first use; step to 310S-class 1.4845 when oxidation margins need to climb Filler/shop note for 1.4833: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

EN 10296-2 is welded product only for this series. When a seamless general-purpose twin is required, look to EN 10297-2 rather than forcing a seamless claim onto a 10296-2 order. When PED pressure welded acceptance is mandatory, use EN 10217-7 for the same chemistry family where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Use thread: furnace parts, heat shields, radiant-section adjacent hardware, and high-temperature mechanical tubing in oxidising gases.

Inside this welded general-purpose series, compare EN 10296-2 1.4845, EN 10296-2 1.4828, EN 10296-2 1.4835. Hub: EN 10296-2.

Chemical Composition of EN 10296-2 1.4833

Every 1.4833 heat under EN 10296-2 must meet the cast (ladle) analysis for X12CrNi23-13 in the austenitic heat-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Use thread: furnace parts, heat shields, radiant-section adjacent hardware, and high-temperature mechanical tubing in oxidising gases.

Chemical limits for 1.4833 / X12CrNi23-13 under EN 10296-2 appear in the table underneath. Source priority is BSSA’s EN 10296-2 article cross-checked to the 2005 grade list. If your client specification cites a different edition footnote for 309S-family welded tube, send it before the heat is melted. Duty thread: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty.

Steel C Si Mn P S Cr Ni N
1.4833 / X12CrNi23-13 ≤0.15 ≤1.00 ≤2.00 ≤0.045 ≤0.015 22.0–24.0 12.0–14.0 ≤0.11

Mechanical Properties of EN 10296-2 1.4833

Table mechanical floors for 1.4833 / X12CrNi23-13 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 210 MPa, Rp1.0 min 250 MPa, Rm min 500 MPa, longitudinal elongation min 35%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Corrosion thread: 23Cr-13Ni oxidation resistance for elevated-temperature oxidising atmospheres; IGC N/A in heat-resisting tables.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 210 250 500 min 35 35 N/A

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4833 / X12CrNi23-13. Guideline solution/anneal band (Annex B): 1050–1150 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4833

EN 10296-2 does not offer a seamless route for 1.4833. Tube in X12CrNi23-13 is made by longitudinal welding of strip or plate edges, then solution annealed (+AT) to meet Table 5 heat-resisting mechanical floors. Order EN 10296-2 1.4833 with an Annex A surface/process symbol — W0 when as-welded is acceptable, W1A/W2A for metallically clean heat-treated descaled tube, W1R/W2R when bright heat treatment is required, WCA/WCR when the weld must be scarcely recognizable, and WG/WP when ground or polished roughness is written into the purchase order. Duty thread: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty.

Austenitic heat-resisting 1.4833 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1050–1150 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. High-temperature service still needs fabricator WPS discipline on site joints after the mill seam. Weld thread: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4833. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Duty thread: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty.

Dimensions and Tolerances for EN 10296-2 1.4833

Order EN 10296-2 1.4833 by outside diameter D and wall thickness T for steel name X12CrNi23-13. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Furnace and heat-shield welded od on +at routes. Weld thread: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

For precision mechanical or decorative duty on 1.4833, cold-rolled W2/W2A/W2R and WCA/WCR routes are the usual conversation; heavier walls may start from hot-rolled strip. Agree bead-worked “b” suffixes when smoothed welds are mandatory. Caution thread: heat-resisting grade — aqueous chloride process is the wrong first use; step to 310S-class 1.4845 when oxidation margins need to climb.

Equivalent Grades for EN 10296-2 1.4833

1.4833 / X12CrNi23-13 is the EN 10296-2 designation for this chemistry as welded general-purpose tube. Commercial alias 309S appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this welded general-purpose series, compare sisters 1.4845, 1.4828, 1.4835. Hook for buyers still using only the 309S alias: lock EN 10296-2 1.4833 on the order line. Weld thread: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

Heat Treatment and Delivery Condition for EN 10296-2 1.4833

Austenitic heat-resisting 1.4833 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1050–1150 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Apps that usually decide +AT versus +AR for this number: furnace parts, heat shields, radiant-section adjacent hardware, and high-temperature mechanical tubing in oxidising gases. Filler/shop note for 1.4833: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4833, restore the delivery condition agreed on the order before corrosive or load-bearing service. Use thread: furnace parts, heat shields, radiant-section adjacent hardware, and high-temperature mechanical tubing in oxidising gases.

Corrosion Resistance of EN 10296-2 1.4833

309S-family marketing claims do not override EN 10296-2 tabulated IGC notes for 1.4833. Corrosion thread: 23Cr-13Ni oxidation resistance for elevated-temperature oxidising atmospheres; IGC N/A in heat-resisting tables. Move to sisters 1.4845, 1.4828, 1.4835 when the medium outgrows this analysis.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4833 is filed as austenitic heat-resisting — pick tests that match that filing. Corrosion thread: 23Cr-13Ni oxidation resistance for elevated-temperature oxidising atmospheres; IGC N/A in heat-resisting tables.

Applications of EN 10296-2 1.4833 Tube

Buyers pick EN 10296-2 1.4833 / X12CrNi23-13 when the duty list looks like this: furnace parts, heat shields, radiant-section adjacent hardware, and high-temperature mechanical tubing in oxidising gases. That is welded general-purpose work — not a silent PED pressure shell. Role in one line: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty. Filler/shop note for 1.4833: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

Typical BOM language pairs EN 10296-2 1.4833 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “309S” substitutions do not creep in. Corrosion thread: 23Cr-13Ni oxidation resistance for elevated-temperature oxidising atmospheres; IGC N/A in heat-resisting tables.

Weldability of EN 10296-2 1.4833

1.4833 / X12CrNi23-13 arrives as a longitudinally welded product under EN 10296-2, and fabricators still add circumferential and attachment welds on mechanical assemblies. Shop guidance: 309-class fillers; control heat input and restraint; mill longitudinal weld already present. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Primary application sketch: furnace parts, heat shields, radiant-section adjacent hardware, and high-temperature mechanical tubing in oxidising gases.

When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Caution thread: heat-resisting grade — aqueous chloride process is the wrong first use; step to 310S-class 1.4845 when oxidation margins need to climb.

Surface Finishes for EN 10296-2 1.4833

Surface finish on EN 10296-2 1.4833 is carried by the Annex A symbol: W0 as-welded where permitted, W1A/W2A descaled heat-treated for general mechanical tube, W1R/W2R/WCR for brighter OD, WCA when the weld must be scarcely recognizable, and WG/WP when roughness is agreed at enquiry. Carbon-steel strapping must not contact the stainless surface. Size context for 1.4833: furnace and heat-shield welded OD on +AT routes.

Special measures to protect 1.4833 / X12CrNi23-13 during delivery or storage may be agreed at enquiry. Bright and polished tubes take sleeve or paper wrap; descaled engineering finishes still need end caps and dry bundling so chloride-bearing dirt does not sit on the OD in transit — especially important for 309S-family decorative or hygienic OD. Caution thread: heat-resisting grade — aqueous chloride process is the wrong first use; step to 310S-class 1.4845 when oxidation margins need to climb.

Inspection and Testing for EN 10296-2 1.4833

Specific inspection applies to EN 10296-2 1.4833 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Use thread: furnace parts, heat shields, radiant-section adjacent hardware, and high-temperature mechanical tubing in oxidising gases.

Inspection intensity on 1.4833 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty. Filler/shop note for 1.4833: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

Packaging and Shipping for EN 10296-2 1.4833

Finished EN 10296-2 1.4833 (X12CrNi23-13) welded tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (W*R/WCR/WG/WP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty.

For 1.4833, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Duty thread: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty.

For 1.4833, packing-list discipline matters when multiple sisters (1.4845, 1.4828, 1.4835) ship on the same vessel — wrong bundle cards create wrong field installs. SHH STEEL can produce and supply photographed mark sets when the EPC file demands them. Weld thread: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10296-2 1.4833 as welded general-purpose tube when you need a mill partner who will not blur EN 10296-2 with EN 10217-7 or EN 10216-5 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty.

Grade advice for 1.4833 stays practical. If the duty needs a sister chemistry, we point to 1.4845, 1.4828, 1.4835. Design caution for this number: heat-resisting grade — aqueous chloride process is the wrong first use; step to 310S-class 1.4845 when oxidation margins need to climb Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Filler/shop note for 1.4833: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

Supply Capability

SHH STEEL can make and supply 309S-family chemistry only when the order locks EN 10296-2 and steel number 1.4833. Capability below is an RFQ map for X12CrNi23-13, not a promise that every OD×wall sits in a Shanghai rack tonight. Duty thread: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4833 / X12CrNi23-13
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

For X12CrNi23-13, tell us which Annex A symbol and whether +AT (or +A/+AR) is locked before we hold strip. Caution that shapes size choice: heat-resisting grade — aqueous chloride process is the wrong first use; step to 310S-class 1.4845 when oxidation margins need to climb Filler/shop note for 1.4833: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

Cut lengths, special ends, IGC Options, and dual enquiries against 1.4845, 1.4828, 1.4835 on the same size list are routine for 1.4833. Peer mill catalogues only sanity-check typical OD × wall bands — acceptance remains EN 10296-2 with dimensional agreements stated on the order. SHH STEEL can produce and supply trial lengths before a production heat when the project schedule allows. Weld thread: 309-class fillers; control heat input and restraint; mill longitudinal weld already present.

FAQ

What is EN 10296-2 1.4833 welded stainless steel tube used for?
EN 10296-2 1.4833 (X12CrNi23-13) is welded tube for mechanical and general engineering — furnace parts, heat shields, radiant-section adjacent hardware, and high-temperature mechanical tubing in oxidising gases. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty.
Is EN 10296-2 1.4833 the same as EN 10216-5 1.4833?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4833 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4833 / X12CrNi23-13?
Delivery framing for 1.4833 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1050–1150 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4833?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4833 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4833 compare with sister grades 1.4845, 1.4828, 1.4835?
1.4833 / X12CrNi23-13 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4845, 1.4828, 1.4835. Design caution: heat-resisting grade — aqueous chloride process is the wrong first use; step to 310S-class 1.4845 when oxidation margins need to climb Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4833 tube on site?
1.4833 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 309-class fillers; control heat input and restraint; mill longitudinal weld already present. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4833?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4833?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4833 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: furnace and heat-shield welded OD on +AT routes. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 309S belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 309S in body text and BOM notes, but lock EN 10296-2 and 1.4833 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4833?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: heat-resisting grade — aqueous chloride process is the wrong first use; step to 310S-class 1.4845 when oxidation margins need to climb Sister pointers: 1.4845, 1.4828, 1.4835. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4833 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4833 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4833 (X12CrNi23-13) is welded stainless tube for mechanical and general engineering — 23Cr-13Ni austenitic heat-resisting welded tube (309S-class) for oxidising elevated-temperature mechanical duty. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4845, 1.4828, 1.4835. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X