EN 10296-2 1.4818 Welded Stainless Steel Tube
What is EN 10296-2 1.4818 Welded Stainless Steel Tube
If the purchase file still names only a commercial alias such as 153MA / Ce-Si-N 19-10 without a product standard, the mill cannot know whether general-purpose welded acceptance or pressure-tube acceptance applies. EN 10296-2 plus steel number 1.4818 (X6CrNiSiNCe19-10) selects welded tube for mechanical and general engineering. When the heat-service BOM names 153MA-class welded tube, EN 10296-2 1.4818 locks X6CrNiSiNCe19-10 onto the general-purpose welded certificate. Family filing for 1.4818 is austenitic heat-resisting.
SHH STEEL can produce and supply EN 10296-2 1.4818 welded stainless steel tube — longitudinal welded from strip or plate on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, flattening, drift expanding, bend, and non-destructive testing Options). Caution thread: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number.
On the shop floor people still say “153MA / Ce-Si-N 19-10 tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4818, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: Ce-Si-N microalloyed 19-10 heat-resisting welded tube for high-temp oxidising mechanical service. Typical duties include heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry. Design caution: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number Primary application sketch: heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry.
Scope discipline matters: 1.4818 under EN 10296-2 is welded general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Corrosion thread: Ce-Si-N for adherent oxide scales at elevated temperature; not filed for aqueous IGC tables.
Inside this welded general-purpose series, compare EN 10296-2 1.4835, EN 10296-2 1.4828, EN 10296-2 1.4301. Hub: EN 10296-2. Related pressure seamless chemistry page: EN 10216-5 1.4301.
Chemical Composition of EN 10296-2 1.4818
Buying 153MA / Ce-Si-N 19-10-family welded tube without locking 1.4818 invites silent chemistry drift. Under EN 10296-2 the cast must satisfy X6CrNiSiNCe19-10; highlight elements for this grade include C 0.04–0.08, Cr 18.0–20.0, Ni 9.0–11.0, N 0.12–0.20, Si 1.00–2.00, Ce 0.03–0.08. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Caution thread: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number.
The table below reproduces public BSSA EN 10296-2 chemical limits for 1.4818 / X6CrNiSiNCe19-10, cross-checked against the EN 10296-2:2005 grade list. Values are maximum unless a range is shown. Commercial talk still says 153MA / Ce-Si-N 19-10, but only the steel-number cast windows below belong on the MTC for this austenitic heat-resisting welded tube. Weld thread: matching heat-resisting fillers; control dilution from leaner 18-8 shop stock.
| Steel | C | Si | Mn | P | S | Cr | Ni | N | Ce |
|---|---|---|---|---|---|---|---|---|---|
| 1.4818 / X6CrNiSiNCe19-10 | 0.04–0.08 | 1.00–2.00 | ≤1.00 | ≤0.045 | ≤0.015 | 18.0–20.0 | 9.0–11.0 | 0.12–0.20 | 0.03–0.08 |
Mechanical Properties of EN 10296-2 1.4818
Ambient mechanical properties for EN 10296-2 1.4818 follow Tables 4–5 by family (wall thickness ≤30 mm framing for Table 4 corrosion-resisting grades). For this grade the delivery-condition floors to watch are: Rp0.2 min 290 MPa, Rp1.0 min 330 MPa, Rm min 600 MPa, longitudinal elongation min 40%. Intergranular corrosion resistance per EN ISO 3651-2 is tabulated where applicable — see the IGC column on the mechanical table below. Caution thread: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 290 | 330 | 600 min | 40 | 40 | N/A |
Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4818 / X6CrNiSiNCe19-10. Guideline solution/anneal band (Annex B): 1020–1120 °C; cooling: water, air or gas.
Welded Tube Manufacture for EN 10296-2 1.4818
EN 10296-2 does not offer a seamless route for 1.4818. Tube in X6CrNiSiNCe19-10 is made by longitudinal welding of strip or plate edges, then solution annealed (+AT) to meet Table 5 heat-resisting mechanical floors. For 1.4818, SHH STEEL aligns the Annex A symbol to the duty: W0 for as-welded economy, W1A/W2A for descaled engineering tube, W2R/WCR for brighter OD, and WG/WP when a measured roughness target is part of the order text. Size context for 1.4818: mid high-temp welded OD on +AT routes.
Austenitic heat-resisting 1.4818 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1020–1120 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. High-temperature service still needs fabricator WPS discipline on site joints after the mill seam. Corrosion thread: Ce-Si-N for adherent oxide scales at elevated temperature; not filed for aqueous IGC tables.
State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4818. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Size context for 1.4818: mid high-temp welded OD on +AT routes.
Dimensions and Tolerances for EN 10296-2 1.4818
Order EN 10296-2 1.4818 by outside diameter D and wall thickness T for steel name X6CrNiSiNCe19-10. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Mid high-temp welded od on +at routes. Corrosion thread: Ce-Si-N for adherent oxide scales at elevated temperature; not filed for aqueous IGC tables.
Tolerance classes on diameter and wall follow the EN 10296-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Use thread: heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry.
Equivalent Grades for EN 10296-2 1.4818
Do not treat ASTM welded or seamless pages as drop-in equals for EN 10296-2 1.4818 / X6CrNiSiNCe19-10. Wall bases, mechanical tables, and optional tests differ. Body alias 153MA / Ce-Si-N 19-10 is fine in BOM notes; H1 and order line stay on the steel number. Compare 1.4835, 1.4828, 1.4301 when the medium outgrows this analysis. Corrosion thread: Ce-Si-N for adherent oxide scales at elevated temperature; not filed for aqueous IGC tables.
Heat Treatment and Delivery Condition for EN 10296-2 1.4818
Austenitic heat-resisting 1.4818 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1020–1120 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Role reminder while setting HT: Ce-Si-N microalloyed 19-10 heat-resisting welded tube for high-temp oxidising mechanical service Family filing for 1.4818 is austenitic heat-resisting.
Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4818, restore the delivery condition agreed on the order before corrosive or load-bearing service. Duty thread: Ce-Si-N microalloyed 19-10 heat-resisting welded tube for high-temp oxidising mechanical service.
Corrosion Resistance of EN 10296-2 1.4818
153MA / Ce-Si-N 19-10-family marketing claims do not override EN 10296-2 tabulated IGC notes for 1.4818. Corrosion thread: Ce-Si-N for adherent oxide scales at elevated temperature; not filed for aqueous IGC tables. Move to sisters 1.4835, 1.4828, 1.4301 when the medium outgrows this analysis.
SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4818. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Size context for 1.4818: mid high-temp welded OD on +AT routes.
Applications of EN 10296-2 1.4818 Tube
Typical field use for 153MA / Ce-Si-N 19-10-named welded tube under steel number 1.4818: heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry. Keep pressure seamless talk on EN 10216-5 pages when that standard is the regulatory home. Filler/shop note for 1.4818: matching heat-resisting fillers; control dilution from leaner 18-8 shop stock.
Skip 1.4818 when the specification locks a different family — for example forcing ferritic 1.4818 into severe chloride process duty, or forcing a heat-resisting number into aqueous chloride service. Sister conversation inside EN 10296-2: 1.4835, 1.4828, 1.4301. Caution thread: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number.
Weldability of EN 10296-2 1.4818
Weldability of EN 10296-2 1.4818 covers both the mill longitudinal seam and downstream fabricator joints. Practical shop note: matching heat-resisting fillers; control dilution from leaner 18-8 shop stock. Caution that shapes WPS choices: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number Primary application sketch: heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry.
Filler selection should match or over-alloy the base X6CrNiSiNCe19-10 chemistry as the WPS demands. Heat input, interpass temperature, and shielding practice follow the family — austenitic, ferritic, duplex, or heat-resisting — not a single shop habit. Duty thread: Ce-Si-N microalloyed 19-10 heat-resisting welded tube for high-temp oxidising mechanical service.
Surface Finishes for EN 10296-2 1.4818
For 1.4818, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Caution thread: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number.
For 1.4818, export and coastal routes need extra wrap discipline on W*R/WCR/WG/WP finishes. Size context: mid high-temp welded OD on +AT routes. SHH STEEL confirms sleeve, paper, or plastic protection against the ordered Annex A symbol before dispatch.
Inspection and Testing for EN 10296-2 1.4818
NDT and technological-test intensity on 1.4818 is Option-driven under EN 10296-2 — leak, flattening, drift expanding, bend, or NDT methods are selected at enquiry. That is a different framing from EN 10217-7 pressure categories; copy the Options you need. Caution thread: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number.
Inspection intensity on 1.4818 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: Ce-Si-N microalloyed 19-10 heat-resisting welded tube for high-temp oxidising mechanical service. Primary application sketch: heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry.
Packaging and Shipping for EN 10296-2 1.4818
Export packing for 1.4818 / X6CrNiSiNCe19-10 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavier descaled bundles use spacers to stop fretting in transit. Use thread: heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry.
For 1.4818, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Size context for 1.4818: mid high-temp welded OD on +AT routes.
Export packing lists for 1.4818 / X6CrNiSiNCe19-10 cross-reference heat numbers to bundle IDs so the EN 10204 3.1 document matches without opening every crate. SHH STEEL aligns packaging with the order text before dispatch and can photograph bundle marks on request for project files that still say 153MA / Ce-Si-N 19-10 in the email subject. Use thread: heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry.
Why Choose SHH STEEL
SHH STEEL can produce and supply X6CrNiSiNCe19-10 as EN 10296-2 1.4818 welded tube with honest scope boundaries. General engineering welded acceptance is what this page sells; pressure welded, seamless pressure, and seamless general-purpose sisters are separate standards with separate MTCs. Weld thread: matching heat-resisting fillers; control dilution from leaner 18-8 shop stock.
Grade advice for 1.4818 stays practical. If the duty needs a sister chemistry, we point to 1.4835, 1.4828, 1.4301. Design caution for this number: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Family filing for 1.4818 is austenitic heat-resisting.
Supply Capability
Supply capability for 1.4818 / X6CrNiSiNCe19-10 is enquiry-led: SHH STEEL can produce and supply welded general-purpose tube with the Annex A finish and +AR/+A/+AT condition you name. Size hint: mid high-temp welded OD on +AT routes. Primary application sketch: heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry.
| Item | Capability |
|---|---|
| Standard | EN 10296-2:2005 welded general-purpose |
| Steel | 1.4818 / X6CrNiSiNCe19-10 |
| Product form | Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–12.7 mm within welded family practice (other by agreement) |
Stock / Available sizes
Stock / Available sizes for 1.4818 means RFQ bands, not published tonnages. Typical conversation starts around commodity-to-process welded OD with walls suited to austenitic heat-resisting practice. Alias on emails may still say 153MA / Ce-Si-N 19-10; the acknowledgement must say 1.4818. Caution thread: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number.
When the project needs both decorative WP and engineering W2A on 1.4818, say so up front — finishing slots differ. Apps that usually drive the mix: heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry. Family filing for 1.4818 is austenitic heat-resisting.
FAQ
-
What is EN 10296-2 1.4818 welded stainless steel tube used for?
- EN 10296-2 1.4818 (X6CrNiSiNCe19-10) is welded tube for mechanical and general engineering — heat-treatment fixtures, furnace-adjacent mechanical lines, and mid-range oxidising service naming 153MA-class chemistry. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: Ce-Si-N microalloyed 19-10 heat-resisting welded tube for high-temp oxidising mechanical service.
-
Is EN 10296-2 1.4818 the same as EN 10216-5 1.4818?
- Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4818 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4818 / X6CrNiSiNCe19-10?
- Delivery framing for 1.4818 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1020–1120 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4818?
- SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4818 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4818 compare with sister grades 1.4835, 1.4828, 1.4301?
- 1.4818 / X6CrNiSiNCe19-10 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4835, 1.4828, 1.4301. Design caution: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
How should fabricators weld EN 10296-2 1.4818 tube on site?
- 1.4818 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: matching heat-resisting fillers; control dilution from leaner 18-8 shop stock. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4818?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10296-2 1.4818?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4818 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: mid high-temp welded OD on +AT routes. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 153MA / Ce-Si-N 19-10 belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 153MA / Ce-Si-N 19-10 in body text and BOM notes, but lock EN 10296-2 and 1.4818 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4818?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: heat-resisting microalloyed grade — aqueous chloride process belongs on corrosion-resisting sisters, not this heat number Sister pointers: 1.4835, 1.4828, 1.4301. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10296-2 1.4818 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4818 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10296-2 1.4818 (X6CrNiSiNCe19-10) is welded stainless tube for mechanical and general engineering — Ce-Si-N microalloyed 19-10 heat-resisting welded tube for high-temp oxidising mechanical service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4835, 1.4828, 1.4301. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.