EN 10296-2 1.4439 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4439 Welded Stainless Steel Tube

EN 10296-2 1.4439 / X2CrNiMoN17-13-5 welded stainless general-purpose tube (317LMN), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 285 MPa, Rm min 580 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4439 / X2CrNiMoN17-13-5 (317LMN — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4439 Welded Stainless Steel Tube

If the purchase file still names only a commercial alias such as 317LMN without a product standard, the mill cannot know whether general-purpose welded acceptance or pressure-tube acceptance applies. EN 10296-2 plus steel number 1.4439 (X2CrNiMoN17-13-5) selects welded tube for mechanical and general engineering. EN 10296-2 1.4439 puts X2CrNiMoN17-13-5 on welded general-purpose tube when 316L failed the last chloride job but 6Mo is still under debate. Filler/shop note for 1.4439: 317L/higher-Mo fillers; strict purge and heat-input control; avoid carbon contamination on fabricator joints.

SHH STEEL can produce and supply EN 10296-2 1.4439 welded stainless steel tube — longitudinal welded from strip or plate on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, flattening, drift expanding, bend, and non-destructive testing Options). Duty thread: 5%Mo nitrogen-bearing austenitic welded tube (317LMN-class) bridging commodity 316L and 6Mo alloys.

On the shop floor people still say “317LMN tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4439, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: 5%Mo nitrogen-bearing austenitic welded tube (317LMN-class) bridging commodity 316L and 6Mo alloys. Typical duties include severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube. Design caution: bridge alloy — confirm whether 1.4547 or superduplex is the real seawater crevice answer before stopping at 1.4439 Primary application sketch: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube.

Scope discipline matters: 1.4439 under EN 10296-2 is welded general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube.

Inside this welded general-purpose series, compare EN 10296-2 1.4435, EN 10296-2 1.4539, EN 10296-2 1.4547. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4439.

Chemical Composition of EN 10296-2 1.4439

Buying 317LMN-family welded tube without locking 1.4439 invites silent chemistry drift. Under EN 10296-2 the cast must satisfy X2CrNiMoN17-13-5; highlight elements for this grade include C ≤0.030, Cr 16.5–18.5, Ni 12.5–14.5, Mo 4.0–5.0, N 0.12–0.22, Si ≤1.00. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Weld thread: 317L/higher-Mo fillers; strict purge and heat-input control; avoid carbon contamination on fabricator joints.

Use the cast table for 1.4439 as the contractual chemistry window for welded general-purpose duty — role reminder: 5%Mo nitrogen-bearing austenitic welded tube (317LMN-class) bridging commodity 316L and 6Mo alloys. Do not substitute a sister analysis from 1.4435, 1.4539, 1.4547 without rewriting the steel number on the order. Primary application sketch: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube.

Steel C Si Mn P S Cr Mo Ni N
1.4439 / X2CrNiMoN17-13-5 ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.015 16.5–18.5 4.0–5.0 12.5–14.5 0.12–0.22

Mechanical Properties of EN 10296-2 1.4439

Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4439 order. General-purpose Table values for this number read: Rp0.2 min 285 MPa, Rp1.0 min 315 MPa, Rm min 580 MPa, longitudinal elongation min 35%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Duty thread: 5%Mo nitrogen-bearing austenitic welded tube (317LMN-class) bridging commodity 316L and 6Mo alloys.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 285 315 580 min 35 30 Yes

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4439 / X2CrNiMoN17-13-5. Guideline solution/anneal band (Annex B): 1060–1140 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4439

EN 10296-2 does not offer a seamless route for 1.4439. Tube in X2CrNiMoN17-13-5 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. Order EN 10296-2 1.4439 with an Annex A surface/process symbol — W0 when as-welded is acceptable, W1A/W2A for metallically clean heat-treated descaled tube, W1R/W2R when bright heat treatment is required, WCA/WCR when the weld must be scarcely recognizable, and WG/WP when ground or polished roughness is written into the purchase order. Corrosion thread: Mo 4–5% plus nitrogen for pitting resistance well above 316L in many chloride media.

For austenitic 1.4439, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4439 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1060–1140 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Caution thread: bridge alloy — confirm whether 1.4547 or superduplex is the real seawater crevice answer before stopping at 1.4439.

Optional tests under EN 10296-2 for 1.4439 include leak testing, flattening, drift expanding, bend testing, and NDT agreed at enquiry. SHH STEEL records the Options actually performed on the inspection document — we do not claim a test that was not run. Caution thread: bridge alloy — confirm whether 1.4547 or superduplex is the real seawater crevice answer before stopping at 1.4439.

Dimensions and Tolerances for EN 10296-2 1.4439

Order EN 10296-2 1.4439 by outside diameter D and wall thickness T for steel name X2CrNiMoN17-13-5. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Process welded od for severe chloride catalogues, often w2a/wca +at. Duty thread: 5%Mo nitrogen-bearing austenitic welded tube (317LMN-class) bridging commodity 316L and 6Mo alloys.

Length supply for 1.4439 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Weld thread: 317L/higher-Mo fillers; strict purge and heat-input control; avoid carbon contamination on fabricator joints.

Equivalent Grades for EN 10296-2 1.4439

1.4439 / X2CrNiMoN17-13-5 is the EN 10296-2 designation for this chemistry as welded general-purpose tube. Commercial alias 317LMN appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this welded general-purpose series, compare sisters 1.4435, 1.4539, 1.4547. Hook for buyers still using only the 317LMN alias: lock EN 10296-2 1.4439 on the order line. Size context for 1.4439: process welded OD for severe chloride catalogues, often W2A/WCA +AT.

Heat Treatment and Delivery Condition for EN 10296-2 1.4439

Austenitic 1.4439 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1060–1140 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Apps that usually decide +AT versus +AR for this number: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube. Primary application sketch: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube.

Hot-working temperature bands in Annex B for X2CrNiMoN17-13-5 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Corrosion thread: Mo 4–5% plus nitrogen for pitting resistance well above 316L in many chloride media.

Corrosion Resistance of EN 10296-2 1.4439

Corrosion behaviour of EN 10296-2 1.4439 tracks its austenitic corrosion-resisting balance: Mo 4–5% plus nitrogen for pitting resistance well above 316L in many chloride media. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: bridge alloy — confirm whether 1.4547 or superduplex is the real seawater crevice answer before stopping at 1.4439 Family filing for 1.4439 is austenitic corrosion-resisting.

SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4439. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Weld thread: 317L/higher-Mo fillers; strict purge and heat-input control; avoid carbon contamination on fabricator joints.

Applications of EN 10296-2 1.4439 Tube

Typical field use for 317LMN-named welded tube under steel number 1.4439: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube. Keep pressure seamless talk on EN 10216-5 pages when that standard is the regulatory home. Filler/shop note for 1.4439: 317L/higher-Mo fillers; strict purge and heat-input control; avoid carbon contamination on fabricator joints.

Typical BOM language pairs EN 10296-2 1.4439 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “317LMN” substitutions do not creep in. Corrosion thread: Mo 4–5% plus nitrogen for pitting resistance well above 316L in many chloride media.

Weldability of EN 10296-2 1.4439

Weldability of EN 10296-2 1.4439 covers both the mill longitudinal seam and downstream fabricator joints. Practical shop note: 317L/higher-Mo fillers; strict purge and heat-input control; avoid carbon contamination on fabricator joints. Caution that shapes WPS choices: bridge alloy — confirm whether 1.4547 or superduplex is the real seawater crevice answer before stopping at 1.4439 Family filing for 1.4439 is austenitic corrosion-resisting.

When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Corrosion thread: Mo 4–5% plus nitrogen for pitting resistance well above 316L in many chloride media.

Surface Finishes for EN 10296-2 1.4439

For 1.4439, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Weld thread: 317L/higher-Mo fillers; strict purge and heat-input control; avoid carbon contamination on fabricator joints.

For 1.4439, export and coastal routes need extra wrap discipline on W*R/WCR/WG/WP finishes. Size context: process welded OD for severe chloride catalogues, often W2A/WCA +AT. SHH STEEL confirms sleeve, paper, or plastic protection against the ordered Annex A symbol before dispatch.

Inspection and Testing for EN 10296-2 1.4439

SHH STEEL EN 10204 3.1 documents for 1.4439 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a leak-test or NDT line unless that Option was executed. Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube.

Inspection intensity on 1.4439 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: 5%Mo nitrogen-bearing austenitic welded tube (317LMN-class) bridging commodity 316L and 6Mo alloys. Family filing for 1.4439 is austenitic corrosion-resisting.

Packaging and Shipping for EN 10296-2 1.4439

Finished EN 10296-2 1.4439 (X2CrNiMoN17-13-5) welded tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (W*R/WCR/WG/WP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Size context for 1.4439: process welded OD for severe chloride catalogues, often W2A/WCA +AT.

Marking typically includes manufacturer identity, dimensions, EN 10296-2, steel name or number 1.4439, cast/code, inspection mark, delivery-condition symbol, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging bright or polished surfaces. Corrosion thread: Mo 4–5% plus nitrogen for pitting resistance well above 316L in many chloride media.

For 1.4439, packing-list discipline matters when multiple sisters (1.4435, 1.4539, 1.4547) ship on the same vessel — wrong bundle cards create wrong field installs. SHH STEEL can produce and supply photographed mark sets when the EPC file demands them. Size context for 1.4439: process welded OD for severe chloride catalogues, often W2A/WCA +AT.

Why Choose SHH STEEL

SHH STEEL can produce and supply X2CrNiMoN17-13-5 as EN 10296-2 1.4439 welded tube with honest scope boundaries. General engineering welded acceptance is what this page sells; pressure welded, seamless pressure, and seamless general-purpose sisters are separate standards with separate MTCs. Weld thread: 317L/higher-Mo fillers; strict purge and heat-input control; avoid carbon contamination on fabricator joints.

SHH STEEL will not stretch X2CrNiMoN17-13-5 into a medium it cannot defend. Typical right-fit duties: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube. When those duties slip toward a sister, we say so before the quote hardens. Family filing for 1.4439 is austenitic corrosion-resisting.

Supply Capability

SHH STEEL can make and supply 317LMN-family chemistry only when the order locks EN 10296-2 and steel number 1.4439. Capability below is an RFQ map for X2CrNiMoN17-13-5, not a promise that every OD×wall sits in a Shanghai rack tonight. Caution thread: bridge alloy — confirm whether 1.4547 or superduplex is the real seawater crevice answer before stopping at 1.4439.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4439 / X2CrNiMoN17-13-5
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

Stock / Available sizes for 1.4439 means RFQ bands, not published tonnages. Typical conversation starts around commodity-to-process welded OD with walls suited to austenitic corrosion-resisting practice. Alias on emails may still say 317LMN; the acknowledgement must say 1.4439. Corrosion thread: Mo 4–5% plus nitrogen for pitting resistance well above 316L in many chloride media.

Cut lengths, special ends, IGC Options, and dual enquiries against 1.4435, 1.4539, 1.4547 on the same size list are routine for 1.4439. Peer mill catalogues only sanity-check typical OD × wall bands — acceptance remains EN 10296-2 with dimensional agreements stated on the order. SHH STEEL can produce and supply trial lengths before a production heat when the project schedule allows. Caution thread: bridge alloy — confirm whether 1.4547 or superduplex is the real seawater crevice answer before stopping at 1.4439.

FAQ

What is EN 10296-2 1.4439 welded stainless steel tube used for?
EN 10296-2 1.4439 (X2CrNiMoN17-13-5) is welded tube for mechanical and general engineering — severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry on welded tube. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: 5%Mo nitrogen-bearing austenitic welded tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Is EN 10296-2 1.4439 the same as EN 10216-5 1.4439?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4439 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4439 / X2CrNiMoN17-13-5?
Delivery framing for 1.4439 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1060–1140 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4439?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4439 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4439 compare with sister grades 1.4435, 1.4539, 1.4547?
1.4439 / X2CrNiMoN17-13-5 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4435, 1.4539, 1.4547. Design caution: bridge alloy — confirm whether 1.4547 or superduplex is the real seawater crevice answer before stopping at 1.4439 Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4439 tube on site?
1.4439 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 317L/higher-Mo fillers; strict purge and heat-input control; avoid carbon contamination on fabricator joints. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4439?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4439?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4439 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: process welded OD for severe chloride catalogues, often W2A/WCA +AT. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 317LMN belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 317LMN in body text and BOM notes, but lock EN 10296-2 and 1.4439 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4439?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: bridge alloy — confirm whether 1.4547 or superduplex is the real seawater crevice answer before stopping at 1.4439 Sister pointers: 1.4435, 1.4539, 1.4547. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4439 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4439 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4439 (X2CrNiMoN17-13-5) is welded stainless tube for mechanical and general engineering — 5%Mo nitrogen-bearing austenitic welded tube (317LMN-class) bridging commodity 316L and 6Mo alloys. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4435, 1.4539, 1.4547. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X