EN 10296-2 1.4311 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4311 Welded Stainless Steel Tube

EN 10296-2 1.4311 / X2CrNiN18-10 welded stainless general-purpose tube (304LN), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 270 MPa, Rm min 550 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4311 / X2CrNiN18-10 (304LN — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4311 Welded Stainless Steel Tube

If the purchase file still names only a commercial alias such as 304LN without a product standard, the mill cannot know whether general-purpose welded acceptance or pressure-tube acceptance applies. EN 10296-2 plus steel number 1.4311 (X2CrNiN18-10) selects welded tube for mechanical and general engineering. When design stress outgrows 1.4307 but the medium is still Mo-free 18-8 territory, EN 10296-2 1.4311 puts 304LN chemistry on welded general-purpose tube. Primary application sketch: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion.

SHH STEEL can produce and supply X2CrNiN18-10 under EN 10296-2 1.4311 as welded tube for mechanical and general engineering — not as a silent dual of EN 10217-7 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Caution thread: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter.

On the shop floor people still say “304LN tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4311, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: nitrogen-strengthened low-carbon 18-8 welded tube needing higher proof strength than 1.4307 without jumping to duplex. Typical duties include higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion. Design caution: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter Filler/shop note for 1.4311: 308L-class fillers; watch nitrogen dilution and ferrite balance on fabricator joints.

EN 10296-2 is welded product only for this series. When a seamless general-purpose twin is required, look to EN 10297-2 rather than forcing a seamless claim onto a 10296-2 order. When PED pressure welded acceptance is mandatory, use EN 10217-7 for the same chemistry family where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion.

Inside this welded general-purpose series, compare EN 10296-2 1.4307, EN 10296-2 1.4301, EN 10296-2 1.4318. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4311. ASTM/ASME related product pages (not interchangeable by default): A269 TP304L.

Chemical Composition of EN 10296-2 1.4311

Cast analysis for EN 10296-2 1.4311 follows the X2CrNiN18-10 limits published for this standard’s corrosion- or heat-resisting tables. Key windows on a typical certificate include C ≤0.030, Cr 17.0–19.5, Ni 8.5–11.5, N 0.12–0.22, Si ≤1.00, S ≤0.015. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Corrosion thread: nitrogen raises proof strength while low carbon supports as-welded IGC; pitting still tracks Mo-free 18-8.

Chemical limits for 1.4311 / X2CrNiN18-10 under EN 10296-2 appear in the table underneath. Source priority is BSSA’s EN 10296-2 article cross-checked to the 2005 grade list. If your client specification cites a different edition footnote for 304LN-family welded tube, send it before the heat is melted. Caution thread: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter.

Steel C Si Mn P S Cr Ni N
1.4311 / X2CrNiN18-10 ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.015 17.0–19.5 8.5–11.5 0.12–0.22

Mechanical Properties of EN 10296-2 1.4311

Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4311 order. General-purpose Table values for this number read: Rp0.2 min 270 MPa, Rp1.0 min 305 MPa, Rm min 550 MPa, longitudinal elongation min 35%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Caution thread: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 270 305 550 min 35 30 Yes

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4311 / X2CrNiN18-10. Guideline solution/anneal band (Annex B): 1000–1100 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4311

EN 10296-2 does not offer a seamless route for 1.4311. Tube in X2CrNiN18-10 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. Welded manufacture for 1.4311 finishes through hot- or cold-rolled strip/plate routes in Table A.1. Pick W1/W2 families for descaled engineering surfaces, W*R for bright anneal atmospheres, and WG or WP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Size context for 1.4311: commodity-to-mid process welded OD where thinner walls need higher proof floors.

For austenitic 1.4311, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4311 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1000–1100 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Corrosion thread: nitrogen raises proof strength while low carbon supports as-welded IGC; pitting still tracks Mo-free 18-8.

When dual documentation against EN 10217-7 is requested for the same 1.4311 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion.

Dimensions and Tolerances for EN 10296-2 1.4311

SHH STEEL aligns OD × wall, tolerance class, and process-route symbol for 1.4311 / X2CrNiN18-10 before strip forming and welding slots are locked. Commodity-to-mid process welded od where thinner walls need higher proof floors. Caution thread: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter.

For precision mechanical or decorative duty on 1.4311, cold-rolled W2/W2A/W2R and WCA/WCR routes are the usual conversation; heavier walls may start from hot-rolled strip. Agree bead-worked “b” suffixes when smoothed welds are mandatory. Caution thread: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter.

Equivalent Grades for EN 10296-2 1.4311

Equivalence talk for 1.4311 starts with X2CrNiN18-10: that is the EN steel name for welded general-purpose tube under this Part 2. Buyers who only write 304LN still need the steel number and EN 10296-2 on the PO. Sister grades often quoted alongside this duty: 1.4307, 1.4301, 1.4318. Design caution stays: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter Family filing for 1.4311 is austenitic corrosion-resisting.

Heat Treatment and Delivery Condition for EN 10296-2 1.4311

Austenitic 1.4311 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1000–1100 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Role reminder while setting HT: nitrogen-strengthened low-carbon 18-8 welded tube needing higher proof strength than 1.4307 without jumping to duplex Filler/shop note for 1.4311: 308L-class fillers; watch nitrogen dilution and ferrite balance on fabricator joints.

Hot-working temperature bands in Annex B for X2CrNiN18-10 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion.

Corrosion Resistance of EN 10296-2 1.4311

For 1.4311 / X2CrNiN18-10, read corrosion through the austenitic corrosion-resisting lens rather than a generic “stainless” slogan. Plain-language summary: nitrogen raises proof strength while low carbon supports as-welded IGC; pitting still tracks Mo-free 18-8. IGC Options follow EN ISO 3651-2 where the tables say Yes — and still do not replace medium-specific design. Caution: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter Family filing for 1.4311 is austenitic corrosion-resisting.

SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4311. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Weld thread: 308L-class fillers; watch nitrogen dilution and ferrite balance on fabricator joints.

Applications of EN 10296-2 1.4311 Tube

Typical field use for 304LN-named welded tube under steel number 1.4311: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion. Keep pressure seamless talk on EN 10216-5 pages when that standard is the regulatory home. Family filing for 1.4311 is austenitic corrosion-resisting.

It is the wrong first choice when a seamless product form is mandatory (use EN 10297-2 or EN 10216-5 as applicable), when PED pressure welded acceptance is locked to EN 10217-7 alone, or when the medium clearly needs a sister such as 1.4307. Size context for 1.4311: commodity-to-mid process welded OD where thinner walls need higher proof floors.

Weldability of EN 10296-2 1.4311

Even though 1.4311 is already a welded tube product, site joints still need a WPS matched to X2CrNiN18-10. Filler and heat-input guidance: 308L-class fillers; watch nitrogen dilution and ferrite balance on fabricator joints. Alias on the shop traveler may say 304LN; the WPS should cite the steel number. Primary application sketch: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter Filler/shop note for 1.4311: 308L-class fillers; watch nitrogen dilution and ferrite balance on fabricator joints.

Surface Finishes for EN 10296-2 1.4311

Interior Ra limits, electropolish, or special protection for X2CrNiN18-10 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4311 when the mill can measure and report the finish. Caution thread: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter.

Descaled 1.4311 engineering finishes still get caps and separators; bright X2CrNiN18-10 OD never rides bare under carbon-steel strapping. Packaging notes on the order should repeat the Annex A symbol so warehouse staff do not treat every bundle as the same 304LN commodity. Duty thread: nitrogen-strengthened low-carbon 18-8 welded tube needing higher proof strength than 1.4307 without jumping to duplex.

Inspection and Testing for EN 10296-2 1.4311

Specific inspection applies to EN 10296-2 1.4311 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Corrosion thread: nitrogen raises proof strength while low carbon supports as-welded IGC; pitting still tracks Mo-free 18-8.

Inspection intensity on 1.4311 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: nitrogen-strengthened low-carbon 18-8 welded tube needing higher proof strength than 1.4307 without jumping to duplex. Filler/shop note for 1.4311: 308L-class fillers; watch nitrogen dilution and ferrite balance on fabricator joints.

Packaging and Shipping for EN 10296-2 1.4311

Export packing for 1.4311 / X2CrNiN18-10 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavier descaled bundles use spacers to stop fretting in transit. Corrosion thread: nitrogen raises proof strength while low carbon supports as-welded IGC; pitting still tracks Mo-free 18-8.

When cut lengths and special ends are part of the 1.4311 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Weld thread: 308L-class fillers; watch nitrogen dilution and ferrite balance on fabricator joints.

For 1.4311, packing-list discipline matters when multiple sisters (1.4307, 1.4301, 1.4318) ship on the same vessel — wrong bundle cards create wrong field installs. SHH STEEL can produce and supply photographed mark sets when the EPC file demands them. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10296-2 1.4311 as welded general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “304LN tube” label on whatever is in the rack. We keep pressure talk honest: when PED welded pressure acceptance is required, we point you to EN 10217-7 for the same chemistry family where it exists. Corrosion thread: nitrogen raises proof strength while low carbon supports as-welded IGC; pitting still tracks Mo-free 18-8.

Why this mill page exists: honest EN 10296-2 1.4311 welded supply with Annex A and delivery-condition clarity — not a generic 304LN rack pull. Sisters on the same RFQ conversation: 1.4307, 1.4301, 1.4318. Caution thread: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter.

Supply Capability

Supply capability for 1.4311 / X2CrNiN18-10 is enquiry-led: SHH STEEL can produce and supply welded general-purpose tube with the Annex A finish and +AR/+A/+AT condition you name. Size hint: commodity-to-mid process welded OD where thinner walls need higher proof floors. Family filing for 1.4311 is austenitic corrosion-resisting.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4311 / X2CrNiN18-10
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

Stock / Available sizes for 1.4311 means RFQ bands, not published tonnages. Typical conversation starts around commodity-to-process welded OD with walls suited to austenitic corrosion-resisting practice. Alias on emails may still say 304LN; the acknowledgement must say 1.4311. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion.

Cut lengths, special ends, IGC Options, and dual enquiries against 1.4307, 1.4301, 1.4318 on the same size list are routine for 1.4311. Peer mill catalogues only sanity-check typical OD × wall bands — acceptance remains EN 10296-2 with dimensional agreements stated on the order. SHH STEEL can produce and supply trial lengths before a production heat when the project schedule allows. Caution thread: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter.

FAQ

What is EN 10296-2 1.4311 welded stainless steel tube used for?
EN 10296-2 1.4311 (X2CrNiN18-10) is welded tube for mechanical and general engineering — higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects that still want 304L-family corrosion. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: nitrogen-strengthened low-carbon 18-8 welded tube needing higher proof strength than 1.4307 without jumping to duplex.
Is EN 10296-2 1.4311 the same as EN 10216-5 1.4311?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4311 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4311 / X2CrNiN18-10?
Delivery framing for 1.4311 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1000–1100 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4311?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4311 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4311 compare with sister grades 1.4307, 1.4301, 1.4318?
1.4311 / X2CrNiN18-10 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4307, 1.4301, 1.4318. Design caution: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4311 tube on site?
1.4311 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 308L-class fillers; watch nitrogen dilution and ferrite balance on fabricator joints. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4311?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4311?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4311 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: commodity-to-mid process welded OD where thinner walls need higher proof floors. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 304LN belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 304LN in body text and BOM notes, but lock EN 10296-2 and 1.4311 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4311?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: strength gain is not chloride PREN gain — Mo-free limits remain; duplex 1.4362/1.4462 when SCC and strength both matter Sister pointers: 1.4307, 1.4301, 1.4318. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4311 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4311 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4311 (X2CrNiN18-10) is welded stainless tube for mechanical and general engineering — nitrogen-strengthened low-carbon 18-8 welded tube needing higher proof strength than 1.4307 without jumping to duplex. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4307, 1.4301, 1.4318. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X