EN 10296-2 1.4404 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4404 Welded Stainless Steel Tube

EN 10296-2 1.4404 / X2CrNiMo17-12-2 welded stainless general-purpose tube (316L), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 190 MPa, Rm min 490 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4404 / X2CrNiMo17-12-2 (316L — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4404 Welded Stainless Steel Tube

Mechanical, decorative, and general engineering projects that need welded stainless tube under a European product standard look to EN 10296-2:2005 — Part 2 of EN 10296 — rather than a PED pressure Part 7 page or an ASTM tubing habit alone. 1.4404 / X2CrNiMo17-12-2 sits in the austenitic corrosion-resisting tables. If the file still says only “316L welded tube,” EN 10296-2 1.4404 selects X2CrNiMo17-12-2 under welded general-purpose acceptance — not EN 10217-7 pressure welded unless that standard is ordered. Filler/shop note for 1.4404: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2.

SHH STEEL can produce and supply X2CrNiMo17-12-2 under EN 10296-2 1.4404 as welded tube for mechanical and general engineering — not as a silent dual of EN 10217-7 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Duty thread: low-carbon Mo-bearing austenitic welded tube for chloride-bearing and chemical general engineering where 316L is the default.

On the shop floor people still say “316L tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4404, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: low-carbon Mo-bearing austenitic welded tube for chloride-bearing and chemical general engineering where 316L is the default. Typical duties include coastal utilities, brine-adjacent process lines, pharma and food lines with chloride sanitiser, and mechanical fabrications that still say “316L welded”. Design caution: commodity 2–2.5% Mo — move to 1.4435/1.4439, 904L, 6Mo, or duplex when chlorides, crevice geometry, and temperature outgrow 316L practice Family filing for 1.4404 is austenitic corrosion-resisting.

EN 10296-2 is welded product only for this series. When a seamless general-purpose twin is required, look to EN 10297-2 rather than forcing a seamless claim onto a 10296-2 order. When PED pressure welded acceptance is mandatory, use EN 10217-7 for the same chemistry family where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Use thread: coastal utilities, brine-adjacent process lines, pharma and food lines with chloride sanitiser, and mechanical fabrications that still say “316L welded”.

Inside this welded general-purpose series, compare EN 10296-2 1.4401, EN 10296-2 1.4571, EN 10296-2 1.4432, EN 10296-2 1.4435. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4404. ASTM/ASME related product pages (not interchangeable by default): A269 TP316L, A213 TP316L, A312 TP316L.

Chemical Composition of EN 10296-2 1.4404

Every 1.4404 heat under EN 10296-2 must meet the cast (ladle) analysis for X2CrNiMo17-12-2 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Size context for 1.4404: broad welded process and utility OD×wall, W2A/WCA common.

Use the cast table for 1.4404 as the contractual chemistry window for welded general-purpose duty — role reminder: low-carbon Mo-bearing austenitic welded tube for chloride-bearing and chemical general engineering where 316L is the default. Do not substitute a sister analysis from 1.4401, 1.4571, 1.4432, 1.4435 without rewriting the steel number on the order. Primary application sketch: coastal utilities, brine-adjacent process lines, pharma and food lines with chloride sanitiser, and mechanical fabrications that still say “316L welded”.

Steel C Si Mn P S Cr Mo Ni N
1.4404 / X2CrNiMo17-12-2 ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.015 16.5–18.5 2.00–2.50 10.0–13.0 ≤0.11

Mechanical Properties of EN 10296-2 1.4404

Ambient mechanical properties for EN 10296-2 1.4404 follow Tables 4–5 by family (wall thickness ≤30 mm framing for Table 4 corrosion-resisting grades). For this grade the delivery-condition floors to watch are: Rp0.2 min 190 MPa, Rp1.0 min 225 MPa, Rm min 490 MPa, longitudinal elongation min 40%. Intergranular corrosion resistance per EN ISO 3651-2 is tabulated where applicable — see the IGC column on the mechanical table below. Caution thread: commodity 2–2.5% Mo — move to 1.4435/1.4439, 904L, 6Mo, or duplex when chlorides, crevice geometry, and temperature outgrow 316L practice.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 190 225 490 min 40 30 Yes

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4404 / X2CrNiMo17-12-2. Guideline solution/anneal band (Annex B): 1030–1110 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4404

EN 10296-2 does not offer a seamless route for 1.4404. Tube in X2CrNiMo17-12-2 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. Welded manufacture for 1.4404 finishes through hot- or cold-rolled strip/plate routes in Table A.1. Pick W1/W2 families for descaled engineering surfaces, W*R for bright anneal atmospheres, and WG or WP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Size context for 1.4404: broad welded process and utility OD×wall, W2A/WCA common.

For austenitic 1.4404, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4404 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1030–1110 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: low-carbon Mo-bearing austenitic welded tube for chloride-bearing and chemical general engineering where 316L is the default.

When dual documentation against EN 10217-7 is requested for the same 1.4404 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 1.4404: broad welded process and utility OD×wall, W2A/WCA common.

Dimensions and Tolerances for EN 10296-2 1.4404

Dimensional orders for 1.4404 name OD × wall, length tolerance, delivery condition, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Broad welded process and utility od×wall, w2a/wca common. Weld thread: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2.

For precision mechanical or decorative duty on 1.4404, cold-rolled W2/W2A/W2R and WCA/WCR routes are the usual conversation; heavier walls may start from hot-rolled strip. Agree bead-worked “b” suffixes when smoothed welds are mandatory. Caution thread: commodity 2–2.5% Mo — move to 1.4435/1.4439, 904L, 6Mo, or duplex when chlorides, crevice geometry, and temperature outgrow 316L practice.

Equivalent Grades for EN 10296-2 1.4404

Do not treat ASTM welded or seamless pages as drop-in equals for EN 10296-2 1.4404 / X2CrNiMo17-12-2. Wall bases, mechanical tables, and optional tests differ. Body alias 316L is fine in BOM notes; H1 and order line stay on the steel number. Compare 1.4401, 1.4571, 1.4432, 1.4435 when the medium outgrows this analysis. Corrosion thread: Mo improves pitting and crevice resistance versus 304L in many chloride media; low carbon supports as-welded IGC.

Heat Treatment and Delivery Condition for EN 10296-2 1.4404

Austenitic 1.4404 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1030–1110 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Delivery framing on the certificate for 1.4404 should match the ordered +AR/+A/+AT symbol — alias 316L alone is not enough. Weld thread: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2.

Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4404, restore the delivery condition agreed on the order before corrosive or load-bearing service. Weld thread: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2.

Corrosion Resistance of EN 10296-2 1.4404

For 1.4404 / X2CrNiMo17-12-2, read corrosion through the austenitic corrosion-resisting lens rather than a generic “stainless” slogan. Plain-language summary: Mo improves pitting and crevice resistance versus 304L in many chloride media; low carbon supports as-welded IGC. IGC Options follow EN ISO 3651-2 where the tables say Yes — and still do not replace medium-specific design. Caution: commodity 2–2.5% Mo — move to 1.4435/1.4439, 904L, 6Mo, or duplex when chlorides, crevice geometry, and temperature outgrow 316L practice Filler/shop note for 1.4404: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2.

SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4404. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Corrosion thread: Mo improves pitting and crevice resistance versus 304L in many chloride media; low carbon supports as-welded IGC.

Applications of EN 10296-2 1.4404 Tube

Applications of EN 10296-2 1.4404 tube centre on mechanical, decorative, and general engineering rather than PED pressure shells: coastal utilities, brine-adjacent process lines, pharma and food lines with chloride sanitiser, and mechanical fabrications that still say “316L welded”. Role summary: low-carbon Mo-bearing austenitic welded tube for chloride-bearing and chemical general engineering where 316L is the default. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists and is live. Primary application sketch: coastal utilities, brine-adjacent process lines, pharma and food lines with chloride sanitiser, and mechanical fabrications that still say “316L welded”.

Skip 1.4404 when the specification locks a different family — for example forcing ferritic 1.4404 into severe chloride process duty, or forcing a heat-resisting number into aqueous chloride service. Sister conversation inside EN 10296-2: 1.4401, 1.4571, 1.4432, 1.4435. Caution thread: commodity 2–2.5% Mo — move to 1.4435/1.4439, 904L, 6Mo, or duplex when chlorides, crevice geometry, and temperature outgrow 316L practice.

Weldability of EN 10296-2 1.4404

1.4404 / X2CrNiMo17-12-2 arrives as a longitudinally welded product under EN 10296-2, and fabricators still add circumferential and attachment welds on mechanical assemblies. Shop guidance: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Family filing for 1.4404 is austenitic corrosion-resisting.

When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Size context for 1.4404: broad welded process and utility OD×wall, W2A/WCA common.

Surface Finishes for EN 10296-2 1.4404

Surface finish on EN 10296-2 1.4404 is carried by the Annex A symbol: W0 as-welded where permitted, W1A/W2A descaled heat-treated for general mechanical tube, W1R/W2R/WCR for brighter OD, WCA when the weld must be scarcely recognizable, and WG/WP when roughness is agreed at enquiry. Carbon-steel strapping must not contact the stainless surface. Corrosion thread: Mo improves pitting and crevice resistance versus 304L in many chloride media; low carbon supports as-welded IGC.

Special measures to protect 1.4404 / X2CrNiMo17-12-2 during delivery or storage may be agreed at enquiry. Bright and polished tubes take sleeve or paper wrap; descaled engineering finishes still need end caps and dry bundling so chloride-bearing dirt does not sit on the OD in transit — especially important for 316L-family decorative or hygienic OD. Corrosion thread: Mo improves pitting and crevice resistance versus 304L in many chloride media; low carbon supports as-welded IGC.

Inspection and Testing for EN 10296-2 1.4404

NDT and technological-test intensity on 1.4404 is Option-driven under EN 10296-2 — leak, flattening, drift expanding, bend, or NDT methods are selected at enquiry. That is a different framing from EN 10217-7 pressure categories; copy the Options you need. Duty thread: low-carbon Mo-bearing austenitic welded tube for chloride-bearing and chemical general engineering where 316L is the default.

Inspection intensity on 1.4404 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: low-carbon Mo-bearing austenitic welded tube for chloride-bearing and chemical general engineering where 316L is the default. Primary application sketch: coastal utilities, brine-adjacent process lines, pharma and food lines with chloride sanitiser, and mechanical fabrications that still say “316L welded”.

Packaging and Shipping for EN 10296-2 1.4404

Export packing for 1.4404 / X2CrNiMo17-12-2 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavier descaled bundles use spacers to stop fretting in transit. Weld thread: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2.

Marking typically includes manufacturer identity, dimensions, EN 10296-2, steel name or number 1.4404, cast/code, inspection mark, delivery-condition symbol, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging bright or polished surfaces. Corrosion thread: Mo improves pitting and crevice resistance versus 304L in many chloride media; low carbon supports as-welded IGC.

For 1.4404, packing-list discipline matters when multiple sisters (1.4401, 1.4571, 1.4432, 1.4435) ship on the same vessel — wrong bundle cards create wrong field installs. SHH STEEL can produce and supply photographed mark sets when the EPC file demands them. Use thread: coastal utilities, brine-adjacent process lines, pharma and food lines with chloride sanitiser, and mechanical fabrications that still say “316L welded”.

Why Choose SHH STEEL

SHH STEEL can produce and supply X2CrNiMo17-12-2 as EN 10296-2 1.4404 welded tube with honest scope boundaries. General engineering welded acceptance is what this page sells; pressure welded, seamless pressure, and seamless general-purpose sisters are separate standards with separate MTCs. Corrosion thread: Mo improves pitting and crevice resistance versus 304L in many chloride media; low carbon supports as-welded IGC.

Grade advice for 1.4404 stays practical. If the duty needs a sister chemistry, we point to 1.4401, 1.4571, 1.4432, 1.4435. Design caution for this number: commodity 2–2.5% Mo — move to 1.4435/1.4439, 904L, 6Mo, or duplex when chlorides, crevice geometry, and temperature outgrow 316L practice Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Filler/shop note for 1.4404: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2.

Supply Capability

Supply capability for 1.4404 / X2CrNiMo17-12-2 is enquiry-led: SHH STEEL can produce and supply welded general-purpose tube with the Annex A finish and +AR/+A/+AT condition you name. Size hint: broad welded process and utility OD×wall, W2A/WCA common. Family filing for 1.4404 is austenitic corrosion-resisting.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4404 / X2CrNiMo17-12-2
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

For X2CrNiMo17-12-2, tell us which Annex A symbol and whether +AT (or +A/+AR) is locked before we hold strip. Caution that shapes size choice: commodity 2–2.5% Mo — move to 1.4435/1.4439, 904L, 6Mo, or duplex when chlorides, crevice geometry, and temperature outgrow 316L practice Filler/shop note for 1.4404: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2.

Trial lengths of 1.4404 / X2CrNiMo17-12-2 help fabricators prove forming and weld procedures before a production heat. Sisters often sampled on the same RFQ: 1.4401, 1.4571, 1.4432, 1.4435. SHH STEEL can produce and supply those trials when strip slots allow. Corrosion thread: Mo improves pitting and crevice resistance versus 304L in many chloride media; low carbon supports as-welded IGC.

FAQ

What is EN 10296-2 1.4404 welded stainless steel tube used for?
EN 10296-2 1.4404 (X2CrNiMo17-12-2) is welded tube for mechanical and general engineering — coastal utilities, brine-adjacent process lines, pharma and food lines with chloride sanitiser, and mechanical fabrications that still say “316L welded”. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: low-carbon Mo-bearing austenitic welded tube for chloride-bearing and chemical general engineering where 316L is the default.
Is EN 10296-2 1.4404 the same as EN 10216-5 1.4404?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4404 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4404 / X2CrNiMo17-12-2?
Delivery framing for 1.4404 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1030–1110 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4404?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4404 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4404 compare with sister grades 1.4401, 1.4571, 1.4432?
1.4404 / X2CrNiMo17-12-2 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4401, 1.4571, 1.4432. Design caution: commodity 2–2.5% Mo — move to 1.4435/1.4439, 904L, 6Mo, or duplex when chlorides, crevice geometry, and temperature outgrow 316L practice Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4404 tube on site?
1.4404 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 316/316L-class fillers; purge and heat-input control on fabricator joints; mill seam already longitudinal under EN 10296-2. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4404?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4404?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4404 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: broad welded process and utility OD×wall, W2A/WCA common. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 316L belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 316L in body text and BOM notes, but lock EN 10296-2 and 1.4404 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4404?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: commodity 2–2.5% Mo — move to 1.4435/1.4439, 904L, 6Mo, or duplex when chlorides, crevice geometry, and temperature outgrow 316L practice Sister pointers: 1.4401, 1.4571, 1.4432. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4404 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4404 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4404 (X2CrNiMo17-12-2) is welded stainless tube for mechanical and general engineering — low-carbon Mo-bearing austenitic welded tube for chloride-bearing and chemical general engineering where 316L is the default. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4401, 1.4571, 1.4432. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X