EN 10296-2 1.4854 Welded Stainless Steel Tube
What is EN 10296-2 1.4854 Welded Stainless Steel Tube
Mechanical, decorative, and general engineering projects that need welded stainless tube under a European product standard look to EN 10296-2:2005 — Part 2 of EN 10296 — rather than a PED pressure Part 7 page or an ASTM tubing habit alone. 1.4854 / X6NiCrSiNCe35-25 sits in the austenitic heat-resisting tables. EN 10296-2 1.4854 is the welded general-purpose designation for X6NiCrSiNCe35-25 when 310S-class life is underspecified for the furnace dossier. Primary application sketch: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
SHH STEEL can produce and supply X6NiCrSiNCe35-25 under EN 10296-2 1.4854 as welded tube for mechanical and general engineering — not as a silent dual of EN 10217-7 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
On the shop floor people still say “353MA tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4854, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service. Typical duties include demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA. Design caution: patented/high-Ni heat-resisting grade — confirm availability and licensing notes at enquiry; not an aqueous chloride process first choice Family filing for 1.4854 is austenitic heat-resisting.
Do not treat an EN 10296-2 1.4854 MTC as automatic clearance for pressure equipment — EN 10217-7 is the welded pressure home. Likewise, seamless pressure tube lives under EN 10216-5 and seamless general-purpose under EN 10297-2. Match the product standard to the duty before dual-marking talk begins. Caution thread: patented/high-Ni heat-resisting grade — confirm availability and licensing notes at enquiry; not an aqueous chloride process first choice.
Inside this welded general-purpose series, compare EN 10296-2 1.4845, EN 10296-2 1.4835, EN 10296-2 1.4833. Hub: EN 10296-2.
Chemical Composition of EN 10296-2 1.4854
Buying 353MA-family welded tube without locking 1.4854 invites silent chemistry drift. Under EN 10296-2 the cast must satisfy X6NiCrSiNCe35-25; highlight elements for this grade include C 0.04–0.08, Cr 24.0–26.0, Ni 34.0–36.0, N 0.12–0.20, Si 1.20–2.00, Ce 0.03–0.08. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Size context for 1.4854: severe heat-service welded OD on +AT routes, often by agreement on heavier walls.
Use the cast table for 1.4854 as the contractual chemistry window for welded general-purpose duty — role reminder: Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service. Do not substitute a sister analysis from 1.4845, 1.4835, 1.4833 without rewriting the steel number on the order. Family filing for 1.4854 is austenitic heat-resisting.
| Steel | C | Si | Mn | P | S | Cr | Ni | N | Ce |
|---|---|---|---|---|---|---|---|---|---|
| 1.4854 / X6NiCrSiNCe35-25 | 0.04–0.08 | 1.20–2.00 | ≤2.00 | ≤0.040 | ≤0.015 | 24.0–26.0 | 34.0–36.0 | 0.12–0.20 | 0.03–0.08 |
Mechanical Properties of EN 10296-2 1.4854
Table mechanical floors for 1.4854 / X6NiCrSiNCe35-25 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 300 MPa, Rp1.0 min 340 MPa, Rm min 650 MPa, longitudinal elongation min 40%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Size context for 1.4854: severe heat-service welded OD on +AT routes, often by agreement on heavier walls.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 300 | 340 | 650 min | 40 | 40 | N/A |
Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4854 / X6NiCrSiNCe35-25. Guideline solution/anneal band (Annex B): 1100–1150 °C; cooling: water, air or gas.
Welded Tube Manufacture for EN 10296-2 1.4854
EN 10296-2 does not offer a seamless route for 1.4854. Tube in X6NiCrSiNCe35-25 is made by longitudinal welding of strip or plate edges, then solution annealed (+AT) to meet Table 5 heat-resisting mechanical floors. Annex A process-route symbols for welded 1.4854 include W0 (as-welded), W1/W1A/W1R (hot-rolled strip routes), W2/W2A/W2R (cold-rolled strip routes), WCA/WCR (cold-worked recrystallised weld), and WG/WP (ground/polished). Bead-worked conditions append “b” (for example W2Ab). Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Austenitic heat-resisting 1.4854 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1100–1150 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. High-temperature service still needs fabricator WPS discipline on site joints after the mill seam. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service.
When dual documentation against EN 10217-7 is requested for the same 1.4854 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service.
Dimensions and Tolerances for EN 10296-2 1.4854
Order EN 10296-2 1.4854 by outside diameter D and wall thickness T for steel name X6NiCrSiNCe35-25. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Severe heat-service welded od on +at routes, often by agreement on heavier walls. Size context for 1.4854: severe heat-service welded OD on +AT routes, often by agreement on heavier walls.
Length supply for 1.4854 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Corrosion thread: high Ni with Ce-Si-N for severe elevated-temperature oxidising and carburising-adjacent service.
Equivalent Grades for EN 10296-2 1.4854
Do not treat ASTM welded or seamless pages as drop-in equals for EN 10296-2 1.4854 / X6NiCrSiNCe35-25. Wall bases, mechanical tables, and optional tests differ. Body alias 353MA is fine in BOM notes; H1 and order line stay on the steel number. Compare 1.4845, 1.4835, 1.4833 when the medium outgrows this analysis. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Heat Treatment and Delivery Condition for EN 10296-2 1.4854
Austenitic heat-resisting 1.4854 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1100–1150 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Apps that usually decide +AT versus +AR for this number: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA. Family filing for 1.4854 is austenitic heat-resisting.
Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4854, restore the delivery condition agreed on the order before corrosive or load-bearing service. Size context for 1.4854: severe heat-service welded OD on +AT routes, often by agreement on heavier walls.
Corrosion Resistance of EN 10296-2 1.4854
353MA-family marketing claims do not override EN 10296-2 tabulated IGC notes for 1.4854. Corrosion thread: high Ni with Ce-Si-N for severe elevated-temperature oxidising and carburising-adjacent service. Move to sisters 1.4845, 1.4835, 1.4833 when the medium outgrows this analysis.
Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4845, 1.4835, 1.4833 when the medium outgrows this number rather than hoping surface finish alone will hold. Weld thread: 353MA-class / matching high-Ni heat-resisting fillers; strict cleanliness and heat-input control.
Applications of EN 10296-2 1.4854 Tube
Buyers pick EN 10296-2 1.4854 / X6NiCrSiNCe35-25 when the duty list looks like this: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA. That is welded general-purpose work — not a silent PED pressure shell. Role in one line: Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service. Primary application sketch: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Skip 1.4854 when the specification locks a different family — for example forcing ferritic 1.4854 into severe chloride process duty, or forcing a heat-resisting number into aqueous chloride service. Sister conversation inside EN 10296-2: 1.4845, 1.4835, 1.4833. Weld thread: 353MA-class / matching high-Ni heat-resisting fillers; strict cleanliness and heat-input control.
Weldability of EN 10296-2 1.4854
Even though 1.4854 is already a welded tube product, site joints still need a WPS matched to X6NiCrSiNCe35-25. Filler and heat-input guidance: 353MA-class / matching high-Ni heat-resisting fillers; strict cleanliness and heat-input control. Alias on the shop traveler may say 353MA; the WPS should cite the steel number. Family filing for 1.4854 is austenitic heat-resisting.
When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Caution thread: patented/high-Ni heat-resisting grade — confirm availability and licensing notes at enquiry; not an aqueous chloride process first choice.
Surface Finishes for EN 10296-2 1.4854
For 1.4854, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Weld thread: 353MA-class / matching high-Ni heat-resisting fillers; strict cleanliness and heat-input control.
Special measures to protect 1.4854 / X6NiCrSiNCe35-25 during delivery or storage may be agreed at enquiry. Bright and polished tubes take sleeve or paper wrap; descaled engineering finishes still need end caps and dry bundling so chloride-bearing dirt does not sit on the OD in transit — especially important for 353MA-family decorative or hygienic OD. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Inspection and Testing for EN 10296-2 1.4854
NDT and technological-test intensity on 1.4854 is Option-driven under EN 10296-2 — leak, flattening, drift expanding, bend, or NDT methods are selected at enquiry. That is a different framing from EN 10217-7 pressure categories; copy the Options you need. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service.
Inspection intensity on 1.4854 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service. Family filing for 1.4854 is austenitic heat-resisting.
Packaging and Shipping for EN 10296-2 1.4854
SHH STEEL ships EN 10296-2 1.4854 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled W1A/W2A engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service.
When cut lengths and special ends are part of the 1.4854 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Weld thread: 353MA-class / matching high-Ni heat-resisting fillers; strict cleanliness and heat-input control.
Export packing lists for 1.4854 / X6NiCrSiNCe35-25 cross-reference heat numbers to bundle IDs so the EN 10204 3.1 document matches without opening every crate. SHH STEEL aligns packaging with the order text before dispatch and can photograph bundle marks on request for project files that still say 353MA in the email subject. Weld thread: 353MA-class / matching high-Ni heat-resisting fillers; strict cleanliness and heat-input control.
Why Choose SHH STEEL
SHH STEEL can produce and supply X6NiCrSiNCe35-25 as EN 10296-2 1.4854 welded tube with honest scope boundaries. General engineering welded acceptance is what this page sells; pressure welded, seamless pressure, and seamless general-purpose sisters are separate standards with separate MTCs. Caution thread: patented/high-Ni heat-resisting grade — confirm availability and licensing notes at enquiry; not an aqueous chloride process first choice.
Grade advice for 1.4854 stays practical. If the duty needs a sister chemistry, we point to 1.4845, 1.4835, 1.4833. Design caution for this number: patented/high-Ni heat-resisting grade — confirm availability and licensing notes at enquiry; not an aqueous chloride process first choice Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Family filing for 1.4854 is austenitic heat-resisting.
Supply Capability
Supply capability for 1.4854 / X6NiCrSiNCe35-25 is enquiry-led: SHH STEEL can produce and supply welded general-purpose tube with the Annex A finish and +AR/+A/+AT condition you name. Size hint: severe heat-service welded OD on +AT routes, often by agreement on heavier walls. Primary application sketch: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
| Item | Capability |
|---|---|
| Standard | EN 10296-2:2005 welded general-purpose |
| Steel | 1.4854 / X6NiCrSiNCe35-25 |
| Product form | Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–12.7 mm within welded family practice (other by agreement) |
Stock / Available sizes
For X6NiCrSiNCe35-25, tell us which Annex A symbol and whether +AT (or +A/+AR) is locked before we hold strip. Caution that shapes size choice: patented/high-Ni heat-resisting grade — confirm availability and licensing notes at enquiry; not an aqueous chloride process first choice Primary application sketch: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Cut lengths, special ends, IGC Options, and dual enquiries against 1.4845, 1.4835, 1.4833 on the same size list are routine for 1.4854. Peer mill catalogues only sanity-check typical OD × wall bands — acceptance remains EN 10296-2 with dimensional agreements stated on the order. SHH STEEL can produce and supply trial lengths before a production heat when the project schedule allows. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
FAQ
-
What is EN 10296-2 1.4854 welded stainless steel tube used for?
- EN 10296-2 1.4854 (X6NiCrSiNCe35-25) is welded tube for mechanical and general engineering — demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service.
-
Is EN 10296-2 1.4854 the same as EN 10216-5 1.4854?
- Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4854 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4854 / X6NiCrSiNCe35-25?
- Delivery framing for 1.4854 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1100–1150 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4854?
- SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4854 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4854 compare with sister grades 1.4845, 1.4835, 1.4833?
- 1.4854 / X6NiCrSiNCe35-25 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4845, 1.4835, 1.4833. Design caution: patented/high-Ni heat-resisting grade — confirm availability and licensing notes at enquiry; not an aqueous chloride process first choice Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
How should fabricators weld EN 10296-2 1.4854 tube on site?
- 1.4854 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 353MA-class / matching high-Ni heat-resisting fillers; strict cleanliness and heat-input control. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4854?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10296-2 1.4854?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4854 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: severe heat-service welded OD on +AT routes, often by agreement on heavier walls. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 353MA belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 353MA in body text and BOM notes, but lock EN 10296-2 and 1.4854 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4854?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: patented/high-Ni heat-resisting grade — confirm availability and licensing notes at enquiry; not an aqueous chloride process first choice Sister pointers: 1.4845, 1.4835, 1.4833. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10296-2 1.4854 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4854 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10296-2 1.4854 (X6NiCrSiNCe35-25) is welded stainless tube for mechanical and general engineering — Ce-Si-N microalloyed high-Ni austenitic heat-resisting welded tube (353MA-class) for severe high-temperature service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4845, 1.4835, 1.4833. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.