EN 10296-2 1.4429 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4429 Welded Stainless Steel Tube

EN 10296-2 1.4429 / X2CrNiMoN17-13-3 welded stainless general-purpose tube (316LN), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 295 MPa, Rm min 580 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4429 / X2CrNiMoN17-13-3 (316LN — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4429 Welded Stainless Steel Tube

EN 10296-2 covers welded stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4429 is the austenitic corrosion-resisting grade X2CrNiMoN17-13-3, commercially discussed as 316LN. When design stress outgrows 1.4404 but the medium is still Mo-austenitic, EN 10296-2 1.4429 puts 316LN chemistry on welded general-purpose tube. Family filing for 1.4429 is austenitic corrosion-resisting.

SHH STEEL can make and supply EN 10296-2 1.4429 / X2CrNiMoN17-13-3 as welded general-purpose tube across process welded OD where thinner walls need higher proof floors with Mo corrosion, annealed or solution annealed as the grade tables and order require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Primary application sketch: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion.

On the shop floor people still say “316LN tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4429, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: nitrogen-strengthened Mo austenitic welded tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty. Typical duties include higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion. Design caution: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex Family filing for 1.4429 is austenitic corrosion-resisting.

Scope discipline matters: 1.4429 under EN 10296-2 is welded general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Weld thread: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints.

Inside this welded general-purpose series, compare EN 10296-2 1.4432, EN 10296-2 1.4404, EN 10296-2 1.4435. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4429. ASTM/ASME related product pages (not interchangeable by default): A269 TP316L.

Chemical Composition of EN 10296-2 1.4429

Buying 316LN-family welded tube without locking 1.4429 invites silent chemistry drift. Under EN 10296-2 the cast must satisfy X2CrNiMoN17-13-3; highlight elements for this grade include C ≤0.030, Cr 16.5–18.5, Ni 11.0–14.0, Mo 2.50–3.00, N 0.12–0.22, Si ≤1.00. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion.

Use the cast table for 1.4429 as the contractual chemistry window for welded general-purpose duty — role reminder: nitrogen-strengthened Mo austenitic welded tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty. Do not substitute a sister analysis from 1.4432, 1.4404, 1.4435 without rewriting the steel number on the order. Family filing for 1.4429 is austenitic corrosion-resisting.

Steel C Si Mn P S Cr Mo Ni N
1.4429 / X2CrNiMoN17-13-3 ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.015 16.5–18.5 2.50–3.00 11.0–14.0 0.12–0.22

Mechanical Properties of EN 10296-2 1.4429

Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4429 order. General-purpose Table values for this number read: Rp0.2 min 295 MPa, Rp1.0 min 330 MPa, Rm min 580 MPa, longitudinal elongation min 35%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Duty thread: nitrogen-strengthened Mo austenitic welded tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 295 330 580 min 35 30 Yes

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4429 / X2CrNiMoN17-13-3. Guideline solution/anneal band (Annex B): 1030–1110 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4429

EN 10296-2 does not offer a seamless route for 1.4429. Tube in X2CrNiMoN17-13-3 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. Welded manufacture for 1.4429 finishes through hot- or cold-rolled strip/plate routes in Table A.1. Pick W1/W2 families for descaled engineering surfaces, W*R for bright anneal atmospheres, and WG or WP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Weld thread: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints.

For austenitic 1.4429, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4429 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1030–1110 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion.

Optional tests under EN 10296-2 for 1.4429 include leak testing, flattening, drift expanding, bend testing, and NDT agreed at enquiry. SHH STEEL records the Options actually performed on the inspection document — we do not claim a test that was not run. Weld thread: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints.

Dimensions and Tolerances for EN 10296-2 1.4429

Dimensional orders for 1.4429 name OD × wall, length tolerance, delivery condition, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Process welded od where thinner walls need higher proof floors with mo corrosion. Caution thread: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex.

For precision mechanical or decorative duty on 1.4429, cold-rolled W2/W2A/W2R and WCA/WCR routes are the usual conversation; heavier walls may start from hot-rolled strip. Agree bead-worked “b” suffixes when smoothed welds are mandatory. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion.

Equivalent Grades for EN 10296-2 1.4429

Do not treat ASTM welded or seamless pages as drop-in equals for EN 10296-2 1.4429 / X2CrNiMoN17-13-3. Wall bases, mechanical tables, and optional tests differ. Body alias 316LN is fine in BOM notes; H1 and order line stay on the steel number. Compare 1.4432, 1.4404, 1.4435 when the medium outgrows this analysis. Weld thread: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints.

Heat Treatment and Delivery Condition for EN 10296-2 1.4429

Austenitic 1.4429 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1030–1110 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Delivery framing on the certificate for 1.4429 should match the ordered +AR/+A/+AT symbol — alias 316LN alone is not enough. Weld thread: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints.

Hot-working temperature bands in Annex B for X2CrNiMoN17-13-3 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Size context for 1.4429: process welded OD where thinner walls need higher proof floors with Mo corrosion.

Corrosion Resistance of EN 10296-2 1.4429

For 1.4429 / X2CrNiMoN17-13-3, read corrosion through the austenitic corrosion-resisting lens rather than a generic “stainless” slogan. Plain-language summary: Mo plus nitrogen for strength and pitting assist versus leaner 316L; still austenitic aqueous practice. IGC Options follow EN ISO 3651-2 where the tables say Yes — and still do not replace medium-specific design. Caution: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex Family filing for 1.4429 is austenitic corrosion-resisting.

Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4432, 1.4404, 1.4435 when the medium outgrows this number rather than hoping surface finish alone will hold. Duty thread: nitrogen-strengthened Mo austenitic welded tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Applications of EN 10296-2 1.4429 Tube

Buyers pick EN 10296-2 1.4429 / X2CrNiMoN17-13-3 when the duty list looks like this: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion. That is welded general-purpose work — not a silent PED pressure shell. Role in one line: nitrogen-strengthened Mo austenitic welded tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty. Filler/shop note for 1.4429: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints.

Typical BOM language pairs EN 10296-2 1.4429 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “316LN” substitutions do not creep in. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion.

Weldability of EN 10296-2 1.4429

Even though 1.4429 is already a welded tube product, site joints still need a WPS matched to X2CrNiMoN17-13-3. Filler and heat-input guidance: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints. Alias on the shop traveler may say 316LN; the WPS should cite the steel number. Primary application sketch: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion.

When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Caution thread: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex.

Surface Finishes for EN 10296-2 1.4429

For 1.4429, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion.

Descaled 1.4429 engineering finishes still get caps and separators; bright X2CrNiMoN17-13-3 OD never rides bare under carbon-steel strapping. Packaging notes on the order should repeat the Annex A symbol so warehouse staff do not treat every bundle as the same 316LN commodity. Caution thread: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex.

Inspection and Testing for EN 10296-2 1.4429

NDT and technological-test intensity on 1.4429 is Option-driven under EN 10296-2 — leak, flattening, drift expanding, bend, or NDT methods are selected at enquiry. That is a different framing from EN 10217-7 pressure categories; copy the Options you need. Corrosion thread: Mo plus nitrogen for strength and pitting assist versus leaner 316L; still austenitic aqueous practice.

For X2CrNiMoN17-13-3 under EN 10296-2, technological Options and IGC (where tabulated) belong on the enquiry checklist beside OD × wall. SHH STEEL correlates marking on 1.4429 bundles to the EN 10204 3.1 document so heat identity survives transit. Caution reminder: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex Family filing for 1.4429 is austenitic corrosion-resisting.

Packaging and Shipping for EN 10296-2 1.4429

Finished EN 10296-2 1.4429 (X2CrNiMoN17-13-3) welded tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (W*R/WCR/WG/WP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Corrosion thread: Mo plus nitrogen for strength and pitting assist versus leaner 316L; still austenitic aqueous practice.

When cut lengths and special ends are part of the 1.4429 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Corrosion thread: Mo plus nitrogen for strength and pitting assist versus leaner 316L; still austenitic aqueous practice.

For 1.4429, packing-list discipline matters when multiple sisters (1.4432, 1.4404, 1.4435) ship on the same vessel — wrong bundle cards create wrong field installs. SHH STEEL can produce and supply photographed mark sets when the EPC file demands them. Duty thread: nitrogen-strengthened Mo austenitic welded tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10296-2 1.4429 as welded general-purpose tube when you need a mill partner who will not blur EN 10296-2 with EN 10217-7 or EN 10216-5 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: nitrogen-strengthened Mo austenitic welded tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Grade advice for 1.4429 stays practical. If the duty needs a sister chemistry, we point to 1.4432, 1.4404, 1.4435. Design caution for this number: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Primary application sketch: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion.

Supply Capability

SHH STEEL can make and supply 316LN-family chemistry only when the order locks EN 10296-2 and steel number 1.4429. Capability below is an RFQ map for X2CrNiMoN17-13-3, not a promise that every OD×wall sits in a Shanghai rack tonight. Weld thread: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4429 / X2CrNiMoN17-13-3
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

For X2CrNiMoN17-13-3, tell us which Annex A symbol and whether +AT (or +A/+AR) is locked before we hold strip. Caution that shapes size choice: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex Family filing for 1.4429 is austenitic corrosion-resisting.

When the project needs both decorative WP and engineering W2A on 1.4429, say so up front — finishing slots differ. Apps that usually drive the mix: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion. Filler/shop note for 1.4429: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints.

FAQ

What is EN 10296-2 1.4429 welded stainless steel tube used for?
EN 10296-2 1.4429 (X2CrNiMoN17-13-3) is welded tube for mechanical and general engineering — higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall-optimisation projects that keep Mo austenitic corrosion. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: nitrogen-strengthened Mo austenitic welded tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.
Is EN 10296-2 1.4429 the same as EN 10216-5 1.4429?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4429 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4429 / X2CrNiMoN17-13-3?
Delivery framing for 1.4429 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1030–1110 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4429?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4429 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4429 compare with sister grades 1.4432, 1.4404, 1.4435?
1.4429 / X2CrNiMoN17-13-3 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4432, 1.4404, 1.4435. Design caution: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4429 tube on site?
1.4429 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 316LN/316L-class fillers; watch nitrogen and ferrite on fabricator joints. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4429?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4429?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4429 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: process welded OD where thinner walls need higher proof floors with Mo corrosion. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 316LN belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 316LN in body text and BOM notes, but lock EN 10296-2 and 1.4429 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4429?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: strength gain does not equal 6Mo PREN — severe seawater crevice duty still points to 1.4547 or superduplex Sister pointers: 1.4432, 1.4404, 1.4435. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4429 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4429 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4429 (X2CrNiMoN17-13-3) is welded stainless tube for mechanical and general engineering — nitrogen-strengthened Mo austenitic welded tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4432, 1.4404, 1.4435. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X