EN 10296-2 1.4547 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4547 Welded Stainless Steel Tube

EN 10296-2 1.4547 / X1CrNiMoCuN20-18-7 welded stainless general-purpose tube (254 SMO / 6Mo), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 300 MPa, Rm min 650 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4547 / X1CrNiMoCuN20-18-7 (254 SMO / 6Mo — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4547 Welded Stainless Steel Tube

If the purchase file still names only a commercial alias such as 254 SMO / 6Mo without a product standard, the mill cannot know whether general-purpose welded acceptance or pressure-tube acceptance applies. EN 10296-2 plus steel number 1.4547 (X1CrNiMoCuN20-18-7) selects welded tube for mechanical and general engineering. EN 10296-2 1.4547 is the welded general-purpose home for X1CrNiMoCuN20-18-7 when the chloride dossier outgrew 904L and commodity 316L. Primary application sketch: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product.

SHH STEEL can produce and supply X1CrNiMoCuN20-18-7 under EN 10296-2 1.4547 as welded tube for mechanical and general engineering — not as a silent dual of EN 10217-7 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Weld thread: 6Mo/over-alloyed nickel-base fillers as WPS demands; strict heat input and purge; no carbon-steel tooling contamination.

On the shop floor people still say “254 SMO / 6Mo tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4547, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service. Typical duties include seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product. Design caution: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier Primary application sketch: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product.

EN 10296-2 is welded product only for this series. When a seamless general-purpose twin is required, look to EN 10297-2 rather than forcing a seamless claim onto a 10296-2 order. When PED pressure welded acceptance is mandatory, use EN 10217-7 for the same chemistry family where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Caution thread: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier.

Inside this welded general-purpose series, compare EN 10296-2 1.4539, EN 10296-2 1.4439, EN 10296-2 1.4410. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4547.

Chemical Composition of EN 10296-2 1.4547

Every 1.4547 heat under EN 10296-2 must meet the cast (ladle) analysis for X1CrNiMoCuN20-18-7 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Caution thread: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier.

Use the cast table for 1.4547 as the contractual chemistry window for welded general-purpose duty — role reminder: 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service. Do not substitute a sister analysis from 1.4539, 1.4439, 1.4410 without rewriting the steel number on the order. Family filing for 1.4547 is austenitic corrosion-resisting.

Steel C Si Mn P S Cr Mo Ni Cu N
1.4547 / X1CrNiMoCuN20-18-7 ≤0.020 ≤0.70 ≤1.00 ≤0.030 ≤0.010 19.5–20.5 6.0–7.0 17.5–18.5 0.50–1.00 0.18–0.25

Mechanical Properties of EN 10296-2 1.4547

Table mechanical floors for 1.4547 / X1CrNiMoCuN20-18-7 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 300 MPa, Rp1.0 min 340 MPa, Rm min 650 MPa, longitudinal elongation min 35%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Caution thread: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 300 340 650 min 35 30 Yes

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4547 / X1CrNiMoCuN20-18-7. Guideline solution/anneal band (Annex B): 1180–1200 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4547

EN 10296-2 does not offer a seamless route for 1.4547. Tube in X1CrNiMoCuN20-18-7 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. For 1.4547, SHH STEEL aligns the Annex A symbol to the duty: W0 for as-welded economy, W1A/W2A for descaled engineering tube, W2R/WCR for brighter OD, and WG/WP when a measured roughness target is part of the order text. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product.

For austenitic 1.4547, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4547 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1180–1200 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Caution thread: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier.

State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4547. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Caution thread: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier.

Dimensions and Tolerances for EN 10296-2 1.4547

Order EN 10296-2 1.4547 by outside diameter D and wall thickness T for steel name X1CrNiMoCuN20-18-7. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Process and seawater-service welded od, typically +at on w2a/wca routes. Duty thread: 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service.

Length supply for 1.4547 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Duty thread: 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service.

Equivalent Grades for EN 10296-2 1.4547

Equivalence talk for 1.4547 starts with X1CrNiMoCuN20-18-7: that is the EN steel name for welded general-purpose tube under this Part 2. Buyers who only write 254 SMO / 6Mo still need the steel number and EN 10296-2 on the PO. Sister grades often quoted alongside this duty: 1.4539, 1.4439, 1.4410. Design caution stays: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier Family filing for 1.4547 is austenitic corrosion-resisting.

Heat Treatment and Delivery Condition for EN 10296-2 1.4547

Austenitic 1.4547 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1180–1200 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Delivery framing on the certificate for 1.4547 should match the ordered +AR/+A/+AT symbol — alias 254 SMO / 6Mo alone is not enough. Caution thread: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier.

Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4547, restore the delivery condition agreed on the order before corrosive or load-bearing service. Caution thread: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier.

Corrosion Resistance of EN 10296-2 1.4547

For 1.4547 / X1CrNiMoCuN20-18-7, read corrosion through the austenitic corrosion-resisting lens rather than a generic “stainless” slogan. Plain-language summary: 6% Mo plus nitrogen and copper for severe seawater and halide pitting/crevice resistance. IGC Options follow EN ISO 3651-2 where the tables say Yes — and still do not replace medium-specific design. Caution: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier Filler/shop note for 1.4547: 6Mo/over-alloyed nickel-base fillers as WPS demands; strict heat input and purge; no carbon-steel tooling contamination.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4547 is filed as austenitic corrosion-resisting — pick tests that match that filing. Size context for 1.4547: process and seawater-service welded OD, typically +AT on W2A/WCA routes.

Applications of EN 10296-2 1.4547 Tube

Typical field use for 254 SMO / 6Mo-named welded tube under steel number 1.4547: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product. Keep pressure seamless talk on EN 10216-5 pages when that standard is the regulatory home. Primary application sketch: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product.

Skip 1.4547 when the specification locks a different family — for example forcing ferritic 1.4547 into severe chloride process duty, or forcing a heat-resisting number into aqueous chloride service. Sister conversation inside EN 10296-2: 1.4539, 1.4439, 1.4410. Weld thread: 6Mo/over-alloyed nickel-base fillers as WPS demands; strict heat input and purge; no carbon-steel tooling contamination.

Weldability of EN 10296-2 1.4547

Weldability of EN 10296-2 1.4547 covers both the mill longitudinal seam and downstream fabricator joints. Practical shop note: 6Mo/over-alloyed nickel-base fillers as WPS demands; strict heat input and purge; no carbon-steel tooling contamination. Caution that shapes WPS choices: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier Family filing for 1.4547 is austenitic corrosion-resisting.

Filler selection should match or over-alloy the base X1CrNiMoCuN20-18-7 chemistry as the WPS demands. Heat input, interpass temperature, and shielding practice follow the family — austenitic, ferritic, duplex, or heat-resisting — not a single shop habit. Duty thread: 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service.

Surface Finishes for EN 10296-2 1.4547

For 1.4547, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Duty thread: 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service.

Special measures to protect 1.4547 / X1CrNiMoCuN20-18-7 during delivery or storage may be agreed at enquiry. Bright and polished tubes take sleeve or paper wrap; descaled engineering finishes still need end caps and dry bundling so chloride-bearing dirt does not sit on the OD in transit — especially important for 254 SMO / 6Mo-family decorative or hygienic OD. Caution thread: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier.

Inspection and Testing for EN 10296-2 1.4547

SHH STEEL EN 10204 3.1 documents for 1.4547 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a leak-test or NDT line unless that Option was executed. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product.

IGC testing for 1.4547, when required, follows EN ISO 3651-2 as referenced by the grade tables. Hardness, flattening, drift expanding, or bend tests are applied when the order invokes them. Marking typically includes manufacturer identity, dimensions, EN 10296-2, steel name or number 1.4547, cast/code, delivery-condition symbol, and inspection correlation — not a bare 254 SMO / 6Mo stencil alone. Duty thread: 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service.

Packaging and Shipping for EN 10296-2 1.4547

Finished EN 10296-2 1.4547 (X1CrNiMoCuN20-18-7) welded tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (W*R/WCR/WG/WP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Size context for 1.4547: process and seawater-service welded OD, typically +AT on W2A/WCA routes.

When cut lengths and special ends are part of the 1.4547 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product.

Ocean-freight wrap for X1CrNiMoCuN20-18-7 repeats cast/code on tags inside and outside the wrap. Duty thread for why identity matters: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product. Family filing for 1.4547 is austenitic corrosion-resisting.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10296-2 1.4547 as welded general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “254 SMO / 6Mo tube” label on whatever is in the rack. We keep pressure talk honest: when PED welded pressure acceptance is required, we point you to EN 10217-7 for the same chemistry family where it exists. Weld thread: 6Mo/over-alloyed nickel-base fillers as WPS demands; strict heat input and purge; no carbon-steel tooling contamination.

SHH STEEL will not stretch X1CrNiMoCuN20-18-7 into a medium it cannot defend. Typical right-fit duties: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product. When those duties slip toward a sister, we say so before the quote hardens. Family filing for 1.4547 is austenitic corrosion-resisting.

Supply Capability

SHH STEEL can produce and supply EN 10296-2 1.4547 welded stainless steel tube against the edition, delivery condition, Annex A symbol, and Options named on your enquiry. The capability table and Stock / Available sizes enquiry map below frame a first-pass size list for X1CrNiMoCuN20-18-7 — role: 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service. Primary application sketch: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4547 / X1CrNiMoCuN20-18-7
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

Stock / Available sizes for 1.4547 means RFQ bands, not published tonnages. Typical conversation starts around commodity-to-process welded OD with walls suited to austenitic corrosion-resisting practice. Alias on emails may still say 254 SMO / 6Mo; the acknowledgement must say 1.4547. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product.

Cut lengths, special ends, IGC Options, and dual enquiries against 1.4539, 1.4439, 1.4410 on the same size list are routine for 1.4547. Peer mill catalogues only sanity-check typical OD × wall bands — acceptance remains EN 10296-2 with dimensional agreements stated on the order. SHH STEEL can produce and supply trial lengths before a production heat when the project schedule allows. Corrosion thread: 6% Mo plus nitrogen and copper for severe seawater and halide pitting/crevice resistance.

FAQ

What is EN 10296-2 1.4547 welded stainless steel tube used for?
EN 10296-2 1.4547 (X1CrNiMoCuN20-18-7) is welded tube for mechanical and general engineering — seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties naming 6Mo welded product. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service.
Is EN 10296-2 1.4547 the same as EN 10216-5 1.4547?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4547 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4547 / X1CrNiMoCuN20-18-7?
Delivery framing for 1.4547 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1180–1200 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4547?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4547 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4547 compare with sister grades 1.4539, 1.4439, 1.4410?
1.4547 / X1CrNiMoCuN20-18-7 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4539, 1.4439, 1.4410. Design caution: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4547 tube on site?
1.4547 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 6Mo/over-alloyed nickel-base fillers as WPS demands; strict heat input and purge; no carbon-steel tooling contamination. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4547?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4547?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4547 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: process and seawater-service welded OD, typically +AT on W2A/WCA routes. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 254 SMO / 6Mo belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 254 SMO / 6Mo in body text and BOM notes, but lock EN 10296-2 and 1.4547 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4547?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: premium alloy — confirm whether superduplex 1.4410 is the strength-efficient alternative for the same chloride dossier Sister pointers: 1.4539, 1.4439, 1.4410. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4547 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4547 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4547 (X1CrNiMoCuN20-18-7) is welded stainless tube for mechanical and general engineering — 6Mo superaustenitic welded tube (254 SMO-class) for severe seawater and halide mechanical service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4539, 1.4439, 1.4410. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X